CN109169579A - 一种粘虫板及其应用 - Google Patents
一种粘虫板及其应用 Download PDFInfo
- Publication number
- CN109169579A CN109169579A CN201811111053.5A CN201811111053A CN109169579A CN 109169579 A CN109169579 A CN 109169579A CN 201811111053 A CN201811111053 A CN 201811111053A CN 109169579 A CN109169579 A CN 109169579A
- Authority
- CN
- China
- Prior art keywords
- insect
- sticking plate
- mythimna separata
- rubber base
- styrene
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种粘虫板及其应用,属于植物保护领域。一种粘虫板,将粘虫胶基料在150℃融化后,添加溶剂和助剂成分混合均匀后,再均匀涂抹到基板上,所述粘虫胶基料为苯乙烯‑丁二烯三元嵌段共聚物或/和苯乙烯‑异戊二烯‑苯乙烯三元嵌段共聚物,所述溶剂为汽油,助剂为增粘剂松香脂、软化剂邻苯二甲酸酯和抗氧化剂乙基苯基二硫代氨基甲酸锌。本发明提供的粘虫板,不仅可以和普通粘虫板一样捕获害虫,还不粘人手和衣服,解决了目前市面上粘虫板在操作过程中粘手的行业痛点问题,更适合推广。
Description
技术领域
本发明涉及植物保护领域,具体涉及一种粘虫板及其在防治害虫中的应用。
背景技术
粘虫板是遵循“公共植保、绿色植保”理念,广泛应用于蔬菜、花卉、林业上的害虫物理防控产品,具有环保、无公害、操作方便、成本相对较低的优点。粘虫板是利用昆虫对特定颜色的趋性,通过在板表面涂抹粘虫胶从而起到诱杀害虫的作用。现有的粘虫板主要由基板、粘虫胶和外膜组成,在存放、揭膜、悬挂、撤除等操作过程中,不可避免接触到粘虫胶,粘在手上和衣服上很难清洗,给生产生活带来麻烦,这是目前粘虫板在应用中的不便之处。
发明内容
针对现有粘虫板的不足,本发明提供的粘虫板,可粘虫但不粘手,可以正常捕获害虫,也不会粘在人手和衣服上,基板上的粘虫胶具有高粘度,且防水,在高温时不流淌,抗日晒雨淋,持久耐用。该粘虫板可应用于温室和露地作物,用于监测和防治多种小型害虫,包括粉虱、蓟马、潜叶蝇、蚜虫等。
一种诱虫板,在基板的一面或两面涂抹有热熔型压敏胶,所述热熔型压敏胶由粘虫胶基料和助剂组成,所述粘虫胶基料为苯乙烯-丁二烯三元嵌段共聚物或/和苯乙烯-异戊二烯-苯乙烯三元嵌段共聚物;所述助剂为增粘剂、软化剂、抗氧化剂中的一种或多种。
所述粘虫胶基料和助剂的重量比为8:1。
所述粘虫胶基料为苯乙烯-丁二烯三元嵌段共聚物和苯乙烯-异戊二烯-苯乙烯三元嵌段共聚物的混合物,其重量比为1:1。
所述增粘剂为松香脂,所述软化剂为邻苯二甲酸酯,所述抗氧化剂为乙基苯基二硫代氨基甲酸锌。
所述助剂为增粘剂、软化剂和抗氧化剂的混合物,其重量比为2:1:1。
所述基板为PVC板或纸板,所述软化剂为邻苯二甲酸二辛酯。所述基板的颜色可根据所诱杀的害虫种类确定,如黄色、蓝色、白色、绿色等。
上述粘虫板的制备方法,其特征在于先将粘虫胶基料在150℃下融化,然后添加溶剂汽油和助剂成分,混合均匀后,均匀涂抹在所述基板的两面,晾干即可。
所述粘虫胶基料、溶剂和助剂的重量比为8:1:1。
上述热熔型压敏胶在基板单面涂抹的厚度为0.02-0.03mm,胶体的粘结力为5-10×10-4N/mm2。
上述粘虫板在蔬菜、花卉、林业领域用于监测和防治害虫中应用。
上述害虫指粉虱、蓟马、潜叶蝇、蚜虫。
本发明的目的是针对目前市面上粘虫板在操作过程中粘手的行业痛点问题,研发出一种可以粘杀害虫而不粘手和衣服的粘虫物质,将这些物质涂抹到基板上,形成一种粘虫不粘手的新型粘虫板。该诱虫板可用于蔬菜、花卉、林业等上防治粉虱、蓟马、潜叶蝇、蚜虫等小型害虫。
