CN113021556A - Sandstone texture painting board treatment process - Google Patents

Sandstone texture painting board treatment process Download PDF

Info

Publication number
CN113021556A
CN113021556A CN202110347382.5A CN202110347382A CN113021556A CN 113021556 A CN113021556 A CN 113021556A CN 202110347382 A CN202110347382 A CN 202110347382A CN 113021556 A CN113021556 A CN 113021556A
Authority
CN
China
Prior art keywords
treatment
wood
cleaning
grinding
steps
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN202110347382.5A
Other languages
Chinese (zh)
Other versions
CN113021556B (en
Inventor
黄宗杰
张玉坡
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhengzhou Institute of Technology
Original Assignee
Zhengzhou Institute of Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhengzhou Institute of Technology filed Critical Zhengzhou Institute of Technology
Priority to CN202110347382.5A priority Critical patent/CN113021556B/en
Publication of CN113021556A publication Critical patent/CN113021556A/en
Application granted granted Critical
Publication of CN113021556B publication Critical patent/CN113021556B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a sandstone texture painting board treatment process, which specifically comprises the following steps: the method comprises the following steps: spraying and cleaning the surface; step two: tailoring treatment; step three: performing seam cleaning treatment; step four: seamless processing; step five: performing anti-fouling treatment on the seam; step six: carrying out primary grinding treatment; step seven: cleaning the board surface; step eight: carrying out middle grinding treatment; step nine: repairing again; step ten: repairing holes, edge cracks and damages; step eleven: grinding corners; step twelve: fine grinding treatment; step thirteen: disease-resistant treatment; fourteen steps: and (5) polishing and crystallizing. The invention has the technical effects of stronger adaptability, complete system and capability of manufacturing the high-quality sandstone texture painting plate.

Description

Sandstone texture painting board treatment process
Technical Field
The invention relates to the technical field of painting board processing, in particular to a sandstone texture painting board processing technology.
Background
With the continuous development of economy, the living and aesthetic level of people is continuously improved, and decorative pictures are often used to decorate the wall surface when hotels and residences are decorated, so that the appearance of the wall surface is of a high grade. The existing decorative painting is mostly canvas and paperboard painting, the canvas and the paperboard painting are directly drawn on cloth or paper, and due to the fact that the canvas and the paperboard painting are hung on a wall, the cloth or the paper is prone to being affected with damp for a long time, when the cloth or the paper is affected with damp, the painting on the canvas or the paper is prone to fading, and is prone to yellowing and deformation for a long time, the grade is low, the canvas and the paperboard painting are planar, and no three-dimensional effect exists. And the painting is directly drawn on cloth or paper, so that the painting is not easy to wipe after being dirty and is not resistant to dirt. Therefore, sandstone texture paintings are more and more favored by people, a sandstone texture painting plate needs to be used before the sandstone texture paintings are manufactured, and the quality of the sandstone texture painting plate directly influences the quality of the sandstone texture painting; the prior sandstone texture painting plate has the advantages of simple treatment process, poorer adaptability, no complete treatment process and flaw in the quality of the treated sandstone texture painting plate.
Therefore, the invention has strong adaptability, complete system and great need for manufacturing the high-quality sandstone texture painting plate.
Disclosure of Invention
The invention aims to provide a sandstone texture painting plate treatment process to solve the problems in the background art.
