KR100535197B1 - 전해 정련용 양극 - Google Patents
전해 정련용 양극 Download PDFInfo
- Publication number
- KR100535197B1 KR100535197B1 KR10-1999-7011944A KR19997011944A KR100535197B1 KR 100535197 B1 KR100535197 B1 KR 100535197B1 KR 19997011944 A KR19997011944 A KR 19997011944A KR 100535197 B1 KR100535197 B1 KR 100535197B1
- Authority
- KR
- South Korea
- Prior art keywords
- anode
- bracket
- support
- electrolytic
- delete delete
- Prior art date
Abstract
두개의 지지부(2)를 포함하며, 전해 공정시에 상기 지지부에 의해 전해 탱크 벽부에 대해 매달리는 구리의 전해 정련에 사용되는 양극(1)에 관한 것이다. 본 발명에 따르면, 양극 지지부(2)에는, 상기 양극(1)을 잡기 위해 및 양극을 한 위치에서 다른 위치로 이송할 때 상기 양극(1)을 지지하기 위해, 브라켓(3)이 형성되어 있다.
Description
본 발명은 전해 정련용 가용 구리 양극(anode)에 관한 것으로, 양극은 전해 정련에 사용되는 탱크 내에 잠기며, 상기 탱크로부터 들어 올려져서, 충전 부재에 설치된 그립핑 부재가 상기 탱크 벽부와 접촉하는 것으로부터 보호된다.
구리의 전해 정련에서 전극으로 작용하는 음극(cathode) 및 양극은 전해질을 보유하는 탱크 내에 교대로 놓인다. 전해 정련을 유리하게 수행하기 위해, 전극은 가능한 한 서로 가까이 위치해야 하며, 전극의 상대 위치 설정은 회로의 쇼트를 방지하기 위해 가능한 한 정확히 수행되어야 한다. 양극 및 음극은 전해 탱크 내에 잠기기 전 및 그곳으로부터 들어 올려진 후에 완전히 다른 공정이 진행된다고 하더라도 충전 부재의 공정에 대해, 상기 충전 부재가 전해 탱크 위에 위치하는 동안 양극과 음극을 동시에 조작할 수 있는 것이 유리하다. 그러므로 충전 부재에는 양극 및 음극에 대해 각각 따로 설계된 별도의 그립핑 부재가 설치되는 것이 유리하다.
전해질에 용해될 수 있는 양극을 사용할 때, 장착시 및 전자적 처리시 모두 양극을 지지하는 양극 러그(lug)는 동일한 가용 재료로 만들어지며, 따라서 양극 러그는 가능한 한 짧게 만들어 진다. 그리하여 장착과 관련된 양극 그리핑 부재는 실질적으로 탱크 벽부 및 상기 탱크 벽부에 매달린 절연체를 구비한 도체 레일 가까이로 신장하며, 이 경우 그리핑 부재의 약간의 잘못된 이동이 있어도 탱크, 도체 레일 또는 절연체의 손상을 초래할 수 있다.
러그와 충전 부재 사이의 그립점이 전해 탱크 벽부와 양극의 판형부 사이에 위치하는 종래 형상의 구리 양극을 사용할 때, 전해 탱크 내에 포함된 전해질 표면은 탱크 벽부로부터 매달린 도체 레일에 대해 실질적으로 낮아서, 양극 처리에 의해 요구되는 양극 러그 설계가 전해질로 들어가는 것이 방지되어 전해 공정 자체를 방해하는 것을 방지한다. 전해질 표면이 낮게 유지되면, 다른 여러 이유들 중, 양극 스크랩량의 증가 때문에 전해 플랜트의 투자비 및 운용비는 증가된다.
본 발명의 목적은 종래 기술의 여러 단점들을 제거하며, 구리의 전해 정련용으로 설계된 더 알맞고 향상된 가용 양극을 실현하는 것인데, 이 양극에서 양극 러그와 충전 부재 사이의 그립(grip) 점은 전해 정련에 사용된 양극 및 음극을 실질적으로 동시에 로드할 수 있기 위해 조절된다.
