CN113123148A - Preparation method of fox fur-imitated real silk fabric - Google Patents

Preparation method of fox fur-imitated real silk fabric Download PDF

Info

Publication number
CN113123148A
CN113123148A CN202110494423.3A CN202110494423A CN113123148A CN 113123148 A CN113123148 A CN 113123148A CN 202110494423 A CN202110494423 A CN 202110494423A CN 113123148 A CN113123148 A CN 113123148A
Authority
CN
China
Prior art keywords
fabric
fox
silk
temperature
wool
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN202110494423.3A
Other languages
Chinese (zh)
Inventor
孙源癸
刘科江
王勇
苏诗越
庄南枫
谭志聪
覃天宋
曾静观
吴昊晟
郭丽娜
谭海岚
杜艺
曾晓金
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Huzhou Golden Seal Silk Technology Co ltd
Guangzhou Panyu Polytechnic
Original Assignee
Huzhou Golden Seal Silk Technology Co ltd
Guangzhou Panyu Polytechnic
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Huzhou Golden Seal Silk Technology Co ltd, Guangzhou Panyu Polytechnic filed Critical Huzhou Golden Seal Silk Technology Co ltd
Priority to CN202110494423.3A priority Critical patent/CN113123148A/en
Publication of CN113123148A publication Critical patent/CN113123148A/en
Pending legal-status Critical Current

Abstract

The invention discloses a preparation method of a fox fur-like real silk fabric, which comprises the following steps: cleaning: soaking and cleaning silk, and air-drying after cleaning; weaving: twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain warp threads, twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain weft threads, and weaving the warp threads and the weft threads to obtain a semi-finished fabric; dyeing: putting the semi-finished fabric into a dye vat, adding a dye, soaking and dyeing for 24-36min at the temperature of 130-; soaking: putting the dyed fabric into a dye vat without dye, adding an antistatic agent, a softening agent and a fluffing agent, soaking for 20-40min at the temperature of 55-65 ℃, and then drying; the preparation method of the fox fur-like real silk fabric can realize the preparation of the fox fur-like real silk fabric, reduce the production cost of products, has lower price and can meet the popular requirements.

