CN1593788A - Colorful solid design wall paint and construction technology - Google Patents

Colorful solid design wall paint and construction technology Download PDF

Info

Publication number
CN1593788A
CN1593788A CN 03150890 CN03150890A CN1593788A CN 1593788 A CN1593788 A CN 1593788A CN 03150890 CN03150890 CN 03150890 CN 03150890 A CN03150890 A CN 03150890A CN 1593788 A CN1593788 A CN 1593788A
Authority
CN
China
Prior art keywords
paint
layered material
emulsion
colored
uneven patterns
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 03150890
Other languages
Chinese (zh)
Other versions
CN1234466C (en
Inventor
徐昌平
卢荣明
吕兆荣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Alligator Coatings Shanghai Co ltd
Original Assignee
SHANGHAI SHENZHEN ALIJIATUO COATING CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANGHAI SHENZHEN ALIJIATUO COATING CO Ltd filed Critical SHANGHAI SHENZHEN ALIJIATUO COATING CO Ltd
Priority to CN 03150890 priority Critical patent/CN1234466C/en
Publication of CN1593788A publication Critical patent/CN1593788A/en
Application granted granted Critical
Publication of CN1234466C publication Critical patent/CN1234466C/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The invention makes public a kind of colorful three-dimensional pattern paint and the method of using it. The paint includes at least four kind of paint as following: base paint, middle paint, colorful paint and face paint. Base paint, middle paint and face paint is liquid, and colorful paint is irregular solid strip. The method is the following: buffing the wall->removing dust->painting base paint->painting middle paint->painting colorful paint->rolling the wall->removing floating pieces->painting face paint. The invention has beautiful color, graceful and three-dimensional appearance, is waterproof, alkali-proof, stain-proof and spot-proof, sticks firmly, and resists bacteria and mildew, improving visual effect of room. It also releases negative ion and optimizes air of the room. Additionally it lowers noise. The invention can be used inside any kind construction.

