CN1611525A - 生物可降解材料的制备方法 - Google Patents

生物可降解材料的制备方法 Download PDF

Info

Publication number
CN1611525A
CN1611525A CN 200310110794 CN200310110794A CN1611525A CN 1611525 A CN1611525 A CN 1611525A CN 200310110794 CN200310110794 CN 200310110794 CN 200310110794 A CN200310110794 A CN 200310110794A CN 1611525 A CN1611525 A CN 1611525A
Authority
CN
China
Prior art keywords
lactic acid
film
polyethyleneglycol
biodegradable
biodegradable material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 200310110794
Other languages
English (en)
Other versions
CN1305928C (zh
Inventor
罗秀文
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chengdu Nanding Medical Material Co ltd
Original Assignee
CHENGDU TUOTAI MEDICINE SCI-TECH DEVELOPMENT Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHENGDU TUOTAI MEDICINE SCI-TECH DEVELOPMENT Co Ltd filed Critical CHENGDU TUOTAI MEDICINE SCI-TECH DEVELOPMENT Co Ltd
Priority to CNB2003101107949A priority Critical patent/CN1305928C/zh
Publication of CN1611525A publication Critical patent/CN1611525A/zh
Application granted granted Critical
Publication of CN1305928C publication Critical patent/CN1305928C/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

本发明是一种生物可降解材料的制备方法,是将乳酸、聚乙二醇通过本体聚合的方法共聚,从而制得乳酸/聚乙二醇共聚物生物可降解材料;其中,各组分的重量比例为:乳酸1%~99.5%,聚乙二醇0.5%~99%;反应温度:90~220℃,时间:1~8小时。本发明工艺简单,成本低廉,所制备的生物可降解材料用于生产生物可降解防粘连膜,得到的生物可降解防粘连膜厚度均匀,质量稳定,降解时间适合,有一定柔韧性和拉伸性。

