CN110564298A - antique paint with repairing function - Google Patents
antique paint with repairing function Download PDFInfo
- Publication number
- CN110564298A CN110564298A CN201910733083.8A CN201910733083A CN110564298A CN 110564298 A CN110564298 A CN 110564298A CN 201910733083 A CN201910733083 A CN 201910733083A CN 110564298 A CN110564298 A CN 110564298A
- Authority
- CN
- China
- Prior art keywords
- instant noodle
- paint
- agent
- water
- noodle cake
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
the invention discloses an antique paint with a repairing function, which comprises the following components: epoxy resin, phthalic anhydride, polyacrylamide, triglyceride, petroleum, sodium fatty acid and instant noodle cake powder, silane coupling agent, dispersing agent, defoaming agent, thickening agent, pigment, Tiana water, alkyd resin and loose water. The color of the repaired paint is closer to the color of the original furniture, and the repaired furniture has better old and worn feeling.
Description
Technical Field
The invention relates to the technical field of paint, in particular to antique paint with a repairing function.
background
The paint is mainly a coating which is prepared by taking resin as a raw material and is used for decorating and protecting objects, and modified materials are added according to different purposes, such as: iron oxide, oxidizing, and the like. The paint is mainly used for improving the color of articles or improving the waterproof and antioxidant performance of the articles at present, and the antique material in the market of furniture and wood artware is an important direction, so that the paint is a promising direction.
but current archaize paint mainly uses on new furniture and wooden handicraft, and the main objective reaches the effect of decoration, and not to the lapse of process time, the paint of the furniture and wooden handicraft of repairing full eye bruise's hair and flesh, this kind of paint not only requires to restore the back colour and reaches the effect as old as, but also the requirement can be restoreed the furniture or wooden handicraft surface of full eye bruise's hair and flesh. Aiming at the problems, the invention provides an antique paint with a repairing function.
disclosure of Invention
based on the technical problems in the background art, the invention provides an antique paint with a repairing function.
The technical scheme of the invention is as follows:
the antique paint with the repairing function comprises the following components: epoxy resin, phthalic anhydride, polyacrylamide, triglyceride, petroleum, sodium fatty acid and instant noodle cake powder, silane coupling agent, dispersing agent, defoaming agent, thickening agent, pigment, Tiana water, alkyd resin and loose water.
Preferably, the archaized paint with the repairing function comprises the following components in percentage by weight: 5-12% of epoxy resin, 2-5% of phthalic anhydride, 6-10% of polyacrylamide, 6-10% of triglyceride, 5-10% of petroleum, 0.5-1% of sodium fatty acid, 10-25% of instant noodle cake powder, 0.2-1% of silane coupling agent, 0.5-2% of dispersing agent, 1-3% of defoaming agent, 2-5% of thickening agent, 1-3% of pigment, 3-8% of Tiana water, 3-5% of alkyd resin and the balance of pine water.
Preferably, the instant noodle cake powder is powder obtained by crushing instant noodle cakes into 250 meshes.
preferably, the instant noodle cake is leftover material of a noodle cake in the production process of an instant noodle manufacturer.
a preparation process of an antique paint with a repairing function is characterized by comprising the following steps:
(1) Weighing epoxy resin, phthalic anhydride, polyacrylamide and petroleum according to the weight, pouring into a reaction kettle, adjusting the rotating speed of the reaction kettle to be 100-150r/min, and stirring for 30-50min at 120-150 ℃;
(2) continuously adding triglyceride, sodium aliphatate and instant noodle cake powder into the reaction kettle, and stirring for 10-20 min;
(3) Cooling the mixture obtained in the step (2) to 65-85 ℃, adding a silane coupling agent, a dispersing agent, a defoaming agent and a thickening agent into the mixture, adjusting the rotating speed of the reaction kettle to 350-450r/min, stirring for 1.5-2h, and cooling to 20-35 ℃ to obtain a semi-finished product;
(4) preparing a primer: adding the semi-finished product, the pigment and the Tianna water according to the proportion, and uniformly mixing at a high-speed mixer at 450-600 r/min;
(5) Preparing finish paint: proportionally adding alkyd resin and loose water, and uniformly mixing the alkyd resin and the loose water at a speed stirrer of 450-600 r/min;
(6) the coating process comprises the following steps: and (3) polishing the surface of the wooden product by using 400-mesh sand paper, uniformly spraying primer on the surface, drying, then finishing and polishing again, and uniformly spraying finish paint.
the invention has the advantages that:
the invention adopts the instant noodle cake powder as the filler in the paint, and has the following advantages: firstly, the main raw material of the instant noodle cake is wheat flour instead of mineral raw material, so that the instant noodle cake is environment-friendly and healthy and belongs to renewable raw materials; secondly, the price is low, after the contact with convenient manufacturers, the leftover materials of the instant noodle manufacturers are mainly used, and the price is very low; compared with the mineral raw material, the instant noodle cake powder is adopted, the density is relatively low, the density is similar to that of wood furniture, and the difference is small after the repair; and fourthly, the color of the repaired paint is closer to that of the original furniture by being matched with petroleum, and the repaired paint has better old and worn feeling.
