CN201922029U - 金属定向凝固洁净锭模 - Google Patents

金属定向凝固洁净锭模 Download PDF

Info

Publication number
CN201922029U
CN201922029U CN2010206716671U CN201020671667U CN201922029U CN 201922029 U CN201922029 U CN 201922029U CN 2010206716671 U CN2010206716671 U CN 2010206716671U CN 201020671667 U CN201020671667 U CN 201020671667U CN 201922029 U CN201922029 U CN 201922029U
Authority
CN
China
Prior art keywords
directional solidification
ingot
mold
steel
mold plate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN2010206716671U
Other languages
English (en)
Inventor
李红洋
朱书成
许少普
张立新
崔冠军
杨东
唐郑磊
徐昭
张涛
庞林
许春
康文举
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nanyang Hanye Special Steel Co Ltd
Original Assignee
Nanyang Hanye Special Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nanyang Hanye Special Steel Co Ltd filed Critical Nanyang Hanye Special Steel Co Ltd
Priority to CN2010206716671U priority Critical patent/CN201922029U/zh
Application granted granted Critical
Publication of CN201922029U publication Critical patent/CN201922029U/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

本实用新型公开了一种金属定向凝固洁净锭模,包括相互连接的底模板、周向模板和保温帽,所述周向模板由三面水冷模板和一面高温模板组成。本实用新型抛弃了传统模铸所采取的低过热度快注法,而是在结构上改变使得金属液从向三面高温模板一面定向凝固,使得钢水在锭模内的凝固时间延长,钢水的偏析加剧,由于定向凝固的作用使得偏析元素、夹杂物等缺陷都聚集到了钢锭宽面的表面上,脱模后再通过对钢锭缺陷富集的表面实行火焰清理或切割,便彻底去除了各类偏析和夹杂物聚集的缺陷部位,剩余部分则是内部组织致密、质量良好的钢锭。

Description

金属定向凝固洁净锭模
技术领域
本实用新型涉及一种金属凝固锭模,特别是一种金属定向凝固洁净锭模。
背景技术
目前,常规模铸钢普遍采用低温快浇的生产工艺,以减轻钢锭内部的疏松和偏析。但是采取低过热度浇注时,不利于钢锭中的夹杂物上浮,同时钢锭中心的疏松和偏析缺陷也并不能有效的缓解或消除。采用常规的定向凝固生产工艺生产模铸洁净钢时,因其生产效率低、成本高和单重限制,不能满足生产特重特厚钢板的要求。
实用新型内容
本实用新型公开了一种金属定向凝固洁净锭模,通过本实用新型的使用,达到生产的模铸钢具有钢水洁净度高、钢锭内部无疏松和偏析缺陷,能够满足采取较小压缩比便能轧制出性能和内部探伤质量都良好的厚板。
一种金属定向凝固洁净锭模,包括相互连接的底模板、周向模板和保温帽,所述周向模板由三面水冷模板和一面高温模板组成。
所述与高温模板相邻的两面水冷模板内壁上设置绝热板。
本实用新型的周向模板由三面水冷模板和一面高温模板组成,抛弃了传统模铸所采取的低过热度快注法,而是在结构上改变使得金属液从向三面高温模板一面定向凝固,采取高过热度浇注和注毕后长时间的镇静作用,使得钢水在锭模内的凝固时间延长,钢水的偏析加剧,由于定向凝固的作用使得偏析元素、夹杂物等缺陷都聚集到了钢锭宽面的表面上,脱模后再通过对钢锭缺陷富集的表面实行火焰清理或切割,便彻底去除了各类偏析和夹杂物聚集的缺陷部位,剩余部分则是内部组织致密、质量良好的钢锭,从而达到了生产洁净钢的目的。彻底消除了钢锭中心的偏析和疏松缺陷,并有效的减少了钢锭内部的夹杂物,由此可以生产出内部组织致密的洁净钢锭。
附图说明
下面结合附图对本实用新型进一步说明:
图1是本实用新型的结构示意图。
具体实施方式
如图1所示:一种金属定向凝固洁净锭模,包括相互连接的底模板、周向模板和保温帽,所述周向模板由三面水冷模板1和一面高温模板2组成。所述与高温模板2相邻的两面水冷模板1内壁上设置与整个水冷模板1内壁紧密接触的绝热板3。洁净钢锭模底模板和模壁三面通水冷却,其中在锭模内的两窄面插上绝热板,并控制窄面的冷却水流量以减缓钢锭窄面的冷却速度,而另一宽面则采取加热或保温措施,同时在钢锭的上部再加上一个保温帽,使钢水在凝固过程中实现在高度方向上自下而上、在横截面上由通冷却水的一宽面向加热或保温的宽面形成定向凝固过程。按照上述设计要求制作好钢锭模,并对各个面的进水管按照阀门做到各面冷却水量可调;在钢水浇注前,对洁净钢锭模的两窄面安装上合适尺寸和符合质量要求的绝热板,在锭模需要保温的一面做好加热或保温措施;在浇注过程中通过控制钢水的合理浇注过热度(钢水浇注过热度≥35℃以上),使钢锭的凝固过程形成定向凝固;钢水注毕后,适当延长钢锭的冷却凝固时间;在钢锭脱模后,对钢锭保温或加热的一面进行火焰清理或切割,使钢锭的缺陷富集部位得到了彻底清除,便得到了内部组织致密的洁净钢钢锭。

Claims (2)

1.一种金属定向凝固洁净锭模,其特征在于:它包括相互连接的底模板、周向模板和保温帽,所述周向模板由三面水冷模板和一面高温模板组成。
2.如权利要求1所述的金属定向凝固洁净锭模,其特征在于:所述与高温模板相邻的两面水冷模板内壁上设置绝热板。
CN2010206716671U 2010-12-21 2010-12-21 金属定向凝固洁净锭模 Expired - Lifetime CN201922029U (zh)