CN1072757C - 纸模板混凝土地砖施工方法 - Google Patents
纸模板混凝土地砖施工方法 Download PDFInfo
- Publication number
- CN1072757C CN1072757C CN 95101376 CN95101376A CN1072757C CN 1072757 C CN1072757 C CN 1072757C CN 95101376 CN95101376 CN 95101376 CN 95101376 A CN95101376 A CN 95101376A CN 1072757 C CN1072757 C CN 1072757C
- Authority
- CN
- China
- Prior art keywords
- concrete
- paper matrix
- floor tile
- matrix plate
- concrete surface
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
本发明为一种纸模板混凝土地砖施工方法,预先将不吸水材质纸料剪裁冲压成所欲拼合地砖相接外形图案部位的空孔,在欲铺设地砖的地面先以混凝土铺敷成平面,再将纸模板覆盖在未干固的混凝土表面,接着洒下一层具有颜色的固化剂,加压使之渗透至表层,待混凝土与颜色固化剂皆干固之后掀掉纸模板,最后涂上一层耐久保护材料即完成全部施工过程,可显著缩短施工周期,增进经济效益。
Description
本发明涉及一种混凝土地砖的施工方法,属于建筑施工铺面技术领域。按照一般常用的地砖施工方法,是在一般混凝土地面完成灌浆、整平、施工过程后,约十五天等待混凝土干固,接着涂敷一层水泥作为地砖与混凝土粘接的界面材料,为了增加地坪坡度的排水与地砖接合时的平整性,第三至十五天之后以水泥内加海菜粉(防止水泥急速干固)搅拌均匀,进行贴地砖工作:施工者必须小心翼翼的将地砖依施工图样花纹予以排列在混凝土上,贴完地砖后三天,接着用泥浆将地砖接缝填平,对于大面积的地面施工,为求地砖排列美观,往往事先须画出指示线条依次铺设施工,由于上述施工程序极为繁复,造成消耗材料、人工、时间甚多,同时地砖施工后,常因天候因素或施工不当,造成地砖与混凝土之间有脱落或凹凸不平的现象,造成长时间的维修,甚是麻烦,而且地砖施工时,会造成大量的垃圾丢弃物,必须人工加以清洁整理,因此地砖铺设成本一直居高不下,影响营建工程的进度掌握,以及施工品质及成本的维持,值得加以改进此种具有明显使用缺点的地砖施工方法。
本发明的目的在于克服上述缺陷的基础上提供一种纸模板混凝土地砖施工方法,施工者可在所铺设的混凝土地面尚未干固之前,以一种不吸水材质的纸模板铺设于混凝土上,并嵌入其表层,使其构成地砖形状之花纹图案排列,接着洒下一层颜色固化剂,使混凝土附着颜色,并增加混凝土表面强度。取下纸模板后涂上一层耐久保护材料,即迅速完成混凝土地砖施工,较一般地砖施工可缩短约四分之三的施工周期,并可节省昂贵地砖材料费用,并且减少三分之二的施工成本,故充分体现施工经济效益原则,上述技术方案确实达到本发明之主要实施目的。
至于本发明之详细施工过程,其他实施目的与功效,参照下列附图作详细说明,即可完全了解:
图一为本发明之纸模板外观构造示意图图二为本发明之纸模板卷绕搁置状态示意图图三为本发明之纸模板敷设时的使用状态示意图图四为本发明之实施流程示意图
图一所示为本发明之纸模板外观构造示意图,将一种不吸水材质纸料予以剪裁冲压成所欲拼合地砖形状空孔100,使所剩余纸模板101作为铺设的地砖相接部位接缝形状,接着将平面展延的纸模板101如图二所示,使之卷绕成束状搁置,由于减少占用的空间,因此储存十分方便。
图三所示为本发明的纸模板敷设时的使用状态示意图,由图可看出当本发明的纸模板101铺设在未干固的混凝土102上时,该纸模板101即承受铺设时迫压的力量而嵌入混凝土表面,使混凝土表层被纸模板101予以模压凹陷形成地砖拼接部位之外表形状。
图四所示为本发明实施流程示意图,由图可看出当本发明欲实施于混凝土地面铺设地砖工程时,首先是在未干固的混凝土表层予以整平,使其表面光滑平整方便施工,接着将如图二所示的呈卷绕状的纸模板101铺设在混凝土表面,轧平后接着洒下色粉材料颜色固化剂,分布于纸模板空孔100部位的混凝土表面,操作者可手持建筑工具墁刀将落在混凝土表面的色粉材料颜色固化剂整平,使其均匀涂布,并依整平所使用的墁刀处的平滑程度以及所洒下的色粉材料颜色固化剂颗粒细度,可在混凝土外部分别形成亮面或粗面的表层构造,当完成铺设纸模板的混凝土完全硬固之后,即可将纸模板101从混凝土表面予以掀起剥离,原来纸模板101覆盖部位形成地砖接缝处,此时可以使用吸尘机将混凝土表面剥落的细石颗粒予以吸除清洁干净,最后再涂上一层擦亮油形成耐久保护层,即可完成整个纸模板混凝土地砖施工过程,此项施工技术运用之范围甚广,而且施工技术效果非常良好,举凡各类桥面、路面、人行道、购物中心、停车场或任何需要以混凝土及地砖作铺设地面的地方皆可加以施工,使其转换成色彩缤纷有如精致砖铺地板一般之使用效果,然而其施工之成本与所耗费之时间仅为一般铺设地砖施工的三分之一而已,因其本身为钢筋混凝土(R、C)结构,故不会有脱落破坏的情形发生,因此可永久不坏,不存在维修的烦恼,具有显著的经济效益和美观,确实为一具有新颖性,创造性和产业上有实用价值的发明。
Claims (1)
1.一种纸模板混凝土地砖施工方法,其特征在于将一种不吸水材质纸料予以剪裁冲压成欲拼合地砖形状空孔,使所剩余纸模板作为铺设的地砖相接部位接缝形状,纸模板铺设在未干固的混凝土上,该纸模板即承受铺设时迫压的力量而嵌入混凝土表面,使混凝土表层被纸模板予以模压凹陷形成地砖拼接部位之外表形状,铺设地砖时,首先在未干固的混凝土表层予以整平,使其表面光滑平整方便施工,接着将呈卷绕状的纸模板铺设在混凝土表面,轧平后接着洒下色粉材料颜色固化剂,分布于纸模板空孔部位的混凝土表面,借助建筑工具墁刀予以整平落在混凝土表面的色粉材料颜色固化剂,使其均匀涂布,并依整平所使用的墁刀处平滑程度以及所洒下的色粉材料固化剂颗粒细度,可在混凝土外部分别形成亮面或粗面的表层构造,当完成铺设纸模板的混凝土完全硬固之后,将纸模板从混凝土表面掀起剥离,原来纸模板覆盖部位形成地砖接缝处,此时可以使用吸尘机将混凝土表面剥落的细石颗粒予以吸除清洁干净,最后再涂上一层擦亮油形成耐久保护层,即可完成整个纸模板混凝土地砖施工过程。