本发明中使用的热熔型压敏胶同时具有橡胶和塑料的特性,来源容易,价格低廉,耐水,不宜老化,适用于温室和户外粘虫;所用增粘剂松香脂与压敏胶相容,可提高压敏胶的粘性;所用软化剂邻苯二甲酸酯类,可提高压敏胶的初粘力性能,让粘虫胶容易均匀涂抹到载体板上;所用抗氧化剂乙基苯基二硫代氨基甲酸锌,可确保压敏胶在150℃高温融化后保持性能和外观颜色。粘虫胶基料融化后,再与溶剂汽油和助剂成分按照本发明提供的比例混合后,再涂抹到载体板上,用手按压后,粘性较大,但松手后,胶不会粘到手上,手感干净,也没有粘性。溶剂汽油有利于更好的溶解粘虫胶基料以及分散均匀整个热熔型压敏胶的组分,涂抹后自然挥发。粘虫板在使用过程中,粘虫胶触碰到衣服上也没有粘性。温室试验表明,这种粘虫不粘手的粘虫板与普通诱虫板的杀虫效果相当(表1)。
具体实施方式
下面结合实施例子对本发明做进一步详细说明。
实施例1制作粘虫板
1.配置粘虫胶基料。先将热熔型压敏胶的两种基料重要成分,苯乙烯-丁二烯三元嵌段共聚物和苯乙烯-异戊二烯-苯乙烯三元嵌段共聚物按照1:1的重量比混合后,用热熔胶机在150℃下融化。
2.添加溶剂和助剂成分。将助剂成分:增粘剂松香脂、软化剂邻苯二甲酸酯类和抗氧化剂乙基苯基二硫代氨基甲酸锌按照重量比为2:1:1混合,再将粘虫胶基料、溶剂汽油和助剂成分按照重量比为8:1:1再次混合。
3.涂抹基板。将上述粘虫溶胶混合物均匀涂抹到PVC板两面。板的长度为15-50cm,宽为10-30cm。粘虫溶胶混合物在载体板单面涂抹的厚度为0.02-0.03mm,胶体粘结力在5-10×10-4N/mm2。
4.覆膜成型。在粘虫板两面平整覆上一层与板尺寸相同的PVC薄膜,即为新型粘虫板。
5.悬挂使用。用铁钉或剪刀在载体板一侧打两个孔,用铁丝或细绳悬挂于温室和田间作物中。诱虫板悬挂高度与植株等高或略高于植株,并随着植株的生长调整粘虫板高度。悬挂数量根据植株密度、害虫发生量和粘虫板尺寸而定,一般每亩30-50张。待诱虫板粘满虫体或粘性不足后更换诱虫板。户外一般持续45天,温室持续60天,与常规粘虫板持续效果相当。
试验例1
将本发明提供的新型粘虫板悬挂于温室茄子作物中。悬挂之前,经随机调查西花蓟马和温室白粉虱的发生量分别为12—30头成虫/株和6—15头成虫/株。将市面上购买的相同大小的普通粘虫板作为试验对照。处理组和对照组分别随机悬挂20张。3天后记录粘虫板上的蓟马和粉虱数,10天后用初粘测试仪检测胶的粘合力。结果表明,本发明提供的粘虫板的粘虫效果与普通粘虫板没有显著差异,且在10天后的粘合力与普通粘虫板也没有显著差异(表1)。
表1新型粘虫板与普通粘虫板对温室蓟马和粉虱的捕杀效果
注:表中同一竖行相同小写字母表示差异不显著。
Claims (10)
1.一种诱虫板,在基板的一面或两面涂抹有热熔型压敏胶,所述热熔型压敏胶由粘虫胶基料和助剂组成,所述粘虫胶基料为苯乙烯-丁二烯三元嵌段共聚物或/和苯乙烯-异戊二烯-苯乙烯三元嵌段共聚物;所述助剂为增粘剂、软化剂、抗氧化剂中的一种或多种。
2.根据权利要求1所述的诱虫板,所述粘虫胶基料和助剂的重量比为8:1。
3.根据权利要求1所述的诱虫板,所述粘虫胶基料为苯乙烯-丁二烯三元嵌段共聚物和苯乙烯-异戊二烯-苯乙烯三元嵌段共聚物的混合物,其重量比为1:1。
4.根据权利要求1所述的诱虫板,所述增粘剂为松香脂,所述软化剂为邻苯二甲酸酯,所述抗氧化剂为乙基苯基二硫代氨基甲酸锌。
5.根据权利要求1所述的诱虫板,所述助剂为增粘剂、软化剂和抗氧化剂的混合物,其重量比为2:1:1。
6.根据权利要求1所述的诱虫板,所述基板为PVC板或纸板,所述软化剂为邻苯二甲酸二辛酯。
7.根据权利要求1所述的诱虫板,所述热熔型压敏胶在基板单面涂抹的厚度为0.02-0.03mm,胶体的粘结力为5-10×10-4N/mm2。
8.权利要求1-7任一所述的粘虫板的制备方法,其特征在于先将粘虫胶基料在150℃下融化,然后添加溶剂汽油和助剂成分,混合均匀后,再均匀涂抹在所述基板的两面,晾干即可。
9.根据权利要求8所述的制备方法,所述粘虫胶基料、溶剂和助剂的重量比为8:1:1。
10.权利要求1-7任一所述的粘虫板在蔬菜、花卉、林业领域用于监测和防治害虫中应用,所述害虫为粉虱、蓟马、潜叶蝇、蚜虫。