CN107128091A - One kind improves wet film dirty oil plate and falls oily technique - Google Patents

One kind improves wet film dirty oil plate and falls oily technique Download PDF

Info

Publication number
CN107128091A
CN107128091A CN201710386843.3A CN201710386843A CN107128091A CN 107128091 A CN107128091 A CN 107128091A CN 201710386843 A CN201710386843 A CN 201710386843A CN 107128091 A CN107128091 A CN 107128091A
Authority
CN
China
Prior art keywords
ink
wet film
degrees celsius
dirty oil
minutes
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710386843.3A
Other languages
Chinese (zh)
Inventor
叶伟坚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dongguan Xiangguo Photoelectric Technology Co Ltd
Original Assignee
Dongguan Xiangguo Photoelectric Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dongguan Xiangguo Photoelectric Technology Co Ltd filed Critical Dongguan Xiangguo Photoelectric Technology Co Ltd
Priority to CN201710386843.3A priority Critical patent/CN107128091A/en
Publication of CN107128091A publication Critical patent/CN107128091A/en
Pending legal-status Critical Current

Abstract

The present invention provides a kind of wet film dirty oil plate that improves and falls oily technique, comprises the following steps:(1) pre-treatment;(2) print:Ink is printed on by substrate surface using silk screen, the diluent that printing-ink adds 200ml by 4KG black ink and 1KG green ink, which stirs, to be formed;(3) it is pre-baked;(4) expose;(5) develop;(6) lettering is accorded with;(7) bake afterwards:It is 4 baking sections by the program setting of oven;Produce.The beneficial effects of the invention are as follows:The diluent that printing-ink adds 200ml by 4KG black ink and 1KG green ink, which stirs, to be formed, and strengthens the adhesive force of black ink, the stability of raising black ink, then bakes 4 baking sections of setting by after, so as to avoid ink corrugation and fall oil.

