CN201310695Y - 一种对焊法兰半成品 - Google Patents
一种对焊法兰半成品 Download PDFInfo
- Publication number
- CN201310695Y CN201310695Y CNU200820161850XU CN200820161850U CN201310695Y CN 201310695 Y CN201310695 Y CN 201310695Y CN U200820161850X U CNU200820161850X U CN U200820161850XU CN 200820161850 U CN200820161850 U CN 200820161850U CN 201310695 Y CN201310695 Y CN 201310695Y
- Authority
- CN
- China
- Prior art keywords
- welding
- boss ring
- straight section
- flange
- finished product
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种对焊法兰半成品,在本实用新型法兰本体的上方直边段的内壁有一凸台环,该凸台环上端面与法兰本体上端面平齐,该凸台环是在对对焊法兰毛坯件锻造时锻造出的。在堆焊时,先堆焊凸台环下方的法兰本体的内壁,堆焊好后,再将凸台环沿法兰内壁加工掉,然后再堆焊直边段的内壁。在直边段内壁处增加凸台环,增强了直边段的强度,这样,在对对焊法兰进行堆焊时,直边段的变形量会非常小或基本没有变形。堆焊好后再加工掉凸台环,也没有改变对焊法兰的结构和尺寸。
Description
技术领域
本实用新型涉及一种半成品,尤其是一种对焊法兰半成品,对焊法兰属于化工压力容器用法兰。
背景技术
对焊法兰在使用前需堆焊其内壁,以免被腐蚀性介质腐蚀,而在堆焊前,人们一般将对焊法兰半成品加工到对焊法兰的基本形状和尺寸。由于加工好的对焊法兰的直边段比较薄,堆焊时,因受热容易发生变形,使对焊法兰直边段部分存在一定的椭圆度,当直边段的端部与管子等部件组装时,会出现较大的错边量,即使与管子等部件焊接好后,焊缝的X检测结果也很难合格。
发明内容
本实用新型提供一种对焊法兰半成品,在其直边段的内壁有一凸台环,以增强法兰直边段的强度,在堆焊时减小直边段因受热变形。
在本实用新型法兰本体的上方直边段的内壁有一凸台环,该凸台环上端面与法兰本体上端面平齐,该凸台环是在对对焊法兰毛坯件锻造时锻造出的。在堆焊时,先堆焊凸台环下方的法兰本体的内壁,堆焊好后,再将凸台环沿法兰内壁加工掉,然后再堆焊直边段的内壁。
在直边段内壁处增加凸台环,增强了直边段的强度,这样,在对对焊法兰进行堆焊时,直边段的变形量会非常小或基本没有变形。堆焊好后再加工掉凸台环,即没有改变对焊法兰的结构和尺寸。
附图说明
图1为本实用新型的截面示意图。
图2为本实用新型的俯视图。
图3为本实用新型堆焊凸台环下方法兰本体内壁的截面示意图。
图4为本实用新型全部堆焊好后的截面示意图。
具体实施方式
如图1所示,在法兰本体1的直边段1-1的内壁有一凸台环1-2,该凸台环1-2上端面与法兰本体上端面1-4平齐。在堆焊时,先堆焊凸台环1-2下方的法兰本体的内壁1-3(如图3所示),堆焊好后,再将凸台环1-2沿法兰本体内壁1-3加工掉,然后再堆焊直边段1-1的内壁(如图4所示)。
使用时,将法兰本体上端面1-4与管子之类的部件焊接在一起。
Claims (2)
1、一种对焊法兰半成品,包括法兰本体,在法兰本体的上方有直边段,其特征在于所说的直边段的内壁有一凸台环。
2、根据权利要求1所述的一种对焊法兰半成品,其特征在于所说的凸台环的上端面与法兰本体上端面平齐。