CN109184253A - 一种外墙渗漏的修补方法 - Google Patents
一种外墙渗漏的修补方法 Download PDFInfo
- Publication number
- CN109184253A CN109184253A CN201811194377.XA CN201811194377A CN109184253A CN 109184253 A CN109184253 A CN 109184253A CN 201811194377 A CN201811194377 A CN 201811194377A CN 109184253 A CN109184253 A CN 109184253A
- Authority
- CN
- China
- Prior art keywords
- repairing
- layer
- mortar
- mending
- exterior wall
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明属于建筑外墙裂缝修补技术领域,具体涉及一种外墙渗漏的修补方法,包括以下步骤:S1、开挖基坑;S2、清理基坑;S3、填充气孔和裂缝;S4、做防水砂浆层;S5、做弹性防水层;S6、做水泥砂浆层;S7、做刚性防水层;S8、铺设混凝土面层;S9、做透明防水面层。本发明可有效完成裂缝的加固和修复,修补质量的可靠性高,大幅减少了复裂复漏的情况发生,本发明的结构合理,投资总经济成本低,实用性高,值得推广。
Description
技术领域
本发明属于建筑外墙裂缝修补技术领域,具体涉及一种外墙渗漏的修补方法。
背景技术
外墙防水是保证建筑物的结构不受水的侵袭的重要工序,其功能就是要使建筑物或构筑物在设计耐久年限内,防止雨水、生活用水的渗漏和地下水的浸蚀,确保建筑结构、内部空间不受到污损,为人们提供一个舒适和安全的生活环境,墙体一旦出现裂缝,每次下雨,房间内就会漏水,严重影响人们的生活环境和居住的心情,由此可见,外墙防水的重要性。
外墙是防水施工一大难点,由于温度变化、地基的不均匀沉降、材料的耐久性及其他因素的影响,都会引起外墙开裂,从而导致渗漏;而外墙的渗漏治理特别是高层建筑的外墙一直是工程中难以彻底解决的问题,现有的外墙渗漏方法大多工序简单,虽快捷但是修补质量的可靠性差,复裂复漏的情况很多。
发明内容
有鉴于此,本发明提供了一种外墙渗漏的修补方法,以便解决现有技术中的不足。
本发明的技术方案是:
一种外墙渗漏的修补方法,包括以下步骤:
S1、沿着裂缝的开裂方向开挖,将裂缝截面扩大为V型,形成裂缝修补用基坑,基坑内表面是粗糙面,表面粗糙面Ra>100;
S2、用毛刷清理基坑内残渣和浮物;
S3、用环氧树脂注浆料灌注裂缝后,逐个把基坑内表面上的气孔和裂缝用环氧胶泥填塞密实,并在基坑内表面均匀的刷一层环氧胶泥;
S4、静置4~12h后,待环氧胶泥基本固化时,在环氧胶泥上表面平铺一层钢丝网,并用保温钉固定,将预先配置好的防水砂浆灌注在基坑内形成防水砂浆层;
S5、防水砂浆层上方均匀涂刷底胶,待底胶固化后,涂刷聚氨酯防水涂料形成弹性防水层,静置12~24h;
S6、待弹性防水层基本固化后,在弹性防水层上方灌注水泥砂浆,水泥砂浆表面抹平后形成水泥砂浆层;
S7、在水泥砂浆层上表面湿润的情况下,向水泥砂浆层上表面均匀的撒一层水泥基渗透结晶型防水材料的干粉,形成刚性防水层;
S8、刚性防水层的上方铺玻璃丝布,并在玻璃丝布上方铺设混凝土面层,将面层压实,抹平到与旧混凝土层上表面平齐后,表层刷漆并带水拉毛,标准养护15d;
S9、混凝土面层固化后,用透明防水胶涂刷3~4次,每次间隔36~48h即可形成透明防水面层。
优选的,所述步骤S3中环氧树脂注浆料是青龙RE504改性环氧化学灌浆液。
优选的,所述步骤S3中环氧胶泥是ECM环氧修补砂浆。
优选的,所述步骤S4中防水砂浆的原料是JC/T984-2011聚合物水泥防水砂浆。
优选的,所述步骤S5中聚氨酯防水涂料每次涂刷的方向必需与前一次垂直交差,依次交叠涂刷三到五次,每次涂刷间隔4~8h,且每次的涂刷厚度为0.35~0.6mm。
优选的,所述步骤S8中的混凝土面层的原料内包括有15%~30%水泥用量的憎水剂,所述憎水剂是有机硅防水剂BP9800。
优选的,所述步骤S9中透明防水胶是OT801透明防水胶。
与现有技术相比,本发明提供的一种外墙渗漏的修补方法的有益效果是:
1、本发明可有效完成裂缝的加固和修复,修补质量的可靠性高,大幅减少了复裂复漏的情况发生;
2、本发明的结构合理,投资总经济成本低,实用性高,值得推广。
附图说明
图1为本发明的流程示意图。
具体实施方式
本发明提供了一种外墙渗漏的修补方法,下面结合图1的流程示意图,对本发明进行说明。
如图1所示,本发明提供了一种外墙渗漏的修补方法,包括以下步骤:
