CN117083404A - 超临界水利用装置用钛合金 - Google Patents
超临界水利用装置用钛合金 Download PDFInfo
- Publication number
- CN117083404A CN117083404A CN202280025108.9A CN202280025108A CN117083404A CN 117083404 A CN117083404 A CN 117083404A CN 202280025108 A CN202280025108 A CN 202280025108A CN 117083404 A CN117083404 A CN 117083404A
- Authority
- CN
- China
- Prior art keywords
- sample
- based material
- supercritical water
- crucible
- test
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B01—PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
- B01J—CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B01J3/00—Processes of utilising sub-atmospheric or super-atmospheric pressure to effect chemical or physical change of matter; Apparatus therefor
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C1/00—Making non-ferrous alloys
- C22C1/02—Making non-ferrous alloys by melting
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C14/00—Alloys based on titanium
Landscapes
- Chemical & Material Sciences (AREA)
- Organic Chemistry (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Manufacture And Refinement Of Metals (AREA)
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2021052789 | 2021-03-26 | ||
| JP2021-052789 | 2021-03-26 | ||
| PCT/JP2022/012956 WO2022202740A1 (ja) | 2021-03-26 | 2022-03-22 | 超臨界水利用装置用チタン合金 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| CN117083404A true CN117083404A (zh) | 2023-11-17 |
Family
ID=83397385
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| CN202280025108.9A Pending CN117083404A (zh) | 2021-03-26 | 2022-03-22 | 超临界水利用装置用钛合金 |
Country Status (3)
| Country | Link |
|---|---|
| JP (1) | JPWO2022202740A1 (https=) |
| CN (1) | CN117083404A (https=) |
| WO (1) | WO2022202740A1 (https=) |
Citations (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2003027259A (ja) * | 2001-07-19 | 2003-01-29 | Hitachi Ltd | 超臨界水処理装置部材の耐食性表面改質方法 |
| JP2005137959A (ja) * | 2003-11-04 | 2005-06-02 | Japan Organo Co Ltd | 超臨界水反応装置 |
| CN102094136A (zh) * | 2010-12-09 | 2011-06-15 | 西安航天博诚新材料有限公司 | 一种眼镜架用纯钛丝材及其制造方法 |
| JP2012241241A (ja) * | 2011-05-20 | 2012-12-10 | Katsuyoshi Kondo | チタン材料およびその製造方法 |
| CN105899314A (zh) * | 2014-01-10 | 2016-08-24 | 近藤胜义 | 钛粉末材料、钛材以及氧固溶钛粉末材料的制备方法 |
| CN107881365A (zh) * | 2017-12-28 | 2018-04-06 | 宁波俐辰新能源有限公司 | 一种抗脆化钛合金及其制造方法 |
| JP2018104778A (ja) * | 2016-12-27 | 2018-07-05 | 勝義 近藤 | 焼結刃物素材およびその製造方法 |
| CN111918983A (zh) * | 2018-03-12 | 2020-11-10 | 三菱综合材料株式会社 | 钛基材、钛基材的制造方法及水电解用电极、水电解装置 |
Family Cites Families (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP2468912A1 (en) * | 2010-12-22 | 2012-06-27 | Sandvik Intellectual Property AB | Nano-twinned titanium material and method of producing the same |
| JP2012189725A (ja) * | 2011-03-09 | 2012-10-04 | Kobe Steel Ltd | Ti合金バリアメタルを用いた配線膜および電極、並びにTi合金スパッタリングターゲット |
| JP2012188691A (ja) * | 2011-03-09 | 2012-10-04 | Kobe Steel Ltd | Ti合金配線膜および電極、並びにTi合金スパッタリングターゲット |
| JP6436481B2 (ja) * | 2014-11-05 | 2018-12-12 | 国立研究開発法人海洋研究開発機構 | 耐圧容器、鋳型、容器側体及びその製造方法 |
| WO2018159774A1 (ja) * | 2017-03-01 | 2018-09-07 | 国立大学法人京都大学 | チタン箔またはチタン板の製造方法、ならびにカソード電極 |
-
2022
- 2022-03-22 WO PCT/JP2022/012956 patent/WO2022202740A1/ja not_active Ceased
- 2022-03-22 CN CN202280025108.9A patent/CN117083404A/zh active Pending
- 2022-03-22 JP JP2023509164A patent/JPWO2022202740A1/ja active Pending
Patent Citations (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2003027259A (ja) * | 2001-07-19 | 2003-01-29 | Hitachi Ltd | 超臨界水処理装置部材の耐食性表面改質方法 |
| JP2005137959A (ja) * | 2003-11-04 | 2005-06-02 | Japan Organo Co Ltd | 超臨界水反応装置 |
| CN102094136A (zh) * | 2010-12-09 | 2011-06-15 | 西安航天博诚新材料有限公司 | 一种眼镜架用纯钛丝材及其制造方法 |
| JP2012241241A (ja) * | 2011-05-20 | 2012-12-10 | Katsuyoshi Kondo | チタン材料およびその製造方法 |
| CN105899314A (zh) * | 2014-01-10 | 2016-08-24 | 近藤胜义 | 钛粉末材料、钛材以及氧固溶钛粉末材料的制备方法 |
| JP2018104778A (ja) * | 2016-12-27 | 2018-07-05 | 勝義 近藤 | 焼結刃物素材およびその製造方法 |
| CN107881365A (zh) * | 2017-12-28 | 2018-04-06 | 宁波俐辰新能源有限公司 | 一种抗脆化钛合金及其制造方法 |
