CN113152119A - Process for keeping luster of commercial knitted fabric after dyeing and fabric - Google Patents
Process for keeping luster of commercial knitted fabric after dyeing and fabric Download PDFInfo
- Publication number
- CN113152119A CN113152119A CN202110495174.XA CN202110495174A CN113152119A CN 113152119 A CN113152119 A CN 113152119A CN 202110495174 A CN202110495174 A CN 202110495174A CN 113152119 A CN113152119 A CN 113152119A
- Authority
- CN
- China
- Prior art keywords
- dyeing
- scutching
- fabric
- cloth
- cylinder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The embodiment of the invention discloses a method for keeping luster of a commercial knitted fabric in dyeing, which comprises the following steps: polishing the grey cloth in a cylinder, adding neutral polishing enzyme for treatment, and inactivating and cleaning; scutching, sizing and drying after scutching and squeezing, stabilizing the weight of the width, and keeping the cloth cover flat at a shrinkage rate of +/-3 percent; folding the nail edge to protect the front side, entering the cylinder, adding a moisture absorption and sweat releasing auxiliary agent when dyeing and washing the disperse dye, and taking the nail edge out of the cylinder when the soaping inspection fastness and the pH value meet the requirements; after dyeing, scutching, squeezing, scutching and shaping, and adding hydrophilic silicone oil and a stiffening agent; pre-shrinking and pressing the light; and (6) inspecting and packaging. The embodiment of the invention also discloses the fabric prepared by the method. The invention can effectively solve the defects of unsaturated two-side color and color of the commercial knitted fabric, solve the problem of physical damage laser mark, ensure difficult adsorption of the hair ash and has the advantages of smooth and soft hand-feeling extended surface.
Description
The application is a divisional application with application date of 2017, 03 and 01, application number of 201710115904.2 and invention name of 'a process and fabric for dyeing and maintaining luster of commercial knitted fabric'.
Technical Field
The invention relates to a garment fabric dyeing process, in particular to a method for keeping luster of a commercial knitted fabric after dyeing and the fabric.
Background
The prior business clothes adopt woven fabrics, and the elasticity of the knitted fabrics is better than that of the woven fabrics, so that the knitted fabrics are softer, comfortable, good in air permeability, good in fracture elongation and elastic recovery rate; in the dyeing and finishing process, the processing difficulty is higher, the cloth cover glossiness is good, the prior art exists as the surface fabric of business suit with knitted fabric, the current looped fabric processing technology that adopts is: the method comprises the following steps of splitting grey cloth, singeing, mercerizing, feeding the grey cloth into a cylinder for neutralization and washing, scutching and squeezing, drying, feeding the grey cloth into the cylinder for dyeing, polishing, treating with polishing enzyme, reducing and washing, dyeing cotton, soaping, scutching and squeezing, scutching and sizing, adding hand feeling, pre-shrinking and polishing, and inspecting and packaging, wherein the processing process has defects: after the singeing treatment, after the crystallization is generated due to the high-temperature singeing of the polyester fiber, the polyester fiber is orderly arranged, the saturation is reduced, the polyester fiber is dyed by the disperse dye to generate luster, and the polyester fiber and the cotton fiber are colored to form positive and negative color difference; the method is characterized in that silicone oil with enlarged molecular chains is subjected to scutching and sizing to form a film on the surface of the fabric, the film is easy to generate laser marks after being touched by hands, the interior of cotton fibers is easy to be damaged and the quality of the fabric is hard due to mercerization and polishing treatment in the production process, and the fabric is easy to scratch when running in a dye vat; the surface forms gloss after pre-compression polishing, and compared with the primary color difference, the color is lightened and unsaturated, dust is easily adsorbed, and the taking effect is influenced; poor reproducibility of dyeing each time, different coloring after cvc singeing, and the like.
Disclosure of Invention
The technical problem to be solved by the embodiment of the invention is to provide a method for keeping the gloss of commercial knitted fabric in dyeing. Can solve the defects of unsaturated two-side color and color, solve the problem of physical impact laser mark, ensure that the putty is not easy to be adsorbed, and ensure that the extended surface is smooth and soft.
In order to solve the technical problem, the embodiment of the invention provides a method for keeping the gloss of a commercial knitted fabric in dyeing, which comprises the following steps:
s1: polishing the grey cloth in a cylinder, adding neutral polishing enzyme for treatment, and inactivating and cleaning;
s2: scutching, sizing and drying after scutching and squeezing, stabilizing the weight of the width, and keeping the cloth cover flat at a shrinkage rate of +/-3 percent;
s3: folding the nail edge to protect the front side, entering the cylinder, adding a moisture absorption and sweat releasing auxiliary agent when dyeing and washing the disperse dye, and taking the nail edge out of the cylinder when the soaping inspection fastness and the pH value meet the requirements;
s4: after dyeing, scutching, squeezing, scutching and shaping, and adding hydrophilic silicone oil and a stiffening agent;
s5: pre-shrinking and pressing the light;
s6: and (6) inspecting and packaging.
