CN108485189A - A kind of high performance color asphalt - Google Patents

A kind of high performance color asphalt Download PDF

Info

Publication number
CN108485189A
CN108485189A CN201810290048.9A CN201810290048A CN108485189A CN 108485189 A CN108485189 A CN 108485189A CN 201810290048 A CN201810290048 A CN 201810290048A CN 108485189 A CN108485189 A CN 108485189A
Authority
CN
China
Prior art keywords
parts
high performance
color asphalt
petropols
pigment
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810290048.9A
Other languages
Chinese (zh)
Inventor
何岳霖
何元发
陈宇轩
杜小挺
傅世君
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Foshan Road Bang Asphalt Co Ltd
Original Assignee
Foshan Road Bang Asphalt Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Foshan Road Bang Asphalt Co Ltd filed Critical Foshan Road Bang Asphalt Co Ltd
Priority to CN201810290048.9A priority Critical patent/CN108485189A/en
Publication of CN108485189A publication Critical patent/CN108485189A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of high performance color asphalts, are made of the raw material of following parts by weight:50 55 parts by weight of epoxy resin, 23 25 parts of Petropols, 38 parts of styrene butadiene styrene block copolymer, 35 40 parts of furfural extract oil, 25 parts of dioctyl phthalate, 58 parts of diatomite, 5 12 parts of inorganic pigment.The present invention can produce the color asphalt of various colors, improve vision, can be widely used in the different places such as street, pavement and landscape road, can not only meet the needs of various places, while can also beautify the environment.The present invention realizes the color asphalt product for being prepared have excellent performance at lower cost by being formulated global design.

Description

A kind of high performance color asphalt
Technical field
The present invention relates to technical field of road engineering, more particularly to a kind of high performance color asphalt.
Background technology
Elasticity of the Colorful Asphalt Pavement with asphalt concrete is strong, damping strong and is easy to clean the formedness such as flushing Can be outer, the monotonicity of plain asphalt road surface black is further improved, can be collocated with each other, coordinate with the building of surrounding, landscape, have Apparent Landscape benefit.In addition, color asphalt increasingly obtains the organization and management effect of traffic the attention of people.Different colours Bituminous paving, the recognition effect of driver can be improved, and the attention of driver can also be made more to concentrate, to play Induce wagon flow, safe driving, the effect for making traffic administration intuitively change.It, can be with such as in the multiple location of Urban Road Traffic Accidents Driver is intuitively reminded note that driving a vehicle with caution, to a certain extent than vertical traffic sign in making red or yellow road surface And stroke markings are more preferable on track.
But the performance of existing color asphalt is still to be improved.
Invention content
In order to make up the defect of prior art, the present invention provides a kind of high performance color asphalt.
The technical problems to be solved by the invention are achieved by the following technical programs:
A kind of high performance color asphalt, is made of the raw material of following parts by weight:Epoxy resin 50-55 parts by weight, oil 23-25 parts of resin, 3-8 parts of Styrene-Butadiene-Styrene Block Copolymer, 35-40 parts of furfural extract oil, phthalic acid 2-5 parts of dioctyl ester, 5-8 parts of diatomite, 5-12 parts of inorganic pigment.
Further, inorganic pigment be iron oxide red pigment, chrome green pigment, iron green pigment, titanium dioxide pigment, in chrome yellow extremely Few one kind.
Further, the preparation method of the Petropols is:(1)By pentadiene, isoprene, 4- vinyl cyclohexyls Alkene and monoene the hydrocarbon component in mass ratio 1: 0.2: 0.3: 1 obtain dispensing A after evenly mixing;(2)In the reaction kettle with blender Interior, input accounts for the solvent for reacting total 40~60wt% of quality of material in advance, adds total quality of material 1.2-2wt%'s Then Friedel-Crafts catalyst is at the uniform velocity added dispensing A, enables reaction mass react 1-3h at a temperature of 25-60 DEG C, obtain To polymer resin liquid;(3)Above-mentioned polymer resin liquid first carries out alkali cleaning Removal of catalyst with the NaOH solution of concentration 5wt%, then uses Clear water is washed repeatedly to neutrality, obtains light yellow, clear Petropols liquid;(4)Temperature of the Petropols liquid at 210-250 DEG C Lower carry out steam distillation obtains Petropols to remove solvent and oligomer.
Further, preparation method includes the following steps:Furfural extract oil is heated to 160-180 DEG C, then adds stone Oleoresin, epoxy resin, Styrene-Butadiene-Styrene Block Copolymer stirring, then 120-140 DEG C is cooled to, then add Dioctyl phthalate is stirred with diatomite, is finally added inorganic pigment and is stirred for can be obtained product.
The present invention has the advantages that:
The present invention can produce the color asphalt of various colors, improve vision, can be widely used in street, pavement and The different places such as landscape road can not only meet the needs of various places, while can also beautify the environment.
The present invention realizes the color asphalt production for being prepared have excellent performance at lower cost by being formulated global design Product.
Specific implementation mode
With reference to embodiment, the present invention will be described in detail, and embodiment is only the preferred embodiment of the present invention, It is not limitation of the invention.
Embodiment 1
A kind of high performance color asphalt, is made of the raw material of following parts by weight:52 parts by weight of epoxy resin, Petropols 24 parts, 5 parts of Styrene-Butadiene-Styrene Block Copolymer, 38 parts of furfural extract oil, 3 parts of dioctyl phthalate, silicon 6 parts of diatomaceous earth, 9 parts of inorganic pigment.
Wherein, inorganic pigment is iron oxide red pigment.
Preparation method includes the following steps:Furfural extract oil is heated to 160-180 DEG C, then add Petropols, Epoxy resin, Styrene-Butadiene-Styrene Block Copolymer stirring, then 120-140 DEG C is cooled to, then add adjacent benzene two Formic acid dioctyl ester is stirred with diatomite, is finally added inorganic pigment and is stirred for can be obtained product.
Embodiment 2
A kind of high performance color asphalt, is made of the raw material of following parts by weight:55 parts by weight of epoxy resin, Petropols 25 parts, 8 parts of Styrene-Butadiene-Styrene Block Copolymer, 40 parts of furfural extract oil, 5 parts of dioctyl phthalate, silicon 8 parts of diatomaceous earth, 12 parts of inorganic pigment.
Wherein, inorganic pigment is chrome yellow.
Preparation method includes the following steps:Furfural extract oil is heated to 160-180 DEG C, then add Petropols, Epoxy resin, Styrene-Butadiene-Styrene Block Copolymer stirring, then 120-140 DEG C is cooled to, then add adjacent benzene two Formic acid dioctyl ester is stirred with diatomite, is finally added inorganic pigment and is stirred for can be obtained product.
Embodiment 3
A kind of high performance color asphalt, is made of the raw material of following parts by weight:55 parts by weight of epoxy resin, Petropols 25 parts, 8 parts of Styrene-Butadiene-Styrene Block Copolymer, 40 parts of furfural extract oil, 5 parts of dioctyl phthalate, silicon 8 parts of diatomaceous earth, 12 parts of inorganic pigment.
Wherein, inorganic pigment is iron green pigment.
Preparation method includes the following steps:Furfural extract oil is heated to 160-180 DEG C, then add Petropols, Epoxy resin, Styrene-Butadiene-Styrene Block Copolymer stirring, then 120-140 DEG C is cooled to, then add adjacent benzene two Formic acid dioctyl ester is stirred with diatomite, is finally added inorganic pigment and is stirred for can be obtained product.
Embodiments of the present invention above described embodiment only expresses, the description thereof is more specific and detailed, but can not Therefore it is interpreted as the limitation to the scope of the claims of the present invention, as long as skill obtained in the form of equivalent substitutions or equivalent transformations Art scheme should all be fallen within the scope and spirit of the invention.