Description

生物可降解材料的制备方法
所属技术领域:本发明属于医疗用品的制备领域,尤其是涉及一种生物可降解材料的制备方法。
技术背景:在外科手术中,常采用防粘连膜作为物理屏障来防止术后粘连。现有的防粘连膜均为生物可吸收医用膜,有聚乳酸膜、透明质酸膜、壳聚糖膜及氧化纤维素膜几种。市售的聚乳酸膜为聚乳酸与乙醇酸共聚物或聚乳酸均聚物的膜,质脆,柔韧性、拉伸性差,降解时间过长,在使用及安全性上都有一定的弊端。而透明质酸膜、壳聚糖膜和氧化纤维素膜,降解时间太短,不能在要求的时间内保持物理屏障的作用,而不能较好地完成防粘连的功能,另外壳聚糖膜柔韧性较差,给临床使用带来许多不便。
发明内容:本发明的目的在于提供一种工艺简单,成本低廉的生物可降解材料的制备方法,所制备的材料可用于生产厚度均匀,质量稳定,降解时间适合的,有一定柔韧性和拉伸性的防粘连膜。
本发明的目的是通过下述方案来实现的:
本发明的生物可降解材料的制备方法,是将乳酸、聚乙二醇通过本体聚合的方法共聚,从而制得乳酸/聚乙二醇共聚物生物可降解材料;其中,各组分的重量比例为:乳酸1%~99.5%,聚乙二醇0.5%~99%;反应温度:90~220℃,时间:1~8小时。
上述方案中,所制得的乳酸/聚乙二醇共聚物生物可降解材料用于制备生物可降解防粘连膜。
上述方案中,生物可降解防粘连膜的制备工艺为:40℃下用2~20倍于乳酸/聚乙二醇共聚物重量的混合溶剂将乳酸/聚乙二醇共聚物溶解完全,把乳酸/聚乙二醇共聚物溶液倒入制膜模具,室温放置3~5小时,于40~60℃下真空干燥至恒重,得初品膜;将初品膜于30~50℃下拉伸10%~120%(以初品膜的原长为基准),在60~80℃下热定型1~2小时后,室温条件下真空干燥12小时,即得生物可降解防粘连膜;其中,混合溶剂为丙酮∶乙酸乙酪∶四氢呋喃∶氯仿=10~90%∶8~88%∶2~82%∶0~80%(重量比例)。
用本发明所制备的生物可降解材料制备的生物可降解防粘连膜的主要参数为:
分子量3~20万Da;
降解时间2周~4个月;
拉伸模量:0.65~1.25Mpa;
重金属含量:小于10μg/g;
烧灼残渣:小于0.2%;
无菌、无致热源性;
溶血性小于5%;
细胞毒性0~1级;
无过敏反应,无遗传毒性。
因此,本发明工艺简单,成本低廉,所制备的生物可降解材料可用于生产厚度均匀,质量稳定,降解时间适合的,有一定柔韧性和拉伸性的防粘连膜。
具体实施方式:
实施例一
将乳酸1克,聚乙二醇99克,在90℃下反应8小时,制得乳酸/聚乙二醇共聚物生物可降解材料。
在40℃下用200克混合溶剂将乳酸/聚乙二醇共聚物溶解完全,把乳酸/聚乙二醇共聚物溶液倒入制膜模具,室温放置3小时,于40℃下真空干燥至恒重,得初品膜;将初品膜于30℃下拉伸120%(以初品膜的原长为基准),在60℃下热定型2小时后,室温条件下真空干燥12小时,即得生物可降解防粘连膜;其中,混合溶剂为丙酮∶乙酸乙酯∶四氢呋喃∶氯仿=10%∶8%∶2%∶80%(重量比例)。
实施例二
将乳酸99.5克,聚乙二醇0.5克,在220℃下反应1小时,制得乳酸/聚乙二醇共聚物生物可降解材料。
在40℃下用2000克的混合溶剂将乳酸/聚乙二醇共聚物溶解完全,把乳酸/聚乙二醇共聚物溶液倒入制膜模具,室温放置5小时,于60℃下真空干燥至恒重,得初品膜;将初品膜于50℃下拉伸10%(以初品膜的原长为基准),在80℃下热定型1小时后,室温条件下真空干燥12小时,即得生物可降解防粘连膜;其中,混合溶剂为丙酮∶乙酸乙酯∶四氢呋喃∶氯仿=90%∶8%∶2%∶0(重量比例)。
实施例三
将乳酸50克,聚乙二醇50克,在150℃下反应3小时,制得乳酸/聚乙二醇共聚物生物可降解材料。
在40℃下用1000克的混合溶剂将乳酸/聚乙二醇共聚物溶解完全,把乳酸/聚乙二醇共聚物溶液倒入制膜模具,室温放置4小时,于50℃下真空干燥至恒重,得初品膜;将初品膜于40℃下拉伸60%(以初品膜的原长为基准),在70℃下热定型2小时后,室温条件下真空干燥12小时,即得生物可降解防粘连膜;其中,混合溶剂为丙酮∶乙酸乙酯∶四氢呋喃∶氯仿=10%∶88%∶2%∶0(重量比例)。
实施例四
将乳酸80克,聚乙二醇20克,在180℃下反应3小时,制得乳酸/聚乙二醇共聚物生物可降解材料。
在40℃下用1000克的混合溶剂将乳酸/聚乙二醇共聚物溶解完全,把乳酸/聚乙二醇共聚物溶液倒入制膜模具,室温放置5小时,于60℃下真空干燥至恒重,得初品膜;将初品膜于50℃下拉伸50%(以初品膜的原长为基准),在80℃下热定型1小时后,室温条件下真空干燥12小时,即得生物可降解防粘连膜;其中,混合溶剂为丙酮∶乙酸乙酪∶四氢呋喃∶氯仿=10%∶8%∶82%∶0(重量比例)。
实施例五
将乳酸30克,聚乙二醇70克,在120℃下反应5小时,制得乳酸/聚乙二醇共聚物生物可降解材料。
在40℃下用800克的混合溶剂将乳酸/聚乙二醇共聚物溶解完全,把乳酸/聚乙二醇共聚物溶液倒入制膜模具,室温放置4小时,于50℃下真空干燥至恒重,得初品膜;将初品膜于40℃下拉伸80%(以初品膜的原长为基准),在60℃下热定型2小时后,室温条件下真空干燥12小时,即得生物可降解防粘连膜;其中,混合溶剂为丙酮∶乙酸乙酯∶四氢呋喃∶氯仿=50%∶20%∶20%∶10%(重量比例)。
实施例六
将乳酸88克,聚乙二醇12克,在180℃下反应3小时,制得乳酸/聚乙二醇共聚物生物可降解材料。
在40℃下用1200克的混合溶剂将乳酸/聚乙二醇共聚物溶解完全,把乳酸/聚乙二醇共聚物溶液倒入制膜模具,室温放置3小时,于60℃下真空干燥至恒重,得初品膜;将初品膜于40℃下拉伸40%(以初品膜的原长为基准),在80℃下热定型2小时后,室温条件下真空干燥12小时,即得生物可降解防粘连膜;其中,混合溶剂为丙酮∶乙酸乙酯∶四氢呋喃∶氯仿=20%∶50%∶10%∶20%(重量比例)。
实施例七
将乳酸85克,聚乙二醇15克,在180℃下反应3小时,制得乳酸/聚乙二醇共聚物生物可降解材料。
在40℃下用1500克的混合溶剂将乳酸/聚乙二醇共聚物溶解完全,把乳酸/聚乙二醇共聚物溶液倒入制膜模具,室温放置5小时,于60℃下真空干燥至恒重,得初品膜;将初品膜于50℃下拉伸30%(以初品膜的原长为基准),在80℃下热定型2小时后,室温条件下真空干燥12小时,即得生物可降解防粘连膜;其中,混合溶剂为丙酮∶乙酸乙酪∶四氢呋喃∶氯仿=30%∶20%∶30%∶20%(重量比例)。
实施例八
将乳酸90克,聚乙二醇10克,在180℃下反应3小时,制得乳酸/聚乙二醇共聚物生物可降解材料。
在40℃下用1800克的混合溶剂将乳酸/聚乙二醇共聚物溶解完全,把乳酸/聚乙二醇共聚物溶液倒入制膜模具,室温放置5小时,于60℃下真空干燥至恒重,得初品膜;将初品膜于50℃下拉伸50%(以初品膜的原长为基准),在80℃下热定型2小时后,室温条件下真空干燥12小时,即得生物可降解防粘连膜;其中,混合溶剂为丙酮∶乙酸乙酯∶四氢呋喃∶氯仿=20%∶20%∶20%∶40%(重量比例)。
实施例九
将乳酸70克,聚乙二醇30克,在150℃下反应4小时,制得乳酸/聚乙二醇共聚物生物可降解材料。
在40℃下用1000克的混合溶剂将乳酸/聚乙二醇共聚物溶解完全,把乳酸/聚乙二醇共聚物溶液倒入制膜模具,室温放置3小时,于40℃下真空干燥至恒重,得初品膜;将初品膜于30℃下拉伸100%(以初品膜的原长为基准),在80℃下热定型2小时后,室温条件下真空干燥12小时,即得生物可降解防粘连膜;其中,混合溶剂为丙酮∶乙酸乙酯∶四氢呋喃∶氯仿=40%∶20%∶20%∶20%(重量比例)。

