CN1260314C - 光固化沾顶漆 - Google Patents

光固化沾顶漆 Download PDF

Info

Publication number
CN1260314C
CN1260314C CN 03142036 CN03142036A CN1260314C CN 1260314 C CN1260314 C CN 1260314C CN 03142036 CN03142036 CN 03142036 CN 03142036 A CN03142036 A CN 03142036A CN 1260314 C CN1260314 C CN 1260314C
Authority
CN
China
Prior art keywords
paint
stained
present
pencil
photocuring
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN 03142036
Other languages
English (en)
Other versions
CN1580159A (zh
Inventor
罗建新
李继彪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China First Pencil Co ltd
Original Assignee
Chinese No1 Pencil Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chinese No1 Pencil Co Ltd filed Critical Chinese No1 Pencil Co Ltd
Priority to CN 03142036 priority Critical patent/CN1260314C/zh
Publication of CN1580159A publication Critical patent/CN1580159A/zh
Application granted granted Critical
Publication of CN1260314C publication Critical patent/CN1260314C/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

一种单组份光固化沾顶漆。它是以环氧丙烯酸树脂为活性齐聚物、三羟甲基丙烷三丙烯酸酯为活性稀释剂,另加3136醇酸树脂和光敏剂等配制而成。由于配方合理,特别是选用了光敏材料,该漆受光照后固化速度快,效果好,顶部丰满,且附着力好,没有剥落现象。沾于细长杆状物如铅笔的顶部后,在紫外线光照下,仅需20秒即可固化,大大缩短了干燥时间,且不受天气湿度的影响,只要再沾一次所需要的颜色漆即可完成,提高了铅笔的表面质量和生产效率。本发明配方中加入3136醇酸树脂,既可提高漆料与被涂物间的结合力,又可有利于降低产品成本。

Description

光固化沾顶漆
所属技术领域
本发明涉及以其物理性质为特征的涂料组合物,且更具体的是涉及一种光固化沾顶漆。
背景技术
已有技术对细长杆状物,例如铅笔的顶部施于涂复时,即铅笔制造过程中的沾顶工艺,都是采用传统的硝基漆,采用这种油漆时,整个沾顶工艺需分三次完成,每次沾顶后必须待油漆干燥后才能进行下一道的沾顶工序,但硝基漆的干燥时间较长,平均每次约需要2小时。如果遇到较潮湿的天气,室内湿度较高,不但干燥所需的时间更长,还会影响到沾顶的质量。
发明内容
为了克服已有技术存在的缺点,本发明提供一种单组份的光固化沾顶漆。它是由活性齐聚物、活性稀释剂、光敏剂、树脂等配制而成。该沾顶漆具有固化速度快,约在30分钟至1小时之间,即可干燥;漆的附着力好,被沾细木杆状物件,如铅笔的顶部沾漆丰满,且无剥落现象,具有高效优质的优异效果。
本发明所述光固化沾项漆按下列配方组成:
  组成物   重量百分比(%)
  活性齐聚物   27~40
  活性稀释剂   40~53
  树脂   20
在按上述配制而成的组成物中,另再加入相当于上述组成物总量1~2%的光敏剂。
上述配方中各组成物都为市售商品。
活性齐聚物为市售的环氧丙烯酸树脂,它是光固化漆最主要的成分,受光作用后能固化。
活性稀释剂为市售的三羟甲基丙烷三丙烯酸酯(简称TMPTA)、三丙二醇二丙烯酸酯(简称TPGDA)中的一种或一种以上的混合物。它是一种粘度降低剂。
树脂为市售的3136醇酸树脂,其既与木材有较好的结合力,又可有利于降低成本。光敏剂为市售的2-羟基-2-甲基-1-苯基-1-丙酮、1-羟基-环己基-苯基甲酮中的一种或一种以上的混合物。它是激发分子,在紫外光线的照射下,产生电子跃迁,处于激发状态,紧接着分解自由基,引发单体和预聚合,是光化学反应的必要条件。
本发明的有益效果是,采用合理科学的配方,克服了已有技术中存在的缺点,所述的光固化沾顶漆,光照后固化速度快,效果好,顶部丰满,且附着力好,没有剥落现象。沾于细长杆状物如铅笔的顶部后,在紫外线光照下,仅需20秒即可固化,大大缩短了干燥时间,且不受天气湿度的影响,只要再沾一次所需要的颜色漆即可完成,提高了铅笔的表面质量和生产效率。
具体实施方式
下面的实施例将对本发明作进一步的阐述,可以更加完整地理解本发明和看到本发明的优点,但并不限制本发明的范围。
  实施例1   实施例2   实施例3
  环氧丙烯酸树脂   32   27   40
  三羟甲基丙烷三丙烯酸酯(TMPTA)   48   53   40
  3136醇酸树脂   20   20   20
  光敏剂(另加)   1   1   1
按此配方配制的光固化沾顶漆,光照后漆的固化速度快,效果好,顶部丰满,且附着力好,没有剥落现象。使用本发明光固化沾顶漆的铅笔,固化后可立刻沾所需颜色的铅笔漆,此时所涂复的颜色油漆约在30分钟到1小时之间即可干燥,这样不仅提高了铅笔质量,而且还大大提高了铅笔生产效率。
光固化沾顶漆的粘度会随着季节的变化而变化。为此,在冬季应增加稀释剂以降低光固化沾顶漆的粘度,在夏季应增加树脂含量以提高光固化沾顶漆的粘度。同时为了提高光固化沾顶漆的附着力和降低产品的成本,产品配方中选用了20%的3136醇酸树脂。

Claims (3)

1.一种光固化沾顶漆,其特征在于按下列配方组成:
组成物重量                 百分比(%)
活性齐聚物                 27~40
活性稀释剂                 40~53
树脂                       20;
所述的活性齐聚物为环氧丙烯酸树脂,所述的树脂为3136醇酸树脂;
另加入相当于上述组成物总量1~2%的光敏剂。
2.按权利要求1所述的光固化沾顶漆,其特征在于:所述的活性稀释剂为三羟甲基丙烷三丙烯酸酯、三丙二醇二丙烯酸酯中的一种或一种以上的混合物。
3.按权利要求1所述的光固化沾顶漆,其特征在于:所述的光敏剂为2-羟基-2-甲基-1-苯基-1-丙酮和1-羟基-环己基-苯基甲酮中的一种或一种以上的混合物。
CN 03142036 2003-08-04 2003-08-04 光固化沾顶漆 Expired - Lifetime CN1260314C (zh)