CN107594612B - Aroma producing material for cigarette capable of being heated and burned and preparation method thereof - Google Patents

Aroma producing material for cigarette capable of being heated and burned and preparation method thereof Download PDF

Info

Publication number
CN107594612B
CN107594612B CN201710794490.0A CN201710794490A CN107594612B CN 107594612 B CN107594612 B CN 107594612B CN 201710794490 A CN201710794490 A CN 201710794490A CN 107594612 B CN107594612 B CN 107594612B
Authority
CN
China
Prior art keywords
weight
extract
parts
aroma
coating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201710794490.0A
Other languages
Chinese (zh)
Other versions
CN107594612A (en
Inventor
王勤龙
杨涛
沈彦文
范馨雷
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yunnan Bazi Biotechnology Co ltd
Yunnan Chunxu Biotechnology Co ltd
Original Assignee
Yunnan Bagu Biotechnology Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yunnan Bagu Biotechnology Co ltd filed Critical Yunnan Bagu Biotechnology Co ltd
Priority to CN201710794490.0A priority Critical patent/CN107594612B/en
Publication of CN107594612A publication Critical patent/CN107594612A/en
Application granted granted Critical
Publication of CN107594612B publication Critical patent/CN107594612B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention relates to an aroma-producing material for heating non-combustion cigarettes and a preparation method thereof. The preparation method comprises the steps of preparing coating materials, coating and the like. The aroma-producing material prepared by using the coating material mainly containing the natural extract has the aroma quality closer to that of the traditional cigarette. Meanwhile, the aroma-producing material is applied to heating non-combustion cigarettes, can improve the heat conduction uniformity and the smoke quantity of the cigarettes, achieves the effect of improving the overall smoking quality of the cigarettes, and can be effectively utilized when the heating non-combustion cigarettes are smoked.

Description

Aroma producing material for cigarette capable of being heated and burned and preparation method thereof
[ technical field ] A method for producing a semiconductor device
The invention belongs to the technical field of tobacco materials. More specifically, the present invention relates to a flavor-producing material for heated non-burning cigarettes, and also relates to a method for producing the flavor-producing material for heated non-burning cigarettes.
[ background of the invention ]
Unlike conventional cigarettes, heated non-burning cigarettes are smoked by heating a non-burning cartridge with electronic equipment, allowing consumers to smoke the tobacco flavor while reducing harmful smoke constituents resulting from combustion and thermal cracking in conventional cigarettes.
The heating non-combustion cigarette smoking product mainly comprises an aerosol generating device, an aerosol cooling device and an aerosol filtering device; the heating element inside the aerosol generating device heats the aerosol generating substrate to generate aerosol, the aerosol is cooled by the heat transfer of the aerosol cooling device to reduce the temperature of the aerosol, and the aerosol is filtered by the aerosol filtering device. The aerosol generating device is composed of a heating element and a fragrance producing base body, and the fragrance producing base body is composed of a fragrance producing material. In a heating non-combustion cigarette system, when the aroma-producing material used in the prior art is heated by a heating element, the heat transfer is not uniform, so that the smoking quantity is often insufficient, the smoking quality is not high, and the smoking feeling of a consumer is further influenced; meanwhile, the aroma-producing material is not effectively utilized due to the non-uniformity of heat transfer; therefore, the present inventors have conducted intensive studies on a fragrance-producing material, and have finally completed the present invention.
[ summary of the invention ]
[ problem to be solved ]
The invention aims to provide an aroma producing material for heating non-combustion cigarettes.
Another object of the present invention is to provide a method for preparing the aroma-producing material for heated non-burning cigarettes.
[ solution ]
The invention is realized by the following technical scheme.
The invention relates to a preparation method of an aroma-producing material for cigarette which is not combusted by heating.
