CN106813968B - A kind of preparation method of hairtail sagitta cross section - Google Patents

A kind of preparation method of hairtail sagitta cross section Download PDF

Info

Publication number
CN106813968B
CN106813968B CN201710072041.5A CN201710072041A CN106813968B CN 106813968 B CN106813968 B CN 106813968B CN 201710072041 A CN201710072041 A CN 201710072041A CN 106813968 B CN106813968 B CN 106813968B
Authority
CN
China
Prior art keywords
otolith
polishing
hot melt
melt adhesive
hairtail
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201710072041.5A
Other languages
Chinese (zh)
Other versions
CN106813968A (en
Inventor
朱建成
赵宪勇
李显森
孙珊
樊钢洲
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yellow Sea Fisheries Research Institute Chinese Academy of Fishery Sciences
Original Assignee
Yellow Sea Fisheries Research Institute Chinese Academy of Fishery Sciences
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yellow Sea Fisheries Research Institute Chinese Academy of Fishery Sciences filed Critical Yellow Sea Fisheries Research Institute Chinese Academy of Fishery Sciences
Priority to CN201710072041.5A priority Critical patent/CN106813968B/en
Publication of CN106813968A publication Critical patent/CN106813968A/en
Application granted granted Critical
Publication of CN106813968B publication Critical patent/CN106813968B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A kind of preparation method of hairtail sagitta cross section, the invention belongs to experimental technique fields, it includes the following steps:1) label otolith center;2) otolith is clamped on thin head self-locking forceps;3) otolith is embedded with hot melt adhesive;4) polishing otolith is to mark line;5) buffed surface of otolith after polishing is close to and is bonded on glass slide;6) it polishes since otolith front end, is polishing to otolith center, stopping when annual ring occurs, polishing plane is always perpendicular to the cephalocaudal axis of otolith.The present invention embeds otolith with hot melt adhesive, plays resin embedding and fixes and while protective effect, can be cooled to the degree that can be polished only several minutes;While saving resin embedding material, improve work efficiency.