Description

Colored uneven patterns wall paint and construction technology
Technical field
The present invention relates to build aqueous inner wall paint and construction technology, specifically a kind of colored uneven patterns wall paint and construction technology.
Background technology
The indoor decorative paint that occurs various class in the market generally all is based on emulsion paint, and its outward appearance is just changing aspect flat matter color and the gloss to some extent.The U.S. in the fifties just begin to develop multicolor finish (oil-in-water, zola-coat).Japan's Northwest paint company has been introduced the U.S. in nineteen fifty-five and " has been looked into and draw coating (ゾ ラ コ-ト) ", the decorative pattern because this coating property good and overtime generation films, thereby Northwest paint company " ゾ ラ コ-ト, (zola-coat) " that produce is a large amount of in decades uses in the buildingss such as at home hospital, school, office building, hotel, restaurant.General multicolor finish has four classes, and wherein oil-in-water-type (O/W), water-in-oil (W/O), oil bag oil (O/O) etc. can distribute a large amount of organic solvents, harmful to human and environment when the construction spraying.This in addition coating has ornamental preferably, but is subjected to understand the defective that obvious yellowing occurs behind the sun exposure.Another kind of is water-in-water type (W/W) multicolor finish, the volatilization and the yellowing problem of filming of nuisance when it has solved spraying, but its decorative effect and storage property are very poor, have hindered and have applied.
Summary of the invention
A kind of colored uneven patterns wall paint and the construction technology that provide at the deficiencies in the prior art is provided, it is the monochromatic emulsion paint of the traditional flat matter of a kind of ratio, the stronger wall paint of traditional multicolor finish decorative effect, its whole lacquer performance has anti-stain characteristic, abrasion resistance, available suds are cleaned, and can cover metope minute crack; The not yellowing variable color of filming can not be peeled off and long service life; Safety and Health, has negative ion-releasing function and antibacterial and mouldproof performance at low VOC (VOC), can dispel film coated surface bacterium, intestinal bacteria, gold-coloured staphylococci etc., makes room air more pure and fresh.
The concrete technical scheme that realizes the object of the invention is:
The colored uneven patterns wall paint comprises at least four kinds of layered materials, be followed successively by priming paint layered material, floating coat material, colored film layered material, finish paint layered material, wherein priming paint layered material, floating coat material, finish paint layered material are the liquid material, the colored film layered material is irregular of solid, bar, and each layered material main component (by weight) is:
(a), priming paint layered material: synthetic emulsion 10-40 part, lime carbonate 10-40 part, titanium dioxide 10-30 part, dispersion agent 0.4-1 part, ether of cellulose and derivative 0.1-1 part thereof, biocide mildewcide 0.1-1.0 part, defoamer 0.1-0.5, water 30-40 part;
(b), floating coat material: synthetic emulsion 15-45 part, titanium dioxide 10-25 part, lime carbonate 10-20 part, talcum powder 0-15 part, kaolin 0-15 part, dispersion agent 0.4-1 part, water-holding agent 0.5-2.5 part, ether of cellulose and derivative 0.1-1 part thereof, thickening material 0.5-2 part, biocide mildewcide 0.1-1.0 part, defoamer 0.1-0.5, water 20-40 part;
(c), colored film layered material: with the polyurethane acroleic acid emulsion is that the emulsion paint toning of base-material is after system film, drying, pulverize, the sieve irregular sheet of solid that makes or strip, bar shaped thin slice, be of a size of: irregular sheet or strip φ 1.0mm-φ 20mm, the bar shaped sheet length is 1.0mm-30mm, thickness 0.05mm-1.5mm;
(d), finish paint layered material: synthetic emulsion 25-60 part, biocide mildewcide 0.1-1.0 part, negative-ion auxiliary agent 1-5 part, thickening material 0.5-2.5 part, water 40-70 part, matting agent 0-1.0 part, defoamer 0.1-0.5.
Described dispersion agent is polyacrylic acid dipersant, polyethenoxy ether class dispersion agent, silicate dispersion agent, condensed phosphoric acid salt dispersion agent.
Described synthetic emulsion can be pure acrylic acid emulsion, vinegar-third copolymer emulsion, uncle's vinegar milk liquid or styrene-propene acid copolymer emulsion, ethene-vinyl acetate copolymer emulsion, acetate emulsion, organosilicon acroleic acid polyurethane emulsion etc.
Described ether of cellulose and derivative thereof can be methylcellulose gum, ethyl cellulose, Walocel MT 20.000PV, Natvosol, hydroxypropylcellulose, carboxymethyl cellulose, methylhydroxypropylcellulose, urethane, acrylic acid or the like, marine alga acids.
Described defoamer can be the composite of siloxane-based defoamer, siloxane-based defoamer.
Described biocide mildewcide can be organic antibacterial agent or inorganic antiseptic, also can adopt organic and inorganic complex antimicrobials, and wherein inorganic antiseptic can be silver, zinc, the isoionic slow release type of copper, nano titanium oxide.
Described negative-ion auxiliary agent can be pure natural mineral, spar, the jewel that contains multiple element.
The construction technology of colored uneven patterns wall paint comprises following operation: wall is criticized the floating sheet of embedding polishing → dedusting → brushing priming paint layered material → brushing floating coat material → color spray sheet layered material → roll-in → cleaning → brushing surface enamelled coating material.
Described colored film layered material is sprayed on the floating coat material with the pneumatics spray gun.
The present invention has tone luxurious, match volume attractive in appearance, elegant, ornamental strong and good scrub resistance, water-fast and alkali resistance, high dirt resistance and spot-resistant, cohesive force is strong, antibacterial and mouldproof also has characteristics such as long service life, anti-xanthochromia, low VOC (volatile organic compounds), easy construction, decorative effect solid are luxurious, stable storing simultaneously.Because of it has unique match volume, not only can change the visual effect of room space but also have the effect that reduces noise.Have a kind of specific function simultaneously and discharge negative ion, obnoxious flavour and foreign flavor indoors such as the formaldehyde that Eradicates brings except that house fitting, ammonia, benzene, and dispel the harmful bacterium of coating surface, intestinal bacteria, gold-coloured staphylococci, effectively improve the air ambient in room.Be a kind of environment-friendly type, anti-xanthochromia, the luxurious coloured coating of multifunctional stereo texture, it is applicable to the decoration of facing (as: multiple substrate surface such as concrete, mortar, mortar, slabstone, wood materials) in the various buildingss.