| CN111918983A (zh) * | 2018-03-12 | 2020-11-10 | 三菱综合材料株式会社 | 钛基材、钛基材的制造方法及水电解用电极、水电解装置 |
Non-Patent Citations (2)
| Title |
|---|
| WAS等: "Corrosion and stress corrosion cracking in supercritical water", JOURNAL OF NUCLEAR MATERIALS, no. 371, 15 September 2007 (2007-09-15), pages 179 * |
| 辛湘杰等: "《钛的腐蚀、防护及工程应用》", 31 January 1988, 合肥:安徽科学技术出版社, pages: 202 - 206 * |
Also Published As
| Publication number | Publication date |
|---|---|
| WO2022202740A1 (ja) | 2022-09-29 |
| JPWO2022202740A1 (https=) | 2022-09-29 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Zhao et al. | Deformation behaviour and mechanisms during hot compression at supertransus temperatures in Ti-10V-2Fe-3Al | |
| Talling et al. | On the mechanism of superelasticity in Gum metal | |
| Motta et al. | Zirconium alloys for supercritical water reactor applications: Challenges and possibilities | |
| Semiatin et al. | Dynamic-coarsening behavior of an α/β titanium alloy | |
| Hosseini et al. | Development of a trimodal microstructure with superior combined strength, ductility and creep-rupture properties in a near alpha titanium alloy | |
| Wang et al. | Effects of specimen and grain size on electrically-induced softening behavior in uniaxial micro-tension of AZ31 magnesium alloy: Experiment and modeling | |
| Khan et al. | Compressive properties of Cu with different grain sizes: sub-micron to nanometer realm | |
| Wang et al. | Cold-rolled Ti-Al-V-Zr-Fe titanium alloy tubing with outstanding tensile properties | |
| Li et al. | Constitutive model and optimal processing parameters of TC17 alloy with a transformed microstructure via kinetic analysis and processing maps | |
| Illarionov et al. | Influence of phase composition on thermal expansion of Ti-0.4 Al, Ti-2.2 Al-2.5 Zr and Ti-3Al-2.5 V alloys | |
| MX2015003057A (es) | Procesamiento termomecanico de aleaciones de niquel-titanio. | |
| Liu et al. | Effects of Al addition on corrosion behavior and mechanical property of high-strength and high-elasticity Cu-20Ni-20Mn-0.3 Nb-0.3 Cr-0.3 Zr alloy | |
| Talha et al. | Long term and electrochemical corrosion investigation of cold worked AISI 316L and 316LVM stainless steels in simulated body fluid | |
| Li et al. | Influence of grain size on electrically assisted tensile behavior of Ti-6Al-4V alloy | |
| Kanyane et al. | Development of spark plasma sintered TiAlSiMoW multicomponent alloy: Microstructural evolution, corrosion and oxidation resistance | |
| Garip et al. | Hot corrosion behavior of Ti-48Al and Ti-48Al-2Cr intermetallic alloys produced by electric current activated sintering | |
| Tanaka et al. | Mechanical properties of 7475 aluminum alloy sheets with fine subgrain structure by warm rolling | |
| Yılmaz et al. | Effects of hot isostatic pressing and heat treatments on structural and corrosion properties of direct metal laser sintered parts | |
| Balasundar et al. | Mechanical, thermal, electrical, and corrosion properties of microwave-sintered Ti-0.8 Ni-0.3 Mo/TiB composites | |
| Anoop et al. | Stress corrosion cracking behavior of selective laser-melted M300 maraging steel in 3.5 wt.% NaCl solution | |
| Hou et al. | Mechanical properties and corrosion behavior of electron beam cold hearth melting high strength and high corrosion resistant Ti-0.3 Mo-0.8 Ni alloy with different states | |
| CN117083404A (zh) | 超临界水利用装置用钛合金 | |
| Xi et al. | Altered microstructure, phase transformation behaviors and shape memory response of CuAlMn shape memory alloys fabricated by selective laser melting | |
| Zhang et al. | Microstructural evolution during hot and cold deformation of Ti–36Nb–2Ta–3Zr–0.35 O alloy | |
| Li et al. | Investigation on ideal mechanical performance of laser direct energy deposited Ti–6Al–2Zr–1Mo–1V alloy without sub-β transus thermal cycles |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| PB01 | Publication | ||
| PB01 | Publication | ||
| SE01 | Entry into force of request for substantive examination | ||
| SE01 | Entry into force of request for substantive examination |