CN1299847C - 一种炉辊隔热保护工艺 - Google Patents

一种炉辊隔热保护工艺 Download PDF

Info

Publication number
CN1299847C
CN1299847C CNB2005100312131A CN200510031213A CN1299847C CN 1299847 C CN1299847 C CN 1299847C CN B2005100312131 A CNB2005100312131 A CN B2005100312131A CN 200510031213 A CN200510031213 A CN 200510031213A CN 1299847 C CN1299847 C CN 1299847C
Authority
CN
China
Prior art keywords
furnace roller
high temperature
furnace
thermal insulation
temperature
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNB2005100312131A
Other languages
English (en)
Other versions
CN1657828A (zh
Inventor
高峰
高晓吾
余桂芬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNB2005100312131A priority Critical patent/CN1299847C/zh
Publication of CN1657828A publication Critical patent/CN1657828A/zh
Application granted granted Critical
Publication of CN1299847C publication Critical patent/CN1299847C/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种炉辊隔热保护工艺,具体为,第一步:在承重品轮炉辊的指定隔热部位刷涂炉辊专用高温结合剂,涂刷时炉辊表面不得有油污,表面光洁度不低于4;第二步:将特制定型的陶纤维块放置于上述部位,并在接口处刷涂高温结合剂,然后加压初步固定;第三步:保持陶纤维块表面清洁,然后对其表面喷涂炉辊专用高温红外复合液乳料,阴干备用;第四步:在喷涂了高温红外复合乳料的陶纤维块上放置耐热钢紧固扣,紧固后即可投入生产使用。工艺简单,成本低;劳动强度轻;抗高温,抗热震性好,不易开裂剥落陨坏;重量轻,减少高温状态下炉辊负荷;导热系数小,节能效果好;使用寿命长,减少了大量维修时间,提高了劳动生产率。

Description

一种炉辊隔热保护工艺
技术领域
本发明涉及一种炉辊隔热保护工艺,尤其是一种用于辊底式均热炉或加热炉的承重凸轮炉辊隔热保护工艺。
背景技术
目前市场上用于工业生产的,如钢铁轧制、陶瓷焙烧、机加工热处理等行业使用的辊底式均热炉,其中的重要零部件——承重凸轮炉辊,因为工作环境温度高达1300-1400℃,长期24小时连续重负荷运转,必须采取隔热保护技术方能实施。目前炉辊隔热保护措施大多是采取缠绕隔热材料、浇注耐水材料或喷绝热材料等方法。这些方法可能导致许多不良现象发生,一是承重凸轮炉辊的热保护装置维护更换工艺复杂,维修极为不方便,消耗工时多,劳动强度大;二是不耐高温,抗热震性差,容易开裂剥落损坏;三是重量大,增加高温状态下的承重重量;四是导致字数高,热损失多,甚至烧坏炉辊,导致使用周期短;五是维护工作频繁,生产工时减少,影响生产效率。
发明内容
本发明的目的就是提供一种克服上述缺陷的一种炉辊隔热保护工艺。
本发明的技术方案是通过以下途径实现的,它的保护工艺是:第一步:在承重品轮炉辊的指定隔热部位刷涂炉辊专用高温结合剂,涂刷时炉辊表面不得有油污,表面光洁度不低于4;第二步:将特制定型的陶纤维块放置于上述部位,并在接口处刷涂高温结合剂,然后加压初步固定;第三步:保持陶纤维块表面清洁,然后对其表面喷涂炉辊专用高温红外复合液乳料,阴干备用;第四步:在喷涂了高温红外复合乳料的陶纤维块上放置耐热钢紧固扣,紧固后即可投入生产使用。
本发明具有工艺简单方便,成本较低;工人劳动强度较轻,劳动环境较好;能抗高温,提高了抗热震性,不易开裂剥落陨坏;同时重量轻,可减少高温状态下的炉辊负荷;导热系数小,热损耗低,节能效果好;使用寿命长,减少了大量维修时间,提高了劳动生产率。
具体实施方式
下面详细描述本发明的具体实施方式。
本发明的具体工艺是:第一步:在承重品轮炉辊的指定隔热部位刷涂炉辊专用高温结合剂,涂刷时炉辊表面不得有油污,表面光洁度不低于4;第二步:将特制定型的陶纤维块放置于上述部位,并在接口处刷涂高温结合剂,然后加压初步固定;第三步:保持陶纤维块表面清洁,然后对其表面喷涂炉辊专用高温红外复合液乳料,阴干备用;第四步:在喷涂了高温红外复合乳料的陶纤维块上放置耐热钢紧固扣,紧固后即可投入生产使用。
高温红外复合液乳料的喷涂厚度,当炉棍工作温度在1100-1250℃时,喷涂厚度是1-2mm,炉棍工作温度在1250-1400℃,喷涂厚度是2-3mm,炉棍工作温度在1400-1600℃,喷涂厚度是3-4mm。
高温红外复合液乳料的型号应该选择与工作温度相对应的产品,以促进节能和防护效果。
耐热钢紧固扣的材料应考虑工作温度的高低,一般应选择比工作温度高的材料,耐热钢紧固扣可采用平面结构或网络结构,其紧固方式可采用扣、钩、铆、焊、螺栓等方式,应视炉内工况而定。
陶纤维块可以是高铝型、锆铝型、锆鉻型和莫来石等材料制成,这些材料的形态可以为毯、板、块、异型件。

Claims (2)

1.一种炉辊隔热保护工艺,其特征在于,它的具体工艺步骤为:
第一步:在承重品轮炉辊的指定隔热部位刷涂炉辊专用高温结合剂,涂刷时炉辊表面不得有油污,表面光洁度不低于4;
第二步:将特制定型的陶纤维块放置于上述部位,并在接口处刷涂高温结合剂,然后加压初步固定;
第三步:保持陶纤维块表面清洁,然后对其表面喷涂炉辊专用高温红外复合液乳料,阴干备用;
第四步:在喷涂了高温红外复合液乳料的陶纤维块上放置耐热钢紧固扣,紧固后即可投入生产使用。
2.根据权利要求1所述的保护工艺,其特征在于所述的高温红外复合液乳料的喷涂厚度,当炉棍工作温度在1100-1250℃时,喷涂厚度是1-2mm,炉棍工作温度在1250-1400℃,喷涂厚度是2-3mm,炉棍工作温度在1400-1600℃,喷涂厚度是3-4mm。
CNB2005100312131A 2005-01-29 2005-01-29 一种炉辊隔热保护工艺 Expired - Fee Related CN1299847C (zh)