CN108655545A - 水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用 - Google Patents
水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用 Download PDFInfo
- Publication number
- CN108655545A CN108655545A CN201710192990.7A CN201710192990A CN108655545A CN 108655545 A CN108655545 A CN 108655545A CN 201710192990 A CN201710192990 A CN 201710192990A CN 108655545 A CN108655545 A CN 108655545A
- Authority
- CN
- China
- Prior art keywords
- water soluble
- pipeline
- soluble paper
- welding
- argon
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用,其特征在于包括以下步骤:a、根据管道管径准备两张直径大于管径100‑200mm的水溶纸(1),b、使用胶水(4)在管道(2)内部各粘上一张水溶纸(1),c、在两张水溶纸中的一张水溶纸(1)上开一个排气孔(3),d、用纸胶带(5)完全封住整个管道(2)的对口缝隙,在缝隙处用连接氩气带(9)的铜管(8)向管道(2)内部充氩气;e、使用仪器检测到管道(2)内部氩气浓度达到99.9%进行焊接。本发明具有水溶纸在管道中设置措施简单、施工方便,进行长管段管道碰口处焊接时,可以方便快捷的完成充氩保护,有效保证管道焊接质量和降低工程成本的优点。
Description
技术领域
本发明涉及一种管道氩弧焊,具体地说,是一种水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用。
背景技术
传统的工业管道在氩弧焊焊接过程中,对整条管线充氩气进行保护,成本太大,施工过程常常采用海绵做的圆形封堵盘组加氩气管组成装置,靠拖动进行封住焊缝的内狭小空间进行充氩气。因此,这样进行气体保护的管道焊缝往往通过要求一端往另一端一个接一个焊过去,通过拖动海绵做的圆形封堵盘组达到对管道充氩保护的效果,是从管道内部充氩。但是这种方法在两个长距离管道进行碰口或者部分管道焊缝不合格切割重新焊接都存在很大的难度。近些年采用在管道内部贴水溶纸进行充氩保护的情况,由管道外部充对口缝隙处进行充氩,但水溶纸使用方法并没有得到规范,仍然存在水溶纸太多,堵塞小管道管口,或者焊接质量很难保证的情况。
因此已知的水溶纸在管道氩弧焊中存在着上述种种不便和问题。
发明内容
本发明的目的,在于提出一种适用于长距离管道氩弧焊的水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用。
为实现上述目的,本发明的技术解决方案是:
一种水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用,不适用于1寸及以下小管径管道焊接,水溶纸是一种可快速溶解的用于封闭管道内保护气体的材料,焊接结束后用水或者蒸汽冲洗焊接后的管道就能使管道里不留下一点水溶纸残渣,里面的气体也很快消失,其特征在于包括以下步骤:
a、长距离管道在进行管道中间接头碰口氩弧焊之前,根据管道管径准备两张直径大于管径100-200mm的水溶纸,使水溶纸折叠成水溶纸圆圈部分和水溶纸褶边部分;
b、在管道对口之前,使用胶水在管道内部焊管口两侧管壁的距离所焊管口200-300mm处各粘上一张水溶纸,使水溶纸距离管道对口处不要太近,以防焊接过程中产生的热量使贴在管道管壁的水溶纸脱落;
c、在两张水溶纸中的一张水溶纸上开一个排气孔用于排气;
d、对口完成后,并用纸胶带完全封住整个管道的对口缝隙,在缝隙处用连接氩气带的铜管向管道内部充氩气;
e、使用仪器检测到管道内部氩气浓度达到99.9%进行焊接,使用焊枪和焊丝施焊,且当环形焊缝焊接到还剩20mm时应拔掉铜管并快速完成焊接。
本发明的水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用还可以采用以下的技术措施来进一步实现。
前述的方法,其中所述水溶纸圆圈部分的直径等于管道管径。
前述的方法,其中所述水溶纸褶边部分的宽度为5-10cm。
前述的方法,其中所述排气孔的直径为4mm-8mm。
前述的方法,其中设有排气孔的水溶纸在立管焊接中设置在接头碰口上方管道中。
前述的方法,其中所述接头碰口在立管焊接中应在上方管道中管道内部充氩气。
前述的方法,其中所述铜管对于大管径管道焊接应采用2根铜管充氩气。
采用上述技术方案后,本发明的水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用具有以下优点:
1、水溶纸在管道中设置措施简单、施工方便;