Decorative effect of the present invention has obvious characteristics such as diversity, fashion-orientation, compares with traditional emulsion paint, and be a quantum jump of wall decoration.
The wall decoration effect The color solid wall paint The tradition emulsion paint
Warm romantic composite color Monochromatic
The natural figure that fashion is generous Do not have
Pleasing match volume The plane does not have texture
Plentiful half soft light gloss Flat matter gloss
Embodiment
Embodiment:
(a), priming paint layered material: get 40 parts of vinegar-third copolymer emulsions, 10 parts in lime carbonate, 15 parts of titanium dioxides, 0.5 part of polyacrylic acid dipersant, 0.5 part of Walocel MT 20.000PV, 0.3 part of defoamer, 0.2 part of biocide mildewcide, 33.5 parts in water, water is injected reactor, added the dispersion agent high speed dispersion 10 minutes, added the Walocel MT 20.000PV high speed dispersion 10 minutes, added the titanium dioxide high speed dispersion 10 minutes, added the lime carbonate high-speed stirring 25 minutes, adding vinegar-third copolymer emulsion stirred at a slow speed 5 minutes, adding biocide mildewcide stirred at a slow speed 5 minutes, adding defoamer stirred at a slow speed 10 minutes, stop to stir, obtain the priming paint layered material.
(b), floating coat material: get 35 parts of pure acrylic acid emulsions, 18 parts of titanium dioxides, 13 parts in lime carbonate, 2 parts of talcum powder, 2 parts of kaolin, 0.6 part of polyacrylic acid dipersant, 0.6 part of water-holding agent, 0.4 part of methylhydroxypropylcellulose, 1 part of polyurethane thickener, 0.3 part of defoamer, biocide mildewcide 0.1,27 parts in water, water is injected reactor, added polyacrylic acid dipersant high speed dispersion 10 minutes, added the methylhydroxypropylcellulose high speed dispersion 10 minutes, added the water-holding agent high speed dispersion 5 minutes, added the titanium dioxide high speed dispersion 10 minutes, add filler (lime carbonate, talcum powder, kaolin) high speed dispersion is 25 minutes, adding the pure acrylic acid emulsion stirred at a slow speed 10 minutes, adding polyurethane thickener stirred at a slow speed 10 minutes, adding biocide mildewcide stirred at a slow speed 5 minutes, add defoamer and stirred at a slow speed 10 minutes, stop to stir.Obtain the floating coat material.
(c), colored film layered material: the emulsion paint toning that with the ACRYLIC EMULSION is base-material is after system film, drying, the irregular sheet of solid, the bar shaped thin slice pulverizing, sieve and make, be of a size of: irregular sheet φ 1.0mm-φ 20mm, the bar shaped sheet length is 1.0mm-30mm, thickness 0.05mm-1.5mm.
(d), finish paint layered material: get 52.1 parts of organosilicon acroleic acid polyurethane emulsions, 2.3 parts of polyurethane thickeners, 2 parts of negative-ion auxiliary agent, 43 parts in water, 0.5 part of matting agent, 0.1 part of defoamer, biocide mildewcide 0.1, water is injected reactor, added matting agent, negative-ion auxiliary agent high speed dispersion 5 minutes, adding the organosilicon acroleic acid polyurethane emulsion stirred at a slow speed 10 minutes, adding polyurethane thickener stirred at a slow speed 10 minutes, adding biocide mildewcide stirred at a slow speed 5 minutes, add defoamer and stirred at a slow speed 10 minutes, stop to stir.Obtain the finish paint layered material.
Construction technology of the present invention is: wall is criticized the floating sheet of embedding polishing → dedusting → brushing priming paint layered material → brushing floating coat material (roller coating or spraying) → color spray sheet layered material → roll-in → cleaning → brushing surface enamelled coating material.
Concrete construction technological process:
1, criticizes face putty
Completely criticize putty on metope after treatment, after first pass is done, after thick polishing, criticize and scrape second time, meticulous polishing dedusting can be carried out coating application then.
2, brushing priming paint layered material:
The priming paint brushing gets final product together, should earlier priming paint be stirred before the brushing, adopts roller to carry out during brushing, and brushing must be evenly, and inaccurate holiday, especially negative and positive angular position must be mended with painting brush and be put in place.
3, brushing floating coat material:
After treating priming paint layered material complete drying, brushing floating coat material gets final product for one time, should earlier the floating coat material be stirred before the brushing, adopts roller coating or spraying method during brushing, and brushing must be evenly, inaccurate holiday, and especially the negative and positive angular position must be mended with painting brush and be put in place.
4, color spray sheet layered material:
(1), usually behind the intact face wall of floating coat material brushing, should finish color spray sheet layered material at short notice, otherwise will lose cohesive force after the floating coat material drying, cause the colored film layered material can't bond on it.
(2), below the metope of need sprayings, spread plastics film in advance, be used to the colored film layered material of accepting to trickle down.
(3), connect the air compressor machine power supply, start air compressor machine and connect spray gun, regulate the pressure of air compressor machine.
(4), the colored film layered material is poured in the bucket, and mixing does pine, on one's body with braces bucket tiltedly being worn at.Regulate braces to appropriate length and draw a colored film layered material in the bucket with convenient.
(5), a suction side of holding the spray gun material sucking pipes, the suction side is floated on and smooth colored film layered material face, middle finger and forefinger block opening for feed with the control inlet amount, one hand-motion suction end moves in bucket during color spray sheet layered material; Another is held spray gun and tries spray facing to collecting film earlier, and then the spray metope.Spray gun keeps vertical with metope during color spray sheet layered material, and moves with arm drive spray gun.It is moderate to note controlling load during color spray sheet layered material, and discharging speed is stable and the spray sheet is even.
(6), after having sprayed, the colored film layered material between 1~2 hour, uses rubber rollers roll-in one time, so that colored film layered material strong bond.
(7), unrestrained colored film layered material can not use separately, as desire to reduce the wastage, then can with this batch residue colored film layered material mixing after can use.
5, brushing surface enamelled coating material:
(1), after the colored film layered material sprayed drying, must brush unstuck colored film layered material on the coating gently, can brushing surface enamelled coating material with hairbrush.
(2), earlier finish paint is stirred before the brushing surface enamelled coating material, brushing requires to get final product for one time, and brushing should be even, and bubble can not be arranged, must not holiday.

