CN106499068A - Acrylate polymer composite waterproof system and its construction method - Google Patents
Acrylate polymer composite waterproof system and its construction method Download PDFInfo
- Publication number
- CN106499068A CN106499068A CN201611111406.2A CN201611111406A CN106499068A CN 106499068 A CN106499068 A CN 106499068A CN 201611111406 A CN201611111406 A CN 201611111406A CN 106499068 A CN106499068 A CN 106499068A
- Authority
- CN
- China
- Prior art keywords
- parts
- waterproof
- acrylate polymer
- basic unit
- waterproof roll
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a kind of acrylate polymer composite waterproof system, including the waterproof material being laid in basic unit, the waterproof material includes the base bond layer being sprayed in basic unit, pastes acrylate polymer waterproof roll thereon and is sprayed on the overcoat of coiled material surface.During construction, chalk line simultaneously ejects in cleaning basic unit, overlaying position spraying base bond layer, take advantage of wet rapid laying acrylate polymer waterproof roll, and flat gauffer is combed with scraper plate, waterproof roll laying is dried after finishing naturally, treats that coiled material is firmly bonded, in its surface even application overcoat, the 24h that dries in the air completes to construct.Triple waterproof constructions of the present invention are cooperateed with mutually, are collectively constituted the waterproof system of high reliability, are overcome the functional limitation of single waterproof material, have impermeability strong, tensile strength is high, and low temperature flexibility is good, and line expansion factor is little, adhesion strength is high, good stability, adaptive deformation ability is strong, long service life, flames of anger operation, the features such as easy construction, environmental protection.
Description
Technical field
The present invention relates to buildings waterproof field, more particularly, to a kind of acrylate polymer composite waterproof system, this
The bright construction method for further relating to the waterproof system.
Background technology
Waterproof material used in China's buildings waterproof construction at present is mainly with elastomer modified asphalt waterproof roll(SBS)
Based on, the technology becomes the mainstream technology of current waterproof construction with easy working feature, accounts for the 70% or so of engineer applied amount.
Its construction method is mainly hot melten type monolayer or double-deck laying, i.e.,:Modified asphalt waterproof coiled material volume is placed on building basal plane, is used
Liquefied gas flame gun is to web edge baking side laying so as to the seam being baked between semi-molten part and roofing or coiled material
Bond together, form the waterproof layer for covering whole building basal plane together, so as to play a part of waterproof.Elastomer modified asphalt
Although waterproof roll and construction technology are the main product of current waterproofing industry and technology, but but there is following defect:1. exist
Substantial amounts of harmful gass are produced in production and work progress, severe contamination is not only caused to environment and also harm workman body is good for
Health;2. main with the construction of high temperature melt process, easily cause disaster hidden-trouble;3. Colophonium class material brittle disconnection in low temperature is split,
Ageing resistance is poor;4. when constructing, the bonding difficulty at the mutual lap-joint of coiled material and edge is larger, and overlap joint and edge are cracked
Become universal leakage hidden trouble;5. coiled material and basal plane cannot strong bond, easily form channeling water between coiled material and basal plane so as to anti-
Water function is lost.
Content of the invention
It is an object of the invention to provide the excellent acrylic ester polymerization of a kind of easy construction, clean and safe and water resistance
Thing composite waterproof system, the present invention also provide the construction method of the waterproof system.
For achieving the above object, the present invention can take following technical proposals:
Acrylate polymer composite waterproof system of the present invention, including the waterproof material being laid in building basic unit,
The waterproof material includes the base bond layer being sprayed in building basic unit, the acrylic acid being pasted onto on the base bond layer
Ester polymer waterproof roll and the overcoat for being sprayed on the waterproof roll surface;
The base bond layer material is by acrylic acid ester emulsion 40-60 parts, film former 8-15 parts, thickening agent 2-6 parts, antifungus agent
2-6 parts, age resister 3-7 parts, defoamer 2-6 parts, soft agent 8-15 parts(Weight portion)It is formulated;
The acrylate polymer waterproof roll is as tire base, and in its two surface impregnations polyphosphazene polymer by polyester filament cloth
Through drying the three-layer composite structure that makes after compound emulsion;
The protection coating materials are by acrylic acid ester emulsion 40-60 parts, film former 8-15 parts, thickening agent 2-6 parts, antifungus agent 2-6
Part, age resister 3-7 parts, defoamer 2-6 parts, wollastonite in powder 6-12 parts, mill base 2-6 parts(Weight portion)It is formulated.
Film former used by present invention preparation base bond layer and protection coating materials, thickening agent, antifungus agent, age resister,
The materials such as defoamer, mill base, soft agent all using commercially available existing product, without other particular/special requirements.