2、进行长管段管道碰口处焊接时,可以方便快捷的完成充氩保护;
3、有效保证管道焊接质量,降低工程成本。
附图说明
图1是水溶纸折叠方法示意图;
图2是贴有水溶纸的管道对口后剖面图;
图3为本发明实施例的中的水溶纸在使用状态下的示意图。
图中:1水溶纸,2管道,3排气孔,4胶水,5纸胶带,6焊丝,7焊枪,8细铜管,9氩气带,10水溶纸圆圈,11水溶纸褶边。
具体实施方式
以下结合实施例及其附图对本发明作更进一步说明。
实施例1
本发明的水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用,其不适用于1寸及以下小管径管道焊接,水溶纸是一种可快速溶解的用于封闭管道内保护气体的材料,焊接结束后用水或者蒸汽冲洗焊接后的管道就能使管道里不留下一点水溶纸残渣,里面的气体也很快消失,具体方法如下:
现请参阅图1,图1是水溶纸折叠方法示意图。如图所示,所述长距离管道2在进行碰口焊接之前,根据管径准备两张直径大于管径200mm的水溶纸1,使水溶纸折叠成水溶纸圆圈10部分和水溶纸褶边11部分。
在管道对口之前,使用胶水4在管道2内部距离所焊管口两侧管壁的约300mm处粘上水溶纸1。这里尤其要保证水溶纸1距离管道对口处不要太近,因为焊接过程中产生的热量会使贴在管道2管避的水溶纸1脱落。
图2是贴有水溶纸的管道对口后剖面图。在其中一张水溶纸1上开一个5mm的排气孔3用于排气。如果是立管焊接,宜开在上方。
图3为本发明实施例的中的水溶纸在使用状态下的示意图。对口完成后,并用纸胶带5完全封住整个管道2的对口缝隙。在缝隙处用连接氩气带9的铜管8管道2内部充氩气。如果是如图3所示的立式环形焊缝,宜在上部作氩气充压,对于大管径管道2可采用2根铜管充氩气。
使用仪器检测到内部氩气浓度达到99.9%方可进行焊接。使用焊枪7和焊丝6进行施焊;当环形焊缝焊接到还剩20mm,应拔掉铜管8并快速完成焊接。
管道2内部充氩所用的水溶纸1遇水即化,可以在管道试压吹洗过程中被完全清除掉。
本发明具有实质性特点和显著的技术进步,本发明的水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用,解决了在焊接管道黄金口或长距离管道碰口焊接的充氩保护难题,节省成本,且方便可靠,并规范化水溶纸的用法及注意要点,确保焊接质量。
以上实施例仅供说明本发明之用,而非对本发明的限制,有关技术领域的技术人员,在不脱离本发明的精神和范围的情况下,还可以作出各种变换或变化。因此,所有等同的技术方案也应该属于本发明的范畴,应由各权利要求限定。
Claims (7)
1.一种水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用,不适用于1寸及以下小管径管道焊接,水溶纸是一种可快速溶解的用于封闭管道内保护气体的材料,焊接结束后用水或者蒸汽冲洗焊接后的管道就能使管道里不留下一点水溶纸残渣,里面的气体也很快消失,其特征在于包括以下步骤:
a、长距离管道(2)在进行管道中间接头碰口氩弧焊之前,根据管道管径准备两张直径大于管径100-200mm的水溶纸(1),使水溶纸折叠成水溶纸圆圈(10)部分和水溶纸褶边(11)部分;
b、在管道对口之前,使用胶水(4)在管道(2)内部焊管口两侧管壁的距离所焊管口200-300mm处各粘上一张水溶纸(1),使水溶纸距离管道对口处不要太近,以防焊接过程中产生的热量使贴在管道(2)管壁的水溶纸脱落;
c、在两张水溶纸中的一张水溶纸(1)上开一个排气孔(3)用于排气;
d、对口完成后,并用纸胶带(5)完全封住整个管道(2)的对口缝隙,在缝隙处用连接氩气带(9)的铜管(8)向管道(2)内部充氩气;
e、使用仪器检测到管道(2)内部氩气浓度达到99.9%进行焊接,使用焊枪(7)和焊丝(6)施焊,且当环形焊缝焊接到还剩20mm时应拔掉铜管(8)并快速完成焊接。
2.如权利要求1所述的水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用,其特征在于,所述水溶纸圆圈(10)部分的直径等于管道管径。
3.如权利要求1所述的水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用,其特征在于,所述水溶纸褶边(11)部分的宽度为5-10cm。
4.如权利要求1所述的水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用,其特征在于,所述排气孔(3)的直径为4mm-8mm。
5.如权利要求1所述的水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用,其特征在于,设有排气孔(3)的水溶纸在立管焊接中设置在接头碰口上方管道中。
6.如权利要求1所述的水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用,其特征在于,所述接头碰口在立管焊接中应在上方管道中管道内部充氩气。
7.如权利要求1所述的水溶纸在长距离工业管道中间接头碰口氩弧焊中的应用,其特征在于,所述铜管(8)对于大管径管道焊接应采用2根铜管充氩气。