CN105625077A - 一种纳米纤维素的制备方法 - Google Patents
一种纳米纤维素的制备方法 Download PDFInfo
- Publication number
- CN105625077A CN105625077A CN201610175749.9A CN201610175749A CN105625077A CN 105625077 A CN105625077 A CN 105625077A CN 201610175749 A CN201610175749 A CN 201610175749A CN 105625077 A CN105625077 A CN 105625077A
- Authority
- CN
- China
- Prior art keywords
- cellulose
- nano
- preparation
- product
- temperature
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种纳米纤维素制备方法,由脱脂棉经过硫酸水解法在一定的温度和时间下制得。本发明的纳米纤维素制备,制备方法简单,通过硫酸水解法控制一定的反应温度,反应时间,获得具有一定形态的纳米纤维素,制得的纳米纤维素具有良好韧性,增强效果好,化学温度性高,广泛应用于工业中。
Description
技术领域
本发明涉及纤维素材料领域,具体涉及一种纳米纤维素的制备方法。
背景技术
纤维素是由葡萄糖组成的大分子多糖。不溶于水及一般有机溶剂。是植物细胞壁的主要成分。纤维素是自然界中分布最广、含量最多的一种多糖,占植物界碳含量的50%以上。棉花的纤维素含量接近100%,为天然的最纯纤维素来源。一般木材中,纤维素占40~50%,还有10~30%的半纤维素和20~30%的木质素。
纤维素有着广泛的应用,木质素纤维是天然木材经过化学处理得到的有机纤维,外观为棉絮状,呈白色或灰白色。通过筛选、分裂、高温处理、漂白、化学处理、中和、筛分成不同长度和粗细度的纤维以适应不同应用材料的需要.由于处理温度高达250℃以上,在通常条件下是化学上非常稳定的物质,不为一般的溶剂、酸、碱腐蚀,具有无毒、无味、无污染、无放射性的优良品质,不影响环境,对人体无害,属绿色环保产品,这是其它矿物质素纤维所不具备的。纤维微观结构是带状弯曲的,凹凸不平的,多孔的,交叉处是扁平的,有良好的韧性、分散性和化学稳定性,吸水能力强,有非常优秀的增稠抗裂性能。
发明内容
本发明目的在于,提供一种,具有良好韧性,增强效果好,化学温度性高,制备简单的纳米纤维素,本发明所采用的技术方案是:
一种纳米纤维素的制备方法,其特征在于,由以下步骤制成:
(1)称取5g脱脂棉,放入100mL的三口烧瓶中;
(2)加入硫酸溶液60mL,在恒温反应1.5-2h;
(3)加入蒸馏水冷却,将产物装入透析袋中,反复冲洗至中性,过滤,产物置于冰箱中冷冻干燥。
进一步地,所述步骤(2)中的硫酸溶液的浓度为55%质量分数。
进一步地,所述步骤(2)中恒温反应的温度在55-60℃。
本发明相对于现有技术的有益效果是:本发明的纳米纤维素制备,制备方法简单,通过硫酸水解法控制一定的反应温度,反应时间,获得具有一定形态的纳米纤维素,制得的纳米纤维素具有良好韧性,增强效果好,化学温度性高,广泛应用于工业中。
具体实施方式
以下将结合实施例对本发明的构思及产生的技术效果进行清楚、完整地描述,以充分地理解本发明的目的、特征和效果。显然,所描述的实施例只是本发明的一部分实施例,而不是全部实施例,基于本发明的实施例,本领域的技术人员在不付出创造性劳动的前提下所获得的其他实施例,均属于本发明保护的范围。
实施例1:一种纳米纤维素的制备方法,由以下步骤制成:
(1)称取5g脱脂棉,放入100mL的三口烧瓶中;
(2)加入硫酸溶液60mL,在恒温反应1.5-2h;
(3)加入蒸馏水冷却,将产物装入透析袋中,反复冲洗至中性,过滤,产物置于冰箱中冷冻干燥。
实施例2:一种纳米纤维素的制备方法,其特征在于,由以下步骤制成:
(1)称取5g脱脂棉,放入100mL的三口烧瓶中;
(2)加入浓度为55%质量分数的硫酸溶液60mL,在在55-60℃恒温反应1.5-2h;
(3)加入蒸馏水冷却,将产物装入透析袋中,反复冲洗至中性,过滤,产物置于冰箱中冷冻干燥。
以上对本发明的较佳实施方式进行了具体说明,但本发明创造并不限于所述实施例,熟悉本领域的技术人员在不违背本发明精神的前提下还可作出种种的等同变型或替换,这些等同的变型或替换均包含在本申请权利要求所限定的范围内。
Claims (3)
1.一种纳米纤维素的制备方法,其特征在于,由以下步骤制成:
(1)称取5g脱脂棉,放入100mL的三口烧瓶中;
(2)加入硫酸溶液60mL,在恒温反应1.5-2h;
(3)加入蒸馏水冷却,将产物装入透析袋中,反复冲洗至中性,过滤,产物置于冰箱中冷冻干燥。
2.根据权利要求1所述的纳米纤维素的制备方法,其特征在于,所述步骤(2)中的硫酸溶液的浓度为55%质量分数。
3.根据权利要求1所述的纳米纤维素的制备方法,其特征在于,所述步骤(2)中恒温反应的温度在55-60℃。