CN108708563A - 一种保持瓷砖原状的瓷砖、石材饰面点面加固修缮工法 - Google Patents

一种保持瓷砖原状的瓷砖、石材饰面点面加固修缮工法 Download PDF

Info

Publication number
CN108708563A
CN108708563A CN201810524240.XA CN201810524240A CN108708563A CN 108708563 A CN108708563 A CN 108708563A CN 201810524240 A CN201810524240 A CN 201810524240A CN 108708563 A CN108708563 A CN 108708563A
Authority
CN
China
Prior art keywords
ceramic tile
stone facing
glue
transparent
stone
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201810524240.XA
Other languages
English (en)
Other versions
CN108708563B (zh
Inventor
杨雨奕
缪德忠
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Tianbu Technology Co ltd
Original Assignee
Shanghai State Mstar Technology Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai State Mstar Technology Ltd filed Critical Shanghai State Mstar Technology Ltd
Priority to CN201810524240.XA priority Critical patent/CN108708563B/zh
Publication of CN108708563A publication Critical patent/CN108708563A/zh
Application granted granted Critical
Publication of CN108708563B publication Critical patent/CN108708563B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开的一种保持瓷砖原状的瓷砖、石材饰面点面加固修缮工法,包括如下步骤:(1)瓷砖、石材饰面勾缝找平步骤;(2)瓷砖、石材饰面清洁及界面处理步骤;(3)涂刷第一道透明防水胶及铺设透明网步骤;(4)钻孔、安装锚固、注胶、重造粘结层时兼植筋及钉孔处理步骤;(5)涂刷第二道透明防水胶步骤;(6)滚涂罩面步骤。注明:步骤(4)安装锚固及注胶步骤也可放于步骤(2)瓷砖、石材饰面清洁及界面处理步骤之前。本发明与现有瓷砖、石材空鼓修缮工法相比,无需铲除瓷砖、石材,具有修缮工序简单,成本低,工期短、垃圾少等优点,修缮后不脱落,不渗漏,解决人居环境的安全。

Description

一种保持瓷砖原状的瓷砖、石材饰面点面加固修缮工法
技术领域
本发明涉及建筑内外墙粘贴瓷砖粘贴空鼓修复技术领域,特别涉及一种保持瓷砖原状的瓷砖饰面点面加固修缮工法。
背景技术
外墙饰面粘贴石材、瓷砖、马赛克等材料属刚性材料,基层有粉刷砂浆层、粘结层或粉刷砂浆层、保温系统层、粘结层,各种不同属性的材料的膨胀系数等技术性能指标差别较大。特别是传统工艺粘贴瓷砖用水泥素灰的砖缝,夏季气温达到35℃时,外墙保温层温度可高达70℃--80℃,突遇降雨瞬间气温可降为10℃--20℃,温差50℃--60℃。两种膨胀系数差别较大的两种材料粘结在一起,时而久之势必造成水泥素灰的瓷砖缝龟裂。冬季,下雪时雨水渗入裂缝中冻融后,就势必会出现瓷砖空鼓、脱落,造成砸死人、砸伤人的安全事故。严重的威胁到人居环境的安全。
发明内容
本发明所要解决的技术问题在于针对瓷砖、石材空鼓修复过程中所存在的问题而提供一种保持瓷砖原状的瓷砖饰面点面加固修缮工法。
本发明所要解决的技术问题可以通过以下技术方案来实现:
一种保持瓷砖、石材原状的瓷砖、石材饰面点面加固修缮工法,包括如下步骤:
(1)瓷砖、石材饰面勾缝找平步骤(也可省略此步骤由透明网性能决定)
该步骤中,首先检查瓷砖、石材饰面勾缝的平整度,不平整的勾缝用防水勾缝剂填平;
(2)瓷砖、石材饰面清洁及界面处理步骤
该步骤中,首先将瓷砖、石材饰面上的表面油污及砂浆清洁干净,然后在清洁后的瓷砖饰面上滚涂功能性界面剂,形成一层界面剂层;
(3)涂刷第一道透明防水胶及铺设透明网步骤
该步骤中,首先在步骤(2)形成的界面剂层上滚涂透明防水胶,然后将透明网铺设在透明防水胶上,铺平并无皱褶,相邻的透明网之间搭接在瓷砖饰面的勾缝处;
(4)钻孔、安装锚固、注胶及钉孔处理步骤
在瓷砖、石材饰面的勾缝内(或瓷砖上),按照上下、左右间隔330-500mm钻孔,钻孔数量为4~9个/m2,清孔后向孔内注入锚固胶,然后向孔内插入锚栓并用锤子敲击锚栓中的膨胀管使之膨胀与基础形成紧固连接,或依据钉形,在膨胀管根部膨胀与基础形成紧固连接后,再从膨胀管端部加压注浆,使浆料从膨胀管侧设计孔与缝喷浆,重造空鼓层粘结层时兼植筋功效;钉孔美观处理。
(5)涂刷第二道透明防水胶步骤
该步骤中,在透明网上滚涂第二道透明防水胶,第二道透明防水胶与透明网、第一道透明防水胶形成高强、耐候、防水复合层;
(6)滚涂罩面步骤
在第二道透明防水胶上滚涂透明罩面保护胶。
注明:步骤(4)安装锚固及注胶步骤也可放于步骤(2)瓷砖、材饰面清洁及界面处理步骤之前。
由于采用了如上的技术方案,本发明与现有瓷砖、石材空鼓修缮工法相比,保持瓷砖、石材装饰效果,无需铲除瓷砖、石材,具有修缮工序简单,成本低,工期短、垃圾少等优点,修缮后使平面每块瓷砖形成整体,防水、防渗漏,通过锚栓与墙体紧固连接,形成不脱落,解决人居环境的安全。
附图说明
图1为本发明锚栓布置示意图。
具体实施方式
一种保持瓷砖、石材原状的瓷砖、石材饰面点面加固修缮工法,包括如下步骤:
(1)瓷砖、石材饰面勾缝找平步骤(也可省略此步骤由透明网性能决定)
该步骤中,首先检查瓷砖饰面勾缝的平整度,不平整的勾缝用防水勾缝剂填平;
(2)瓷砖、石材饰面清洁及界面处理步骤
该步骤中,首先将瓷砖、石材饰面上的表面油污及砂浆清洁干净,保证瓷砖饰面五明显污渍等杂质;然后在清洁后的瓷砖、石材饰面上滚涂界面剂,形成一层界面剂层,增加双向附着,提高耐久性;
(3)涂刷第一道透明防水胶及铺设透明网步骤
该步骤中,首先在步骤(2)形成的界面剂层上滚涂透明防水胶,施涂均匀,确保无漏涂;然后将透明网铺设在透明防水胶上,铺平并无皱褶,相邻的透明网之间搭接在瓷砖饰面的勾缝处;
(4)钻孔、安装锚固、注胶及钉孔处理步骤
参见图1,在瓷砖、石材饰面的勾缝内(或瓷砖、石材上),按照上下、左右间隔330-500mm钻孔,钻孔数量为4~9个/m2,清孔后向孔内注入锚固胶,然后向孔内插入锚栓并用锤子敲击锚栓10中的膨胀管使之膨胀与基础形成紧固连接,或依据钉形,在膨胀管根部膨胀与基础形成紧固连接后,再从膨胀管端部加压注浆,使浆料从膨胀管侧设计孔与缝喷浆,重造空鼓层粘结层时兼植筋功效;钉孔美观处理。
(5)涂刷第二道透明防水胶步骤
该步骤中,在透明网上滚涂第二道透明防水胶,第二道透明防水胶与透明网、第一道透明防水胶形成高强、耐候、防水复合层;
(6)滚涂罩面步骤
在第二道透明防水胶上滚涂透明罩面保护胶。
注明:步骤(4)安装锚固及注胶步骤也可放于步骤(2)瓷砖、石材饰面清洁及界面处理步骤之前。

