CN202428295U - 一种连铸结晶器铜板清扫工具 - Google Patents
一种连铸结晶器铜板清扫工具 Download PDFInfo
- Publication number
- CN202428295U CN202428295U CN2012200303176U CN201220030317U CN202428295U CN 202428295 U CN202428295 U CN 202428295U CN 2012200303176 U CN2012200303176 U CN 2012200303176U CN 201220030317 U CN201220030317 U CN 201220030317U CN 202428295 U CN202428295 U CN 202428295U
- Authority
- CN
- China
- Prior art keywords
- motor
- crystallizer
- copperplates
- control stick
- cleaning tool
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
本实用新型公开了一种连铸结晶器铜板清扫工具,其包括,操纵杆;电机或气动马达,设置于操纵杆前端,相应的电源线或压缩空气管沿操纵杆布置,电源控制开关或空气阀门设置于操纵杆上;两只砂轮,分别通过连接轴连接于电机或气动马达的输出轴两端。本实用新型可很快将结晶器铜板上的密封膏和氧化膜等附着物清理干净,清理简便、彻底,清理劳动强度低,确保结晶器传热均匀,防治裂纹的发生,对设备的使用寿命和铸坯表面质量的提高有很大的好处。
Description
技术领域
本实用新型涉及连铸设备,特别涉及一种连铸结晶器铜板清扫工具。
背景技术
连铸结晶器铜板主要用于连铸坯的初期凝固成形,是控制连铸坯表面质量、防止各种表面裂纹和生产事故的重要区域;为提高结晶器铜板表面的强度,一般铜板采用钴镍或铁镍镀层或熔射技术。因使用方法和环境原因,在使用一段时间后铜板表面会出现结垢现象(主要是密封膏残留物,在结晶器准备过程中需要在长边和短边铜板的夹角中涂上密封膏,用于防止开浇钢水溅入角部间隙并导致调宽时划伤铜板和发生漏钢事故)和表面氧化膜(高温和保护渣腐蚀作用导致)。铜板表面密封膏的残留物和长期使用后的表面氧化膜会影响结晶器铜板的传热效果,导致铸坯表面因冷却不均匀造成的纵裂和其它裂纹。故很多炼钢厂的铸机在浇注间隙时,用砂纸、油石等各种手段对结晶器铜板表面进行打磨维护,但这些现有的清理维护工具缺陷较多,存在清理劳动强度大、清理效果差或漏清面积多等缺陷。
发明内容
本实用新型的目的在于设计一种连铸结晶器铜板清扫工具,可以清理结晶器铜板表面残留的密封膏、氧化渣和氧化膜,提高浇注过程中结晶器铜板传热的均匀性,防止因传热问题造成的铸坯纵裂等表面缺陷的发生,防止调宽过程中角间隙增大,划伤铜板或嵌入冷钢后造成漏钢事故,同时使结晶器铜板的清理工作既简便,又快捷、到位。
为达到上述目的,本实用新型的技术方案是:
一种连铸结晶器铜板清扫工具,其包括,操纵杆;电机或气动马达,设置于操纵杆前端,相应的电源线或压缩空气管沿操纵杆布置,电源控制开关或空气阀门设置于操纵杆上;两只砂轮,分别通过连接轴连接于电机或气动马达的输出轴两端。
进一步,还包括用于调节两个砂轮之间距离的张紧弹簧箱,内设有张紧弹簧,该张紧弹簧套设于电机或气动马达的输出轴,所述的一侧砂轮连接一套管,该套管套设于所述的输出轴上,套管外壁设有压圈或压块,压圈或压块抵靠于张紧弹簧外端。
又,所述的操纵杆后端设手柄。
本实用新型的有益效果
使用本实用新型,可很快将结晶器铜板上的密封膏和氧化膜等附着物清理干净,清理简便、彻底,清理劳动强度低,结晶器铜板的清理可有效控制宽边铜板和窄边铜板角间隙并因此造成的铜板划伤,确保结晶器传热均匀,防治裂纹的发生,对结晶器的使用寿命和铸坯表面质量的提高有很大的好处。
附图说明
图1为本实用新型一实施例的正视图。
图2为图1的俯视图。
具体实施方式
参见图1、图2,本实用新型的一种连铸结晶器铜板清扫工具,其包括,操纵杆1;电机或气动马达2,设置于操纵杆1前端,相应的电源线或压缩空气管3沿操纵杆布置,电源控制开关或空气阀门4设置于操纵杆1上;两只砂轮5、5’,分别通过连接轴6、6’连接于电机或气动马达2的输出轴两端。
在本实施例中,本实用新型还包括用于调节两个砂轮5、5’之间距离的张紧弹簧箱7,内设有张紧弹簧71,该张紧弹簧71套设于电机或气动马达的输出轴即连接轴6,所述的一侧砂轮5连接一套管51,该套管51套设于所述的输出轴即连接轴6上,套管51外壁设有压圈或压块52,压圈或压块52抵靠于张紧弹簧71外端。
所述的操纵杆1后端设手柄8。
使用时,调节张紧弹簧箱的伸缩宽度,使两个砂轮之间的距离大于结晶器厚度尺寸2mm以上,将工具至于结晶器内,两个砂轮紧贴铜板,打开电源开关或空气阀门,带动马达旋转,操作人员用手柄和操作杆控制砂轮在结晶器内的走形、清洗。
Claims (3)
1.一种连铸结晶器铜板清扫工具,其特征在于,包括,
操纵杆;
电机或气动马达,设置于操纵杆前端,相应的电源线或压缩空气管沿操纵杆布置,电源控制开关或空气阀门设置于操纵杆上;
两只砂轮,分别通过连接轴连接于电机或气动马达的输出轴两端。
2.如权利要求1所述的连铸结晶器铜板清扫工具,其特征在于,还包括用于调节两个砂轮之间距离的张紧弹簧箱,内设有张紧弹簧,该张紧弹簧套设于电机或气动马达的输出轴,所述的一侧砂轮连接一套管,该套管套设于所述的输出轴上,套管外壁设有压圈或压块,压圈或压块抵靠于张紧弹簧外端。
3.如权利要求1所述的连铸结晶器铜板清扫工具,其特征在于,所述的操纵杆后端设手柄。