The construction method of acrylate polymer composite waterproof system of the present invention includes following concrete steps:
The first step, Dai Pu basic units are cleared up, and remove floating dust, greasy dirt and debris, and basic unit is for example damaged, loose or uneven, uses water
Mud waterproof mortar is repaired;
Second step, ejects chalk line or the line of ink marker, in the basic unit for handling well by acrylate polymer waterproof roll in precalculated position
Opening carries out overlaying rear backrush, is then overlaying spraying base bond layer at position:Quantity for spray is 0.75kg/m2~1kg/m2, spray
Apply thickness >=1 millimeter;
3rd step, take advantage of base bond layer wet when rapid laying acrylate polymer waterproof roll, and with scraper plate along web width
Flat gauffer is combed in direction, alice, gauffer, hollowing phenomenon must not occurs;
4th step, the laying of acrylate polymer waterproof roll are dried 4 ~ 8 hours after finishing naturally, after coiled material is firmly bonded,
In its surface even application overcoat:Quantity for spray 1kg/m2~1.2kg/m2, coating thickness >=1.2 millimeter, dry in the air after the completion of spraying 24h
Complete to construct.
The acrylate polymer composite waterproof system of the present invention, is waterproof material that is different by three kinds of performances and having complementary advantages
Material forms the waterproof system with triple safeguard structures by spraying bonding.Ground floor is the base with building basic unit directly contact
Plinth adhesive linkage, with extensibility height, permeates the features such as bonding force is strong, low temperature flexibility is good, can not only be with building basic unit and waterproof volume
Material carries out good combination, can also the minute crack for building basic unit be repaired.The second layer is waterproof roll enhancement layer, adopts
Acrylate polymer waterproof roll be that applicant applies on January 28th, 2016《Environment-friendly type composite of water-proof coiled material and its life
Product method》(Application number:201610059435.2)Waterproof roll, with Ultra-Drawing intensity and water resistance, pulling force is reachable
More than 1000N/50mm.Third layer is surface protecting layer, using spraying coating process, is formed on waterproof roll surface and have together well
Rigidity and high-low temperature resistant, uvioresistant, aging resistance, erosion-resisting fish tail and waterproof layer, are not only carried out to waterproof roll well
Protection, can also be effectively prevented coiled material lapping position and produce alice phenomenon.Triple waterproof constructions are cooperateed with mutually, collectively constitute one
The waterproof system of complete high reliability, overcomes the functional limitation of single waterproof material, and strong with impermeability, tension is strong
Degree is high, and low temperature flexibility is good, and line expansion factor is little, and adhesion strength is high, good stability, and adaptive deformation ability is strong, and long service life, without bright
The features such as fiery operation, easy construction, environmental protection.
The waterproof system construction method of the present invention is simple and environmentally-friendly, using cold technology, in production and work progress not
Any pollution can be produced, the waterproof system after construction is checked through national building materials monitoring center, complies fully with national green ring
Protect product standard;The technique combined with coiled material wet-laid process using spraying technology during construction, high working efficiency, without high-temperature heating and
Work with torches, is effectively guaranteed construction quality and safety;Acrylate polymer has superpower anti-ultraviolet, anti-height
Temperature, ageing resistace, have more reliable water resistance and longer service life using the waterproof material that acrylate is produced;
Using flexible water latex between waterproof roll and building basic unit(Base bond layer)Using full bonding construct, it is ensured that coiled material with build
Build base adhesive firmly, so as to overcome the defect that channeling water occurs between coiled material and basic unit;The waterproof of coiled material surface spraying is anti-old
Change film(Overcoat), make whole waterproof system form an entirety, not only increase intensity and the thickness of waterproof system, also
Effect the phenomenon for occurring alice at coiled material lapping is prevented.
The waterproof system of the present invention can be in building basic unit that is moist or drying(Concrete, timber, metallic plate, plastic plate, guarantor
Adiabator and other waterproof materials)Upper directly construction, can be widely used in the waterproofs such as the roofing of new and old building, underground, interior, pond
Engineering, and the special waterproofing work such as subway, tunnel, road and bridge, water channel.It is applied to China major part climatological region and ambient temperature
In subzero 20 DEG C or so of extremely frigid zones, for selection by the adjustable multicolour of allotting of mill base, there is good decorative effect.
Description of the drawings
Fig. 1 is the section structure schematic diagram of waterproof system of the present invention.
Specific embodiment
As shown in figure 1, the acrylate polymer composite waterproof system of the present invention, it is by being sprayed in building basic unit 1
Base bond layer 2, the acrylate polymer waterproof roll 3 being pasted onto on base bond layer 2 and it is sprayed on waterproof roll surface
Overcoat 4 constitute, wherein the present invention used by acrylate polymer waterproof roll 3 be by polyester filament cloth as tire base,
And in its two surface impregnations emulsion polymerization(By acrylic acid ester emulsion, film former, thickening agent, defoamer, antifungus agent,
Solid packing etc. is formulated)By the three-layer composite structure that drying is made.