In order to realize the purpose, the invention provides the following technical scheme: a sandstone texture painting board treatment process specifically comprises the following steps:
the method comprises the following steps: surface spraying and cleaning: firstly, cleaning with clear water, then cleaning with weak base cleaning liquid, and then cleaning with weak acid cleaning liquid;
step two: tailor treatment: performing tailoring treatment on the sandstone texture painting plate according to the conditions that a seam needs to be straight, a seam opening needs to be thin, and the surface of a wood plate cannot be broken, wherein the thickness of a cutting piece is 0.1-0.3;
step three: and (3) seam cleaning treatment: cleaning the seam with a dust collector or a brush, and scraping the seam with a blade;
step four: seamless processing: selecting liquid repairing glue to perform glue repairing treatment on the seam, ensuring full filling, and standing and solidifying by taking the bulge as a standard;
step five: and (3) seam anti-fouling treatment: uniformly coating an anti-fouling agent and an anti-coking agent on the seam of the wood of the sandstone texture painting board, wherein the coating is performed for three times in total, and the interval is 10-12min each time;
step six: primary grinding treatment: using 12 special wood leveling machines to polish and level the cut, the height and the scratch caused in the construction of the wood due to deformation, pavement and processing factors, and cleaning the hole pollution through primary grinding;
step seven: cleaning the board surface: cleaning dirt at the damaged or broken part of the wood by using a special machine and a wood pore cleaning brush or a steel wire brush;
step eight: and (3) medium grinding treatment: removing the repairing glue which is solidified in the excess of the wood board surface in the process of repairing the grinding mark and the hole of the primary grinding, and further adjusting the flatness of the grinding surface;
step nine: and (3) repairing treatment again: the omission or glue dropping problem in each step is checked, repaired and re-repaired according to the regulations and the flow when the omission, repair and leakage are found;
step ten: hole, edge burst and damage repairing treatment: after the above steps are finished, cleaning the wood board surface, and inspecting the wood board surface after the wood board surface is dried;
step eleven: and (3) corner grinding treatment: carrying out corner grinding and polishing connection treatment on corner positions which cannot be finished by a large machine or side line scratches left by primary grinding and middle grinding by using a water grinding sheet and angle matching grinder;
step twelve: fine grinding treatment: grinding the glossiness of the wood, namely grinding the four peripheral lines, and then grinding the middle of the wood;
step thirteen: disease-resistant treatment: after the steps are finished and the wood is completely dried, brushing a solvent with alkali-inhibiting factors and an oily protective agent with a brush to uniformly brush the surface of the wood, and standing for 22-26 hours;
fourteen steps: polishing and crystallizing treatment: polishing and crystallizing the wood board surface by using a polishing machine and a maintenance crystallizing agent, then cleaning the wood board surface, and standing for 22-26h to obtain the sandstone texture painting board.
Preferably, the weak acid cleaning solution is prepared by wetting 5 g of potassium dichromate with a small amount of water, slowly adding 100 ml of concentrated sulfuric acid while stirring, heating to dissolve the potassium dichromate, and then adding 1: 1 adding water and heating to 50-60 ℃ for use.
Preferably, the surface is cleaned by spraying with an airless spray nozzle in the first step.
Preferably, the weak base cleaning liquid comprises 5-8% of fatty alcohol-polyoxyethylene ether (AEO-9), 8-10% of coconut oil alkanolamide (6501), 2-4% of triethanolamine oleate, 8-10% of monoethanolamine, 0-1% of benzotriazole, 1-2% of EDTA disodium and 70-75% of water.
Preferably, the anti-fouling agent is a succinic anhydride derivative.
Preferably, the medium grinding treatment standard is as follows: no No. 50 scratches and no residual repair glue.
Preferably, the repair adhesive is a two-component liquid silica gel, the component A is a liquid silica gel, the component B is a silica gel curing agent, wherein the component A: the component B = 1: 1.
preferably, the hole, edge burst, and damage repairing process criteria are:
if the holes are large and small, selecting solid repair glue with similar modulated color phases for repairing;
if the holes are large and small, selecting liquid repairing glue to carry out glue repairing;
if there is linear damage, the wood grain color is determined, and then the glue similar to the wood culture color is selected for repairing.
Preferably, the standard of the corner grinding process is as follows: the edge has no cut and no burr and scratch.
Preferably, when the wood is completely dried in the disease-resistant treatment of the wood, the wood is kept still for 48 to 50 hours at normal temperature.
