CN105971132A - 一种高层建筑外墙窗间墙防渗漏处理方法 - Google Patents
一种高层建筑外墙窗间墙防渗漏处理方法 Download PDFInfo
- Publication number
- CN105971132A CN105971132A CN201610394406.1A CN201610394406A CN105971132A CN 105971132 A CN105971132 A CN 105971132A CN 201610394406 A CN201610394406 A CN 201610394406A CN 105971132 A CN105971132 A CN 105971132A
- Authority
- CN
- China
- Prior art keywords
- wall
- mortar
- joint
- windows
- building
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种高层建筑外墙窗间墙防渗漏处理方法,包括灰缝、窗间墙和混凝土剪力墙,步骤一:选材,水泥砖或粉煤灰混凝土加气块,对进场的水泥砖或粉煤灰混凝土加气块坚持严格地取样检验试验制度,步骤二﹕砌筑,砌筑砂浆严格按照配合比配制,砌筑时,采用满铺浆挤浆工艺方法砌筑,灰缝厚度严格控制在10~12mm,砂浆饱满度必须达到百分之九十以上,水泥砖或粉煤灰混凝土加气块与混凝土剪力墙处竖向缝一定保证15~20mm,砌筑完成后立即进行清扫、压缝、勾缝,留4~6mm左右的凹缝,步骤三﹕粉刷,严格按照工艺操作规程执行,使其做到内外密实,光洁平整,无缝隙,无裂缝,无毛细孔等。暴雨侵袭时,而起到了防渗漏的作用。
Description
技术领域
本发明涉及一种高层建筑外墙窗间墙防渗漏处理方法。
背景技术
近年来,随着经济的快速发展,城市高层建筑越来越多。为了满足抗震性能的要求,普遍采用剪刀墙结构型式。同时,随着人民环境保护意识的不断增强,保护有效的农业耕地面积的需要,普通粘土砖已禁止生产,取而代之的墙体填充材料为水泥砖或粉煤灰混凝土加气块。由于混凝土剪刀墙结构的收缩与水泥砖或粉煤灰混凝土加气块的收缩存在着较大的差异,从而导致外墙、窗间墙处砌筑粉刷完成后或住户入住后,经常发现外墙、窗间墙处渗漏或出现大面积水印,影响使用功能,并导致大量投诉。故此,只有发明一种区别于常规砌筑方法的简单有效的特殊砌筑处理技术方法,以根治外墙、窗间墙的渗漏或大面积水印的质量通病。
发明内容
本发明要解决的技术问题是克服现有窗间墙在任何狂风暴雨侵袭时,岀现渗漏或大面积水印等质量问题的缺陷,提供一种高层建筑外墙窗间墙防渗漏处理方法。
为了解决上述技术问题,本发明提供了如下的技术方案:
本发明一种高层建筑外墙窗间墙防渗漏处理方法,包括灰缝、窗间墙和混凝土剪力墙,其特征在于,步骤一:选材,水泥砖或粉煤灰混凝土加气块,对进场的水泥砖或粉煤灰混凝土加气块坚持严格地取样检验试验制度,经检试验复检合格后,用于工程砌筑,用于外墙、窗间墙的水泥砖或粉煤灰混凝土加气块要选择形状规正、有棱有角的用于此处砌筑;步骤二﹕砌筑,砌筑砂浆严格按照配合比配制,砌筑时,采用满铺浆挤浆工艺方法砌筑,灰缝厚度严格控制在10~12mm,砂浆饱满度必须达到百分之九十以上,水泥砖或粉煤灰混凝土加气块与混凝土剪力墙处竖向缝一定保证15~20mm,规范强制条文要求的拉结筋,严格按照规范或图纸要求设置,砌筑完成后立即进行清扫、压缝、勾缝,留4~6mm左右的凹缝,其目的是﹕压实严密,防止不实或收缩裂缝的产生。若出现收缩裂缝,粉刷时也增加砂浆填缝处的厚度;步骤三﹕粉刷,严格按照工艺操作规程执行,清理湿底,做点找平,分层粉刷,分层压实,到位到边,内外密实,光洁平整。
