CN1388151A - 壳聚糖接枝聚乳酸溶致液晶的制备方法 - Google Patents

壳聚糖接枝聚乳酸溶致液晶的制备方法 Download PDF

Info

Publication number
CN1388151A
CN1388151A CN 02112484 CN02112484A CN1388151A CN 1388151 A CN1388151 A CN 1388151A CN 02112484 CN02112484 CN 02112484 CN 02112484 A CN02112484 A CN 02112484A CN 1388151 A CN1388151 A CN 1388151A
Authority
CN
China
Prior art keywords
chitosan
liquid crystal
polylactic acid
solution
dissolved
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 02112484
Other languages
English (en)
Other versions
CN1176141C (zh
Inventor
刘预
田丰
陈刚
胡克鳌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Jiaotong University
Original Assignee
Shanghai Jiaotong University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Jiaotong University filed Critical Shanghai Jiaotong University
Priority to CNB021124841A priority Critical patent/CN1176141C/zh
Publication of CN1388151A publication Critical patent/CN1388151A/zh
Application granted granted Critical
Publication of CN1176141C publication Critical patent/CN1176141C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

一种壳聚糖接枝聚乳酸溶致液晶的制备方法,将各种脱乙酰度达的壳聚糖在真空下脱气1小时,充入氮气,加入甲苯作分散液,逐滴加入与壳聚糖1-3倍摩尔量的三乙基铝的甲苯溶液作催化剂,在溶液中使丙交酯发生开环聚合,生成壳聚糖与聚乳酸的接枝共聚物,溶解在三氟乙酸,乙酸,二氯乙酸或水中,在溶液浓度大于1%的条件下,都可在偏光显微镜观察到它们的液晶行为。本发明制备的共聚接枝物具有特殊性能,既可以用作甲壳素,壳聚糖和聚乳酸共混物的界面偶联剂,也可以作为药物缓释剂材料和其它人体植入生物材料;同时它具有溶致液晶性能,可以纺制成高性能的壳聚糖纤维,及其它生物复合材料的增强纤维。