Description

A kind of preparation method of hairtail sagitta cross section
Technical field
The invention belongs to experimental technique fields, more particularly to a kind of preparation method of hairtail sagitta cross section.
Background technology
When carrying out hairtail Age Determination, sagitta (hairtail 3 to maximum 1 pair in otolith, hereinafter abbreviation otolith) is Most commonly used material.Band fish otolith is shaped like rice grain, small and crisp fritter;The band fish otolith of 500 grams of weight, length and width Only 5-6mm and 2.5mm or so, leisure opinion bodily form smaller person.Therefore in conventional method, when preparing otolith cross section, it is mostly used asphalt mixtures modified by epoxy resin Fat is embedded, to carry out subsequent operation.It has main steps that:1) otolith center 2 is marked) carry out embedding 3 with resin) wait for Resin embedding block solidification after, carry out cutting 4 with otolith cutting machine) on otolith polishing and burnishing machine with varigrained sand paper to cutting after Resin embedding block carry out grinding and buffing, to obtain required otolith cross section.
Since the hardening time of resin embedding block is usually more than ten to twenties hours, required time is longer, therefore tight Important place affects working efficiency.
Invention content
The technical problem to be solved in the present invention is to provide a kind of preparation method of hairtail sagitta cross section, the method Embedding speed is fast, can be obtained band fish otolith cross section without cutting.
The present invention is achieved by the following technical solution:
A kind of preparation method of hairtail sagitta cross section, includes the following steps:
1) label otolith center;
2) otolith is clamped on thin head self-locking forceps;
3) otolith is embedded with hot melt adhesive;
Further, the specific method of the embedding is heating hot melt adhesive to 180 degrees Celsius;Otolith is immersed into hot melt adhesive liquid In, otolith fore-end is reserved, hot melt adhesive is not adhered to, the other parts of otolith is allowed uniformly to be embedded by hot melt adhesive.
4) polishing otolith is to mark line;
Further, the polishing process is to polish since otolith rear end, and polishing plane is always perpendicular to the head of otolith Tailing axle.
5) buffed surface of otolith after polishing is close to and is bonded on glass slide;
6) polish since otolith front end, be polishing to otolith center, stopping when annual ring occurs, polishing plane always perpendicular to The cephalocaudal axis of otolith.
The advantageous effect of the present invention compared with prior art
The present invention does not use resin embedding otolith, uses hot melt adhesive instead and is embedded to otolith, plays resin embedding and fixes While with protective effect, because hot melt adhesive cooling velocity is fast, the degree that can be polished can be cooled to only several minutes;So Substantially eliminate the time needed for resin solidification.Meanwhile directly polished using polishing and burnishing machine otolith and after being cut with cutting machine again In contrast, required time is suitable for the mode of polishing.Therefore while saving resin embedding material, work is preferably improved Make efficiency.
Description of the drawings
Fig. 1 hairtail sagitta structural schematic diagrams:1- winged petioles, 2- auditory nerve ditches, the front ends 3-, 4- base leaves, 5- cephalocaudal axis, 6- Ventral margin, the rear ends 7-, 8- otoliths center, 9- back edges, 10- dorsoventral axis;
Fig. 2 label otoliths center;
Otolith is clamped on thin head self-locking forceps by Fig. 3;
Fig. 4 embed otolith with hot melt adhesive;
Fig. 5 polish otolith for the first time;
Otolith is bonded on glass slide by Fig. 6;
Fig. 7 are polishing to otolith center, annual ring occurs.
Specific implementation mode
Embodiment
Technical scheme of the present invention is further explained below by embodiment combination attached drawing, but the protection of the present invention Range is not limited in any form by embodiment.
1) it crosses otolith back edge peak with pencil and draws a line perpendicular to the wide about 0.6mm of its cephalocaudal axis with otolith center (Fig. 2).
2) otolith after label is clamped on thin head self-locking forceps, tweezer point is placed on otolith in auditory nerve ditch, after otolith It is outer (Fig. 3) that end (needing the part ground off) is placed in tweezer point.
3) utilize the hot melt adhesive (CrystalbondTM) in thermal station heating container to 180 degrees Celsius;Otolith is immersed and is heated Glue reserves otolith fore-end, not adhere to hot melt adhesive (convenient for the otolith after polishing for the first time to be bonded on glass slide), allow The other parts of otolith uniformly embed (Fig. 4) by hot melt adhesive.
4) otolith after embedding is placed on experimental bench;After hot melt adhesive cooling, hand-held tweezers are used on otolith polishing and burnishing machine 240 grit papers are polished;When polishing nearly to mark line, uses 400 and 600 grit papers instead successively and be polishing to mark line (Fig. 5).
5) glass slide is placed in thermal station, temperature is adjusted to 160 degree or so.One hand-held self-locking forceps, by the otolith after polishing It is placed on glass slide, buffed surface is close to glass slide;One holds thin head tweezers, after the hotmelt melts of otolith to be wrapped, open from Tweezers are locked, the non-viscose glue part in otolith base leaf front end is clamped with thin head tweezers, is placed on glass slide (Fig. 6).
6) glass slide is removed from thermal station, after hot melt adhesive cooling, sets glass slide on glass slide fixture.Successively with 240, The sand paper of 400 and 600 granularities is polished from otolith front end, is during which inspected with anatomical lens, be milled at otolith center, annual ring it is clear Stop (Fig. 7) when appearance.

Claims (2)

1. a kind of preparation method of hairtail sagitta cross section, it is characterised in that it includes the following steps:
1) label otolith center;
2) otolith is clamped on thin head self-locking forceps;
3) otolith is embedded with hot melt adhesive;
4) polishing otolith is to mark line;
5) buffed surface of otolith after polishing is close to and is bonded on glass slide;
6) it polishes since otolith front end, is polishing to otolith center, stopping when annual ring occurs, polishing plane is always perpendicular to otolith Cephalocaudal axis;The step 3)The specific method of embedding is heating hot melt adhesive to 180 degrees Celsius;Otolith is immersed into hot melt adhesive liquid In, otolith fore-end is reserved, hot melt adhesive is not adhered to, the other parts of otolith is allowed uniformly to be embedded by hot melt adhesive.
2. a kind of preparation method of hairtail sagitta cross section according to claim 1, it is characterised in that the step 4) Polishing process be polish since otolith rear end, polishing plane always perpendicular to the cephalocaudal axis of otolith.
CN201710072041.5A 2017-02-09 2017-02-09 A kind of preparation method of hairtail sagitta cross section Expired - Fee Related CN106813968B (en)