CN201535037U - 钢筋直螺纹挤压连接套筒 - Google Patents

钢筋直螺纹挤压连接套筒 Download PDF

Info

Publication number
CN201535037U
CN201535037U CN2009200700183U CN200920070018U CN201535037U CN 201535037 U CN201535037 U CN 201535037U CN 2009200700183 U CN2009200700183 U CN 2009200700183U CN 200920070018 U CN200920070018 U CN 200920070018U CN 201535037 U CN201535037 U CN 201535037U
Authority
CN
China
Prior art keywords
connecting sleeve
sleeve
steel bar
steel
cold extrusion
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009200700183U
Other languages
English (en)
Inventor
储宏道
储士强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANGHAI HONGXUAN ELECTROMECHANICAL TECHNOLOGY Co Ltd
Original Assignee
SHANGHAI HONGXUAN ELECTROMECHANICAL TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANGHAI HONGXUAN ELECTROMECHANICAL TECHNOLOGY Co Ltd filed Critical SHANGHAI HONGXUAN ELECTROMECHANICAL TECHNOLOGY Co Ltd
Priority to CN2009200700183U priority Critical patent/CN201535037U/zh
Application granted granted Critical
Publication of CN201535037U publication Critical patent/CN201535037U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型提供一种冷挤压成形的钢筋直螺纹连接套筒,其内孔是能与钢筋端头螺牙相啮合的圆柱螺纹,外形横截面为圆形,且表面带有至少两条平行于套筒轴线的均匀连续的纵肋,也可以改变模具设计使挤压出的套筒有更多纵肋,纵肋在圆周上均匀分布。钢筋直螺纹挤压连接套筒的金属材料致密硬化,强度性能全面提高,不仅可满足各种牌号等级钢筋直螺纹连接的强度和变形设计要求,而且节省钢材,增厚混凝土保护层,接头连接操作更安全可靠。

Description

钢筋直螺纹挤压连接套筒
技术领域
本发明涉及一种钢筋直螺纹连接套筒,特别涉及一种用钢套坯料冷挤压制作的钢筋直螺纹连接套筒。
背景技术
目前,建筑工程用的钢筋直螺纹连接套筒是用45#钢棒或无缝钢管直接加工制成,但钢厂提供的45#钢材的屈服强度为350Mpa,与所连接的钢筋牌号HRB335相当,却仅是牌号HRB400、RRB400、HRB500钢筋屈服强度的0.88、0.80和0.70倍,这与JGJ107-2003《钢筋机械连接通用规程》(以下简称“规程”)规定“接头连接件的屈服承载力的标准值应不小于被连接钢筋的屈服承载力标准值的1.10倍”差距较大,故常态的45#钢直螺纹连接套筒难以满足“规程”关于接头连接套筒屈服承载及变形性能要求,容易影响钢筋接头的连接质量。
发明内容
本发明目的,是提供一种冷挤压成形的钢筋直螺纹连接套筒,使金属材料致密硬化,使强度性能全面提高,可满足各种钢筋直螺纹连接的强度和变形设计要求。
本发明连接套筒内孔是能与钢筋端头螺牙相啮合的圆柱螺纹,外形横截面为圆形,且表面带有至少两条平行于套筒轴线的均匀连续的纵肋,纵肋在圆周上均匀分布。如图1所示为外形有2条纵肋的钢筋直螺纹挤压连接套筒。
本发明以45#钢为原材料,经冷挤压加工,使钢套坯料直径缩小至所需尺寸,并在外圆柱面留下至少2条合模飞边,即2条纵肋,也可以根据需要改变模具设计使挤压出的套筒有更多的纵肋。由此获得钢筋直螺纹挤压连接套筒横截面外径减少,增厚了混凝土保护层;套筒上的纵肋不仅增强了与混凝土的握裹力,还使钢筋连接更安全可靠,用管子钳拧紧不会打滑。套筒材料经挤压变形使金属致密硬化,综合强度性能显著提高:其抗拉强度提高30%,套筒的截面积可相应减少,节省钢材20~30%,其抗剪强度提高8%,屈服强度提高20~50%,套筒的抗变形性能提高,钢筋接头拉伸检测中即使母材拉断,套筒螺牙仍能顺利从钢筋端头螺纹旋出;其抗疲劳性能提高40%以上,接头能顺利通过循环荷载200万次疲劳检测。
附图说明
图1是有2条纵肋的钢筋挤压连接套筒的立体图;
图2是纵肋高度近于零的钢筋挤压连接套筒立体图。
具体实施方式
将长度和内外圆直径为规定尺寸的无缝钢管坯料送入挤压装置,经模具挤压成外圆柱面有均布纵肋的直螺纹连接套筒坯料,然后把内孔加工成与所连接钢筋端头螺纹相匹配的内螺纹。套筒至少设置有2条纵肋(如图1所示)。纵肋高度只能在钢套坯料与连接套两者外圆半径之差值间设计选择,若选取纵肋高度近于零,则连接套内外面都是圆柱形(如图2所示)。

Claims (1)

1.一种钢筋直螺纹连接套筒,内孔是能与钢筋端头螺牙相啮合的圆柱螺纹,其特征是:套筒经冷挤压制成,外形截面为圆形,表面带有至少两条平行于套筒轴线的均匀连续的纵肋,纵肋在圆周上均匀分布。
CN2009200700183U 2009-04-08 2009-04-08 钢筋直螺纹挤压连接套筒 Expired - Fee Related CN201535037U (zh)