Compared with the prior art, the invention has the beneficial effects that:
1. the sandstone texture painting board processing technology sequentially performs surface spraying cleaning, seam cutting processing, seam cleaning processing, seamless processing, seam mouth anti-pollution processing, board cleaning, middle grinding processing, secondary repairing processing, hole, edge blasting, damage repairing processing, corner grinding processing, fine grinding processing, wood disease-resistant processing and polishing crystallization processing on the sandstone texture painting board, can perform high-quality processing on the sandstone texture painting board with a complete system, and avoids influencing the quality of sandstone texture painting during various post-processing.
2. According to the processing technology of the sandstone texture painting board, the antifouling agent and the anti-coking agent are uniformly coated on the seam of the wood of the sandstone texture painting board for three times in total, wherein the interval between every two times is 10-12min, and the antifouling agent is a succinic anhydride derivative, so that the high-temperature oxidation resistance is realized, the polymerization reaction can be effectively inhibited, and the coking is effectively reduced; the method has the advantages that metal deactivation is realized, carbonization reaction of metal ions caused by overhigh temperature in the polishing treatment in the later period is avoided, and the metal ions are combined with an anti-coking agent, so that the metal activity is reduced, the dehydrogenation carbonization reaction can be effectively inhibited, and the quality of sandstone texture painting plate treatment is ensured.
3. This sandstone texture picture panel processing technology, during seamless processing, choose for use liquid to repair to glue and mend the seam and glue the processing, guarantee to fill plump to use the bulging as the standard, can shrink after avoiding the colloid solidification, can present the problem of half seam after polishing, the solidification of stewing, wherein repair glue is two ingredient liquid silica gel, and A component is liquid silica gel, and B component is the silica gel curing agent, wherein A component: the component B = 1: 1, the problem that the colloid is not dried after being placed for a long time or is burnt when being polished at high temperature is avoided.
4. The sandstone texture painting board treatment process comprises the following steps of primary grinding treatment: the 12-head special wood leveling machine is used for polishing and leveling the cut, the height and the scratch caused by the deformation, the pavement and the processing factors of the wood and the construction, and cleaning the pollution of the holes through primary grinding to create conditions for the subsequent hole repairing, fine grinding and other processes.
5. According to the processing technology of the sandstone texture painting board, the sandstone texture painting board is polished by performing primary grinding treatment, middle grinding treatment and fine grinding treatment in a grading manner, so that the polishing quality is improved, and the quality of the sandstone texture painting board is ensured.
6. The sandstone texture painting board treatment process comprises the following steps of: after the steps are completed, the wood is thoroughly dried, the solvent with the alkali-inhibiting factors and the oily protective agent are brushed by a brush to uniformly brush the surface of the wood, and the wood is kept standing for 22 to 26 hours to perform disease-resistant treatment on the sandstone texture painting board so as to ensure the quality of the sandstone texture painting board.
Drawings
Fig. 1 is a schematic flow diagram of a sandstone texture painting board treatment process.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.
