CN104018192A - 一种有色金属冶炼的高电效阴极板 - Google Patents

一种有色金属冶炼的高电效阴极板 Download PDF

Info

Publication number
CN104018192A
CN104018192A CN201410223473.8A CN201410223473A CN104018192A CN 104018192 A CN104018192 A CN 104018192A CN 201410223473 A CN201410223473 A CN 201410223473A CN 104018192 A CN104018192 A CN 104018192A
Authority
CN
China
Prior art keywords
layer
conducting rod
negative plate
current conducting
protection layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410223473.8A
Other languages
English (en)
Inventor
吴用
吴俊义
李至青
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sanmen Sanyou Metallurgy & Chemical Technologies Co Ltd
Original Assignee
Sanmen Sanyou Metallurgy & Chemical Technologies Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sanmen Sanyou Metallurgy & Chemical Technologies Co Ltd filed Critical Sanmen Sanyou Metallurgy & Chemical Technologies Co Ltd
Priority to CN201410223473.8A priority Critical patent/CN104018192A/zh
Publication of CN104018192A publication Critical patent/CN104018192A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种有色金属冶炼的高电效阴极板,主要包括阴极极板和导电棒,阴极极板和导电棒通过焊接固定连接,导电棒采用三层大U字型结构,第一层为固定梁,第二层为不锈钢保护层,第三层为实心铜层,在导电棒的上端设置有吊装窗口;固定梁与不锈钢保护层通过焊接固定连接,实心铜层过盈配合设置在不锈钢保护层内部,并在导电棒两端底部露出形成悬挂接触点。不锈钢保护层与实心铜层通过热涨冷缩原理成型,确保不锈钢保护层与实心铜层为过盈配合。本发明的有益效果为:提高阴极板的导电性能,使阴极板面更加完整,从而达到降低生产成本,提高产能。

Description

一种有色金属冶炼的高电效阴极板
技术领域
本发明属于有色金属电解、电积精炼领域,尤其涉及一种有色金属冶炼的高电效阴极板。
背景技术
目前,在有色金属电解,电积精炼工艺中,其阴极一般采用一字型导电棒,由于一字型导电棒距离槽液面较远,导电距离与导电面积相对增加,电流在传导过程中损耗较大,且其在阴极板面上直接冲击缺口充当吊装工位的做法破坏了阴极的完整性,使阴极存在缺陷。
发明内容
本发明的目的在于克服现有技术存在的不足,而提供一种有色金属冶炼的高电效阴极板,使导电面积减少,导电率提高,使阴极板面更加完整的阴极结构。
本发明的目的是通过如下技术方案来完成的。这种有色金属冶炼的高电效阴极板,主要包括阴极极板和导电棒,阴极极板和导电棒通过焊接固定连接,导电棒采用三层大U字型结构,第一层为固定梁,第二层为不锈钢保护层,第三层为实心铜层,在导电棒的上端设置有吊装窗口;固定梁与不锈钢保护层通过焊接固定连接,实心铜层过盈配合设置在不锈钢保护层内部,并在导电棒两端底部露出形成悬挂接触点。不锈钢保护层与实心铜层通过热涨冷缩原理成型,确保不锈钢保护层与实心铜层为过盈配合。
所述的悬挂接触点的底面与阴极极板高度差为60CM,导电棒两端超出阴极极板边缘的悬挂部分与中间的不锈钢结合部分采用圆弧过渡,圆角半径大于80mm。
本发明的有益效果为:提高阴极板的导电性能,使阴极板面更加完整,从而达到降低生产成本,提高产能。
附图说明
图1是本发明的结构示意图;
图2是本发明的新型导电棒结构示意图。
图3是本发明的新型B处的放大示意图。
附图中的标号分别为:阴极极板1,导电棒2,吊装窗口3,固定梁4,不锈钢保护层5,实心铜层6,悬挂接触点7。
具体实施方式
下面将结合附图对本发明做详细的介绍:
如图所示,这种有色金属冶炼的高电效阴极板,主要包括阴极极板1和导电棒2,阴极极板1和导电棒2通过焊接固定连接,导电棒2采用三层大U字型结构,第一层为固定梁4,第二层为不锈钢保护层5,第三层为实心铜层6;在导电棒2的上端设置有吊装窗口3。固定梁4与不锈钢保护层5通过焊接固定连接,实心铜层6过盈配合设置在不锈钢保护层5内部,并在导电棒2两端底部露出形成悬挂接触点7。不锈钢保护层与实心铜层通过热涨冷缩原理成型,确保不锈钢保护层与实心铜层为过盈配合。所述的悬挂接触点7的底面与阴极极板1高度差(P处)为60CM,导电棒2两端超出阴极极板1边缘的悬挂部分与中间的不锈钢结合部分采用圆弧过渡,圆角半径大于80mm。
本发明采用不锈钢保护层与铜导电棒紧密结合,导电率好,防腐蚀性能好,导电棒两侧底部露出实心铜层形成悬挂接触点7,不锈钢主板焊接固定在不锈钢保护层上,接触电阻小,电流效率高。
本发明不局限于上述实施方式,不论在其形状或材料构成上作任何变化,凡是采用本发明所提供的结构设计,都是本发明的一种变形,均应认为在本发明保护范围之内。

Claims (2)

1.一种有色金属冶炼的高电效阴极板,主要包括阴极极板(1)和导电棒(2),其特征在于:阴极极板(1)和导电棒(2)通过焊接固定连接,导电棒(2)采用三层大U字型结构,第一层为固定梁(4),第二层为不锈钢保护层(5),第三层为实心铜层(6),在导电棒(2)的上端设置有吊装窗口(3);固定梁(4)与不锈钢保护层(5)通过焊接固定连接,实心铜层(6)过盈配合设置在不锈钢保护层(5)内部,并在导电棒(2)两端底部露出形成悬挂接触点(7)。
2.根据权利要求1所述的有色金属冶炼的高电效阴极板,其特征在于:所述的悬挂接触点(7)的底面与阴极极板(1)高度差为60CM,导电棒(2)两端超出阴极极板(1)边缘的悬挂部分与中间的不锈钢结合部分采用圆弧过渡,圆角半径大于80mm。
CN201410223473.8A 2014-05-23 2014-05-23 一种有色金属冶炼的高电效阴极板 Pending CN104018192A (zh)