Claims (9)

1, a kind of colored uneven patterns wall paint, it is characterized in that it comprises at least four kinds of layered materials, be followed successively by priming paint layered material, floating coat material, colored film layered material, finish paint layered material, wherein priming paint layered material, floating coat material, finish paint layered material are the liquid material, the colored film layered material is irregular of solid, bar, and each layered material main component (by weight) is:
(a), priming paint layered material: synthetic emulsion 10-40 part, lime carbonate 10-40 part, titanium dioxide 10-30 part, dispersion agent 0.4-1 part, ether of cellulose and derivative 0.1-1 part thereof, biocide mildewcide 0.1-1.0 part, defoamer 0.1-0.5, water 30-40 part;
(b), floating coat material: synthetic emulsion 15-45 part, titanium dioxide 10-25 part, lime carbonate 10-20 part, talcum powder 0-15 part, kaolin 0-15 part, dispersion agent 0.4-1 part, water-holding agent 0.5-2.5 part, ether of cellulose and derivative 0.1-1 part thereof, thickening material 0.5-2 part, biocide mildewcide 0.1-1.0 part, defoamer 0.1-0.5, water 20-40 part;
(c), colored film layered material: with the polyurethane acroleic acid emulsion is that the emulsion paint toning of base-material is after system film, drying, pulverize, the sieve irregular sheet of solid that makes or strip, bar shaped thin slice, be of a size of: irregular sheet or strip φ 1.0mm-φ 20mm, the bar shaped sheet length is 1.0mm-30mm, thickness 0.05mm-1.5mm;
(d), finish paint layered material: synthetic emulsion 25-60 part, biocide mildewcide 0.1-1.0 part, negative-ion auxiliary agent 1-5 part, thickening material 0.5-2.5 part, water 40-70 part, matting agent 0-1.0 part, defoamer 0.1-0.5.
2, colored uneven patterns wall paint according to claim 1 is characterized in that described dispersion agent is polyacrylic acid dipersant, polyethenoxy ether class dispersion agent, silicate dispersion agent, condensed phosphoric acid salt dispersion agent.
3, colored uneven patterns wall paint according to claim 1 is characterized in that described synthetic emulsion can be pure acrylic acid emulsion, vinegar-third copolymer emulsion, uncle's vinegar milk liquid or styrene-propene acid copolymer emulsion, ethene-vinyl acetate copolymer emulsion, acetate emulsion, organosilicon acroleic acid polyurethane emulsion etc.
4, colored uneven patterns wall paint according to claim 1 is characterized in that described ether of cellulose and derivative thereof can be methylcellulose gum, ethyl cellulose, Walocel MT 20.000PV, Natvosol, hydroxypropylcellulose, carboxymethyl cellulose, methylhydroxypropylcellulose, urethane, acrylic acid or the like, marine alga acids.
5, colored uneven patterns wall paint according to claim 1 is characterized in that described defoamer can be the composite of siloxane-based defoamer, siloxane-based defoamer.
6, colored uneven patterns wall paint according to claim 1, it is characterized in that described antibacterial mildew inhibitor can be organic antibacterial agent or inorganic antiseptic, also can adopt organic and inorganic complex antimicrobials, wherein inorganic antiseptic can be silver, zinc, the isoionic slow release type of copper, nano titanium oxide.
7, colored uneven patterns wall paint according to claim 1 is characterized in that described negative-ion auxiliary agent can be pure natural mineral, spar, the jewel that contains multiple element.
8, the construction technology of the described colored uneven patterns wall paint of a kind of claim 1 is characterized in that it comprises following operation: wall is criticized the floating sheet of embedding polishing → dedusting → brushing priming paint layered material → brushing floating coat material → color spray sheet layered material → roll-in → cleaning → brushing surface enamelled coating material.
9, construction technology according to claim 8 is characterized in that the colored film layered material is sprayed on the floating coat material with the pneumatics spray gun.
CN 03150890 2003-09-10 2003-09-10 Colorful solid design wall paint and construction technology Expired - Fee Related CN1234466C (en)