S1、沿着裂缝的开裂方向开挖,将裂缝截面扩大为V型,形成裂缝修补用基坑,基坑内表面是粗糙面,表面粗糙面Ra>100;
S2、用毛刷清理基坑内残渣和浮物;
S3、用环氧树脂注浆料灌注裂缝后,逐个把基坑内表面上的气孔和裂缝用环氧胶泥填塞密实,并在基坑内表面均匀的刷一层环氧胶泥;
S4、静置4~12h后,待环氧胶泥基本固化时,在环氧胶泥上表面平铺一层钢丝网,并用保温钉固定,将预先配置好的防水砂浆灌注在基坑内形成防水砂浆层;
S5、防水砂浆层上方均匀涂刷底胶,待底胶固化后,涂刷聚氨酯防水涂料形成弹性防水层,静置12~24h;
S6、待弹性防水层基本固化后,在弹性防水层上方灌注水泥砂浆,水泥砂浆表面抹平后形成水泥砂浆层;
S7、在水泥砂浆层上表面湿润的情况下,向水泥砂浆层上表面均匀的撒一层水泥基渗透结晶型防水材料的干粉,形成刚性防水层;
S8、刚性防水层的上方铺玻璃丝布,并在玻璃丝布上方铺设混凝土面层,将面层压实,抹平到与旧混凝土层上表面平齐后,表层刷漆并带水拉毛,标准养护15d;
S9、混凝土面层固化后,用透明防水胶涂刷3~4次,每次间隔36~48h即可形成透明防水面层。
进一步的,所述步骤S3中环氧树脂注浆料是青龙RE504改性环氧化学灌浆液。
进一步的,所述步骤S3中环氧胶泥是ECM环氧修补砂浆。
进一步的,所述步骤S4中防水砂浆的原料是JC/T984-2011聚合物水泥防水砂浆。
进一步的,所述步骤S5中聚氨酯防水涂料每次涂刷的方向必需与前一次垂直交差,依次交叠涂刷三到五次,每次涂刷间隔4~8h,且每次的涂刷厚度为0.35~0.6mm。
进一步的,所述步骤S8中的混凝土面层的原料内包括有15%~30%水泥用量的憎水剂,所述憎水剂是有机硅防水剂BP9800。
进一步的,所述步骤S9中透明防水胶是OT801透明防水胶。
整个施工完成后,可以采用连续淋水法进行外墙渗漏检验,即用φ20mm的水管,采用3kpa压力水,在建筑物外墙施工处连续淋水6h,观察内墙面有无渗水痕迹。
利用本发明提供的外墙渗漏的修补方法进行外墙修补,外墙修补的质量高,复裂率低,修补可靠性提高了90%,与传统的修补方法相比,节省总经济成本60%。
与现有技术相比,本发明提供的一种外墙渗漏的修补方法,可有效完成裂缝的加固和修复,修补质量的可靠性高,大幅减少了复裂复漏的情况发生,本发明的结构合理,投资总经济成本低,实用性高,值得推广。
以上公开的仅为本发明的较佳的具体实施例,但是,本发明实施例并非局限于此,任何本领域技术人员能思之的变化都应落入本发明的保护范围。
Claims (7)
1.一种外墙渗漏的修补方法,其特征在于,包括以下步骤:
S1、沿着裂缝的开裂方向开挖,将裂缝截面扩大为V型,形成裂缝修补用基坑,基坑内表面是粗糙面,表面粗糙面Ra>100;
S2、用毛刷清理基坑内残渣和浮物;
S3、用环氧树脂注浆料灌注裂缝后,逐个把基坑内表面上的气孔和裂缝用环氧胶泥填塞密实,并在基坑内表面均匀的刷一层环氧胶泥;
S4、静置4~12h后,待环氧胶泥基本固化时,在环氧胶泥上表面平铺一层钢丝网,并用保温钉固定,将预先配置好的防水砂浆灌注在基坑内形成防水砂浆层;
S5、防水砂浆层上方均匀涂刷底胶,待底胶固化后,涂刷聚氨酯防水涂料形成弹性防水层,静置12~24h;
S6、待弹性防水层基本固化后,在弹性防水层上方灌注水泥砂浆,水泥砂浆表面抹平后形成水泥砂浆层;
S7、在水泥砂浆层上表面湿润的情况下,向水泥砂浆层上表面均匀的撒一层水泥基渗透结晶型防水材料的干粉,形成刚性防水层;
S8、刚性防水层的上方铺玻璃丝布,并在玻璃丝布上方铺设混凝土面层,将面层压实,抹平到与旧混凝土层上表面平齐后,表层刷漆并带水拉毛,标准养护15d;
S9、混凝土面层固化后,用透明防水胶涂刷3~4次,每次间隔36~48h即可形成透明防水面层。
2.根据权利要求1所述的一种外墙渗漏的修补方法,其特征在于,所述步骤S3中环氧树脂注浆料是青龙RE504改性环氧化学灌浆液。
3.根据权利要求1所述的一种外墙渗漏的修补方法,其特征在于,所述步骤S3中环氧胶泥是ECM环氧修补砂浆。
4.根据权利要求1所述的一种外墙渗漏的修补方法,其特征在于,所述步骤S4中防水砂浆的原料是JC/T984-2011聚合物水泥防水砂浆。
5.根据权利要求1所述的一种外墙渗漏的修补方法,其特征在于,所述步骤S5中聚氨酯防水涂料每次涂刷的方向必需与前一次垂直交差,依次交叠涂刷三到五次,每次涂刷间隔4~8h,且每次的涂刷厚度为0.35~0.6mm。
6.根据权利要求1所述的一种外墙渗漏的修补方法,其特征在于,所述步骤S8中的混凝土面层的原料内包括有15%~30%水泥用量的憎水剂,所述憎水剂是有机硅防水剂BP9800。
7.根据权利要求1所述的一种外墙渗漏的修补方法,其特征在于,所述步骤S9中透明防水胶是OT801透明防水胶。