Detailed Description
Example 1:
the antique paint with the repairing function comprises the following components in percentage by weight: 10% of epoxy resin, 3% of phthalic anhydride, 8% of polyacrylamide, 7% of triglyceride, 8% of petroleum, 0.8% of sodium fatty acid, 18% of instant noodle cake powder, 0.7% of silane coupling agent, 0.8% of dispersing agent, 1.5% of defoaming agent, 3% of thickening agent, 2% of pigment, 7% of Tiana water, 4% of alkyd resin and the balance of pine water.
the powder of the instant noodle cake is obtained by crushing the instant noodle cake into 250 meshes of powder;
the instant noodle cake is leftover material of the instant noodle manufacturer in the production process.
A preparation process of an antique paint with a repairing function is characterized by comprising the following steps:
(1) Weighing epoxy resin, phthalic anhydride, polyacrylamide and petroleum according to the weight, pouring into a reaction kettle, adjusting the rotating speed of the reaction kettle to 120r/min, and rotating and stirring at 135 ℃ for 45 min;
(2) continuously adding triglyceride, sodium aliphatate and instant noodle cake powder into the reaction kettle, and stirring for 15 min;
(3) cooling the mixture obtained in the step (2) to 80 ℃, adding a silane coupling agent, a dispersing agent, a defoaming agent and a thickening agent into the mixture, adjusting the rotating speed of the reaction kettle to 400r/min, stirring for 1.8h, and cooling to 30 ℃ to obtain a semi-finished product;
(4) preparing a primer: adding the semi-finished product, the pigment and the Tianna water according to the proportion, and uniformly mixing at 480r/min of a high-speed stirrer;
(5) preparing finish paint: adding alkyd resin and loose water according to the proportion, and uniformly mixing the alkyd resin and the loose water at 480r/min in a high-speed mixer;
(6) The coating process comprises the following steps: and (3) polishing the surface of the wooden product by using 400-mesh sand paper, uniformly spraying primer on the surface, drying, then finishing and polishing again, and uniformly spraying finish paint.
Example 2:
the antique paint with the repairing function comprises the following components in percentage by weight: 12% of epoxy resin, 2% of phthalic anhydride, 10% of polyacrylamide, 6% of triglyceride, 10% of petroleum, 0.5% of sodium fatty acid, 25% of instant noodle cake powder, 0.2% of silane coupling agent, 2% of dispersing agent, 1% of defoaming agent, 5% of thickening agent, 1% of pigment, 8% of Tiana water, 3% of alkyd resin and the balance of loose water.
the powder of the instant noodle cake is obtained by crushing the instant noodle cake into 250 meshes of powder;
The instant noodle cake is leftover material of the instant noodle manufacturer in the production process.
a preparation process of an antique paint with a repairing function is characterized by comprising the following steps:
(1) weighing epoxy resin, phthalic anhydride, polyacrylamide and petroleum according to the amount, pouring into a reaction kettle, adjusting the rotating speed of the reaction kettle to be 150r/min, and stirring for 50min at 120 ℃;
(2) Continuously adding triglyceride, sodium aliphatate and instant noodle cake powder into the reaction kettle, and stirring for 20 min;
(3) cooling the mixture obtained in the step (2) to 65 ℃, adding a silane coupling agent, a dispersing agent, a defoaming agent and a thickening agent into the mixture, adjusting the rotating speed of the reaction kettle to be 450r/min, stirring for 1.5h, and cooling to 35 ℃ to obtain a semi-finished product;
(4) Preparing a primer: adding the semi-finished product, the pigment and the Tianna water according to the proportion, and uniformly mixing at 450r/min in a high-speed mixer;
(5) Preparing finish paint: adding alkyd resin and loose water according to the proportion, and uniformly mixing the alkyd resin and the loose water at 600r/min in a high-speed mixer;
(6) The coating process comprises the following steps: and (3) polishing the surface of the wooden product by using 400-mesh sand paper, uniformly spraying primer on the surface, drying, then finishing and polishing again, and uniformly spraying finish paint.
Example 3:
the antique paint with the repairing function comprises the following components in percentage by weight: 5% of epoxy resin, 5% of phthalic anhydride, 6% of polyacrylamide, 10% of triglyceride, 5% of petroleum, 1% of sodium fatty acid, 10% of instant noodle cake powder, 1% of silane coupling agent, 0.5% of dispersing agent, 3% of defoaming agent, 2% of thickening agent, 3% of pigment, 3% of Tiana water, 5% of alkyd resin and the balance of pine water.
the powder of the instant noodle cake is obtained by crushing the instant noodle cake into 250 meshes of powder;
the instant noodle cake is leftover material of the instant noodle manufacturer in the production process.