구리의 전해 정련을 위한 가용 양극에서는, 양극 주조시에 있어서, 전해 공정중 전해 탱크 내에서 양극을 매다는 양극 지지부에 브라켓을 설치하되, 양극 지지부로부터 멀어지는 방향으로 향한 상기 브라켓의 단부를 양극의 중앙선 쪽으로 또는 상기 중앙선의 가상적인 연장선 쪽으로 향하게 하는 것이 유리하다. 그리하여, 브라켓이 설치된 양극의 지지부는 전해 탱크내에 포함된 전해질의 액체 표면 위에서 실질적으로 전해 탱크 벽부로부터 먼 곳에서 발생하는 그리핑 부재의 운동을 이용하여 완전히 잡힐 수 있다. 본 발명에 따르면, 양극 지지부 내에 형성된 브라켓은, 전해질로 이송시, 전해 탱크로의 담글 때 및 꺼낼 때, 및 전해 탱크로부터 멀리 이송할 때, 상기 양극을 지지한다. 그리하여 상기 지지부는 양극이 전해 탱크 내에 잠겨있는 동안에만 양극을 지지한다.
전해 탱크 내에서 수행되는 구리의 전해 정련에 사용되는 전극, 즉 음극과 양극은 전해 공정 동안 전극의 중앙선을 기준으로 맞은 편에 위치한 두개의 독립된 지지부에 의해 전해 탱크의 벽부로부터 매달리기 때문에, 본 발명에 따른 양극에서 그립 브라켓은 양 지지부에 대해 독립적으로 형성되어, 지지부로부터 멀어지는 쪽으로 향한 브라켓 단부는 서로 마주보게 되는 것이 유리하다.
본 발명에 따르면, 양극 지지부에 형성된 브라켓은 상기 지지부로부터 멀어지는 쪽으로 향한 상기 브라켓 단부가 양극의 중앙선으로부터 멀어지는 쪽으로 향한 지지부의 단부와 실질적으로 같은 높이에 위치하도록 배치하는 것이 유리하다. 상기 브라켓은 그 전체 길이를 따라 지지부에 실질적으로 평행한 것이 유리하다. 상기 지지부로부터 멀어지는 쪽을 향한 브라켓의 단부는 양극 중앙선으로부터 멀어지는 쪽으로 향한 단부보다 높거나 또는 낮은 다른 높이에 위치할 수도 있다. 그 경우, 적어도 브라켓의 일부분은 상기 지지부에 대해 예각을 형성한다. 브라켓의 길이는 양극을 한 위치에서 다른 위치로 이송시키기 위해 충전 부재에 제공된 그리핑 부재에 의해 충분한 지지가 얻어지도록 하는 것이 유리하다. 또한, 본 발명에 따른 양극의 지지부에 설치된 브라켓은 상기 브라켓이 실질적으로 양극 중앙선에 대해 대칭이 되도록 놓인다.
양극의 지지부에 이송과 관련하여 그 양극을 매달기 위한 브라켓을 설치한 본 발명에 따른 전해 정련용 가용 양극을 사용하는 경우에는, 충전 부재에 설치되어 브라켓을 잡는 그리핑 부재는 양극 그리핑 부재에 대한 여유 공간이 보통 없는 양극과 음극 사이를 침투하는 것이 필요없기 때문에, 혼합된 양극 및 음극 하중을 충전부재에 의해 조작하기가 쉽다. 또한, 본 발명에 따른 브라켓이 설치된 양극은 잡힐 수 있어서 그리핑 부재에 대한 양극의 위치가 실질적으로 정확하게 조절될 수 있다. 또한, 브라켓을 잡는 그리핑 부재는 실질적으로 전해 탱크 벽부 및 벽부 상에 설치된 절연체를 갖는 도체 레일로부터 먼 곳에 놓여질 수 있어서, 적어도 약간의 잘못된 이동으로 인해 상기 그리핑 부재가 상기 벽부 또는 레일을 치는 일은 없다.