Claims (3)

1.一种生物可降解材料的制备方法,其特征在于将乳酸、聚乙二醇通过本体聚合的方法共聚,从而制得乳酸/聚乙二醇共聚物生物可降解材料;其中,各组分的重量比例为:乳酸1%~99.5%,聚乙二醇0.5%~9%;反应温度:90~220℃,时间:1~8小时。
2.根据权利要求1所述的生物可降解材料的制备方法,其特征在于所制得的乳酸/聚乙二醇共聚物生物可降解材料用于制备生物可降解防粘连膜。
3.根据权利要求2所述的生物可降解材料的制备方法,其特征在于生物可降解防粘连膜的制备工艺为:40℃下用2~20倍于乳酸/聚乙二醇共聚物重量的混合溶剂将乳酸/聚乙二醇共聚物溶解完全,把乳酸/聚乙二醇共聚物溶液倒入制膜模具,室温放置3~5小时,于40~60℃下真空干燥至恒重,得初品膜;将初品膜于30~50℃下拉伸10%~120%(以初品膜的原长为基准),在60~80℃下热定型1~2小时后,室温条件下真空干燥12小时,即得生物可降解防粘连膜;其中,混合溶剂为丙酮∶乙酸乙酯∶四氢呋喃∶氯仿=10~90%∶8~88%∶2~82%∶0~80%(重量比例)。
CNB2003101107949A 2003-10-27 2003-10-27 生物可降解材料的制备方法 Expired - Lifetime CN1305928C (zh)