Description

壳聚糖接枝聚乳酸溶致液晶的制备方法
技术领域:
本发明涉及一种壳聚糖接枝聚乳酸溶致液晶的制备方法,制备的材料具有液晶态,可以扩大其加工范围,如通过在溶液状态下液晶溶液纺丝得到高强度的纤维,有可能作为外科手术的缝合线以及其它生物复合材料的增强纤维。
背景技术:
甲壳素是仅次于纤维素第二大产量天然合成的高分子材料,每年由生物合成的这种材料的产量高达近十亿吨之多。但由于在甲壳素分子中存在的氢键,使其既没有特定的熔点,也不能溶于普通溶剂,这极大地限制了它的使用性。壳聚糖是甲壳素的脱乙酰产物,它和甲壳素一样,具有消炎,止血,促进细胞再生等独特的生物功能,在医药,食品,化妆品,农业和环保诸多方面可能找到其广泛地用途。
近三十年来,聚乳酸及其共聚物作为一类具有生物降解性和生物相容性的合成高分子材料,已被用来制造手术缝合线,人造骨钉,人造皮肤,外科整形材料,和药物缓释剂等医用材料,在临床已经获得了广泛地应用。但由于其表面的亲水性较差,所以在人体内的降解时间长,以至于引起身体的不良反应。人们长期以来,用其它的亲水性和水溶性的材料来改良聚乳酸的表面亲水性能,如Breitenbach及其合作者,(Polymer,Vol.39,No.14,p3261-3271,1998.)用水溶性聚乙烯醇作主干,合成了聚乙烯醇和聚乳酸的接枝共聚物,但聚乙烯醇的生理作用目前还不清楚,使其应用受到一定的限制。
发明内容:
本发明的目的在于针对现有技术的不足,提出一种新的壳聚糖接枝聚乳酸溶致液晶的制备方法,用聚乳酸这种合成的高分子来对壳聚糖这种天然高分子进行改性,提高聚乳酸的表面亲水性,改善壳聚糖的加工性能,制得的溶液可以用于纺制高性能的壳聚糖纤维,提高其经济价值。
为实现这样的目的,本发明的技术方案中,将聚乳酸这种具有优良生物降解性和生物相容性的合成聚合物,与壳聚糖这类具有独特生物功效的天然高分子共聚,利用各种脱乙酰度的壳聚糖,与丙交酯摩尔比为1∶1至1∶60的范围内,加入1-3倍摩尔量的三乙基铝做催化剂,在溶液中发生反应,使丙交酯开环聚合,生成壳聚糖与聚乳酸的接枝共聚物。并将其溶解在三氟乙酸,乙酸,水,二氯乙酸等溶剂中,使其具有液晶性,可用于纺制高性能的壳聚糖纤维。
本发明具体的实施方法如下:
在经过反复干燥的反应器中,加入经过严格干燥不同脱乙酰度的壳聚糖,使其在真空脱气1小时,充入氮气,加入将其配制成0.01-6摩尔的甲苯分散液的干燥甲苯。在室温条件下,逐滴加入与壳聚糖1-3倍摩尔量的三乙基铝的甲苯溶液。待无气体放出时,使其继续反应1小时。然后加入定量的经过真空脱气熔点范围在124℃-126℃的丙交酯,放入到预先加热到70℃的油浴中,反应20小时后,将反应液倒入到乙醇中,过滤,干燥得到原始产物。将以上产物溶解在三氟乙酸,乙酸,二氯乙酸或水中,在溶液浓度大于1%的条件下,都可在偏光显微镜观察到它们的液晶行为。
这个反应可以从壳聚糖与丙交酯的摩尔比为1∶1至1∶60宽广范围内,均能顺利进行。
本发明制备的壳聚糖与丙交酯的共聚接枝物具有特殊性能,与一般条件下聚乳酸的表面亲水性较差相比,其在常温条件下,在水中的溶解性大大提高。由于其接枝物的结构,既可以用作甲壳素,壳聚糖和聚乳酸共混物的界面偶联剂,也可以作为药物缓释剂材料和其它人体植入生物材料。同时由于它具有溶致液晶性能,可以纺制成壳聚糖的高性能纤维,这又可以作为供临床使用的手术缝合线,也可以作为其它生物复合材料的增强纤维。
具体实施方式:
以下结合具体的实施例对本发明的技术方案作进一步描述。
实施例1:
脱乙酰度50%的壳聚糖与丙交酯摩尔比1∶1的实施。
将脱乙酰度50%的壳聚糖在真空烘箱中干燥48小时,脱除其表面的吸附水。称取0.05mol壳聚糖加入到反应器中,在真空下脱气1小时,加入40ml经过干燥的甲苯作为分散剂,将其配制成1.25摩尔的甲苯分散液。称取0.05mol的三乙基铝,配制成15%的甲苯溶液。在室温下将三乙基铝溶液逐滴加入到壳聚糖甲苯的分散液中,待无气体产生时,再反应1小时。加入0.05mol经过真空脱气1小时的丙交酯,然后将反应器置于预先加热到70℃的油浴中,反应20小时以上,将反应液倒入乙醇中,使其充分沉淀,过滤干燥后溶解在水中,在其溶液浓度大于1%时,在偏光显微镜下可以观察到它的胆甾型溶液液晶行为。
实施例2:
脱乙酰度94%的壳聚糖与丙交酯1∶1的实施。
将脱乙酰度94%的壳聚糖在真空烘箱中干燥48小时,脱除其表面的吸附水。称取0.05mol壳聚糖加入到反应器中,在真空下脱气1小时。加入60ml经过干燥的甲苯作分散,将其配制成0.83摩尔的甲苯分散液。称取0.05mol的三乙基铝,配制成15%的甲苯溶液。在室温下将三乙基铝溶液逐滴加入到壳聚糖甲苯的分散液中,待无气体产生时,再反应1小时。加入0.05mol经过真空脱气1小时的丙交酯,然后将反应器置于预先加热到70℃的油浴中,反应20小时以上,将反应液倒入乙醇中,使其充分沉淀,过滤干燥后溶解在三氟乙酸中,在其溶液浓度大于1%时,在偏光显微镜下可以观察到它的胆甾型溶液液晶行为。
实施例3:
乙酰度94%的壳聚糖与丙交酯1∶60的实施。将脱乙酰度94%的壳聚糖在真空烘箱中干燥48小时,脱除其表面的吸附水。称取0.005mol壳聚糖加入到反应器中,在真空下脱气1小时。加入100ml经过干燥的甲苯作分散剂,将其配制成0.05摩尔的甲苯分散液。称取0.005mol的三乙基铝,配制成15%的甲苯溶液。在室温下将三乙基铝溶液逐滴加入到壳聚糖甲苯的分散液中,待无气体产生时,再反应1小时。加入0.3mol经过真空脱气1小时的丙交酯,然后将反应器置于预先加热到70℃的油浴中,反应20小时以上,将反应液倒入乙醇中,使其充分沉淀,过滤干燥后溶解在二氯乙酸中,在其溶液浓度大于1%时,在偏光显微镜下可以观察到它的胆甾型溶液液晶行为。

Claims (2)

1、一种壳聚糖接枝聚乳酸溶致液晶的制备方法,其特征在于将壳聚糖真空脱气1小时,充入氮气,加入甲苯配制成0.01-6摩尔的甲苯分散液,在室温条件下,逐滴加入与壳聚糖1-3倍摩尔量的三乙基铝的甲苯溶液作催化剂,待无气体放出时,使其继续反应1小时,然后加入经过真空脱气的丙交酯,丙交酯与壳聚糖摩尔比为1∶1至60∶1,在70℃的油浴中反应20小时以上,将反应液倒入到乙醇中,过滤干燥后溶解在三氟乙酸、乙酸、水或二氯乙酸中,溶液浓度保持1%以上。
2、用权利要求1方法制备的壳聚糖接枝聚乳酸溶致液晶,其特征在于具有溶致液晶性,用于纺制高性能的壳聚糖纤维。
CNB021124841A 2002-07-11 2002-07-11 壳聚糖接枝聚乳酸溶致液晶的制备方法 Expired - Fee Related CN1176141C (zh)