A preparation process of an antique paint with a repairing function is characterized by comprising the following steps:
(1) weighing epoxy resin, phthalic anhydride, polyacrylamide and petroleum according to the amount, pouring into a reaction kettle, adjusting the rotating speed of the reaction kettle to be 100r/min, and stirring for 30min at 150 ℃;
(2) Continuously adding triglyceride, sodium aliphatate and instant noodle cake powder into the reaction kettle, and stirring for 10 min;
(3) Cooling the mixture obtained in the step (2) to 85 ℃, adding a silane coupling agent, a dispersing agent, a defoaming agent and a thickening agent into the mixture, adjusting the rotating speed of the reaction kettle to 350r/min, stirring for 2h, and cooling to 20 ℃ to obtain a semi-finished product;
(4) preparing a primer: adding the semi-finished product, the pigment and the Tianna water according to the proportion, and uniformly mixing at 600r/min in a high-speed mixer;
(5) Preparing finish paint: adding alkyd resin and loose water according to the proportion, and uniformly mixing the alkyd resin and the loose water at the speed of 450r/min in a high-speed mixer;
(6) The coating process comprises the following steps: and (3) polishing the surface of the wooden product by using 400-mesh sand paper, uniformly spraying primer on the surface, drying, then finishing and polishing again, and uniformly spraying finish paint.
Comparative example 1
the instant noodle cake powder in the example 1 is replaced by the mixed powder of titanium dioxide and kaolin with the same particle size and the mass ratio of 2:1, and the rest proportion and the preparation method are unchanged.
comparative example 2
the petroleum in example 1 was removed, and the rest of the formulation and preparation method were unchanged.
The ingredients of the instant noodle cakes in the above examples and comparative examples were: wheat flour, refined palm oil, starch, acetic ester starch, edible salt, vital gluten, a compound acidity regulator, a compound thickener, sodium carboxymethylcellulose, a compound colorant and vitamin E.
The repaired samples of examples 1-3 and comparative examples 1-2 were examined below (primer coating thickness 1.0mm, topcoat coating thickness 0.2 mm; severe damage was first filled with atomic ash and then sprayed with the primer and topcoat of the present invention) and the repaired furniture was redwood furniture in the 60's of the 20 th century, and the following examination results were obtained, and the specific results are shown in table 1.
Table 1: the results of examination of the samples of examples 1 to 3 and comparative examples 1 to 2;
According to the test data, the antique paint with the repairing function has the special effect that the repaired furniture has the old-fashioned effect.
The above description is only for the preferred embodiment of the present invention, but the scope of the present invention is not limited thereto, and any person skilled in the art should be considered to be within the technical scope of the present invention, and the technical solutions and the inventive concepts thereof according to the present invention should be equivalent or changed within the scope of the present invention.
Claims (5)
1. The antique paint with the repairing function is characterized by comprising the following components: epoxy resin, phthalic anhydride, polyacrylamide, triglyceride, petroleum, sodium fatty acid and instant noodle cake powder, silane coupling agent, dispersing agent, defoaming agent, thickening agent, pigment, Tiana water, alkyd resin and loose water.
2. the antique paint with the repairing function of claim 1 is characterized by comprising the following components in percentage by weight: 5-12% of epoxy resin, 2-5% of phthalic anhydride, 6-10% of polyacrylamide, 6-10% of triglyceride, 5-10% of petroleum, 0.5-1% of sodium fatty acid, 10-25% of instant noodle cake powder, 0.2-1% of silane coupling agent, 0.5-2% of dispersing agent, 1-3% of defoaming agent, 2-5% of thickening agent, 1-3% of pigment, 3-8% of Tiana water, 3-5% of alkyd resin and the balance of pine water.
3. The repair-functional antique paint according to claim 1 or 2, wherein the instant noodle cake powder is prepared by pulverizing an instant noodle cake to 250 mesh.
4. the repair-function archaized paint according to claim 1 or 2, wherein the instant noodle cake is cake leftover bits and pieces of an instant noodle manufacturer in the production process.
5. The process for preparing an antique paint with a repairing function according to any one of claims 1 to 4, which comprises the following steps:
(1) Weighing epoxy resin, phthalic anhydride, polyacrylamide and petroleum according to the weight, pouring into a reaction kettle, adjusting the rotating speed of the reaction kettle to be 100-150r/min, and stirring for 30-50min at 120-150 ℃;
(2) Continuously adding triglyceride, sodium aliphatate and instant noodle cake powder into the reaction kettle, and stirring for 10-20 min;
(3) Cooling the mixture obtained in the step (2) to 65-85 ℃, adding a silane coupling agent, a dispersing agent, a defoaming agent and a thickening agent into the mixture, adjusting the rotating speed of the reaction kettle to 350-450r/min, stirring for 1.5-2h, and cooling to 20-35 ℃ to obtain a semi-finished product;
(4) Preparing a primer: adding the semi-finished product, the pigment and the Tianna water according to the proportion, and uniformly mixing at a high-speed mixer at 450-600 r/min;
(5) Preparing finish paint: proportionally adding alkyd resin and loose water, and uniformly mixing the alkyd resin and the loose water at a speed stirrer of 450-600 r/min;
(6) the coating process comprises the following steps: and (3) polishing the surface of the wooden product by using 400-mesh sand paper, uniformly spraying primer on the surface, drying, then finishing and polishing again, and uniformly spraying finish paint.