CN107716777A - 一种cs10前副车架加强板生产工艺 - Google Patents
一种cs10前副车架加强板生产工艺 Download PDFInfo
- Publication number
- CN107716777A CN107716777A CN201610653010.4A CN201610653010A CN107716777A CN 107716777 A CN107716777 A CN 107716777A CN 201610653010 A CN201610653010 A CN 201610653010A CN 107716777 A CN107716777 A CN 107716777A
- Authority
- CN
- China
- Prior art keywords
- cutting edge
- workpiece
- carried out
- hydraulic press
- punch press
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种CS10前副车架加强板生产工艺,其特征是先根据设计的工件展开尺寸,利用剪板机将板料剪下成条料再进行顺序加工:利用专用拉深模,在冲床或液压机上对剪下成的条料进行预拉深加工,利用专用剪边和冲腰形孔模,在冲床或液压机上对工件进行剪边和冲腰型孔加工,利用专用剪边和冲圆形孔模,在冲床或液压机上对已剪边和冲腰型孔的工件进行剪边和冲圆形孔加工,利用专用整形模具,在冲床或液压机上对已剪边和冲圆形孔的工件进行整形加工,再将工件放入滚砂机或研磨机内进行去毛刺加工。产品形状和尺寸一致性好,质量稳定可靠,操作简便、安全,生产周期短,材料利用率高、成本低,具有推广应用价值。
Description
技术领域
本发明涉及一种汽车零部件生产方法,特别是一种CS10前副车架加强板生产工艺。
背景技术
目前,在前副车架加强板的生产中,普遍采用简易模具手工成形,钻孔加工,存在零件加工后形状、尺寸一致性差,操作繁琐,生产周期长,生产效率低、成本高。
发明内容
本发明的目的是为了克服现有技术的上述不足之处,而提供一种产品形状和尺寸一致性好,质量稳定可靠,操作简便、安全,生产周期短,材料利用率高、成本低的CS10前副车架加强板生产工艺。
为实现上述发明目的,本发明采用的具体工艺方法是先根据设计的工件展开尺寸,利用剪板机将板料剪下成条料再进行顺序加工:利用专用拉深模,在冲床或液压机上对剪下成的条料进行预拉深加工,利用专用剪边和冲腰形孔模,在冲床或液压机上对工件进行剪边和冲腰型孔加工,利用专用剪边和冲圆形孔模,在冲床或液压机上对已剪边和冲腰型孔的工件进行剪边和冲圆形孔加工,利用专用整形模具,在冲床或液压机上对已剪边和冲圆形孔的工件进行整形加工,再将工件放入滚砂机或研磨机内进行去毛刺加工。
本发明由于采用以上工艺方法,产品形状和尺寸一致性好,质量稳定可靠,操作简便、安全,生产周期短,材料利用率高、成本低,具有推广应用价值。
具体实施方案
先根据设计的工件展开尺寸,利用剪板机将板料剪下成条料再进行顺序加工:利用专用拉深模,在冲床或液压机上对剪下成的条料进行预拉深加工,利用专用剪边和冲腰形孔模,在冲床或液压机上对工件进行剪边和冲腰型孔加工,利用专用剪边和冲圆形孔模,在冲床或液压机上对已剪边和冲腰型孔的工件进行剪边和冲圆形孔加工,利用专用整形模具,在冲床或液压机上对已剪边和冲圆形孔的工件进行整形加工,再将工件放入滚砂机或研磨机内进行去毛刺加工。
Claims (1)
1.一种CS10前副车架加强板生产工艺,其特征是先根据设计的工件展开尺寸,利用剪板机将板料剪下成条料再进行顺序加工:利用专用拉深模,在冲床或液压机上对剪下成的条料进行预拉深加工,利用专用剪边和冲腰形孔模,在冲床或液压机上对工件进行剪边和冲腰型孔加工,利用专用剪边和冲圆形孔模,在冲床或液压机上对已剪边和冲腰型孔的工件进行剪边和冲圆形孔加工,利用专用整形模具,在冲床或液压机上对已剪边和冲圆形孔的工件进行整形加工,再将工件放入滚砂机或研磨机内进行去毛刺加工。