Claims (1)

1.一种保持瓷砖、石材原状的瓷砖、石材饰面点面加固修缮工法,其特征在于,包括如下步骤:
(1)瓷砖、石材饰面勾缝找平步骤
该步骤中,首先检查瓷砖、石材饰面勾缝的平整度,不平整的勾缝用防水勾缝剂填平;
(2)瓷砖、石材饰面清洁及界面处理步骤
该步骤中,首先将瓷砖、石材饰面上的表面油污及砂浆清洁干净,然后在清洁后的瓷砖、石材饰面上滚涂界面剂,形成一层界面剂层;
(3)涂刷第一道透明防水胶及铺设透明网步骤
该步骤中,首先在步骤(2)形成的界面剂层上滚涂透明防水胶,然后将透明网铺设在透明防水胶上,铺平并无皱褶,相邻的透明网之间搭接在瓷砖、石材饰面的勾缝处;
(4)钻孔、安装锚固、注胶及钉孔处理步骤
在瓷砖、石材饰面的勾缝内(或瓷砖上),按照上下、左右间隔330-500mm钻孔,钻孔数量为4~9个/m2,清孔后向孔内注入锚固胶,然后向孔内插入锚栓并用锤子敲击锚栓中的膨胀管使之膨胀与基础形成紧固连接,或依据钉形,在膨胀管根部膨胀与基础形成紧固连接后,再从膨胀管端部加压注浆,使浆料从膨胀管侧设计孔与缝喷浆,重造空鼓层粘结层时兼植筋;钉孔美观处理。
(5)涂刷第二道透明防水胶步骤
该步骤中,在透明网上滚涂第二道透明防水胶,第二道透明防水胶与透明网、第一道透明防水胶形成高强、耐候、防水复合层;
(6)滚涂罩面步骤
在第二道透明防水胶上滚涂透明罩面保护胶。
注明:步骤(4)安装锚固及注胶步骤也可放于步骤(2)瓷砖、石材饰面清洁及界面处理步骤之前。
CN201810524240.XA 2018-05-28 2018-05-28 一种保持瓷砖原状的瓷砖、石材饰面点面加固修缮工法 Active CN108708563B (zh)