CN202865357U - 一种电积、电解的阴极 - Google Patents
一种电积、电解的阴极 Download PDFInfo
- Publication number
- CN202865357U CN202865357U CN 201220401866 CN201220401866U CN202865357U CN 202865357 U CN202865357 U CN 202865357U CN 201220401866 CN201220401866 CN 201220401866 CN 201220401866 U CN201220401866 U CN 201220401866U CN 202865357 U CN202865357 U CN 202865357U
- Authority
- CN
- China
- Prior art keywords
- electrodeposition
- electrolysis
- cathode
- cathode plate
- conducting rod
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
本实用新型涉及一种电积、电解的阴极,主要包括阴极板和导电棒,阴极板和导电棒以焊接方式固定连接;导电棒两端用不锈钢板焊接封堵;导电棒两侧底部露出实心铜棒;在阴极板底部延长度方向带有V型沟槽;导电棒底部表面为圆弧形面;阴极板材质为不锈钢,V型沟槽的长度为阴极板宽度的五分之四,呈中心对称;V型沟槽的两侧端部保证有0.1至0.15mm的厚度。本实用新型的有益效果为:有效降低了电积、电解工艺过程中,阴极板的机械损伤、提高剥离效率;延长阴极板的修复周期从而降低生产成本。
Description
技术领域
本实用新型涉及电积、电解工艺技术领域,涉及铜、镍、锰、铅、金、银及其它电积、电解精炼工艺中的种板阴极和永久阴极电积、电解精炼工艺中的阴极,主要是一种电积、电解的阴极。
背景技术
随着国家着力调整产业结构使之向着产业结构合理化和高级化两个方面发展,使有色金属冶炼行业的发展向大规模、高产能、高自动化程度趋势发展。另一方面随着我国资源进一步匮乏,中国企业急需走出国门寻找资源。主要资源开采地为亚洲和非洲国家。面对海外市场的当地人才稀缺,高昂的人工费用,为了更快的实现盈利,多数企业都会选择自动化程度高、使用寿命长的设备来解决问题。一般永久法电解都会配备剥片机组、自动天车。在实际生产过程中,阴极板的本身寿命可达15年以上。但是随着自动化程度的提高,阴极板在剥片机组、天车、槽面上的吊装等工艺环节中受到的机械磨损和碰撞的频率也大大提高。也因为机械损伤使阴极板的报废率和维修率大幅提高。主要体现在:导电棒的磨损和导电棒遭受撞击后的破损;底部V型槽的磨损和撞击破损。
发明内容
本实用新型的目的在于克服上述存在的不足,而提供一种提高了耐机械磨损和质量稳定的电积、电解的阴极。
本实用新型的目的是通过如下技术方案来完成的,它主要包括阴极板和导电棒,阴极板和导电棒以焊接方式固定连接;导电棒两端用不锈钢板焊接封堵;导电棒两侧底部露出实心铜棒,实心铜棒露出部分呈圆弧面;在阴极板底部延长度方向带有V型沟槽。
作为优选,所述的导电棒外表面不锈钢层与里面实心铜棒通过热胀冷缩原理成型;确保不锈钢层与实心铜棒为过盈配合。
作为优选,所述的阴极板的材质为不锈钢;V型沟槽的长度为阴极板宽度的五分之四,呈中心对称;V型沟槽的两侧端部保证有0.1至0.15mm的厚度。
本实用新型的有益效果为:有效降低了电积、电解工艺过程中,阴极板的机械损伤、提高剥离效率;延长阴极板的修复周期从而降低生产成本。
附图说明
图1是本实用新型的结构示意图。
图2是本实用新型A-A剖视结构示意图。
图3是本实用新型B-B剖视结构示意图。
附图中的标号分别为:1、阴极板,2、导电棒,3、不锈钢层,4、实心铜棒,5、不锈钢板,6、V型沟槽。
具体实施方式
下面将结合附图对本实用新型做详细的介绍:如附图1至3所示,本实用新型主要包括阴极板1和导电棒2,阴极板1和导电棒2以焊接方式固定连接;导电棒2两端用不锈钢板5焊接封堵;导电棒2两侧底部露出实心铜棒4;在阴极板1底部延长度方向带有V型沟槽6。所述的实心铜棒4露出部分呈圆弧面。所述的导电棒2外表面不锈钢层3与里面实心铜棒4通过热胀冷缩原理成型;确保不锈钢层3与实心铜棒4为过盈配合。所述的阴极板1的材质为不锈钢;V型沟槽6的长度为阴极板1宽度的五分之四,呈中心对称;V型沟槽6的两侧端部保证有0.1至0.15mm的厚度。
除上述实施例外,凡采用等同替换或等效变换形成的技术方案,均落在本实用新型要求的保护范围。
Claims (2)
1.一种电积、电解的阴极,主要包括阴极板(1)和导电棒(2),其特征在于:阴极板(1)和导电棒(2)以焊接方式固定连接;导电棒(2)两端用不锈钢板(5)焊接封堵;导电棒(2)两侧底部露出实心铜棒(4),实心铜棒(4)露出部分呈圆弧面;在阴极板(1)底部延长度方向带有V型沟槽(6),所述的导电棒(2)外表面的不锈钢层(3)与里面的实心铜棒(4)为过盈配合连接。
2.根据权利要求1所述的电积、电解的阴极,其特征在于:所述的阴极板(1)的材质为不锈钢;V型沟槽(6)的长度为阴极板(1)宽度的五分之四,呈中心对称;V型沟槽(6)的两侧端部保证有0.1至0.15mm的厚度。