본 발명에 따른 양극 그립부에 형성된 브라켓 및 상기 브라켓을 잡는 그리핑 부재는 항상 전해 탱크 내에 포함된 전해질 위에 위치하므로, 본 발명에 따른 양극의 처리는 전해질 표면의 있을 수 있는 상승을 결코 제한하지 않는다. 전해질 표면을 상승시킴으로써, 전해 정련 플랜트의 투자비 및 운용비는 유리하게 절감될 수 있다. 그리하여, 예를 들어 양극 스크랩량은 독립된 그립 브라켓에 관계없이 감소된다. 또한, 그립 브라켓이 본 발명에 따른 양극 그립부에 사용되면, 전해 탱크 및 전극으로서 작용하는 음극과 양극의 상대 치수를 정의할 때 양극의 그리핑은 고려하지 않아도 된다.
본 발명은 본 발명의 바람직한 실시예의 정면도를 도시하는 첨부된 도면을 참조하여 하기에 더 상세히 기재된다.
도 1 에 따르면, 주조 구리 양극(1)에는, 주조와 관련하여 전해 탱크 내에서 발생하는 용해 공정 동안 양극을 매달기 위해 지지부(2)가 형성되어 있다. 또한, 주조와 관련하여, 상기 지지부(2)에는, 충전 부재에 연결되고 그런 것으로 알려진 그리핑 부재(도시되어 있지 않음)에 의해 양극을 이동시키는 동안 그 양극을 지지하기 위해, 그립 브라켓(3)이 설치되어 있다. 이와 더불어, 참조 부호 4 는 지지부로부터 멀어지는 쪽을 향한 그립 브라켓(3)의 단부를 나타내며, 참조 부호 5 는 양극으로부터 멀어지는 쪽을 향한 지지부(2)의 단부를 나타낸다.
Claims (11)
- 삭제
- 삭제
- 삭제
- 삭제
- 삭제
- 삭제
- 삭제
- 두개의 지지부(2)를 포함하며, 전해 공정시에 상기 지지부에 의해 전해 탱크 벽부에 대해 매달릴 수 있는 구리의 전해 정련용 양극(1)에 있어서, 상기 양극(1) 주조시, 양극 지지부(2)에는 상기 양극(1)을 잡기 위하여 및 양극을 한 위치에서 다른 위치로 이송할 때 상기 양극(1)을 지지하기 위하여 브라켓(3)이 형성되어 있으며, 상기 지지부(2)로부터 멀어지는 쪽으로 향한 브라켓(3)의 단부(4)는, 양극으로부터 멀어지는 쪽으로 향한 지지부(2)의 단부(5)와 실질적으로 같은 높이에 놓여 있는 것을 특징으로 하는 양극.
- 제 8 항에 있어서, 상기 브라켓(3)은, 지지부로부터 멀어지는 쪽으로 향한 상기 브라켓(3)의 단부(4)가, 상기 양극의 제 2 지지부(2)에 놓여 그 제 2 지지부로부터 멀어지는 쪽으로 향한 브라켓의 단부(4)를 향하도록 하여 형성되어 있는 것을 특징으로 하는 양극.
- 제 8 항 또는 제 9 항에 있어서, 상기 브라켓(3)이 전체 길이를 따라 상기 지지부(2)에 실질적으로 평행한 것을 특징으로 하는 양극.
- 제 8 항 또는 제 9 항에 있어서, 상기 지지부(2)에 형성된 상기 브라켓(3)은 상기 양극(1)의 중앙선에 대해 실질적으로 대칭 위치에 있는 것을 특징으로 하는 양극.