Referring to fig. 1, the present invention provides a technical solution: a sandstone texture painting board treatment process specifically comprises the following steps:
the method comprises the following steps: surface spraying and cleaning: firstly, cleaning with clear water, then cleaning with weak base cleaning liquid, and then cleaning with weak acid cleaning liquid;
step two: tailor treatment: performing tailoring treatment on the sandstone texture painting plate according to the conditions that a seam needs to be straight, a seam opening needs to be thin, and the surface of a wood plate cannot be broken, wherein the thickness of a cutting piece is 0.1-0.3;
step three: and (3) seam cleaning treatment: cleaning the seam with a dust collector or a brush, and scraping the seam with a blade;
step four: seamless processing: selecting liquid repairing glue to perform glue repairing treatment on the seam, ensuring full filling, and standing and solidifying by taking the bulge as a standard;
step five: and (3) seam anti-fouling treatment: uniformly coating an anti-fouling agent and an anti-coking agent on the seam of the wood of the sandstone texture painting board, wherein the coating is performed for three times in total, and the interval is 10-12min each time;
step six: primary grinding treatment: using 12 special wood leveling machines to polish and level the cut, the height and the scratch caused in the construction of the wood due to deformation, pavement and processing factors, and cleaning the hole pollution through primary grinding;
step seven: cleaning the board surface: cleaning dirt at the damaged or broken part of the wood by using a special machine and a wood pore cleaning brush or a steel wire brush;
step eight: and (3) medium grinding treatment: removing the repairing glue which is solidified in the excess of the wood board surface in the process of repairing the grinding mark and the hole of the primary grinding, and further adjusting the flatness of the grinding surface;
step nine: and (3) repairing treatment again: the omission or glue dropping problem in each step is checked, repaired and re-repaired according to the regulations and the flow when the omission, repair and leakage are found;
step ten: hole, edge burst and damage repairing treatment: after the above steps are finished, cleaning the wood board surface, and inspecting the wood board surface after the wood board surface is dried;
step eleven: and (3) corner grinding treatment: carrying out corner grinding and polishing connection treatment on corner positions which cannot be finished by a large machine or side line scratches left by primary grinding and middle grinding by using a water grinding sheet and angle matching grinder;
step twelve: fine grinding treatment: grinding the glossiness of the wood, namely grinding the four peripheral lines, and then grinding the middle of the wood;
step thirteen: disease-resistant treatment: after the steps are finished and the wood is completely dried, brushing a solvent with alkali-inhibiting factors and an oily protective agent with a brush to uniformly brush the surface of the wood, and standing for 22-26 hours;
fourteen steps: polishing and crystallizing treatment: polishing and crystallizing the wood board surface by using a polishing machine and a maintenance crystallizing agent, then cleaning the wood board surface, and standing for 22-26h to obtain the sandstone texture painting board.
In this embodiment, the preparation method of the weak acid cleaning solution includes wetting 5 g of potassium dichromate with a small amount of water, slowly adding 100 ml of concentrated sulfuric acid while stirring, heating to dissolve the potassium dichromate, and then dissolving the potassium dichromate in a solvent of 1: 1 adding water and heating to 50-60 ℃ for use.
In this embodiment, the airless spray nozzle is used for cleaning the surface in the first step.
In the embodiment, the weak base cleaning liquid comprises 5-8% of fatty alcohol-polyoxyethylene ether (AEO-9), 8-10% of coconut oil alkanolamide (6501), 2-4% of triethanolamine oleate, 8-10% of monoethanolamine, 0-1% of benzotriazole, 1-2% of EDTA disodium and 70-75% of water.
In this embodiment, the anti-fouling agent is a succinic anhydride derivative.
In this embodiment, the standard of the middle milling process is as follows: no No. 50 scratches and no residual repair glue.
In this embodiment, the repair adhesive is a two-component liquid silica gel, the component a is a liquid silica gel, and the component B is a silica gel curing agent, wherein the component a: the component B = 1: 1.
in this embodiment, the hole, edge burst, and damage repairing criteria are as follows:
if the holes are large and small, selecting solid repair glue with similar modulated color phases for repairing;
if the holes are large and small, selecting liquid repairing glue to carry out glue repairing;
if there is linear damage, the wood grain color is determined, and then the glue similar to the wood culture color is selected for repairing.
In this embodiment, the standard of the corner grinding process is: the edge has no cut and no burr and scratch.
In the embodiment, when the wood is completely dried in the disease-resistant treatment of the wood, the wood is kept stand for 48 to 50 hours at normal temperature.