Claims (4)

1. a kind of high performance color asphalt, is made of the raw material of following parts by weight:Epoxy resin 50-55 parts by weight, stone 23-25 parts of oleoresin, 3-8 parts of Styrene-Butadiene-Styrene Block Copolymer, 35-40 parts of furfural extract oil, O-phthalic 2-5 parts of dioctyl phthalate, 5-8 parts of diatomite, 5-12 parts of inorganic pigment.
2. high performance color asphalt as described in claim 1, which is characterized in that inorganic pigment is iron oxide red pigment, chrome green face At least one of material, iron green pigment, titanium dioxide pigment, chrome yellow.
3. high performance color asphalt as described in claim 1, which is characterized in that the preparation method of the Petropols is: (1)Pentadiene, isoprene, 4 vinyl cyclohexene and monoene the hydrocarbon component in mass ratio 1: 0.2: 0.3: 1 are uniformly mixed After obtain dispensing A;(2)In the reaction kettle with blender, input accounts for the molten of the total 40~60wt% of quality of material of reaction in advance Agent adds the Friedel-Crafts catalyst of total quality of material 1.2-2wt%, and dispensing A is then at the uniform velocity added, enables reactant Material reacts 1-3h at a temperature of 25-60 DEG C, obtains polymer resin liquid;(3)Above-mentioned polymer resin liquid is first with concentration 5wt%'s NaOH solution carries out alkali cleaning Removal of catalyst, then is washed repeatedly to neutrality with clear water, obtains light yellow, clear Petropols Liquid;(4)Petropols liquid carries out steam distillation at a temperature of 210-250 DEG C, to remove solvent and oligomer, obtains oil Resin.
4. high performance color asphalt as described in claim 1, which is characterized in that preparation method includes the following steps:It will Furfural extract oil is heated to 160-180 DEG C, then adds Petropols, epoxy resin, s-B-S block Copolymer stirs, then cools to 120-140 DEG C, then adds dioctyl phthalate and is stirred with diatomite, finally adds nothing Machine pigment is stirred for can be obtained product.
CN201810290048.9A 2018-03-30 2018-03-30 A kind of high performance color asphalt Pending CN108485189A (en)