CN201155652Y - 一种用于油气田的不锈钢化纳米涂镀管 - Google Patents
一种用于油气田的不锈钢化纳米涂镀管 Download PDFInfo
- Publication number
- CN201155652Y CN201155652Y CNU2007201177926U CN200720117792U CN201155652Y CN 201155652 Y CN201155652 Y CN 201155652Y CN U2007201177926 U CNU2007201177926 U CN U2007201177926U CN 200720117792 U CN200720117792 U CN 200720117792U CN 201155652 Y CN201155652 Y CN 201155652Y
- Authority
- CN
- China
- Prior art keywords
- stainless steel
- alloy layer
- gas field
- coating
- oil gas
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种用于油气田的不锈钢化纳米涂镀管。该不锈钢化纳米涂镀管包括管本体(1),管本体(1)内外壁镀有铁铝多元合金层(2),铁铝多元合金层(2)外依次有纯合金层(3)及纳米聚合物涂层(4)。该不锈钢化纳米涂镀管具有良好的耐腐蚀性能、结合力大、机械性能好、抗老化以及强防蜡防垢的特点。
Description
技术领域:
本实用新型涉及油田采油领域所用的一种油管或套管,属于一种用于油气田的不锈钢化纳米涂镀管。
背景技术:
采油时采用油管或套管来对液体进行运输,油管或套管在长期使用会出现腐蚀、穿孔现象,导致油管或套管未达使用年限即不能再使用了。而现场目前所应用的油套管防腐方法均为表面隔离层法,只能起到暂时隔离环境腐蚀介质的作用,随着使用时间的延长,防腐层则开始出现气层脱落现象,致使油管或套管腐蚀加剧,同时表面隔离层主要为环氧树脂类涂层,这些环氧树脂类涂层存在吸水率高,抗机械冲击、抗机械划伤性能差的问题,在施工和搬运时防腐层会损坏,严重影响防腐效果,降低了油管的使用寿命,且这些隔离层的防蜡、防垢性能差,导致油套管结蜡、结垢现象严重,缩短油套管的维修期,造成相当的经济损失。
实用新型内容:
为了克服现有的油管或套管防腐、防蜡、防垢效果差及使用寿命短的不足,本实用新型提供一种不锈钢化纳米涂镀管,该油管或套管不仅具有良好的耐腐蚀性能、结合力大、机械性能好、抗老化,而且还具有强防蜡防垢的优点。
本实用新型所采取的技术方案是:该用于油气田的不锈钢化纳米涂镀管包括油管或套管本体,油管或套管本体内外壁镀有铁铝多元合金层,铁铝多元合金层外依次有纯合金层及纳米聚合物涂层。
上述的铁铝多元合金层的厚度为80~120μm;纳米涂料层厚度为90~120μm
本实用新型的有益效果是:该油管或套管的多元合金层具有不锈钢特性,涂镀层间形成冶金化学结合,附着力强,且具有牺牲阳极保护作用,具有较高的机械强度和耐蚀性;同时,将不锈钢化的油套管再经纯化、进行纳米聚涂料旋转喷涂;该管材表面光亮、光滑,无针孔、不结垢、不粘油;可耐酸、碱、盐、表面活性剂、污水、天然气、微生物等介质腐蚀;具有防腐、防垢、防蜡和防脱层四防特性。
附图说明:
附图1是本实用新型的结构剖视图。
1-管本体,2-铁铝多元合金层,3-纯合金层,4-纳米聚合物涂层。
具体实施方式:
下面结合附图将对本实用新型作进一步说明:
由图1所示,该用于油气田的不锈钢化纳米涂镀管包括油管或套管的本体1,油管或套管的本体1内外壁镀有铁铝多元合金层2,铁铝多元合金层2外依次有纯合金层3及纳米聚合物涂层4。铁铝多元合金层2的厚度为80~120μm;纳米聚合物涂层厚度为90~120μm。
该油管或套管具有良好的耐腐蚀能力,并可以保证在施工、运输过程中外表面不起层、不脱落;主要应用于聚驱油水井、三元驱油水井、注气驱油气井、强腐蚀、强结垢水井、严重结蜡油井、天然气井及CO2注入采出井等。
Claims (3)
1、一种用于油气田的不锈钢化纳米涂镀管,包括管本体(1),其特征在于:管本体(1)内外壁镀有铁铝多元合金层(2),铁铝多元合金层(2)外依次有纯合金层(3)及纳米聚合物涂层(4)。
2、根据权利要求1所述的一种用于油气田的不锈钢化纳米涂镀管,其特征在于:铁铝多元合金层(2)的厚度为80~120μm。
3、根据权利要求1所述的一种用于油气田的不锈钢化纳米涂镀管,其特征在于:纳米聚合物涂层(4)厚度为90~120μm。