Description

One kind improves wet film dirty oil plate and falls oily technique
Technical field
Fall oily technique the present invention relates to board production technical field, more particularly to a kind of wet film dirty oil plate that improves.
Background technology
In board production technique, the purpose of welding resistance technique has three:First is anti-welding, reserves through hole to be welded on plate And its pad, all circuits and copper face are all covered, the short circuit caused during wave soldering are placed, and save the consumption of scolding tin;Second It is backplate, preventing the infringement of moisture and various electrolyte makes circuit aoxidize and endanger electric property, and prevents external machinery wound Do harm to maintain the insulation of plate face well;3rd is insulation, due to plank more and more thinner, and line width is away from more and more thin, thus between conductor Insulation Problems increasingly highlight, also increase the importance of anti-welding varnished insulation.
In the prior art, it is common to use KSM-S6189 dirty oils are printed, and using normal pre-baked exposure imaging ginseng Count, the problem of such technology mode is present is:, easily there is oil in the ink corrugation of printing.
The content of the invention
Based on this, the present invention provides a kind of wet film dirty oil plate that improves and falls oily technique, by reconfiguring matching somebody with somebody for printing-ink Put, and adjust the machined parameters of each processing step, so as to avoid the problem of ink wrinkles, ink is difficult, and improves product Quality.
The present invention provides a kind of wet film dirty oil plate that improves and falls oily technique, comprises the following steps:
(1) pre-treatment:The oxide of substrate surface is removed, increases the roughness of substrate surface, strengthens the attachment of substrate surface ink Power;
(2) print:Ink is printed on by substrate surface using silk screen, printing-ink is by 4KG black ink and 1KG green oil The diluent that ink adds 200ml stirs and formed;
(3) it is pre-baked:Pre-baked temperature be 70 degrees Celsius -75 degrees Celsius, the pre-baked time be 50 points -55 minutes, slightly dry;
(4) expose:Image transfer is carried out using exposure machine;
(5) develop:Unpolymerized photosensitive-ink is removed using solution of potassium carbonate;
(6) lettering is accorded with:The place specified by the way of silk-screen printing in substrate surface stamps character or part symbol;
(7) bake afterwards:It is 4 baking sections by the program setting of oven;First paragraph is 80 degrees Celsius, and baking time is 60 minutes;The Two sections are 100 degrees Celsius, and baking time is 30 minutes;3rd section is 120 degrees Celsius, and baking time is 30 minutes;4th section is 150 degrees Celsius, baking time is 60 minutes;Produce.
It is preferred that, black ink model KSM-S6189 in above-mentioned steps (2).
It is preferred that, above-mentioned steps (2) Green ink types are KSM-S6188.
It is preferred that, pre-baked temperature is 72 degrees Celsius in above-mentioned steps (3).
It is preferred that, the pre-baked time is 52 minutes in above-mentioned steps (3).
It is preferred that, the lattice of 10 lattice of exposure guide rule -12 in above-mentioned steps (4).
It is preferred that, the speed 1.8-2.0M/MIN of development in above-mentioned steps (5).
Beneficial effects of the present invention are:Printing-ink adds 200ml by 4KG black ink and 1KG green ink Diluent stir and form, strengthen the adhesive force of black ink, improve the stability of black ink, then will after bake setting 4 Individual baking section, so as to avoid ink corrugation and fall oil.
Embodiment
For the feature, technological means and the specific purposes reached, function of the present invention can be further appreciated that, with reference to Embodiment is described in further detail to the present invention.
First embodiment:
The present invention provides a kind of wet film dirty oil plate that improves of present invention offer and falls oily technique, comprises the following steps:
(1) pre-treatment:The oxide of substrate surface is removed, increases the roughness of substrate surface, strengthens the attachment of substrate surface ink Power;
(2) print:Ink is printed on by substrate surface using silk screen, printing-ink is by 4KG black ink and 1KG green oil The diluent that ink adds 200ml stirs and formed;Wherein, black ink model KSM-S6189, green ink model KSM-S6188;
(3) it is pre-baked:Pre-baked temperature is 70 degrees Celsius, and the pre-baked time is 50 points, is slightly dried;
(4) expose:Image transfer is carried out using exposure machine;The lattice of 10 lattice of exposure guide rule -12;
(5) develop:Unpolymerized photosensitive-ink is removed using solution of potassium carbonate;The speed 1.8-2.0M/MIN of development;
(6) lettering is accorded with:The place specified by the way of silk-screen printing in substrate surface stamps character or part symbol;
(7) bake afterwards:It is 4 baking sections by the program setting of oven;First paragraph is 80 degrees Celsius, and baking time is 60 minutes;The Two sections are 100 degrees Celsius, and baking time is 30 minutes;3rd section is 120 degrees Celsius, and baking time is 30 minutes;4th section is 150 degrees Celsius, baking time is 60 minutes;Produce.
Second embodiment:
One kind improves wet film dirty oil plate and falls oily technique, comprises the following steps:
(1) pre-treatment:The oxide of substrate surface is taken out, increases the roughness of substrate surface, strengthens the attachment of substrate surface ink Power;
(2) print:Ink is printed on by substrate surface using silk screen, printing-ink is by 4KG black ink and 1KG green oil The diluent that ink adds 200ml stirs and formed;Wherein, black ink model KSM-S6189, green ink model KSM-S6188;
(3) it is pre-baked:Pre-baked temperature is 72 degrees Celsius, and the pre-baked time is 52 points, is slightly dried;
(4) expose:Image transfer is carried out using exposure machine;The lattice of 10 lattice of exposure guide rule -12;
(5) develop:Unpolymerized photosensitive-ink is removed using solution of potassium carbonate;The speed 1.8-2.0M/MIN of development;
(6) lettering is accorded with:The place specified by the way of silk-screen printing in substrate surface stamps character or part symbol;
(7) bake afterwards:It is 4 baking sections by the program setting of oven;First paragraph is 80 degrees Celsius, and baking time is 60 minutes;The Two sections are 100 degrees Celsius, and baking time is 30 minutes;3rd section is 120 degrees Celsius, and baking time is 30 minutes;4th section is 150 degrees Celsius, baking time is 60 minutes;Produce.
3rd embodiment:
One kind improves wet film dirty oil plate and falls oily technique, comprises the following steps:
(1) pre-treatment:The oxide of substrate surface is taken out, increases the roughness of substrate surface, strengthens the attachment of substrate surface ink Power;
(2) print:Ink is printed on by substrate surface using silk screen, printing-ink is by 4KG black ink and 1KG green oil The diluent that ink adds 200ml stirs and formed;Wherein, black ink model KSM-S6189, green ink model KSM-S6188;
(3) it is pre-baked:Pre-baked temperature is 75 degrees Celsius, and the pre-baked time is 55 points, is slightly dried;
(4) expose:Image transfer is carried out using exposure machine;The lattice of 10 lattice of exposure guide rule -12;
(5) develop:Unpolymerized photosensitive-ink is removed using solution of potassium carbonate;The speed 1.8-2.0M/MIN of development;
(6) lettering is accorded with:The place specified by the way of silk-screen printing in substrate surface stamps character or part symbol;
(7) bake afterwards:It is 4 baking sections by the program setting of oven;First paragraph is 80 degrees Celsius, and baking time is 60 minutes;The Two sections are 100 degrees Celsius, and baking time is 30 minutes;3rd section is 120 degrees Celsius, and baking time is 30 minutes;4th section is 150 degrees Celsius, baking time is 60 minutes;Produce.
Embodiment described above only expresses three kinds of embodiments of the present invention, and it describes more specific and detailed, but simultaneously Therefore the limitation to the scope of the claims of the present invention can not be interpreted as.It should be pointed out that for one of ordinary skill in the art For, without departing from the inventive concept of the premise, various modifications and improvements can be made, these belong to the guarantor of the present invention Protect scope.Therefore, the protection domain of patent of the present invention should be determined by the appended claims.