The working principle is as follows: the sandstone texture painting board processing technology sequentially performs surface spraying cleaning, seam cutting processing, seam cleaning processing, seamless processing, seam mouth anti-pollution processing, board cleaning, middle grinding processing, secondary repairing processing, hole, edge blasting, damage repairing processing, corner grinding processing, fine grinding processing, wood disease-resistant processing and polishing crystallization processing on the sandstone texture painting board, can perform high-quality processing on the sandstone texture painting board with a complete system, and avoids influencing the quality of sandstone texture painting during various post-processing. According to the processing technology of the sandstone texture painting board, the antifouling agent and the anti-coking agent are uniformly coated on the seam of the wood of the sandstone texture painting board for three times in total, wherein the interval between every two times is 10-12min, and the antifouling agent is a succinic anhydride derivative, so that the high-temperature oxidation resistance is realized, the polymerization reaction can be effectively inhibited, and the coking is effectively reduced; the method has the advantages that metal deactivation is realized, carbonization reaction of metal ions caused by overhigh temperature in the polishing treatment in the later period is avoided, and the metal ions are combined with an anti-coking agent, so that the metal activity is reduced, the dehydrogenation carbonization reaction can be effectively inhibited, and the quality of sandstone texture painting plate treatment is ensured. This sandstone texture picture panel processing technology, during seamless processing, choose for use liquid to repair to glue and mend the seam and glue the processing, guarantee to fill plump to use the bulging as the standard, can shrink after avoiding the colloid solidification, can present the problem of half seam after polishing, the solidification of stewing, wherein repair glue is two ingredient liquid silica gel, and A component is liquid silica gel, and B component is the silica gel curing agent, wherein A component: the component B = 1: 1, the problem that the colloid is not dried after being placed for a long time or is burnt when being polished at high temperature is avoided. The sandstone texture painting board treatment process comprises the following steps of primary grinding treatment: the 12-head special wood leveling machine is used for polishing and leveling the cut, the height and the scratch caused by the deformation, the pavement and the processing factors of the wood and the construction, and cleaning the pollution of the holes through primary grinding to create conditions for the subsequent hole repairing, fine grinding and other processes. According to the processing technology of the sandstone texture painting board, the sandstone texture painting board is polished by performing primary grinding treatment, middle grinding treatment and fine grinding treatment in a grading manner, so that the polishing quality is improved, and the quality of the sandstone texture painting board is ensured. The sandstone texture painting board treatment process comprises the following steps of: after the steps are completed, the wood is thoroughly dried, the solvent with the alkali-inhibiting factors and the oily protective agent are brushed by a brush to uniformly brush the surface of the wood, and the wood is kept standing for 22 to 26 hours to perform disease-resistant treatment on the sandstone texture painting board so as to ensure the quality of the sandstone texture painting board.
It will be apparent to those skilled in the art that various changes and modifications may be made in the present invention without departing from the spirit and scope of the invention. Thus, if such modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include such modifications and variations.

Claims (10)

1. A sandstone texture painting board treatment process is characterized by comprising the following steps: the method specifically comprises the following steps:
the method comprises the following steps: surface spraying and cleaning: firstly, cleaning with clear water, then cleaning with weak base cleaning liquid, and then cleaning with weak acid cleaning liquid;
step two: tailor treatment: performing tailoring treatment on the sandstone texture painting plate according to the conditions that a seam needs to be straight, a seam opening needs to be thin, and the surface of a wood plate cannot be broken, wherein the thickness of a cutting piece is 0.1-0.3;
step three: and (3) seam cleaning treatment: cleaning the seam with a dust collector or a brush, and scraping the seam with a blade;
step four: seamless processing: selecting liquid repairing glue to perform glue repairing treatment on the seam, ensuring full filling, and standing and solidifying by taking the bulge as a standard;
step five: and (3) seam anti-fouling treatment: uniformly coating an anti-fouling agent and an anti-coking agent on the seam of the wood of the sandstone texture painting board, wherein the coating is performed for three times in total, and the interval is 10-12min each time;