The preparation method comprises the following steps:
A. preparation of the coating Material
Mixing 20-50 parts by weight of tobacco extract, 3-4 parts by weight of red date extract, 2-5 parts by weight of plum extract, 0.5-1.5 parts by weight of fenugreek extract, 0.5-1.0 part by weight of maple extract, 5-15 parts by weight of propylene glycol, 1-4 parts by weight of glyceryl triacetate, 2.0-3.5 parts by weight of 1.3 butanediol, 1.0-2.5 parts by weight of triethylene glycol and 2-5 parts by weight of water, supplementing to 100 parts by weight of glycerol, mixing and stirring uniformly to obtain the coating material;
B. coating of
B, using a forming paper coating machine to apply the coating material obtained in the step A to a coating machine, wherein the unreeling tension is 10-20N, the vehicle speed is 80-100 m/min, and the coating material amount is 1.0-1.5 g/m2And dip-coating the coating material on transfer aluminum foil paper at the temperature of 40-45 ℃ and the drying temperature of 100-140 ℃ to obtain the aroma-producing material for the cigarette which is not combusted by heating.
According to another preferred embodiment of the present invention, in step a, the weight ratio of tobacco extract, red date extract, plum extract, fenugreek extract, maple extract, propylene glycol, glyceryl triacetate, 1.3 butanediol, triethylene glycol to water is 28-42: 3.2-3.8: 2.4-3.6: 0.8-1.2: 0.6-0.9: 8-12: 1.6-3.2: 2.4-3.0: 1.6-1.8: 2.8 to 4.2.
According to another preferred embodiment of the present invention, the tobacco extract is a yunyan tobacco extract or a Hunan tobacco extract.
According to another preferred embodiment of the invention, in the step B, the gram weight of the transfer aluminum foil paper is 25-65 g/m2
According to another preferred embodiment of the present invention, in the step B, the trough of the forming paper coating machine is a heat-insulating trough capable of reaching a heating temperature of 40 to 45 ℃.
The invention also relates to the fragrance-producing material prepared by the preparation method.
The present invention will be described in more detail below.
The invention relates to a preparation method of an aroma-producing material for cigarette which is not combusted by heating.
The preparation method comprises the following steps:
A. preparation of the coating Material
Mixing 20-50 parts by weight of tobacco extract, 3-4 parts by weight of red date extract, 2-5 parts by weight of plum extract, 0.5-1.5 parts by weight of fenugreek extract, 0.5-1.0 part by weight of maple extract, 5-15 parts by weight of propylene glycol, 1-4 parts by weight of glyceryl triacetate, 2.0-3.5 parts by weight of 1.3 butanediol, 1.0-2.5 parts by weight of triethylene glycol and 2-5 parts by weight of water, supplementing to 100 parts by weight of glycerol, mixing and stirring uniformly to obtain the coating material;
in the invention, tobacco extract, red date extract, plum extract, fenugreek extract and maple extract form aroma components; wherein the tobacco extract mainly has the functions of providing the tobacco original fragrance and constructing a tobacco fragrance framework; the red date extract has the main functions of improving the thick feeling and the aroma texture; the plum extract has the main functions of improving the suction comfort, improving the taste and reducing the stimulation; the common fenugreek seed extract has the main functions of improving aroma texture and richness; the maple extract has the main functions of improving the aroma texture and reducing the miscellaneous gas.
The main functions of the invention using propylene glycol, glyceryl triacetate, butylene glycol, triethylene glycol and glycerol are two-fold, on one hand, to dissolve the aroma components and act as a solvent, and on the other hand, to generate smoke when the aroma-producing material is smoked and act as a smoke generator.
In the invention, when the using amount of the tobacco extract is 20-50 parts by weight, the red date extract is 3-4 parts by weight, the plum extract is 2-5 parts by weight, the fenugreek extract is 0.5-1.5 parts by weight and the maple extract is 0.5-1.0 part by weight, the sensory evaluation aroma amount of aroma components is sufficient, the aroma is rich, the aroma texture is good, the smoke concentration is moderate, the stimulation is small, the offensive odor is low, the comfort is good, and the harmony is good. If the dosage of the tobacco extract, the red date extract, the plum extract, the fenugreek extract and the maple extract exceeds the respective dosage range, namely the dosage of the tobacco extract, the red date extract, the plum extract, the fenugreek extract and the maple extract is lower than the respective dosage lower limit or higher than the respective dosage upper limit, sensory evaluation of aroma components or unclear aroma skeleton, slightly less aroma amount, poor aroma richness, poor aroma texture, or slightly obvious stimulation, poor taste and large offensive odor.