Further, step S1 is preceded by a step of mercerizing the grey cloth, and step S1 includes a step of adding acid for neutralization.
Furthermore, the mercerization step uses the liquid caustic soda concentration of 24-26 DEG Be, the shrinkage is carried out at the temperature of 18-22 ℃, and the speed is 18-24 m/min.
Furthermore, the unit of activity of the neutral polishing enzyme is 2000, and the dosage of the neutral polishing enzyme is 0.3-0.4%.
Further, the moisture absorption and sweat releasing auxiliary agent of the step S3 is added into the cloth in an amount of 1-1.5%, the temperature is kept at 130 +/-2 ℃, and the action time is 30-45 min.
Furthermore, the step S3 also comprises the steps of reacting 2-2.5g/L of sodium hydrosulfite with 4-5g/L of soda ash at 80 +/-5 ℃ for 20-25min, reducing and washing the cotton.
Furthermore, the step S3 further includes adding 1% -1.5% of the softening agent into the bath after the color is matched.
Furthermore, in the step S2, water drying is carried out at 180 +/-5 ℃, the width gram weight is stabilized, and the cloth surface is kept flat and taken off the machine with the shrinkage rate of less than or equal to 3 percent.
Furthermore, the hydrophilic silicone oil added in step S4 is 4% + -0.5% of the weight of the cloth, 1% + -0.5% of the stiffening agent, and the mixed solution of the two is input into a rolling groove and processed at the temperature of 150 +/-3 ℃, the rolling pressure of 2.5kg +/-0.5 kg, the speed of 18 +/-2 m/min and the air volume of 80%.
The embodiment of the invention also discloses the fabric manufactured by the method for dyeing and maintaining the luster of the commercial knitted fabric.
The embodiment of the invention has the following beneficial effects: the invention can effectively solve the defects of unsaturated two-side color and color of the commercial knitted fabric, solve the problem of physical damage laser marks, ensure that the textile fabric is not easy to adsorb the putty, and has the advantages of extended and soft handfeel.
Detailed Description
In order to make the objects, technical solutions and advantages of the present invention more apparent, the present invention will be described in further detail below.
The method for keeping the gloss of the commercial knitted fabric in the dyeing process comprises the following process steps: the method comprises the following steps of splitting a grey cloth, mercerizing, polishing in a cylinder, scutching and squeezing, drying, sewing edge protection of the front face, dyeing and washing, reduction cleaning, dyeing cotton, soaping, scutching and squeezing, scutching and sizing, pre-shrinking and press polishing, inspecting and packaging.
The specific operation steps are as follows:
1. splitting and coiling during grey cloth weaving and cropping: and (5) unfolding the package to reduce the crease in the grey cloth.
2. The mercerizing process of each batch is uniform and stable, standard operation specifications are established, the concentration of the liquid caustic soda is 24-26 degrees Be, and the speed is 22 +/-2 m/min. The fabric is contracted in concentrated alkaline liquid at the temperature of 18-22 ℃ at the speed of 18-24m/min, a four-roller tension water tank is adopted to keep the plane of the fabric relaxed and unfolded, the fabric is washed with hot water at the temperature of 60 ℃, and then the fabric passes through a rubber roller pressing and sucking machine, so that the fabric gloss is improved, the internal stress is eliminated, the size stability is good, the dye adsorption capacity is high, the fabric flatness is high, and the strength and extensibility wearability are changed; and the weight of the door width of the machine entering and exiting is recorded, so that the control of the specification of the finished product is facilitated.
3. Polishing the grey cloth in a cylinder, carrying out acid neutralization (acetic acid HAc, 1g/L) after mercerizing by using alkali lye, carrying out neutral polishing after washing the cloth, polishing the cloth by using 0.3-0.4% of neutral polishing enzyme (Novien) activity unit 2000-2200, removing surface hairiness without damaging fiber strength, detecting that bursting strength is more than or equal to 300N, inactivating and cleaning (soda Na)2CO30.5g/L), detecting the pH value to be 6-7.5, and taking out of the cylinder; and the impurities such as the hair ash on the cloth surface are cleaned separately from dyeing, and then the impurities enter the subsequent working procedure, so that the phenomena of uneven dyeing and the like caused by the hair ash impurities and the dyeing in one bath are reduced.
Preferably, the softening agent is added into a bath for boiling the cloth in a jar, the weight of the cloth is 1 percent, the cloth is neutralized, washed and polished, and then the cloth is taken out of the jar after being inactivated by soda ash, so that the abrasion of the cloth hair and the cloth in the jar is reduced.
4. And (3) scutching, shaping, drying by water at 180 +/-5 ℃, stabilizing the width gram weight, and keeping the cloth cover flat at the shrinkage rate of less than or equal to 3%.
