CN202799387U - 一种保持pcb表面平整度一致的结构 - Google Patents
一种保持pcb表面平整度一致的结构 Download PDFInfo
- Publication number
- CN202799387U CN202799387U CN 201220522073 CN201220522073U CN202799387U CN 202799387 U CN202799387 U CN 202799387U CN 201220522073 CN201220522073 CN 201220522073 CN 201220522073 U CN201220522073 U CN 201220522073U CN 202799387 U CN202799387 U CN 202799387U
- Authority
- CN
- China
- Prior art keywords
- solder mask
- lower solder
- pcb
- copper foil
- planeness
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
本实用新型公开了一种保持PCB表面平整度一致的结构,包括基材,所述基材表面贴设有相连接的铜箔层和下阻焊层,铜箔层上表面贴设有上阻焊层,上阻焊层和下阻焊层间具有高度差,下阻焊层上表面丝印有油墨层。本实用新型表面平整度一致,与结构件安装时能实现无缝贴合,不会影响产品的轻薄性。
Description
技术领域
本实用新型涉及一种PCB板,具体地说是一种主要应用在电子数码产品内的PCB板结构。
背景技术
随着电子产品的迅速发展,目前的电子数码产品,如手机、平板电脑等都向轻薄化的方向发展。由于产品的轻薄化要求,对产品内部各结构部件之间贴合的精密度要求越来越高。在产品内安装PCB板时,经常会出现PCB板表面平整度不一致的问题,如射频模块的天线净空区域,如附图1所示,需要将PCB板上的局部铜箔层挖掉,使PCB板表面不平整,造成PCB板表面不平整具有高度差。当有结构件与PCB板表面进行贴合时,由于高度差的存在,结构件的贴合面与PCB表面之间会存在缝隙,贴合后会使结构件失去平衡,影响产品的稳定性。对产品的设计带来较大影响。
发明内容
本实用新型要解决的技术问题是提供一种表面平整度一致,能够无缝贴合安装的主要保持PCB表面平整度一致的结构。
为了解决上述技术问题,本实用新型采取以下技术方案:
一种保持PCB表面平整度一致的结构,包括基材,所述基材表面贴设有相连接的铜箔层和下阻焊层,铜箔层上表面贴设有上阻焊层,上阻焊层和下阻焊层间具有高度差,下阻焊层上表面丝印有油墨层。
所述油墨层的厚度等于上阻焊层和下阻焊层间的高度差。
作为对上述方案的改进,所述上阻焊层和下阻焊层为一体结构。
本实用新型产品与传统的相比,不具有挖空区域,表面的平整度一致,与结构件贴合安装时能实现无缝贴合,保证整个产品的薄度,使产品内部各部件紧凑贴合固定,利于产品设计的实现。
附图说明
附图1为现有技术产品的局部剖面结构示意图;
附图2为本实用新型的局部剖面结构示意图。
具体实施方式
为了便于本领域技术人员的理解,下面结合附图对本实用新型作进一步的描述。
如附图2所示,本实用新型揭示了一种主要应用在电子数码产品上的PCB板,包括基材1,该基材1表面贴设有铜箔层2和下阻焊层4,该铜箔层2和下阻焊层4相连接,铜箔层2上表面贴设有上阻焊层3,上阻焊层3和下阻焊层4间具有高度差,下阻焊层4上表面丝印有油墨层5。铜箔层2和下阻焊层4一起贴满基材1上表面,铜箔层2的厚度和下阻焊层4的厚度可设为一样。油墨层4的厚度与上阻焊层3和下阻焊层4间的高度差相等,保证油墨层上表面和上阻焊层的上表面水平一致,使整个产品表面的平整度保持一致。
另外,上阻焊层和下阻焊层为一体成型结构,便于加工制造。
本实用新型通过在PCB板表面天线净空区域设置油墨层,利用该油墨层填补原先PCB板上的高度差,使整个产品表面的平整度保持一致,与结构件相安装时,能够实现无缝贴合,保证各配件的稳定性,使各部件紧凑贴合固定,便于产品设计的实现。
Claims (3)
1.一种保持PCB表面平整度一致的结构,包括基材(1),其特征在于:所述基材表面贴设有相连接的铜箔层(2)和下阻焊层(4),铜箔层上表面贴设有上阻焊层(3),上阻焊层和下阻焊层间具有高度差,下阻焊层上表面丝印有油墨层(5)。
2.根据权利要求1所述的保持PCB表面平整度一致的结构,其特征在于:所述油墨层的厚度等于上阻焊层和下阻焊层间的高度差。
3.根据权利要求1或2所述的保持PCB表面平整度一致的结构,其特征在于:所述上阻焊层和下阻焊层为一体结构。