According to the invention, propylene glycol, glyceryl triacetate, 1.3 butanediol, triethylene glycol and water form a fuming component, and when the using amount of propylene glycol is 5-15 parts by weight, 1-4 parts by weight of glyceryl triacetate, 2.0-3.5 parts by weight of 1.3 butanediol, 1.0-2.5 parts by weight of triethylene glycol and 2-5 parts by weight of water, the obtained coating material has good solubility, moderate viscosity and good coating uniformity, and the smoke concentration generated when the fragrance-producing material is sucked is high. When the propylene glycol, glyceryl triacetate, 1.3 butanediol, triethylene glycol and water are used in amounts exceeding their respective ranges, i.e., the amounts are below their respective lower limits or above their respective upper limits, the resulting coating has poor solubility, too low or too high a viscosity, poor coating uniformity, or low smoke concentration when the fragrance-producing material is smoked.
Therefore, the weight ratio of the tobacco extract, the red date extract, the plum extract, the fenugreek extract, the maple extract, the propylene glycol, the glyceryl triacetate, the 1.3 butanediol, the triethylene glycol and the water is 20-50: 3-4: 2-5: 0.5-1.5: 0.5-1.0: 5-15: 1-4: 2.0-3.5: 1.0-2.5: 2 to 5.
Preferably, the weight ratio of the tobacco extract, the red date extract, the plum extract, the fenugreek extract, the maple extract, the propylene glycol, the glyceryl triacetate, the 1.3 butanediol, the triethylene glycol and the water is 28-42: 3.2-3.8: 2.4-3.6: 0.8-1.2: 0.6-0.9: 8-12: 1.6-3.2: 2.4-3.0: 1.6-1.8: 2.8 to 4.2.
The tobacco extract, the red date extract, the plum extract, the fenugreek extract and the maple extract used in the invention are all products sold in the current market, for example, the tobacco extract is a product sold under the trade name of Yunyan tobacco extract by Henban scientific and technological Limited in Yunnan or a product sold under the trade name of Hunan tobacco extract by Hendeyang biological scientific and technological Limited in Hendeyang; the red date extract, plum extract, fenugreek extract and maple extract are, for example, products sold under the trade names red date extract, plum extract, fenugreek extract and maple extract by Xinzheng gold leaf essence and perfume Limited or Kaihe elegant essence and perfume Limited.
In the present invention, propylene glycol, glyceryl triacetate, butylene glycol, triethylene glycol, glycerol, which are currently commercially available food grade products such as those sold under the trade names propylene glycol, glycerol by guangzhou exhibition chemical company; products sold under the trade names glyceryl triacetate, butanediol, triethylene glycol by the company of Enoku chemical, Lucobia, Yoshiguan.
B. Coating of
B, using a forming paper coating machine to apply the coating material obtained in the step A to a coating machine, wherein the unreeling tension is 10-20N, the vehicle speed is 80-100 m/min, and the coating material amount is 1.0-1.5 g/m2And dip-coating the coating material on transfer aluminum foil paper at the temperature of 40-45 ℃ and the drying temperature of 100-140 ℃ to obtain the aroma-producing material for the cigarette which is not combusted by heating.
In the step of the invention, the gram weight of the transfer aluminum foil paper is 25-65 g/m2. The transfer aluminum foil used in the present invention is a product generally used in the field of tobacco production, such as a product sold under the trade name JZ-0167 by yuxichun and tipping paper limited.
In the present invention, the coating apparatus used is a forming paper coater, which is a product currently marketed, for example, by Virgie fine mechanical packaging, Inc. of Changzhou under the trade name coater LZ-0704Z.