Description

Preparation method of fox fur-imitated real silk fabric
Technical Field
The invention relates to the field of fabric processing, in particular to a preparation method of a fox fur-like real silk fabric.
Background
The weaving principle is a general name taken from spinning and weaving, but with the continuous development and perfection of a weaving knowledge system and a subject system, particularly after non-woven textile materials and three-dimensional composite weaving and other technologies are produced, the fabrics for clothing, industry and decoration are produced by not only traditional hand spinning and weaving but also non-woven fabric technology, modern three-dimensional weaving technology, modern electrostatic nano-net forming technology and the like, so that modern weaving refers to a multi-scale structure processing technology of fibers or fiber aggregates, more and more people start to pursue fashion of clothing in life, various fabrics and clothing of animal hair start to appear, and the clothing of the fabrics is expensive and cannot meet the requirements of most people.
Disclosure of Invention
The invention aims to overcome the defects in the prior art, provides the preparation method of the fox fur-like real silk fabric, can realize the preparation of the fox fur-like real silk fabric, reduces the production cost of products, has low price, can meet the popular requirements, and can effectively solve the problems in the background art.
In order to achieve the purpose, the invention provides the following technical scheme: a preparation method of a fox fur-imitated real silk fabric comprises the following steps:
1) soaking and cleaning silk, and air-drying after cleaning;
2) twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain warp threads, twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain weft threads, and weaving the warp threads and the weft threads to obtain a semi-finished fabric;
3) dyeing: putting the semi-finished fabric into a dye vat, adding a dye, soaking and dyeing for 24-36min at the temperature of 130-;
4) soaking: putting the dyed fabric into a dye vat without dye, adding an antistatic agent, a softening agent and a fluffing agent, soaking for 20-40min at the temperature of 55-65 ℃, and then drying;
5) shaping: adopting a compound of polyurethane and N-methylol compound resin as a cross-linking non-ironing agent, controlling the baking temperature to be 145-155 ℃, controlling the baking time to be 6-8min, and brushing and ironing after shaping;
6) printing: printing the fur tips in a roller printing mode, wherein the printing temperature is 45-55 ℃, washing the fabric by using clear water, and drying after washing;
7) and (3) fixation: soaking the cleaned fabric in a color-fixing soft solution for 5-15min, and then heating;
8) and (3) after finishing: shaping, brushing and ironing the fabric again to obtain a finished fabric;
as a preferred technical scheme of the invention, when the silk is soaked and cleaned, the soaking time is 60-80min, and the temperature of clean water used for cleaning is 40-60 ℃.
As a preferred technical scheme of the invention, in the after-treatment, the ironing temperature is 200-210 ℃, and the fiber of the cotton layer is straightened.
As a preferred technical scheme of the invention, in the color fixing process, the fabric is conveyed and heated in a tunnel furnace, and the heating temperature of the tunnel furnace is 70-90 ℃.
As a preferred technical scheme of the invention, when the dyed real silk fabric is cleaned, water with the temperature of 30-40 ℃ is used for cleaning, and the cleaning time is 8-10 min.
As a preferred technical scheme of the invention, the content of the softening agent adopted in the color fixing softening solution is 2-3g/L, and the content of the color fixing agent is 3-5 g/L.
As a preferred technical scheme of the invention, when the printed fabric is washed, the temperature of clear water is 40-50 ℃, and the washing time is 10-12 min.
Compared with the prior art, the invention has the beneficial effects that: the preparation method of the fox fur-imitated real silk fabric has the following advantages:
1. the fabric prepared by the invention combines the functionality of the cotton fiber and the silk, has better hygroscopicity and air permeability, high glossiness, smooth and soft hand feeling and comfortable wearing, improves the integral aesthetic feeling, and is more similar to the texture of fox hair.
2. The mode that utilizes roller stamp prints to the hair point, can further improve the fidelity, heats the fixation after the stamp, can effectively improve the colour fastness of hair point colour, avoids losing colour.
3. The fox wool-like silk fabric prepared by the method is low in manufacturing cost, further reduces the manufacturing cost of clothes, is suitable for the consumption concept of most people, and meets the requirement of popularization on fashion of clothes.
Drawings
FIG. 1 is a flow chart of a preparation method of the fox-fur-like silk fabric.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.
The invention provides the following technical scheme:
the first embodiment is as follows: a preparation method of a fox fur-imitated real silk fabric comprises the following steps:
1) soaking and cleaning silk, and air-drying after cleaning, wherein the soaking time is 60min, and the temperature of clean water used for cleaning is 40 ℃;
2) twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain warp threads, twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain weft threads, and weaving the warp threads and the weft threads to obtain a semi-finished fabric;
3) dyeing: putting the semi-finished fabric into a dye vat, adding a dye, soaking and dyeing for 24min at 130 ℃, cleaning the dyed real silk fabric with clear water, and cleaning with water at 30 ℃ for 8 min;
4) soaking: putting the dyed fabric into a dye vat without dye, adding an antistatic agent, a softening agent and a fluffing agent, soaking for 20min at the temperature of 55 ℃, and then drying;
5) shaping: the method comprises the following steps of (1) adopting a compound of polyurethane and N-methylol compound resin as a crosslinking non-ironing agent, controlling the baking temperature to be 145 ℃, baking for 6min, brushing and ironing after shaping, wherein the ironing temperature is 200 ℃, and straightening the fibers of a cotton layer;
6) printing: printing the fur tips by adopting a roller printing mode, wherein the printing temperature is 45 ℃, washing the fabric by using clean water, drying after washing, and washing the printed fabric at the clean water temperature of 40 ℃ for 10 min;
7) and (3) fixation: soaking the cleaned fabric in a color fixing soft solution for 5min, and then heating, wherein in the color fixing process, the fabric is conveyed and heated in a tunnel furnace, the heating temperature of the tunnel furnace is 70-90 ℃, the content of a softening agent adopted in the color fixing soft solution is 2g/L, and the content of the color fixing agent is 3 g/L;
8) and (3) after finishing: and (5) shaping, brushing and polishing the fabric again to obtain the finished fabric.
Example two: a preparation method of a fox fur-imitated real silk fabric comprises the following steps:
1) soaking and cleaning silk, and air-drying after cleaning, wherein the soaking time is 70min, and the temperature of clean water used for cleaning is 50 ℃;
2) twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain warp threads, twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain weft threads, and weaving the warp threads and the weft threads to obtain a semi-finished fabric;
3) dyeing: putting the semi-finished fabric into a dye vat, adding a dye, soaking and dyeing for 30min at 132 ℃, cleaning the dyed real silk fabric with clear water, and cleaning with water at 35 ℃ for 9 min;
4) soaking: putting the dyed fabric into a dye vat without dye, adding an antistatic agent, a softening agent and a fluffing agent, soaking for 30min at the temperature of 60 ℃, and then drying;
5) shaping: the method comprises the following steps of (1) adopting a compound of polyurethane and N-methylol compound resin as a crosslinking non-ironing agent, controlling the baking temperature to be 150 ℃, baking for 7 min, brushing and ironing after shaping, wherein the ironing temperature is 205 ℃, and straightening the fibers of a cotton layer;
6) printing: printing the fur tips by adopting a roller printing mode, wherein the printing temperature is 50 ℃, washing the fabric by using clean water, drying after washing, and washing the printed fabric, wherein the temperature of the clean water is 45 ℃, and the washing time is 11 min;
7) and (3) fixation: soaking the cleaned fabric in a color fixing soft solution for 10min, and then heating, wherein in the color fixing process, the fabric is conveyed and heated in a tunnel furnace, the heating temperature of the tunnel furnace is 80 ℃, the content of the adopted softening agent is 2.5g/L, and the content of the color fixing agent is 4 g/L;
8) and (3) after finishing: and (5) shaping, brushing and polishing the fabric again to obtain the finished fabric.
Example three: a preparation method of a fox fur-imitated real silk fabric comprises the following steps:
1) soaking and cleaning silk, and air-drying after cleaning, wherein the soaking time is 80min, and the temperature of clean water used for cleaning is 60 ℃;
2) twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain warp threads, twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain weft threads, and weaving the warp threads and the weft threads to obtain a semi-finished fabric;
3) dyeing: putting the semi-finished fabric into a dye vat, adding a dye, soaking and dyeing for 36min at 135 ℃, cleaning the dyed real silk fabric with clear water, and cleaning with water at 40 ℃ for 10 min;
4) soaking: putting the dyed fabric into a dye vat without dye, adding an antistatic agent, a softening agent and a fluffing agent, soaking for 40min at 65 ℃, and then drying;
5) shaping: the method comprises the following steps of (1) adopting a compound of polyurethane and N-methylol compound resin as a crosslinking non-ironing agent, controlling the baking temperature to be 155 ℃, baking for 8min, brushing and ironing after shaping, and straightening the fibers of a cotton layer at the ironing temperature of 210 ℃;
6) printing: printing the fur tips by adopting a roller printing mode, wherein the printing temperature is 55 ℃, washing the fabric by using clean water, drying after washing, and washing the printed fabric, wherein the temperature of the clean water is 50 ℃, and the washing time is 12 min;
7) and (3) fixation: soaking the cleaned fabric in a color fixing soft solution for 15min, and then heating, wherein in the color fixing process, the fabric is conveyed and heated in a tunnel furnace, the heating temperature of the tunnel furnace is 790 ℃, the content of the adopted softening agent is 3g/L, and the content of the color fixing agent is 5 g/L;
8) and (3) after finishing: and (5) shaping, brushing and polishing the fabric again to obtain the finished fabric.
Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that changes, modifications, substitutions and alterations can be made in these embodiments without departing from the principles and spirit of the invention, the scope of which is defined in the appended claims and their equivalents.

