CN201922003U - 结晶器铜管外模 - Google Patents
结晶器铜管外模 Download PDFInfo
- Publication number
- CN201922003U CN201922003U CN2010206803294U CN201020680329U CN201922003U CN 201922003 U CN201922003 U CN 201922003U CN 2010206803294 U CN2010206803294 U CN 2010206803294U CN 201020680329 U CN201020680329 U CN 201020680329U CN 201922003 U CN201922003 U CN 201922003U
- Authority
- CN
- China
- Prior art keywords
- mould body
- outer mould
- outer die
- internal layer
- die body
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了结晶器铜管外模,属于外模,其结构包括外模本体,所述的外模本体为双层结构,所述的外模本体包括外层外模本体和内层外模本体,所述的内层外模本体设置在外层外模本体的内侧,所述的外层外模本体为45号钢材质,所述的内层外模本体为硬铬镀层,所述的内层外模本体的上段和下段分别呈锥度设置,所述的内层外模本体的上段的上部开口大,下部开口小,所述的内层外模本体的下段的上部开口小,下部开口大。与现有技术相比,本实用新型的结晶器铜管外模具有减小了加工难度,锻打时不容易出现裂纹等缺陷,增加了使用寿命,降低了生产成本,容易进料和走料,不容易损坏外模等特点,因而具有很好的推广应用价值。
Description
技术领域
本实用新型涉及一种外模,尤其是一种结晶器铜管外模。
背景技术
现在所使用的结晶器铜管外模,外模为单层结构,外模采用40Cr合金钢材质制成,硬度高,加工难度大,锻打容易出现缺陷,容易出现裂纹,寿命短,而且40Cr合金钢价格较高,增加了生产成本,而且外模内腔为筒状结构,不容易进料和走料,容易与外模内壁碰触摩擦,容易损坏模具。目前,还未有好的解决方案。
实用新型内容
本实用新型的技术任务是针对上述现有技术中的不足提供一种结晶器铜管外模,该结晶器铜管外模具有减小了加工难度,锻打时不容易出现裂纹等缺陷,增加了使用寿命,降低了生产成本,容易进料和走料,不容易损坏外模的特点。
本实用新型解决其技术问题所采用的技术方案是:它包括外模本体,所述的外模本体为双层结构,所述的外模本体包括外层外模本体和内层外模本体,所述的内层外模本体设置在外层外模本体的内侧,所述的外层外模本体为45号钢材质,所述的内层外模本体为硬铬镀层,所述的内层外模本体的上段和下段分别呈锥度设置,所述的内层外模本体的上段的上部开口大,下部开口小,所述的内层外模本体的下段的上部开口小,下部开口大。
所述的内层外模本体的厚度为0.06-0.08mm。
所述的内层外模本体的厚度为0.07mm。
所述的内层外模本体的上段与垂直面的夹角为10°-40°。
所述的内层外模本体的上段与垂直面的夹角为24°。
所述的内层外模本体的下段与垂直面的夹角为5°-45°。
所述的内层外模本体的下段与垂直面的夹角为30°。
本实用新型的结晶器铜管外模和现有技术相比,具有以下突出的有益效果:外模本体为双层结构,外层外模本体采用45号钢材质制作,内层外模本体为硬铬镀层,减小了加工难度,锻打时不容易出现裂纹等缺陷,增加了使用寿命,降低了生产成本,内层外模本体的上段和下段分别呈锥度设置,容易进料和走料,不容易损坏外模,使用方便等特点。
附图说明
附图1是结晶器铜管外模的结构示意图;附图标记说明:1、外层外模本体,2、内层外模本体,3、上段,4、下段。
具体实施方式
参照说明书附图1对本实用新型的结晶器铜管外模作以下详细地说明。
本实用新型的结晶器铜管外模,其结构包括外模本体,所述的外模本体为双层结构,所述的外模本体包括外层外模本体1和内层外模本体2,所述的内层外模本体2设置在外层外模本体1的内侧,所述的外层外模本体1为45号钢材质,所述的内层外模本体2为硬铬镀层,所述的内层外模本体2的上段3和下段4分别呈锥度设置,所述的内层外模本体2的上段3的上部开口大,下部开口小,所述的内层外模本体2的下段4的上部开口小,下部开口大。
所述的内层外模本体2的厚度为0.06-0.08mm。
所述的内层外模本体2的厚度为0.07mm。
所述的内层外模本体2的上段3与垂直面的夹角为10°-40°。
所述的内层外模本体2的上段3与垂直面的夹角为24°。
所述的内层外模本体2的下段4与垂直面的夹角为5°-45°。
所述的内层外模本体2的下段4与垂直面的夹角为30°。
外层外模本体1采用45号钢材质制作,内层外模本体2为硬铬镀层,45号钢较40Cr硬度低,减小了加工难度,锻打时不容易出现裂纹等缺陷,增加了外模的使用寿命,45号钢较40Cr价格便宜,降低了生产成本,内层外模本体2的上段3和下段4分别呈锥度设置,容易进料和走料,不容易损坏外模,使用方便。
除说明书所述的技术特征外,均为本专业技术人员的已知技术。
Claims (7)
1.结晶器铜管外模,包括外模本体,其特征是:所述的外模本体为双层结构,所述的外模本体包括外层外模本体和内层外模本体,所述的内层外模本体设置在外层外模本体的内侧,所述的外层外模本体为45号钢材质,所述的内层外模本体为硬铬镀层,所述的内层外模本体的上段和下段分别呈锥度设置,所述的内层外模本体的上段的上部开口大,下部开口小,所述的内层外模本体的下段的上部开口小,下部开口大。
2.根据权利要求1所述的结晶器铜管外模,其特征是:所述的内层外模本体的厚度为0.06-0.08mm。
3.根据权利要求2所述的结晶器铜管外模,其特征是:所述的内层外模本体的厚度为0.07mm。
4.根据权利要求1所述的结晶器铜管外模,其特征是:所述的内层外模本体的上段与垂直面的夹角为10°-40°。
5.根据权利要求4所述的结晶器铜管外模,其特征是:所述的内层外模本体的上段与垂直面的夹角为24°。
6.根据权利要求1所述的结晶器铜管外模,其特征是:所述的内层外模本体的下段与垂直面的夹角为5°-45°。
7.根据权利要求6所述的结晶器铜管外模,其特征是:所述的内层外模本体的下段与垂直面的夹角为30°。