China
Prior art keywords
layer
stones
brick
working lining
laying bricks
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN 201220336339
Other languages
English (en)
Inventor
齐春富
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Qi Chunfu
Original Assignee
QIQIHAR BEIGONG METALLURGY EQUIPMENT MANUFACTURING PLANT
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by QIQIHAR BEIGONG METALLURGY EQUIPMENT MANUFACTURING PLANT filed Critical QIQIHAR BEIGONG METALLURGY EQUIPMENT MANUFACTURING PLANT
Priority to CN 201220336339 priority Critical patent/CN202639316U/zh
Application granted granted Critical
Publication of CN202639316U publication Critical patent/CN202639316U/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Images

Abstract

本实用新型的精炼包工作层砌筑锁砖装置属于无机非金属材料的砌筑装置,是由壳体、隔热板、浇注料永久层和工作层构成,其从外至内依次为由壳体、隔热板、浇注料永久层和工作层,工作层上的锁砖的长度小于工作层,在工作层和浇注料永久层之间设有镁碳砖砌筑永久层。镁碳砖砌筑永久层是由电熔镁砂和鳞片石墨制成的镁碳砖砌筑成的永久层。本实用新型精炼包工作层砌筑锁砖方式的改进,解决钢包每一工作层锁砖合理锁紧的问题,同而提高钢包工作层的使用寿命,从而保证工作层砖的极限使用寿命。

Description

精炼包工作层砌筑锁砖装置
技术领域
本实用新型属于无机非金属材料的砌筑装置,尤其涉及一种精炼包工作层砌筑锁砖装置。
现有技术
目前冶金钢包工作层砌筑是根据钢包直径的大小每环留有二道以上锁砖合紧。一种砌筑方式是工作层与永久层之间不靠紧,留有30-40mm的间隙,锁砖处用一块或两块砖退入10-30mm,每一环砌筑完后,将锁砖拉回与砖面平整,如图2所示,图中1是壳体、2是隔热板、3是浇注料永久层、4是调整砂缝、5是工作层、6是锁钻。另一种砌筑方式是工作层与永久层之间靠紧,而锁砖无处可退,只好将锁砖反插打紧,如图3所示,图中1是壳体、2是隔热板、3是浇注料永久层、5是工作层、6是锁钻。这两种锁砖方式都不能满足要求。第一种砌筑方式,由于留有30-40mm的砂缝间隙,无论怎样锁紧,钢包使用过程中在热应力的作用下,永久层与工作层之间的间隙都会动,从而容易导致工作层出现立缝或环缝,钢包无法使用。第二种砌筑方式,由于锁砖是倒插,钢包使用过程中需要多次放倒和难免受外力的撞击,从而容易导致锁砖脱出,钢包无法使用。
发明内容
本实用新型旨在针对背景技术中存在的不足,而提出的一种精炼包工作层砌筑锁砖装置。   
本实用新型的精炼包工作层砌筑锁砖装置,是由壳体、隔热板、浇注料永久层和工作层构成,其从外至内依次为由壳体、隔热板、浇注料永久层和工作层,工作层上的锁砖的长度小于工作层,在工作层和浇注料永久层之间设有镁碳砖砌筑永久层。
作为本实用新型的进一步改进,镁碳砖砌筑永久层是由电熔镁砂和鳞片石墨制成的镁碳砖砌筑成的永久层。
作为本实用新型的进一步改进,工作层与镁碳砖砌筑永久层靠紧。
作为本实用新型的进一步改进,锁砖与镁碳砖砌筑永久层之间填充耐火材料。
本实用新型精炼包工作层砌筑锁砖方式的改进,解决钢包每一工作层锁砖合理锁紧的问题,同而提高钢包工作层的使用寿命,从而保证工作层砖的极限使用寿命。即传统工艺中由于留有30-40mm的砂缝间隙,无论怎样锁紧,钢包使用过程中在热应力的作用下,永久层与工作层之间的间隙都会动,从而容易导致工作层出现立缝或环缝,钢包无法使用的问题,和由于锁砖是倒插,钢包使用过程中需要多次放倒和难免受外力的撞击,从而容易导致锁砖脱出,钢包无法使用的技术难题,通过应用使钢包寿命直线上升,使精炼包使用寿命提高了百分之三十以上,效果非常良好。
附图说明
图1为本实用新型的结构示意图;
图2、图3为现有精炼包工作层砌筑锁砖装置的结构示意图。
具体实施方式
下面结合图1对本实用新型精炼包工作层砌筑锁砖装置做进一步说明:
本实用新型的精炼包工作层砌筑锁砖装置,其从外至内依次为由壳体1、隔热板2、浇注料永久层3工作层5构成,工作层5上的锁砖6的长度小于工作层5,锁砖6与镁碳砖砌筑永久层4之间填充耐火材料7。在工作层5和浇注料永久层3之间设有镁碳砖砌筑永久层4。镁碳砖砌筑永久层4是由电熔镁砂和鳞片石墨制成的镁碳砖砌筑成的永久层。工作层5与镁碳砖砌筑永久层4靠紧。
采用工作层5与镁碳砖砌筑永久层4之间靠紧的砌筑方式,镁碳砖砌筑永久层用的是电熔镁砂和鳞片石墨制成的镁碳砖砌筑。充分计算好工作层5砖的所需长度,与其配套制成相应的锁砖6,即锁砖6比工作层5砖短。根据钢包直径大小,予留出相应的锁砖6道数,砌筑到锁砖6时将锁砖6退回,每一环砌筑完了将锁砖6用专用工具拉回与砖面一平,拉回后工作层工作层5与镁碳砖砌筑永久层4之间的间隙用自制的耐火材料填充捣实。