The trough of the forming paper coating machine used in the invention is a heat-insulating trough with heating temperature of 40-45 ℃.
The invention also relates to the fragrance-producing material prepared by the preparation method.
Compared with the conventional heating non-combustion cigarette product, the aroma-producing material can improve the heat conduction uniformity of the heating non-combustion cigarette when applied to the heating non-combustion cigarette, for example, the aroma-producing base body composed of the aroma-producing material is divided into 3 sections at equal intervals and placed in a cigarette filter stick, the middle point is selected for each section, the aerosol temperature of the middle points is measured under the conditions that the temperature is 22 +/-2 ℃ and the relative humidity is 60 +/-2% according to a thermocouple method, and the temperature of the aroma-producing base body is sequentially improved by more than 60 ℃, more than 40 ℃ and more than 30 ℃ from the middle point close to the electronic heating element section; meanwhile, according to the sensory quality evaluation method of the YCT 138-.
[ advantageous effects ]
The invention has the beneficial effects that: the aroma-producing material prepared by using the coating material mainly containing the natural extract has the aroma quality closer to that of the traditional cigarette. Meanwhile, the aroma-producing material is applied to heating non-combustion cigarettes, can improve the heat conduction uniformity and the smoke quantity of the cigarettes, achieves the effect of improving the overall smoking quality of the cigarettes, and can be effectively utilized when the heating non-combustion cigarettes are smoked.
[ detailed description ] embodiments
The invention will be better understood from the following examples.
Example 1: preparation of aroma-producing material for cigarette
The implementation steps of this example are as follows:
A. preparation of the coating Material
Mixing 20 parts by weight of Yunyan tobacco extract sold by Henan gang Hengji science and technology Limited, 3 parts by weight of red date extract sold by Kaifeng river elegant essence and spice Limited, 2 parts by weight of plum extract sold by Kaifeng river elegant essence and spice Limited, 0.5 part by weight of fenugreek extract sold by Kaifeng river elegant essence and spice Limited, 0.5 part by weight of maple extract sold by Kaifeng river elegant essence and spice Limited, 5 parts by weight of propylene glycol, 1 part by weight of glyceryl triacetate, 2.0 parts by weight of 1.3 butanediol, 1.0 part by weight of triethylene glycol and 2 parts by weight of water, supplementing to 100 parts by weight of glycerol, and uniformly mixing and stirring to obtain the coating material;
B. coating of
The coating obtained in step A was applied to a forming paper coater sold under the trade name of coater LZ-0704Z by Virgi Seiko, Van at a unwinding tension of 10N, a vehicle speed of 80m/min, and a coating amount of 1.0g/m2The coating material is dipped and coated at 25g/m under the conditions of 40 ℃ of coating material temperature and 100 ℃ of drying temperature2Transferring the aluminum foil paper to obtain the aroma-producing material for the cigarette which is not combusted by heating.
According to the determination of the method described in the specification, compared with the conventional heating non-combustion cigarette product, the aroma-producing material prepared by the embodiment can improve the uniformity of heat conduction of the heating non-combustion cigarette when used for heating the non-combustion cigarette, the aroma-producing base body composed of the aroma-producing material is divided into 3 sections at equal intervals and placed in a cigarette filter stick, the middle point of each section is selected, and the temperature of the aroma-producing base body is sequentially improved by 60 ℃, 40 ℃ and 30 ℃ from the middle point close to the electronic heating element section; meanwhile, sensory evaluation results show that when the aroma-producing material is applied to the cigarette with the heating non-combustion cigarette, the aroma texture and richness are good, the comfort of the oral cavity is good, the overall smoking quality is high, and the smoke output is also high.
