CN202247584U - 一种新型的沥青路面 - Google Patents

一种新型的沥青路面 Download PDF

Info

Publication number
CN202247584U
CN202247584U CN2011203132254U CN201120313225U CN202247584U CN 202247584 U CN202247584 U CN 202247584U CN 2011203132254 U CN2011203132254 U CN 2011203132254U CN 201120313225 U CN201120313225 U CN 201120313225U CN 202247584 U CN202247584 U CN 202247584U
Authority
CN
China
Prior art keywords
asphalt
layer
mastic
grain type
performance
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011203132254U
Other languages
English (en)
Inventor
关永胜
韩超
张志祥
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Transportation Research Institute Co Ltd
Original Assignee
Jiangsu Transportation Research Institute Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu Transportation Research Institute Co Ltd filed Critical Jiangsu Transportation Research Institute Co Ltd
Priority to CN2011203132254U priority Critical patent/CN202247584U/zh
Application granted granted Critical
Publication of CN202247584U publication Critical patent/CN202247584U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种新型的沥青路面,铺设于路的基层上,包括上细粒式沥青玛蹄脂碎石层,下细粒式沥青玛蹄脂碎石层、中粒式高性能沥青混凝土层以及粘结层,所述下细粒式沥青玛蹄脂碎石层设置于基层上,所述中粒式高性能沥青混凝土层设置于下细粒式沥青玛蹄脂碎石层上,所述上细粒式沥青玛蹄脂碎石层设置于所述中粒式高性能沥青混凝土层上,所述上细粒式沥青玛蹄脂碎石层、中粒式高性能沥青混凝土层、下细粒式沥青玛蹄脂碎石层之间以及基层各层之间均以粘结层连接。本实用新型提供的一种新型的沥青路面,采用了细粒式的沥青玛蹄脂碎石层,减薄了结构层厚度,节省了造价。本实用新型提供的一种新型的沥青路面经过试验证明,具有更好的抗裂性。

Description

一种新型的沥青路面
技术领域
本实用新型涉及一种新型的沥青路面。
背景技术
一般沥青路面面层结构由上、中、下三层组成,各结构层粒径大小从上到下分别由细至粗;粗粒式沥青混凝土层一般较厚,即使达到最小摊铺厚度要求,该结构层厚度一般达到18-20cm;另外,粗粒径的混凝土更容易发生离析,致使混凝土的质量更不容易得到保证。
发明内容
本发明目的在于提供一种新型的沥青路面,具体由以下技术方案实现:
一种新型的沥青路面,铺设于路的基层上,包括上细粒式沥青玛蹄脂碎石层,下细粒式沥青玛蹄脂碎石层、中粒式高性能沥青混凝土层以及粘结层,所述下细粒式沥青玛蹄脂碎石层设置于基层上,所述中粒式高性能沥青混凝土层设置于下细粒式沥青玛蹄脂碎石层上,所述上细粒式沥青玛蹄脂碎石层设置于所述中粒式高性能沥青混凝土层上,所述上细粒式沥青玛蹄脂碎石层与中粒式高性能沥青混凝土层之间、中粒式高性能沥青混凝土层与下细粒式沥青玛蹄脂碎石层之间、以及下细粒式沥青玛蹄脂碎石层与基层之间均以粘结层连接。
所述的一种新型的沥青路面,其进一步设计在于,所述两个细粒式沥青玛蹄脂碎石层厚度均为4cm,所述中粒式高性能沥青混凝土层厚度为6-8cm。
本实用新型提供的一种新型的沥青路面,采用了细粒式的沥青玛蹄脂碎石层,减薄了结构层厚度,节省了造价。本发明提供的一种新型的沥青路面经过试验证明,具有更好的抗裂性,降低了沥青路面发生车辙病害的风险。
附图说明
图1为本实用新型提供的沥青路面结构图。
图中,1-上细粒式沥青玛蹄脂碎石层,2-中粒式高性能沥青混凝土层,3-基层,4-粘结层,5-下细粒式沥青玛蹄脂碎石层。
具体实施方式
以下结合说明书附图及实施例对本实用新型作进一步说明:
本实用新型的沥青路面,包括上细粒式沥青玛蹄脂碎石层1,中粒式高性能沥青混凝土层2、下细粒式沥青玛蹄脂碎石层5、基层3以及粘结层4,如图1所示,下细粒式沥青玛蹄脂碎石层5设置于基层3上,中粒式高性能沥青混凝土层2设置于下细粒式沥青玛蹄脂碎石层5上,上细粒式沥青玛蹄脂碎石层1设置于中粒式高性能沥青混凝土层2上,上细粒式沥青玛蹄脂碎石层1与中粒式高性能沥青混凝土层2之间、中粒式高性能沥青混凝土层2与下细粒式沥青玛蹄脂碎石层之间5、以及下细粒式沥青玛蹄脂碎石层5与基层3之间均以粘结层4连接。上细粒式沥青玛蹄脂碎石层1和下细粒式沥青玛蹄脂碎石层5的厚度均为4cm,中粒式高性能沥青混凝土层2厚度为6-8cm。
本实用新型的采用了细粒式的沥青玛蹄脂碎石层替换原有的粗粒式高性能沥青混凝土层,既减薄了结构层厚度。而且采用更细粒径,使结构层厚度减薄4CM,节约了整体造价,经过工程实践证明,该结构抗裂性能较好,而且在一定程度上降低了沥青路面发生车辙缺陷的风险。

Claims (2)

1.一种沥青路面,铺设于路的基层上,其特征在于包括上细粒式沥青玛蹄脂碎石层,下细粒式沥青玛蹄脂碎石层、中粒式高性能沥青混凝土层以及粘结层,所述下细粒式沥青玛蹄脂碎石层设置于基层上,所述中粒式高性能沥青混凝土层设置于下细粒式沥青玛蹄脂碎石层上,所述上细粒式沥青玛蹄脂碎石层设置于所述中粒式高性能沥青混凝土层上,所述上细粒式沥青玛蹄脂碎石层与中粒式高性能沥青混凝土层之间、中粒式高性能沥青混凝土层与下细粒式沥青玛蹄脂碎石层之间、以及下细粒式沥青玛蹄脂碎石层与基层之间均以粘结层连接。
2.根据权利要求1所述的一种新型的沥青路面,其特征在于,所述两个细粒式沥青玛蹄脂碎石层厚度均为4cm,所述中粒式高性能沥青混凝土层厚度为6-8cm。
CN2011203132254U 2011-08-26 2011-08-26 一种新型的沥青路面 Expired - Fee Related CN202247584U (zh)