CN109703266A - 一种纯银编丝景泰蓝银碗制作的规范方法 - Google Patents

一种纯银编丝景泰蓝银碗制作的规范方法 Download PDF

Info

Publication number
CN109703266A
CN109703266A CN201811650093.7A CN201811650093A CN109703266A CN 109703266 A CN109703266 A CN 109703266A CN 201811650093 A CN201811650093 A CN 201811650093A CN 109703266 A CN109703266 A CN 109703266A
Authority
CN
China
Prior art keywords
silver
bowl
colored
muffle painting
colored bowl
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201811650093.7A
Other languages
English (en)
Inventor
王国春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
DANZHAI COUNTY GUOCHUN SILVER ORNAMENT Co Ltd
Original Assignee
DANZHAI COUNTY GUOCHUN SILVER ORNAMENT Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by DANZHAI COUNTY GUOCHUN SILVER ORNAMENT Co Ltd filed Critical DANZHAI COUNTY GUOCHUN SILVER ORNAMENT Co Ltd
Priority to CN201811650093.7A priority Critical patent/CN109703266A/zh
Publication of CN109703266A publication Critical patent/CN109703266A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种纯银编丝景泰蓝银碗的规范方法,包括如下步骤:根据银碗的大小尺寸来定;备好一块银片;把银片烧制锤打,反复做出银碗的造型;把设计好的图案粘贴在银碗胚胎上面;用银丝跟着设计好的图案粘附在银碗上;将填好丝的银碗放在兑比好的硫酸中浸泡;清洗;烘干银碗;给银碗上釉彩;把上好釉彩的碗胎放在100℃的纯净水中浸泡5分钟,清洗完后,然后用玛瑙刀在银胎的光银部分进行刮亮即可。采用上述方法制作的景泰蓝银碗质量稳定,层次感极强,纤巧细腻,灵秀生动,古拙朴实,浑厚凝重,展现苗族传统银饰艺术价值。

Description

一种纯银编丝景泰蓝银碗制作的规范方法
技术领域:
本发明涉及景泰蓝银碗的制作方法,尤其是一种编丝景泰蓝银碗的规范制作方法。
技术背景
银饰作为一种文化现象在历史上被各民族青睐,成为多元文化交流的载体之一,苗族银饰全系手工制作,有30多道工序,形成熔铸、捶打、焊接、编丝、洗涤等一整套工艺。纯银编丝工艺的银饰制作是将各种拉好的银丝组件合成的过程,编结辅以纯银拉丝焊接方法等工艺的使用,将不同的组件固定在一起焊接成型。
然而,现有银饰产品质量参差不齐,究其原因,因其加工方法的不规范造成。
发明内容:针对现有技术不足之处,本发明旨在提供一种纯银编丝景泰蓝银碗制作方法的规范方法,提高编丝景泰蓝银碗质量的稳定性,使编丝景泰蓝银碗纹路清晰、立体感强。
为达成上述目的,本发明采用的技术方案,一种纯银编丝景泰蓝银碗的规范方法,包括如下步骤:
①备好一块银片,银片厚度为0.7一0.8mm,银片的宽度根据银碗的大小尺寸来定;
②准备一根直径6—8cm的铁管,铁管的高度为3—5cm,把银片烧制一次,待冷却后把银片放在铁管口上放平,用木锤或胶锤在银片中间轻轻的压或锤打做出凹槽,压出凹槽后用火枪烧透烧红,待冷却后又用木锤进行压制,反复直到做出银碗的造型;
③先把图案设计好,再把做好的银碗胚胎上涂上适当的白乳胶,把设计好的图案粘贴在银碗胚胎上面,用温风慢慢来吹干,让图案与银碗凝固在一起;
④用0.26mm的银丝跟着设计好的图案,顺着图案填上银丝,填丝的过程中,用适当的胶水来固定,银丝将所有图纹填完后,然后用焊粉调兑适量硼砂撒在银碗上,焊粉与硼砂的质量兑比为15:20,将火枪的温度控制在850℃,进行烘烤,直至到整个银碗上面的银丝完全粘附在银碗上;
⑤将填好丝的银碗放在兑比好的硫酸中浸泡,硫酸与水的质量配比为2:10,浸泡的时间为10一15分钟,把填好丝的银碗反复浸泡;
⑥将清洗干净的银碗放在烧开至1OO℃的纯净水中,用铜刷清洗;
⑦将清洗干净的碗,把火枪的温度调至文火,快速烘干银碗的水分;
⑧按照设计图稿的颜色,把相对应颜色的釉彩用小碟子分类装好,用纯净水冲洗三次釉彩;
⑨用皮管,将分类好的釉彩吸入到皮管中,按设计图稿上的颜色,分类逐步把釉彩滴入到做好的碗胎上,将上好釉彩的银胎碗放入烤箱内,然后把烤箱温度调至800℃,当温度达到800℃时,断电让烤箱的温度下降至680℃,然后将上好釉彩的银碗从烤箱内取出,冷却后,检查银碗上的釉彩,是否有脱落,然后进行釉彩填补,再放入烤箱,反复检查,反复进行釉彩填补,烧制,直到釉彩均匀,平整,光滑的粘附在碗胎上;
⑩把上好釉彩的碗胎放在100℃的纯净水中浸泡5分钟,清洗完后,然后用玛瑙刀在银胎的光银部分进行刮亮即可。
采用上述方法制作的景泰蓝银碗质量稳定,层次感极强,纤巧细腻,灵秀生动,古拙朴实,浑厚凝重,展现苗族传统银饰艺术价值。
具体实施方式
①备好一块银片,银片厚度为o.7 mm,银片的宽度根据银碗的大小尺寸来定;
②准备一根直径8cm的铁管,铁管的高度为5cm,把银片烧制一次,待冷却后把银片放在铁管口上放平,用木锤或胶锤在银片中间轻轻的压或锤打做出凹槽,压出凹槽后用火枪烧透烧红,待冷却后又用木锤进行压制,这样反复直到做出银碗的造型;
③先把图案设计好,再把做好的银碗胚胎上涂上适当的白乳胶,把设计好的图案粘贴在银碗胚胎上面,用温风慢慢来吹干,让图案与银碗凝固在一起;
④用0.26mm的银丝跟着设计好的图案,顺着图案填上银丝,填丝的过程中,用适当的胶水来固定,这样才使银丝不会移动,才能保证设计图纹不会变形,银丝将所有图纹填完后,检查银丝的平衡,然后用焊粉调兑适量硼砂撒在银碗上,焊粉与硼砂的质量兑比为15:20,将火枪的温度控制在850℃,进行烘烤,直至到整个银碗上面的银丝完全粘附在银碗上,银碗表面看不到焊粉;
⑤将填好丝的银碗放在兑比好的硫酸中浸泡,硫酸与水的质量配比为2:10的比例,浸泡的时间为15分钟,把填好丝的银碗反复浸泡,用铜刷反复进行刷洗,直到银碗上的杂质完全去掉,银碗的颜色呈现出银本来的乳白色;
⑥将清洗干净的银碗放在烧开至1OO℃的纯净水中,反复用铜刷清洗,这一过程是为了将银碗上细微的杂质清除干净,为下一步在银碗上进行上釉彩打下基础;
⑦将清洗干净的碗,把火枪的温度调至文火,快速烘干碗的水分;
⑧按照设计图稿的颜色,把相对应颜色的釉彩用小碟子分类装好,用纯净水冲洗三次釉彩,冲洗完的釉彩,里面不能含有任何的杂质,这样才能保证烧制出来的颜色干净、鲜艳,釉彩不容开裂,脱落;
⑨用皮管,将分类好的釉彩吸入到皮管中,按设计图稿上的颜色,分类逐步把釉彩滴入到做好的碗胎上,在上釉彩的过程中,一定要让釉彩把银胎填满,反复检查,反复填补釉彩,将上好釉彩的银胎碗放入烤箱内,然后把烤箱温度调至800℃,当温度达到800℃时,断电让烤箱的温度自然下降至680℃,然后将上好釉彩的银碗从烤箱内取出,冷却后,检查银碗上的釉彩,是否有脱落,然后进行釉彩填补,再放入烤箱,反复检查,反复进行釉彩填补,烧制,直到釉彩均匀,平整,光滑的粘附在碗胎上;
⑩把上好釉彩的碗胎放在100℃的纯净水中浸泡5分钟,清洗完后,然后用玛瑙刀在银胎的光银部分进行刮亮即可。