Example 2: preparation of aroma-producing material for cigarette
The implementation steps of this example are as follows:
A. preparation of the coating Material
Mixing 30 parts by weight of Yunyan tobacco extract sold by Henan gang Hengbo science and technology Limited, 3.3 parts by weight of red date extract sold by Kaifeng river elegant essence and flavor Limited, 3 parts by weight of plum extract sold by Kaifeng river elegant essence and flavor Limited, 0.8 part by weight of fenugreek extract sold by Kaifeng river elegant essence and flavor Limited, 0.65 part by weight of maple extract sold by Kaifeng river elegant essence and flavor Limited, 8 parts by weight of propylene glycol, 2 parts by weight of glyceryl triacetate, 2.5 parts by weight of 1.3 butanediol, 1.5 parts by weight of triethylene glycol and 3 parts by weight of water, supplementing to 100 parts by weight of glycerol, and uniformly mixing and stirring to obtain the coating material;
B. coating of
The coating obtained in step A was applied to a forming paper coater sold under the trade name of coater LZ-0704Z by Virgi Seiko, Van at a unwinding tension of 13N, a vehicle speed of 86m/min, and a coating amount of 1.2g/m2The coating material is dipped and coated at 38g/m under the conditions of the temperature of 41.5 ℃ and the drying temperature of 115 DEG C2Transferring the aluminum foil paper to obtain the aroma-producing material for the cigarette which is not combusted by heating.
According to the determination of the method described in the specification, compared with the conventional heating non-combustion cigarette product, the aroma-producing material prepared by the embodiment can improve the uniformity of heat conduction of the heating non-combustion cigarette when used for heating the non-combustion cigarette, the aroma-producing base body composed of the aroma-producing material is divided into 3 sections at equal intervals and placed in a cigarette filter stick, the middle point of each section is selected, and the temperature of the aroma-producing base body is sequentially improved by 60 ℃, 45 ℃ and 40 ℃ from the middle point close to the electronic heating element section; meanwhile, the sensory evaluation results were similar to those of example 1.
Example 3: preparation of aroma-producing material for cigarette
The implementation steps of this example are as follows:
A. preparation of the coating Material
Mixing 40 parts by weight of Yunyan tobacco extract sold by Henan gang Hengbo science and technology Limited, 3.6 parts by weight of red date extract sold by Kaifeng river elegant essence and flavor Limited, 4 parts by weight of plum extract sold by Kaifeng river elegant essence and flavor Limited, 1.1 parts by weight of fenugreek extract sold by Kaifeng river elegant essence and flavor Limited, 0.8 part by weight of maple extract sold by Kaifeng river elegant essence and flavor Limited, 11 parts by weight of propylene glycol, 3 parts by weight of glyceryl triacetate, 3 parts by weight of 1.3 butanediol, 2 parts by weight of triethylene glycol and 4 parts by weight of water, supplementing to 100 parts by weight with glycerol, and uniformly mixing and stirring to obtain the coating material;
B. coating of
Using a commercial product from Virgie Seiko K.K.The coating material obtained in the step A is coated by a forming paper coating machine sold by a brand coating machine LZ-0704Z under the conditions of unwinding tension of 16N, vehicle speed of 92m/min and coating material amount of 1.5g/m2The coating material is dipped and coated at 51g/m under the conditions of 43 ℃ of coating material temperature and 130 ℃ of drying temperature2Transferring the aluminum foil paper to obtain the aroma-producing material for the cigarette which is not combusted by heating.
According to the determination of the method described in the specification, compared with the conventional heating non-combustion cigarette product, the aroma-producing material prepared by the embodiment can improve the uniformity of heat conduction of the heating non-combustion cigarette when used for heating the non-combustion cigarette, the aroma-producing base body composed of the aroma-producing material is divided into 3 sections at equal intervals and placed in a cigarette filter stick, the middle point of each section is selected, and the temperature of the aroma-producing base body is sequentially improved by 75 ℃, 45 ℃ and 32 ℃ from the middle point close to the electronic heating element section; meanwhile, the sensory evaluation results were similar to those of example 1.
