CN1260846A - 用于电解精练的阴极 - Google Patents

用于电解精练的阴极 Download PDF

Info

Publication number
CN1260846A
CN1260846A CN98806323A CN98806323A CN1260846A CN 1260846 A CN1260846 A CN 1260846A CN 98806323 A CN98806323 A CN 98806323A CN 98806323 A CN98806323 A CN 98806323A CN 1260846 A CN1260846 A CN 1260846A
Authority
CN
China
Prior art keywords
negative electrode
bracket
support section
deviates
anode
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN98806323A
Other languages
English (en)
Other versions
CN1203215C (zh
Inventor
亨利·维尔塔宁
伊斯莫·维尔塔宁
图奥莫·基维斯特
汤姆·马蒂拉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Metso Corp
Original Assignee
Outokumpu Oyj
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Outokumpu Oyj filed Critical Outokumpu Oyj
Publication of CN1260846A publication Critical patent/CN1260846A/zh
Application granted granted Critical
Publication of CN1203215C publication Critical patent/CN1203215C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本发明涉及一种用于铜的电解精练的阴极,所述阴极(1)包括两个支撑部分(2),由此阴极(1)可以在电解过程中悬挂在电解池壁上。根据本发明,在阴极支撑部分(2)中形成有当将阴极从一个位置传递至另一个位置用于卡紧阴极(1)并用于支撑阴极(1)的托座(3)。

Description

用于电解精练的阴极
本发明涉及一种用于电解精练的可溶的铜阴极,此阴极浸在一用于电解精练的池中并从所述池中抬起,这样防止设在装填件中的卡紧件与池壁接触。
在铜的电解精练中起电极作用的阳极和阴极以交替的方式放入盛有电解溶液的一池中。为了方便地进行电解精练,电极尽可能彼此靠近,而且电极的相互位置中须尽可能精确,以避免短路。尽管阴极和阳极在其浸入电解池之前和从中抬起之后都经历完全不同的操作,但最好当装填件位于电解池之上时装填件的操作可以同时处理阳极和阴极。因此装填件最好设有分别为阴极和阳极设计的单独的卡紧件。
当使用可在电解溶液中溶解的一阴极时,在装载和在电子处理过程中都支撑阴极的阴极凸缘由同一种可溶材料制成,因此阴极凸缘应尽可能短。这样与装载有关的阴极卡紧件延伸基本接近池壁并接近带有与池壁悬置隔开的绝缘体的导体轨道,在此情况下卡紧件甚至很微小的误差移动也会损伤池、导体轨道或绝缘体。
当使用常规形状的铜阴极、其中凸缘和装填件之间的卡紧点位于电解池壁和阴极的板形部分之间时,包含在电解池中的电解液表面必须相对于与池壁悬置开的导体轨道很低,这样由阴极处理所需的阴极凸缘的设计可以防止进入电解液并防止与电解过程本身相干涉。当电解液的表面保持较低时,电解设备的投资和运行成本会增加,这是因为在其他原因中阳极报废的数量增大。
本发明的目的是避免现有技术的一些缺陷并实现为铜的电解精练设计的可溶性阴极得到改进和成为可能,在此阴极中阴极凸缘和装填件之间的卡紧点得到调整以便能以一基本同时的方式装载都用于电解精练的阴极和阳极。本发明的新颖特征从权利要求中显而易见。
在用于铜电解精练的可溶阴极中,在阴极的悬置部分中,悬置部分在电解过程中将阴极悬置在电解池中,最好当铸造阴极时形成一托座,这样背离阴极悬置部分的所述托座的端部指向阴极的中心线或指向所述中心线的一虚连接部分。这样设有一托座的一阴极的悬置部分可以被完全卡紧在包含在电解池中的电解液的液面之上,并利用卡紧件产生的一运动远离电解池壁。根据本发明,形成在阴极悬置部分中的托座在传递至电解池的过程中、在浸入并抬出电解池过程中并在进一步离开电解池过程中支撑阴极。这样只有当阴极浸在电解池中时支撑部分才适当地支撑阴极。
由于用于在电解池中进行的铜的电解精练的电极-阳极和阴极-在电解过程中由两个位于电极中心线相对侧上的单独的支撑件悬挂在电解池壁上,在本发明的阴极中,卡紧托座同样为两个支撑件分别形成,这最好使得背离支撑件的托座端部彼此相对指向。
根据本发明,形成在阴极支撑部分中的托座最好定位成背离支撑部分的托架端部与背离阴极中心线的支撑部分基本处于同一高度。托架最好基本沿其全长与支撑部分平行。背离支撑部分的托座的端部也可以与背离阴极中心线的端部相比处于一不同的高度,或者较高或者较低。在此情况下,至少一部分托座相对于支撑部分形成一尖角。托座的长度最好使得由设在装填件中的卡紧件取得一充分的支撑,以使阴极从一个位置传递至另一个位置。此外,设在本发明一阴极的支撑部分中的托座定位成托座基本相对于阴极中心线对称设置。
当使用用于电解精练的本发明的一可溶阴极时,其中所述阴极的支撑部分设有用于与传递相联系的悬挂阴极的一托座,可以很容易地用一装填件处理混合的阴极和阳极负载,因为设在装填件中并与托座配套的卡紧件不需要渗入阴极和阳极之间,其中通常设有阴极卡紧件的空间。另外,本发明有托座的阴极可以被卡紧,这样阴极相对于卡紧件的位置可以以精确的方式调整。此外,卡紧托座的卡紧件远离电解池壁并远离带有设在壁上的绝缘体的导体轨道,这样卡紧件至少不会由于轻微的误差运动碰到壁到轨道上。
最好形成在本发明的阴极卡紧部分中的托座以及卡紧所述托座的卡紧件总是位于包含在电解池中的电解液表面之上,这样本发明阴极的处理绝不会限制电解液表面的可能的升高。通过升高电解液表面,电解精练设备的投资和运行成本会降低。这样不论各个单独的卡紧托座如何阴极报废量就会降低。此外,当一卡紧托座用于本发明的阴极卡紧部分中时,不需要考虑阴极的卡紧,同时限定电解池以及用做电极的阳极和阴极的各个尺寸。
下面参照附图更详细地说明本发明,附图是本发明一优选实施例的一前视图。
根据附图,在一铸造的铜阴极1中,同铸造相联系形成支撑件2,以便在电解池中进行溶解过程中悬置阴极。此外,与铸造相关联,支撑件2设有卡紧托座3,以便当阴极由同装填件相连并公知的卡紧件(未示出)移动时支撑阴极。除此之外,标号4表示背离支撑件的卡紧托座3的端部,而标号5表示背向阳极的支撑件2的端部。