Claims (1)

1.一种纯银编丝景泰蓝银碗的规范方法,其特征在于包括如下步骤:
①备好一块银片,银片厚度为0.7一0.8mm,银片的宽度根据银碗的大小尺寸来定;
②准备一根直径6—8cm的铁管,铁管的高度为3—5cm,把银片烧制一次,待冷却后把银片放在铁管口上放平,用木锤或胶锤在银片中间轻轻的压或锤打做出凹槽,压出凹槽后用火枪烧透烧红,待冷却后又用木锤进行压制,反复直到做出银碗的造型;
③先把图案设计好,再把做好的银碗胚胎上涂上适当的白乳胶,把设计好的图案粘贴在银碗胚胎上面,用温风慢慢来吹干,让图案与银碗凝固在一起;
④用0.26mm的银丝跟着设计好的图案,顺着图案填上银丝,填丝的过程中,用适当的胶水来固定,银丝将所有图纹填完后,然后用焊粉调兑适量硼砂撒在银碗上,焊粉与硼砂的质量兑比为15:20,将火枪的温度控制在850℃,进行烘烤,直至到整个银碗上面的银丝完全粘附在银碗上;
⑤将填好丝的银碗放在兑比好的硫酸中浸泡,硫酸与水的质量配比为2:10,浸泡的时间为10一15分钟,把填好丝的银碗反复浸泡;
⑥将清洗干净的银碗放在烧开至1OO℃的纯净水中,用铜刷清洗;
⑦将清洗干净的碗,把火枪的温度调至文火,快速烘干银碗的水分;
⑧按照设计图稿的颜色,把相对应颜色的釉彩用小碟子分类装好,用纯净水冲洗三次釉彩;
⑨用皮管,将分类好的釉彩吸入到皮管中,按设计图稿上的颜色,分类逐步把釉彩滴入到做好的碗胎上,将上好釉彩的银胎碗放入烤箱内,然后把烤箱温度调至800℃,当温度达到800℃时,断电让烤箱的温度下降至680℃,然后将上好釉彩的银碗从烤箱内取出,冷却后,检查银碗上的釉彩,是否有脱落,然后进行釉彩填补,再放入烤箱,反复检查,反复进行釉彩填补,烧制,直到釉彩均匀,平整,光滑的粘附在碗胎上;
⑩把上好釉彩的碗胎放在100℃的纯净水中浸泡5分钟,清洗完后,然后用玛瑙刀在银胎的光银部分进行刮亮即可。
CN201811650093.7A 2018-12-31 2018-12-31 一种纯银编丝景泰蓝银碗制作的规范方法 Pending CN109703266A (zh)