Claims (4)

1.精炼包工作层砌筑锁砖装置,是由壳体(1)、隔热板(2)、浇注料永久层(3)和工作层(5)构成,其从外至内依次为由壳体(1)、隔热板(2)、浇注料永久层(3)和工作层(5),其特征在于工作层(5)上的锁砖(6)的长度小于工作层(5),在工作层(5)和浇注料永久层(3)之间设有镁碳砖砌筑永久层(4)。
2.如权利要求1所述的精炼包工作层砌筑锁砖装置,其特征在于镁碳砖砌筑永久层(4)是由电熔镁砂和鳞片石墨制成的镁碳砖砌筑成的永久层。
3.如权利要求1所述的精炼包工作层砌筑锁砖装置,其特征在于工作层(5)与镁碳砖砌筑永久层(4)靠紧。
4.如权利要求1所述的精炼包工作层砌筑锁砖装置,其特征在于锁砖(6)与镁碳砖砌筑永久层(4)之间填充耐火材料(7)。
CN 201220336339 2012-07-12 2012-07-12 精炼包工作层砌筑锁砖装置 Expired - Lifetime CN202639316U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201220336339 CN202639316U (zh) 2012-07-12 2012-07-12 精炼包工作层砌筑锁砖装置

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201220336339 CN202639316U (zh) 2012-07-12 2012-07-12 精炼包工作层砌筑锁砖装置

Publications (1)

Publication Number Publication Date
CN202639316U true CN202639316U (zh) 2013-01-02

Family

ID=47408494

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201220336339 Expired - Lifetime CN202639316U (zh) 2012-07-12 2012-07-12 精炼包工作层砌筑锁砖装置

Country Status (1)

Country Link
CN (1) CN202639316U (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105081300A (zh) * 2015-08-03 2015-11-25 丹东播磨耐火材料有限公司 钢包复合砌筑技术
CN114643351A (zh) * 2022-05-19 2022-06-21 河北纵横集团丰南钢铁有限公司 一种耐候钢钢液的余渣清洁转运钢包

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105081300A (zh) * 2015-08-03 2015-11-25 丹东播磨耐火材料有限公司 钢包复合砌筑技术
CN114643351A (zh) * 2022-05-19 2022-06-21 河北纵横集团丰南钢铁有限公司 一种耐候钢钢液的余渣清洁转运钢包
CN114643351B (zh) * 2022-05-19 2022-07-22 河北纵横集团丰南钢铁有限公司 一种耐候钢钢液的余渣清洁转运钢包

Similar Documents

Publication Publication Date Title
CN104390461B (zh) 一种节能水泥回转窑内衬及其砌筑工艺
CN203956035U (zh) 浇注钒铁的锭模
CN105347824A (zh) 一种矿热炉整体筑炉专用冷捣糊的制备方法
CN106595314A (zh) 一种回转窑窑衬结构及砌筑方法
CN202639316U (zh) 精炼包工作层砌筑锁砖装置
CN202126183U (zh) 复合结构矿热炉炉衬
CN105523751A (zh) 一种水泥窑窑口用棕刚玉-氮化硅铁复合材料的制备方法
CN202621906U (zh) 一种铁水罐
CN202329164U (zh) 一种还原性矿热电炉内衬结构
CN203076574U (zh) 一种钢水包浇注渣线衬层
CN202461500U (zh) 精炼炉钢包高效保温结构
CN104529485A (zh) 双层复合耐火材料及双层复合耐火材料沟罩与其制造方法和应用
CN103433472A (zh) 扩容钢包
CN204214268U (zh) 大型矿热炉防漂炭键炉底
CN101392991B (zh) 一种精炼炉炉底的砌筑方法
CN203203398U (zh) 一种低导热复合砖
CN207095298U (zh) 一种耐火材料内衬结构
CN207091448U (zh) 一种复合型浇注料的出铁沟沟盖内衬
CN203764968U (zh) 一种用于精炼钢包渣线的预制件
CN204881189U (zh) 一种镍铁电炉用高导抗侵蚀炉衬结构
CN205732944U (zh) 一种连铸中间包用镁碳砖抗冲击板预制件
CN204665905U (zh) 一种新型白刚玉冶炼炉
CN203731863U (zh) 一种机压烧成砖砌筑的中频感应炉炉衬及感应炉
CN202499880U (zh) 一种转炉的炉口
CN214950619U (zh) 一种81000kva电石炉结构

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
ASS Succession or assignment of patent right

Owner name: QI CHUNFU

Free format text: FORMER OWNER: QIQIHAR BEIGONG METALLURG EQUIPMENT MANUFACTURING PLANT

Effective date: 20150819

C41 Transfer of patent application or patent right or utility model
TR01 Transfer of patent right

Effective date of registration: 20150819

Address after: Qigihar City, Heilongjiang province 161000 Ruby street Fulaerji District 7 Street District Qunying building

Patentee after: Qi Chunfu

Address before: 161042, 39 blocks, Fulaerji District, Heilongjiang, Qigihar

Patentee before: QIQIHAR BEIGONG METALLURG EQUIPMENT MFG PLANT

CX01 Expiry of patent term

Granted publication date: 20130102

CX01 Expiry of patent term