Claims (7)

1.一种用于铜的电解精练的阴极,所述阴极(1)包括两个支撑部分(2),由此阴极(1)可以在电解过程中悬挂在电解池壁上,其特征在于,当铸造阴极(1)时,在阴极支撑部分(2)中形成有当将阴极从一个位置传递至另一个位置用于卡紧阴极(1)并用于支撑阴极(1)的托座(3)。
2.如权利要求1所述的阴极,其特征在于,托座(3)形成为使得背离支撑部分的托座(3)的端部(4)指向位于阴极的第二支撑部分(2)中并与其背离的托座的端部(4)。
3.如权利要求1或2所述的阴极,其特征在于,托座(3)形成为使得背离支撑部分的托座(3)的端部(4)与背离阴极的支撑部分(2)的端部(5)基本一样高。
4.如权利要求1、2或3所述的阴极,其特征在于,托座(3)基本沿其全长平行于支撑部分(2)。
5.如权利要求1或2所述的阴极,其特征在于,托座(3)形成为使得背离支撑部分的托座(3)的端部(4)与背离阴极的支撑部分(2)的端部(5)处于不同的高度。
6.如权利要求5所述的阴极,其特征在于,至少一部分托座(3)相对于支撑部分形成一尖角。
7.如上述任一项权利要求所述的阴极,其特征在于,形成在支撑部分(2)中的托座(3)基本相对于阴极(1)的中心线处于对称的位置中。
CNB988063239A 1997-06-18 1998-06-05 用于电解精炼的阴极 Expired - Fee Related CN1203215C (zh)