本发明所达到的有益效果是:在外墙、窗间墙砌筑粉刷施工过程中,采取特殊的工艺处理技术方法,使其做到内外密实,光洁平整,无缝隙,无裂缝,无毛细孔等。暴雨侵袭时,吸附在墙上的水分无法导入室内,而起到了防渗漏的作用。
附图说明
附图用来提供对本发明的进一步理解,并且构成说明书的一部分,与本发明的实施例一起用于解释本发明,并不构成对本发明的限制。在附图中:
图1是本发明的结构示意图;
图中:1、灰缝;2、窗间墙;3、混凝土剪力墙。
具体实施方式
以下结合附图对本发明的优选实施例进行说明,应当理解,此处所描述的优选实施例仅用于说明和解释本发明,并不用于限定本发明。
实施例1
如图1所示,本发明提供一种高层建筑外墙窗间墙防渗漏处理方法,包括灰缝1、窗间墙2和混凝土剪力墙3,步骤一:选材,水泥砖或粉煤灰混凝土加气块,对进场的水泥砖或粉煤灰混凝土加气块坚持严格地取样检验试验制度,经检试验复检合格后,用于工程砌筑,用于外墙、窗间墙2的水泥砖或粉煤灰混凝土加气块要选择形状规正、有棱有角的用于此处砌筑;步骤二﹕砌筑,砌筑砂浆严格按照配合比配制,砌筑时,采用满铺浆挤浆工艺方法砌筑,灰缝1厚度严格控制在10~12mm,砂浆饱满度必须达到百分之九十以上,水泥砖或粉煤灰混凝土加气块与混凝土剪力墙3处竖向缝一定保证15~20mm,规范强制条文要求的拉结筋,严格按照规范或图纸要求设置,砌筑完成后立即进行清扫、压缝、勾缝,留4~6mm左右的凹缝,其目的是﹕压实严密,防止不实或收缩裂缝的产生。若出现收缩裂缝,粉刷时也增加砂浆填缝处的厚度;步骤三﹕粉刷,严格按照工艺操作规程执行,清理湿底,做点找平,分层粉刷,分层压实,到位到边,内外密实,光洁平整。
进一步的,步骤一﹕满铺浆挤浆施工工艺处理技术方法砌筑;水平竖向(靠剪力处竖向缝除外)灰缝1厚度严格控制在10~12mm之间;砂浆饱满度必须达到百分之九十以上。1与混凝土剪力墙4相连处竖向灰缝1一定保证在15~20mm之间。
步骤二﹕粉刷按照操作规程规定的施工工艺严格执行,最终使粉刷产品内外密实,光洁平整。
采用满铺浆挤浆施工工艺处理技术方法砌筑,简单有效,防渗漏止水效果显著,根治好了外墙、窗间墙2渗漏或大面积水印的质量通病,在外墙、窗间墙2砌筑粉刷施工过程中,采取特殊的工艺处理技术方法,使其做到内外密实,光洁平整,无缝隙,无裂缝,无毛细孔等。暴雨侵袭时,吸附在墙上的水分无法导入室内,而起到了防渗漏的作用。
最后应说明的是:以上所述仅为本发明的优选实施例而已,并不用于限制本发明,尽管参照前述实施例对本发明进行了详细的说明,对于本领域的技术人员来说,其依然可以对前述各实施例所记载的技术方案进行修改,或者对其中部分技术特征进行等同替换。凡在本发明的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本发明的保护范围之内。
Claims (1)
1.一种高层建筑外墙窗间墙防渗漏处理方法,包括灰缝(1)、窗间墙(2)和混凝土剪力墙(3),其特征在于,步骤一:选材,水泥砖或粉煤灰混凝土加气块,对进场的水泥砖或粉煤灰混凝土加气块坚持严格地取样检验试验制度,经检试验复检合格后,用于工程砌筑,用于外墙、窗间墙(2)的水泥砖或粉煤灰混凝土加气块要选择形状规正、有棱有角的用于此处砌筑;步骤二﹕砌筑,砌筑砂浆严格按照配合比配制,砌筑时,采用满铺浆挤浆工艺方法砌筑,灰缝(1)厚度严格控制在10~12mm,砂浆饱满度必须达到百分之九十以上,水泥砖或粉煤灰混凝土加气块与混凝土剪力墙(3)处竖向缝一定保证15~20mm,规范强制条文要求的拉结筋,严格按照规范或图纸要求设置,砌筑完成后立即进行清扫、压缝、勾缝,留4~6mm左右的凹缝,其目的是﹕压实严密,防止不实或收缩裂缝的产生,若出现收缩裂缝,粉刷时也增加砂浆填缝处的厚度;步骤三﹕粉刷,严格按照工艺操作规程执行,清理湿底,做点找平,分层粉刷,分层压实,到位到边,内外密实,光洁平整。