Example 4: preparation of aroma-producing material for cigarette
The implementation steps of this example are as follows:
A. preparation of the coating Material
Mixing 50 parts by weight of Yunyan extract sold by Changde Zhengyang biotechnology limited company, 4 parts by weight of red date extract sold by Kaifeng river elegant essence and spice limited company, 5 parts by weight of plum extract sold by Kaifeng river elegant essence and spice limited company, 1.5 parts by weight of fenugreek extract sold by Kaifeng river elegant essence and spice limited company, 1 part by weight of maple extract sold by Kaifeng river elegant essence and spice limited company, 15 parts by weight of propylene glycol, 4 parts by weight of glyceryl triacetate, 3.5 parts by weight of 1.3 butanediol, 2.5 parts by weight of triethylene glycol and 5 parts by weight of water, supplementing to 100 parts by weight of glycerol, and uniformly mixing and stirring to obtain the coating material;
B. coating of
The coating obtained in step A was applied to a forming paper coater sold under the trade name of coater LZ-0704Z by Virgi Seiko, Van at a unwinding tension of 20N, a vehicle speed of 100m/min, and a coating amount of 1.3g/m2The temperature of the coating material is 45 ℃ and the drying temperature is 140 DEG CDipping and coating 65g/m2Transferring the aluminum foil paper to obtain the aroma-producing material for the cigarette which is not combusted by heating.
According to the determination of the method described in the specification, compared with the conventional heating non-combustion cigarette product, the aroma-producing material prepared by the embodiment can improve the uniformity of heat conduction of the heating non-combustion cigarette when used for heating the non-combustion cigarette, the aroma-producing base body composed of the aroma-producing material is divided into 3 sections at equal intervals and placed in a cigarette filter stick, the middle point of each section is selected, and the temperature of the aroma-producing base body is sequentially increased by 68 ℃, 50 ℃ and 35 ℃ from the middle point close to the electronic heating element section; meanwhile, the sensory evaluation results were similar to those of example 1.

Claims (5)

1. A preparation method of an aroma-producing material for cigarette by heating and non-burning is characterized in that the preparation method comprises the following steps:
A. preparation of the coating Material
Mixing 20-50 parts by weight of tobacco extract, 3-4 parts by weight of red date extract, 2-5 parts by weight of plum extract, 0.5-1.5 parts by weight of fenugreek extract, 0.5-1.0 part by weight of maple extract, 5-15 parts by weight of propylene glycol, 1-4 parts by weight of glyceryl triacetate, 2.0-3.5 parts by weight of 1.3 butanediol, 1.0-2.5 parts by weight of triethylene glycol and 2-5 parts by weight of water, supplementing to 100 parts by weight of glycerol, mixing and stirring uniformly to obtain the coating material; the tobacco extract is a Yunyan tobacco extract or a Hunan tobacco extract;
B. coating of
B, using a forming paper coating machine to apply the coating material obtained in the step A to a coating machine, wherein the unreeling tension is 10-20N, the vehicle speed is 80-100 m/min, and the coating material amount is 1.0-1.5 g/m2And dip-coating the coating material on transfer aluminum foil paper at the temperature of 40-45 ℃ and the drying temperature of 100-140 ℃ to obtain the aroma-producing material for the cigarette which is not combusted by heating.
2. The preparation method according to claim 1, wherein in the step A, the weight ratio of the tobacco extract, the red date extract, the plum extract, the fenugreek extract, the maple extract, the propylene glycol, the glyceryl triacetate, the 1.3 butanediol, the triethylene glycol and the water is 28-42: 3.2-3.8: 2.4-3.6: 0.8-1.2: 0.6-0.9: 8-12: 1.6-3.2: 2.4-3.0: 1.6-1.8: 2.8 to 4.2.
3. The preparation method of claim 1, wherein in the step B, the grammage of the transfer aluminum foil paper is 25-65 g/m2
4. The manufacturing method according to claim 1, wherein in the step B, the trough of the form paper coating machine is a heat-insulating trough capable of heating to 40 to 45 ℃.
5. The fragrance-producing material produced by the production method according to any one of claims 2 to 4.
CN201710794490.0A 2017-09-06 2017-09-06 Aroma producing material for cigarette capable of being heated and burned and preparation method thereof Active CN107594612B (en)