The base bond layer material of the present invention is by acrylic acid ester emulsion 40-60 parts, film former 8-15 parts, thickening agent 2-6
Part, antifungus agent 2-6 parts, age resister 3-7 parts, defoamer 2-6 parts, the flexibility that soft agent 8-15 parts are formed after mixing
Waterproof glue;
Protection coating materials are by acrylic acid ester emulsion 40-60 parts, film former 8-15 parts, thickening agent 2-6 parts, antifungus agent 2-6 parts, resist
Aging dose of 3-7 part, defoamer 2-6 parts, wollastonite in powder 6-12 parts, the rigid waterproofing glue that mill base 2-6 parts are formed after mixing.
Film former used by present invention preparation base bond layer and protection coating materials, thickening agent, antifungus agent, age resister,
The materials such as defoamer, mill base, soft agent are all using commercially available existing product.As defoamer can adopt NXZ defoamer, film former
12 film former of alcohol ester, thickening agent can be adopted to adopt TRM-203 thickening agents, etc..
The construction method of acrylate polymer composite waterproof system of the present invention is:
The first step, Dai Pu basic units 1 are cleared up, and remove floating dust, greasy dirt and debris, and basic unit is for example damaged, loose or uneven, uses water
Mud waterproof mortar is repaired;
Second step, ejects chalk line or the line of ink marker, in the basic unit 1 for handling well by acrylate polymer waterproof roll 3 in pre-determined bit
Putting opening carries out overlaying rear backrush, is then overlaying spraying base bond layer 2 at position:Quantity for spray is 0.75kg/m2~1kg/m2,
Coating thickness >=1 millimeter;
3rd step, take advantage of base bond layer 2 wet when rapid laying acrylate polymer waterproof roll 3, and with scraper plate along coiled material width
Flat gauffer is combed in degree direction, alice, gauffer, hollowing phenomenon must not occurs;
4th step, the laying of acrylate polymer waterproof roll 3 are dried 4 ~ 8 hours after finishing naturally, after coiled material is firmly bonded,
In its surface even application overcoat 4:Quantity for spray 1kg/m2~1.2kg/m2, coating thickness >=1.2 millimeter are noted in spraying process
Spray coating mechanical must not damage sprayed coating, and the 24h that dries in the air after the completion of spraying completes to construct.
5th step, the waterproof system after completion need installation Technology code to test, and such as find unqualified part
Must do over again immediately process, until engineering all qualified.
Claims (2)
1. a kind of acrylate polymer composite waterproof system, including the waterproof material being laid in building basic unit, its feature exists
In:The waterproof material includes the base bond layer being sprayed in building basic unit, the propylene being pasted onto on the base bond layer
Acid ester polymer waterproof roll and the overcoat for being sprayed on the waterproof roll surface;
The base bond layer material is by acrylic acid ester emulsion 40-60 parts, film former 8-15 parts, thickening agent 2-6 parts, antifungus agent
2-6 parts, age resister 3-7 parts, defoamer 2-6 parts, soft agent 8-15 parts are formulated;
The acrylate polymer waterproof roll is as tire base, and in its two surface impregnations polyphosphazene polymer by polyester filament cloth
Through drying the three-layer composite structure that makes after compound emulsion;
The protection coating materials are by acrylic acid ester emulsion 40-60 parts, film former 8-15 parts, thickening agent 2-6 parts, antifungus agent 2-6
Part, age resister 3-7 parts, defoamer 2-6 parts, wollastonite in powder 6-12 parts, mill base 2-6 parts are formulated.
2. the construction method of acrylate polymer composite waterproof system described in claim 1, it is characterised in that:Using following tools
Body step:
The first step, Dai Pu basic units are cleared up, and remove floating dust, greasy dirt and debris, and basic unit is for example damaged, loose or uneven, uses water
Mud waterproof mortar is repaired;
Second step, ejects chalk line or the line of ink marker, in the basic unit for handling well by acrylate polymer waterproof roll in precalculated position
Opening carries out overlaying rear backrush, is then overlaying spraying base bond layer at position:Quantity for spray is 0.75kg/m2~1kg/m2, spray
Apply thickness >=1 millimeter;
3rd step, take advantage of base bond layer wet when rapid laying acrylate polymer waterproof roll, and with scraper plate along web width
Flat gauffer is combed in direction, alice, gauffer, hollowing phenomenon must not occurs;
4th step, the laying of acrylate polymer waterproof roll are dried 4 ~ 8 hours after finishing naturally, after coiled material is firmly bonded,
In its surface even application overcoat:Quantity for spray 1kg/m2~1.2kg/m2, coating thickness >=1.2 millimeter, dry in the air after the completion of spraying 24h
Complete to construct.