Claims (7)

1. one kind, which improves wet film dirty oil plate, falls oily technique, it is characterised in that comprise the following steps:
(1) pre-treatment:The oxide of substrate surface is removed, increases the roughness of substrate surface, strengthens the attachment of substrate surface ink Power;
(2) print:Ink is printed on by substrate surface using silk screen, printing-ink is by 4KG black ink and 1KG green oil The diluent that ink adds 200ml stirs and formed;
(3) it is pre-baked:Pre-baked temperature be 70 degrees Celsius -75 degrees Celsius, the pre-baked time be 50 points -55 minutes, slightly dry;
(4) expose:Image transfer is carried out using exposure machine;
(5) develop:Unpolymerized photosensitive-ink is removed using solution of potassium carbonate;
(6) lettering is accorded with:The place specified by the way of silk-screen printing in substrate surface stamps character or part symbol;
(7) bake afterwards:It is 4 baking sections by the program setting of oven;First paragraph is 80 degrees Celsius, and baking time is 60 minutes;The Two sections are 100 degrees Celsius, and baking time is 30 minutes;3rd section is 120 degrees Celsius, and baking time is 30 minutes;4th section is 150 degrees Celsius, baking time is 60 minutes;Produce.
2. a kind of wet film dirty oil plate that improves according to claim 1 falls oily technique, it is characterised in that in above-mentioned steps (2) Black ink model KSM-S6189.
3. a kind of wet film dirty oil plate that improves according to claim 1 falls oily technique, it is characterised in that in above-mentioned steps (2) Green ink model KSM-S6188.
4. a kind of wet film dirty oil plate that improves according to claim 1 falls oily technique, it is characterised in that in above-mentioned steps (3) Pre-baked temperature is 72 degrees Celsius.
5. a kind of wet film dirty oil plate that improves according to claim 1 falls oily technique, it is characterised in that in above-mentioned steps (3) The pre-baked time is 52 minutes.
6. a kind of wet film dirty oil plate that improves according to claim 1 falls oily technique, it is characterised in that in above-mentioned steps (4) The lattice of 10 lattice of exposure guide rule -12.
7. a kind of wet film dirty oil plate that improves according to claim 1 falls oily technique, it is characterised in that in above-mentioned steps (5) The speed 1.8-2.0M/MIN of development.
CN201710386843.3A 2017-05-26 2017-05-26 One kind improves wet film dirty oil plate and falls oily technique Pending CN107128091A (en)