5. Folding the nail edge to protect the front surface, putting the nail edge into a vat to protect the front cloth and reduce the abrasion of the front surface of the cloth and the vat in the running process, adding a moisture absorption and sweat releasing auxiliary agent (nonionic high polymer polyester type dispersion liquid) when a high-fastness disperse dye (an Nuo brand PUD series) is selected for dyeing and washing, softening the fabric and reducing the abrasion mark generated by the friction in the vat; 2g/L of sodium hydrosulfite and 4g/L of soda, reducing and cleaning at 85 ℃/20min, detecting fastness OK, dyeing cotton again, ensuring surface phase color difference, forming full color, and taking out of the vat when pH value of soaping and detecting fastness and the like meet requirements.
Adding a moisture-absorbing and sweat-releasing auxiliary agent 1% (based on the weight of the cloth) into the dyeing and washing process, carrying out one-bath treatment at 130 ℃ for 30-45min to soften the polyester fiber and reduce the friction in the dyeing and washing process, reducing and washing cotton by using 2g/L of sodium hydrosulfite and 4g/L of soda at 80 ℃/20min, carrying out soaping and adding into the bath for softening by 1% after the color is OK, and reducing the friction in the dyeing and washing process.
6. The fabric is dyed, then scutching, water-squeezing, scutching and sizing are carried out, Delume hydrophilic silicone oil DM-1274 (4% +/-0.5% of the weight of the fabric) is added, the antistatic property and the comfort of the fabric are improved, simultaneously Delume stiffening agent DM-3568 is added, 1% +/-0.5% (of the weight of the fabric) is added, the water is added into a material barrel before sizing by three times, the stiffening agent DM-3568 is added and stirred uniformly while adding, then the hydrophilic silicone oil DM-1274 is added, the mixture is input into a rolling groove after being uniformly dissolved, the sizing process is set, the temperature is 150 +/-3 ℃, the rolling pressure is 2.5 +/-0.5 kg, the speed is 18 +/-2 m/min, and the air volume is 80%, and after the process is subjected to crosslinking, the effect of good straightening elasticity is achieved, meanwhile, the hydrophilicity is good, and the purpose of preventing the hair from being adsorbed.
7. Pre-calendering: after pre-shrinking and press polishing, the fabric has the advantages of increased surface gloss, better hand feeling and good shrinkage.
8. And (3) inspecting and packaging: and finally, the finished product is qualified in terms of breadth, gram weight, shrinkage, pH value, fastness to washing and the like before packaging, and is packaged and put in storage.
In the process, compared with the woven fabric, the process of singeing is reduced, the cost is saved, and the phenomenon that polyester fiber molecules are orderly arranged to generate luster due to high-temperature singeing is avoided, so that two-side color is formed.
Through the process, the fabric processed by the method for dyeing and keeping the luster of the commercial knitted fabric can be obtained.
While the invention has been described in connection with what is presently considered to be the most practical and preferred embodiment, it is to be understood that the invention is not to be limited to the disclosed embodiment, but on the contrary, is intended to cover various modifications and equivalent arrangements included within the spirit and scope of the appended claims.
Claims (2)
1. A method for keeping luster of commercial knitted fabric in dyeing is characterized by comprising the following steps:
s1: carrying out mercerizing on the grey cloth, and adding acid for neutralization after finishing mercerizing; in the mercerizing step, the concentration of liquid caustic soda is 24-26 degrees Be, the shrinkage is carried out at the temperature of 18-22 ℃, and the speed is 18-24 m/min; the acid is acetic acid;
s2: polishing the grey cloth in a cylinder, adding neutral polishing enzyme for treatment, and inactivating and cleaning, wherein the neutral polishing enzyme has the activity unit of 2000 and the using amount of 0.3-0.4%; the reagent for inactivation and cleaning is soda ash;
s3: scutching, sizing and drying after scutching and squeezing, stabilizing the weight of the width, and keeping the cloth cover flat at a shrinkage rate of +/-3 percent; the drying is carried out by water drying at 180 +/-5 ℃;
s4: folding the nail edge protection front into a cylinder, adding a moisture absorption and sweat releasing auxiliary agent when dyeing the disperse dyes, reacting for 20min at 80 ℃ by using 2g/L of sodium hydrosulfite and 4g/L of soda, adding 1% of a softening agent in a bath after the color of the dyed cotton meets the requirement, and taking the dyed cotton out of the cylinder when the soaping inspection fastness and the pH value meet the requirement; the moisture absorption and sweat releasing auxiliary agent accounts for 1 percent of the weight of the cloth, the temperature is kept at 130 ℃, and the action time is 30-45 min;
s5: dyeing, scutching, squeezing, scutching and shaping, adding hydrophilic silicone oil, namely 4% +/-0.5% of the weight of the cloth, 1% +/-0.5% of a stiffening agent, and inputting a mixed solution of the two into a rolling groove, and processing at the temperature of 150 +/-3 ℃, the rolling pressure of 2.5kg +/-0.5 kg, the speed of 18 +/-2 m/min and the air volume of 80%; the hydrophilic silicone oil is German hydrophilic silicone oil DM-1274; the stiffening agent is a German stiffening agent DM-3568;
s6: pre-shrinking and pressing the light;
s7: and (6) inspecting and packaging.
2. A commercial knitted fabric produced by the method of claim 1 for dyeing and maintaining gloss.