Claims (7)

1. A preparation method of a fox fur-imitated real silk fabric is characterized by comprising the following steps of:
1) cleaning: soaking and cleaning silk, and air-drying after cleaning;
2) weaving: twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain warp threads, twisting silk and cotton fibers according to the weight ratio of 2:1 to obtain weft threads, and weaving the warp threads and the weft threads to obtain a semi-finished fabric;
3) dyeing: putting the semi-finished fabric into a dye vat, adding a dye, soaking and dyeing for 24-36min at the temperature of 130-;
4) soaking: putting the dyed fabric into a dye vat without dye, adding an antistatic agent, a softening agent and a fluffing agent, soaking for 20-40min at the temperature of 55-65 ℃, and then drying;
5) shaping: adopting a compound of polyurethane and N-methylol compound resin as a cross-linking non-ironing agent, controlling the baking temperature to be 145-155 ℃, controlling the baking time to be 6-8min, and brushing and ironing after shaping;
6) printing: printing the fur tips in a roller printing mode, wherein the printing temperature is 45-55 ℃, washing the fabric by using clear water, and drying after washing;
7) and (3) fixation: soaking the cleaned fabric in a color-fixing soft solution for 5-15min, and then heating;
8) and (3) after finishing: and (5) shaping, brushing and polishing the fabric again to obtain the finished fabric.
2. The preparation method of the fox-wool-like silk fabric according to claim 1, wherein the fox-wool-like silk fabric is prepared by the following steps: when the silk is soaked and cleaned, the soaking time is 60-80min, and the temperature of clean water used for cleaning is 40-60 ℃.
3. The preparation method of the fox-wool-like silk fabric according to claim 1, wherein the fox-wool-like silk fabric is prepared by the following steps: in the post-finishing, the ironing temperature is 200-210 ℃, and the fiber of the cotton layer is straightened.
4. The preparation method of the fox-wool-like silk fabric according to claim 1, wherein the fox-wool-like silk fabric is prepared by the following steps: in the color fixing process, the fabric is conveyed and heated in a tunnel furnace, and the heating temperature of the tunnel furnace is 70-90 ℃.
5. The preparation method of the fox-wool-like silk fabric according to claim 1, wherein the fox-wool-like silk fabric is prepared by the following steps: and when the dyed real silk fabric is cleaned, cleaning the real silk fabric by using water at the temperature of 30-40 ℃ for 8-10 min.
6. The preparation method of the fox-wool-like silk fabric according to claim 1, wherein the fox-wool-like silk fabric is prepared by the following steps: in the color fixing softening solution, the content of the adopted softening agent is 2-3g/L, and the content of the color fixing agent is 3-5 g/L.
7. The preparation method of the fox-wool-like silk fabric according to claim 1, wherein the fox-wool-like silk fabric is prepared by the following steps: when the printed fabric is washed, the temperature of clear water is 40-50 ℃, and the washing time is 10-12 min.
CN202110494423.3A 2021-05-07 2021-05-07 Preparation method of fox fur-imitated real silk fabric Pending CN113123148A (en)