CN202349422U - 氩弧焊薄壁不锈钢管连接件 - Google Patents
氩弧焊薄壁不锈钢管连接件 Download PDFInfo
- Publication number
- CN202349422U CN202349422U CN2011205107948U CN201120510794U CN202349422U CN 202349422 U CN202349422 U CN 202349422U CN 2011205107948 U CN2011205107948 U CN 2011205107948U CN 201120510794 U CN201120510794 U CN 201120510794U CN 202349422 U CN202349422 U CN 202349422U
- Authority
- CN
- China
- Prior art keywords
- stainless steel
- argon arc
- welding
- pipe
- bell
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种氩弧焊薄壁不锈钢管连接件,包括本体,所述的本体设有两个以上的承插管,所述的承插管的入口内壁处设置有熔焊部。该氩弧焊薄壁不锈钢管连接件在实施氩弧焊焊接时,无需补充焊丝,焊接工序简单、效率较高、焊缝精细平滑、焊接成本低。
Description
技术领域
本实用新型属于不锈钢管材连接件技术领域,具体涉及一种承插式氩弧焊薄壁不锈钢管连接件。
背景技术
不锈钢管具有安全耐用、环保卫生、价格合理、美观豪华等优异的综合性能,目前已大量应用于建筑给水和直饮水管道。
与其他管材相比,不锈钢管的优点很多:一、抗拉强度高。一般的钢管抗拉强度约为300mpa,铜管的抗拉强度约为200mpa,而不锈钢管抗拉强度为钢管的2倍,为铜管的3倍。二、腐蚀性能好。管道漏水的原因,其最大的“杀手”就是氯离子,而在实践中304不锈钢能耐200ppm氯化物、316不锈钢能抵御1000ppm氯化物的天然水,这对大型的建筑尤为重要。从电势序列看,不锈钢和铸铁更不易起化学作用,在实际应用中,可与铜基合金接头(或铜制热水泵)组装,实用性强,效果好。不锈钢在引用水中具有更明显的耐腐蚀性,是因为其表面有一层致密的铬氧化保护膜,且一旦划纹时,在有空气存在的情况下能立即形成新的氧化保护膜;同时还由于它能承受高流速的冲击,因此能抵御流经管口、弯管、阀门和泵后涡流造成的腐蚀;导热系树小,保温性能好。四、环保。不锈钢管无毒、不积垢,能杜绝管路的二次污染;耐各种酸碱盐溶液;与其他管材相比,浸析到水中的重金属(Ni、Cr、Mo)量及少,浸析到纯净水中金属(Na、Fe、Ca)量最少;产品能100%回收。
薄壁不锈钢管于上世界90年代末才在国内市场上出现,由于薄壁不锈钢管的壁厚可以小到0.5mm,所以其连接方式以及连接效果对整个管道的影响很大。目前国内对薄壁不锈钢管采用的焊接方式多是承插式氩弧焊和对接式氩弧焊。
氩弧焊技术是在普通电弧焊的原理的基础上,利用氩气对金属焊材的保护,通过高电流使焊材在被焊基材上融化成液态形成溶池,使被焊金属和焊材达到冶金结合的一种焊接技术,由于在高温熔融焊接中不断送上氩气,使焊材不能和空气中的氧气接触,从而防止了焊材的氧化,因此可以焊接铜、铝、合金钢等有色金属。由于氩弧焊在焊接中能够形成1000多摄氏度的溶池,其结合力为冶金结合,焊接后结合的很牢固。但是目前的连接薄壁不锈钢管时的承插式氩弧焊焊接和对接式氩弧焊,均需要在管件的连接处补充不锈丝作为焊料,其缺点是:(1)焊接工序复杂,难度较高,对焊工的操作技能要求较高,效率较低,生产成本也因此提高,且焊缝难以做到精细平滑。(2)焊接电流较大,易造成焊接部位管壁熔透结瘤,在实际使用中,即阻滞了水的流速流量,又易使薄壁不锈钢管产生晶间腐蚀,缩短使用寿命。
发明内容
本实用新型的目的是提供一种在实施氩弧焊焊接时,无需补充焊丝,焊接工序简单、效率较高、焊缝精细平滑、焊接成本低的氩弧焊薄壁不锈钢管连接件。
本实用新型是通过如下技术方案来实现的:
氩弧焊薄壁不锈钢管连接件,包括本体,所述的本体设有两个以上的承插管,所述的承插管的入口内壁处设置有熔焊部。
所述的熔焊部涂覆在承插管入口内壁为圆筒结构,其筒高为承插管长度的四分之一至三分之一。
所述的熔焊部的筒壁厚度不大于1 mm。
所述的承插管为等径或变径管。
本实用新型具有积极的效果:本实用新型在实施氩弧焊焊接时,无需补充焊丝,只需先将被连接管件插入本实用新型中的承插口,然后进行焊接,所述熔焊部在高温下熔化,取代了传统氩弧焊焊接时所必须的焊丝,与传统氩弧焊焊接相比,具有焊接工序简单、效率较高、焊缝精细平滑的优点;无需使用焊丝,从而降低材料消耗,降低成本。
附图说明
图1是本实用新型的结构示意图。
图中序号:1、本体,2、承插管,3、熔焊部。
具体实施方式
下面结合附图和实施例进一步说明本实用新型:
参见图1,一种氩弧焊薄壁不锈钢管三通连接件,包括本体1,所述的本体1设有三个等径承插管2,所述的承插管2的入口内壁处设置有熔焊部3,所述的熔焊部3涂覆在承插管2入口内壁为圆筒结构,其筒高为承插管2长度的四分之一,所述的熔焊部3的筒壁厚度为0.5 mm。
实施例只是为了便于理解本实用新型的技术方案,并不构成对本实用新型保护范围的限制,本实用新型不仅仅局限于三通,还适用于四通、直通或弯头等连接件,即可用于连接等径的不锈钢管,也可用于连接变径的不锈钢管。凡是未脱离本实用新型技术方案的内容或依据本实用新型的技术实质对以上方案所作的任何简单修改、等同变化与修饰,均仍属于本实用新型保护范围之内。
Claims (5)
1.氩弧焊薄壁不锈钢管连接件,包括本体(1),所述的本体(1)设有两个以上的承插管(2),其特征在于:所述的承插管(2)的入口内壁处设置有熔焊部(3)。
2. 根据权利要求1所述的氩弧焊薄壁不锈钢管连接件,其特征在于:所述的熔焊部(3)涂覆在承插管(2)入口内壁为圆筒结构,其筒高为承插管(2)长度的四分之一至三分之一。
3.根据权利要求1或2所述的氩弧焊薄壁不锈钢管连接件,其特征在于:所述的熔焊部(3)的筒壁厚度不大于1 mm。
4.根据权利要求1或2所述的氩弧焊薄壁不锈钢管连接件,其特征在于:所述的承插管(2)为等径或变径管。
5.根据权利要求3所述的氩弧焊薄壁不锈钢管连接件,其特征在于:所述的承插管(2)为等径或变径管。