CN201873766U - 铜包钢的镀锡前处理装置 - Google Patents

铜包钢的镀锡前处理装置 Download PDF

Info

Publication number
CN201873766U
CN201873766U CN2010202835243U CN201020283524U CN201873766U CN 201873766 U CN201873766 U CN 201873766U CN 2010202835243 U CN2010202835243 U CN 2010202835243U CN 201020283524 U CN201020283524 U CN 201020283524U CN 201873766 U CN201873766 U CN 201873766U
Authority
CN
China
Prior art keywords
tank
pretreatment device
tinplating
alkaline
bath
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN2010202835243U
Other languages
English (en)
Inventor
张荣良
方彪
董毓敏
潘超鹰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Baichuan Conductor Technology Co., Ltd.
Original Assignee
Zhejiang Pujiang Baichuan Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhejiang Pujiang Baichuan Industrial Co Ltd filed Critical Zhejiang Pujiang Baichuan Industrial Co Ltd
Priority to CN2010202835243U priority Critical patent/CN201873766U/zh
Application granted granted Critical
Publication of CN201873766U publication Critical patent/CN201873766U/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

本实用新型涉及一种铜包钢的镀锡前处理装置,依次由碱洗槽、第二水洗槽、酸洗槽、第一水洗槽连接而成,第二水洗槽与酸洗槽之间设有抛光模具;因为该前处理装置中增加了这道调整的抛光模具,使得原材料表面的毛刺、波纹都得到了一定程度的清除和改善,使得表面光洁度增加;同时也可将酸洗和碱洗过程中未能去除的物质进行清除,有效地增加了清洗效果。

Description

铜包钢的镀锡前处理装置
技术领域
本实用新型涉及一种电镀的前处理装置。
背景技术
现有的镀锡铜包钢的前处理过程是这样的:原材料铜包钢先进行碱洗,除去表面的油污,然后进行水洗,洗去碱洗液,再进行酸洗,除去表面的锈点、氧化物,然后又水洗,除去酸洗液,完成前处理,进入镀液槽开始电镀。这样的前处理过程在原材料比较正常的情况下是无可厚非的,也是效果明显的,因为经过了碱洗和酸洗二道工序,铜包钢表面已处理得比较洁净和光滑,完全能达到镀锡的要求。
然而,实际生产过程中,原材料往往会有一定的缺陷,比如表面不光滑,有波纹,严重氧化导致的发黑、发红等现象,尤其是经过退火的特软铜包钢线,由于其经过了高温,线材有时有些变形,缺陷更多,这些情况不是光靠碱洗和酸洗能完成的,用上述工艺是解决不了的,这就意味着这些原材料会给镀锡过程带来一定的风险。
实用新型内容
本实用新型所要解决的技术问题是提供一种镀锡铜包钢前处理装置,克服铜包钢在镀锡过程中因铜包钢表面质量问题产生的镀锡质量问题,改善铜包钢缺陷,提升最终产品的质量。
本实用新型的技术方案:一种铜包钢的镀锡前处理装置依次由碱洗槽、酸洗槽和第一水洗槽连接而成,碱洗槽与酸洗槽之间设有抛光模具。
优选地,所述的碱洗槽与酸洗槽之间还设有第二水洗槽,抛光模具设于第二水洗槽与酸洗槽之间。
本实用新型由于在前处理过程中增加了这道调整模具,原材料表面的毛刺、波纹都得到了一定程度的清除和改善,使得表面光洁度增加;同时也可将酸洗和碱洗过程中未能去除的物质进行清除,增加了清洗效果。
附图说明
图1是本实用新型实施例的结构示意图
具体实施方式
下列是结合实施例对本实用新型做进一步的详细描述,但本实用新型的保护范围并不限于此。
实施例
参考图1所示,一种铜包钢的镀锡前处理装置,所述的处理装置依次由碱洗槽1、第二水洗槽2、酸洗槽3和第一水洗槽4连接而成,第二水洗槽2与酸洗槽3之间设有抛光模具5。
铜包钢线材从碱洗槽1处进入对线材进行表面除油处理,经第二水洗槽2,将表面残留的碱洗液清除,再经过抛光模具5对线材表面的毛刺、波纹等不良进行抛光,然后进入酸洗槽3对线材氧化进行清除,最后进入第一水洗槽4将对线材表面残留的酸洗液清除。形成表面光滑、无毛刺、无波纹、无氧化利于后续镀锡的铜包钢线材。

Claims (2)

1.一种铜包钢的镀锡前处理装置,其特征在于,所述的处理装置依次由碱洗槽、酸洗槽和第一水洗槽连接而成,碱洗槽与酸洗槽之间设有抛光模具。
2.按照权利要求1所述的铜包钢的镀锡前处理装置,其特征在于,所述的碱洗槽与酸洗槽之间还设有第二水洗槽,抛光模具设于第二水洗槽与酸洗槽之间。
CN2010202835243U 2010-08-05 2010-08-05 铜包钢的镀锡前处理装置 Expired - Lifetime CN201873766U (zh)