step six: primary grinding treatment: using 12 special wood leveling machines to polish and level the cut, the height and the scratch caused in the construction of the wood due to deformation, pavement and processing factors, and cleaning the hole pollution through primary grinding;
step seven: cleaning the board surface: cleaning dirt at the damaged or broken part of the wood by using a special machine and a wood pore cleaning brush or a steel wire brush;
step eight: and (3) medium grinding treatment: removing the repairing glue which is solidified in the excess of the wood board surface in the process of repairing the grinding mark and the hole of the primary grinding, and further adjusting the flatness of the grinding surface;
step nine: and (3) repairing treatment again: the omission or glue dropping problem in each step is checked, repaired and re-repaired according to the regulations and the flow when the omission, repair and leakage are found;
step ten: hole, edge burst and damage repairing treatment: after the above steps are finished, cleaning the wood board surface, and inspecting the wood board surface after the wood board surface is dried;
step eleven: and (3) corner grinding treatment: carrying out corner grinding and polishing connection treatment on corner positions which cannot be finished by a large machine or side line scratches left by primary grinding and middle grinding by using a water grinding sheet and angle matching grinder;
step twelve: fine grinding treatment: grinding the glossiness of the wood, namely grinding the four peripheral lines, and then grinding the middle of the wood;
step thirteen: disease-resistant treatment: after the steps are finished and the wood is completely dried, brushing a solvent with alkali-inhibiting factors and an oily protective agent with a brush to uniformly brush the surface of the wood, and standing for 22-26 hours;
fourteen steps: polishing and crystallizing treatment: polishing and crystallizing the wood board surface by using a polishing machine and a maintenance crystallizing agent, then cleaning the wood board surface, and standing for 22-26h to obtain the sandstone texture painting board.
2. The sandstone-texture drawing board treatment process of claim 1, wherein the treatment process comprises the following steps: the preparation method of the weak acid cleaning solution comprises the steps of wetting 5 g of potassium dichromate with a small amount of water, slowly adding 100 ml of concentrated sulfuric acid while stirring, heating to dissolve the potassium dichromate, and then adding 1: 1 adding water and heating to 50-60 ℃ for use.
3. The sandstone-texture drawing board treatment process of claim 1, wherein the treatment process comprises the following steps: and in the first step, an airless spray nozzle is adopted for surface spraying and cleaning.
4. The sandstone-texture drawing board treatment process of claim 1, wherein the treatment process comprises the following steps: the weak base cleaning liquid comprises 5-8% of fatty alcohol-polyoxyethylene ether (AEO-9), 8-10% of coconut oil alkanolamide (6501), 2-4% of triethanolamine oleate, 8-10% of monoethanolamine, 0-1% of benzotriazole, 1-2% of EDTA disodium and 70-75% of water.
5. The sandstone-texture drawing board treatment process of claim 1, wherein the treatment process comprises the following steps: the anti-fouling agent is a succinic anhydride derivative.
6. The sandstone-texture drawing board treatment process of claim 1, wherein the treatment process comprises the following steps: the standard of the middle grinding treatment is as follows: no No. 50 scratches and no residual repair glue.
7. The sandstone-texture drawing board treatment process of claim 1, wherein the treatment process comprises the following steps: the repair adhesive is two-component liquid silica gel, the component A is liquid silica gel, the component B is a silica gel curing agent, wherein the component A: the component B = 1: 1.
8. the sandstone-texture drawing board treatment process of claim 1, wherein the treatment process comprises the following steps: the hole, edge burst and damage repairing treatment standard is as follows:
if the holes are large and small, selecting solid repair glue with similar modulated color phases for repairing;
if the holes are large and small, selecting liquid repairing glue to carry out glue repairing;
if there is linear damage, the wood grain color is determined, and then the glue similar to the wood culture color is selected for repairing.
9. The sandstone-texture drawing board treatment process of claim 1, wherein the treatment process comprises the following steps: the standard of the corner grinding treatment is as follows: the edge has no cut and no burr and scratch.
10. The sandstone-texture drawing board treatment process of claim 1, wherein the treatment process comprises the following steps: when the wood is completely dried in the disease-resistant treatment of the wood, standing for 48-50h at normal temperature.
CN202110347382.5A 2021-03-31 2021-03-31 Sandstone texture painting board treatment process Expired - Fee Related CN113021556B (en)