CN202317002U - 连铸用浸入式水口烘烤装置 - Google Patents

连铸用浸入式水口烘烤装置 Download PDF

Info

Publication number
CN202317002U
CN202317002U CN2011205085296U CN201120508529U CN202317002U CN 202317002 U CN202317002 U CN 202317002U CN 2011205085296 U CN2011205085296 U CN 2011205085296U CN 201120508529 U CN201120508529 U CN 201120508529U CN 202317002 U CN202317002 U CN 202317002U
Authority
CN
China
Prior art keywords
water gap
baking
continuous casting
baking device
upper cover
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011205085296U
Other languages
English (en)
Inventor
刘刚
吴静
何勇力
黄静
李国敏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuhan Iron and Steel Group Kunming Iron and Steel Co Ltd
Original Assignee
Wuhan Iron and Steel Group Kunming Iron and Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuhan Iron and Steel Group Kunming Iron and Steel Co Ltd filed Critical Wuhan Iron and Steel Group Kunming Iron and Steel Co Ltd
Priority to CN2011205085296U priority Critical patent/CN202317002U/zh
Application granted granted Critical
Publication of CN202317002U publication Critical patent/CN202317002U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型提供一种连铸用浸入式水口烘烤装置,其特征在于它包括其上设插孔的上盖体,以及其内设空腔、其底部设进气口的壳体,壳体空腔内设加热器。改变了现有技术因受热不合理,水口烘烤不均匀,而导致水口寿命较短的问题,同时在水口烘烤时,能方便地拿出和放入,避免了因拿放不便而损坏水口的问题。使用本浸入式水口烘烤装置,还可降低工人的操作难度,减轻劳动强度,保障安全生产。

Description

连铸用浸入式水口烘烤装置
技术领域
本实用新型提供一种烘烤装置,特别是一种连铸用浸入式水口烘烤装置,属于钢铁企业连铸设备技术领域。
背景技术
在对钢水进行浇注时,为了提高浇注效率,往往采用连铸机浇注的方式,这样能连续浇注多个钢坯。连铸浇注时,为了避免空气与钢水接触,防止钢水在浇注时产生二次氧化,需要使用浸入式水口作为浇注口。这样在浇注钢水前,就需要对浸入式水口进行烘烤预热,以防止浸入式水口因预热不良或者长时间低温预热,而导致强度降低,或者出现严重的氧化现象,甚至使浸入式水口在使用过程中发生炸裂。而现有的烘烤预热存在着受热不合理,烘烤不均匀等问题,且在烘烤时频繁地取出和放入浸入式水口,容易损坏水口,不仅影响生产效率,还存在安全隐患。因此有必要对现有烘烤技术加以改进。
发明内容
为解决现有浸入式水口在烘烤预热中,因受热不合理、烘烤不均匀而存在强度低、性能差等问题,本实用新型提供一种连铸用浸入式水口烘烤装置。
本实用新型通过下列技术方案完成:一种连铸用浸入式水口烘烤装置,其特征在于它包括其上设插孔的上盖体,以及其内设空腔、其底部设进气口的壳体,壳体空腔内设加热器,以便在上盖体和壳体之间形成一个加热室,使插入上盖体插孔内的浸入式水口置于加热室内,再通过加热器对浸入式水口进行均匀加热。
所述上盖体及壳体内壁均设有耐火保温材料层,以便形成均匀的热环境,避免发生受热不均匀的情况。
所述加热器设为其上开有多个通孔的环形管,该环形管通过进气管与外部供气装置相接,以便向环形管提供可燃气体,以向整个壳体空腔提供热能,便于浸入式水口的均匀加热。
本实用新型具有下列优点和效果:采用上述方案,改变了现有技术因受热不合理,水口烘烤不均匀,而导致水口寿命较短的问题,同时在水口烘烤时,能方便地拿出和放入,避免了因拿放不便而损坏水口的问题。使用本实用新型的浸入式水口烘烤装置,还可降低工人的操作难度,减轻劳动强度,保障安全生产。实为一理想的浸入式水口烘烤装置。
附图说明
图1为本实用新型之剖视图。
具体实施方式
下面结合附图对本实用新型作进一步描述。
如图1,本实用新型提供的连铸用浸入式水口烘烤装置,它包括其上设插孔4的上盖体3,以及其内设空腔2、其底部设进气口7的壳体1,壳体1空腔2内设加热器8,上盖体3及壳体1内壁均设有耐火保温材料层,加热器8设为其上开有多个通孔5的环形管,该环形管通过进气管6与外部供气装置相接。

Claims (3)

1.一种连铸用浸入式水口烘烤装置,其特征在于它包括其上设插孔的上盖体,以及其内设空腔、其底部设进气口的壳体,壳体空腔内设加热器。
2.根据权利要求1所述的连铸用浸入式水口烘烤装置,其特征在于所述上盖体及壳体内壁均设有耐火保温材料层。
3.根据权利要求1所述的连铸用浸入式水口烘烤装置,其特征在于所述加热器设为其上开有多个通孔的环形管,该环形管通过进气管与外部供气装置相接。
CN2011205085296U 2011-12-08 2011-12-08 连铸用浸入式水口烘烤装置 Expired - Fee Related CN202317002U (zh)