CN105523727A - 一种喷射混凝土促凝剂的制备方法 - Google Patents

一种喷射混凝土促凝剂的制备方法 Download PDF

Info

Publication number
CN105523727A
CN105523727A CN201410581603.5A CN201410581603A CN105523727A CN 105523727 A CN105523727 A CN 105523727A CN 201410581603 A CN201410581603 A CN 201410581603A CN 105523727 A CN105523727 A CN 105523727A
Authority
CN
China
Prior art keywords
sprayed concrete
preparation
mixture
water
setting accelerator
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410581603.5A
Other languages
English (en)
Inventor
顾海萍
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuhan Hong Xintong Science And Technology Ltd
Original Assignee
Wuhan Hong Xintong Science And Technology Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuhan Hong Xintong Science And Technology Ltd filed Critical Wuhan Hong Xintong Science And Technology Ltd
Priority to CN201410581603.5A priority Critical patent/CN105523727A/zh
Publication of CN105523727A publication Critical patent/CN105523727A/zh
Pending legal-status Critical Current

Abstract

本发明公开一种喷射混凝土促凝剂的制备方法,按重量百分比计:半水硫酸钙5-10%、聚羧酸减水剂10-15%、消泡剂10-17%、乙醇胺3-5%、亚烷基三胺1-20%、余量为水。按以上配比取得上述原料,混合半水硫酸钙、聚羧酸减水剂、三乙醇胺、亚烷基二胺、水,然后加热至55℃左右,搅拌,得到pH值为5.8~7.2之间的混合溶液。之后,停止加热。并投入玉米油,静置约2分钟,缓慢搅拌。直至冷却至常温,停止搅拌。置于阴凉通风处,风干即可。

Description

一种喷射混凝土促凝剂的制备方法
技术领域
本发明属于水泥外加剂技术领域,涉及一种喷射混凝土促凝剂的制备方法。
背景技术
为了控制建筑建材等工程施工的周期、分段、工效等,需要针对耗时长的施工单元做优化处理,其中混凝土的凝结时间周期成为了一个重要课题。所以,对于促凝剂的发展提出了高要求。以往的促凝剂多为氯化钙、氯化钠及其他卤素化合物,但是,该方案的问题在于,化合物反应过程中会严重腐蚀钢筋板材结构的硬性,对于施工单元的硬化标准大打折扣。所以,需要研发一种不损耗物料单元的混凝土促凝剂。保证在缩短凝结时间的同时,不至于影响工程质量。
发明内容
针对以上技术中存在的缺陷,本发明提供一种喷射混凝土促凝剂的制备方法。
为解决上述技术问题,本发明所述喷射混凝土促凝剂的制备方法,其特征在于包括以下步骤:
第一步,取半水硫酸钙5-10%、聚羧酸减水剂10-15%、消泡剂10-17%、乙醇胺3-5%、亚烷基三胺1-20%、余量为水。
第二步,混合半水硫酸钙、聚羧酸减水剂、乙醇胺、亚烷基三胺、水。
第三步,加热至60-65℃,搅拌,得到pH值为5.8~7.2之间的混合溶液。
第四步,停止加热。并投入消泡剂,再次搅拌。
第五步,冷却至常温,停止搅拌。
第六步,风干。
具体实施方式
实施例1
一种喷射混凝土促凝剂,其特征在于包括以下组成,按重量份数计:半水硫酸钙10%、聚羧酸减水剂15%、消泡剂13%、乙醇胺4%、亚烷基三胺15%、余量为水。
本发明所述的喷射混凝土促凝剂的制备方法如下:
混合半水硫酸钙、聚羧酸减水剂、乙醇胺、亚烷基三胺、水,然后加热至60-65℃,搅拌,得到pH值为5.8~7.2之间的混合溶液。之后,停止加热。并投入消泡剂,再次搅拌。直至冷却至常温,停止搅拌。置于阴凉通风处,风干即可。
实施例2
一种喷射混凝土促凝剂,其特征在于包括以下组成,按重量份数计:半水硫酸钙10%、聚羧酸减水剂15%、玉米油13%、乙醇胺4%、亚烷基二胺15%、余量为水。
本发明所述的喷射混凝土促凝剂的制备方法如下:
混合半水硫酸钙、聚羧酸减水剂、三乙醇胺、亚烷基二胺、水,然后加热至55℃左右,搅拌,得到pH值为5.8~7.2之间的混合溶液。之后,停止加热。并投入玉米油,静置约2分钟,缓慢搅拌。直至冷却至常温,停止搅拌。置于阴凉通风处,风干即可。

Claims (4)

1.一种喷射混凝土促凝剂的制备方法,其特征在于包括以下步骤:
第一步,取半水硫酸钙5-10%、聚羧酸减水剂10-15%、消泡剂10-17%、乙醇胺3-5%、亚烷基三胺1-20%、余量为水。
第二步,混合半水硫酸钙、聚羧酸减水剂、乙醇胺、亚烷基三胺、水。
第三步,加热至60-65℃,搅拌,得到pH值为5.8~7.2之间的混合溶液。
第四步,停止加热。并投入消泡剂,再次搅拌。
第五步,冷却至常温,停止搅拌。
第六步,风干。
2.根据权利要求1所述的喷射混凝土促凝剂,其特征在于所述消泡剂可用玉米油替代。
3.根据权利要求1所述的喷射混凝土促凝剂,其特征在于所述乙醇胺可用任意一种低级乙醇胺代替,如三乙醇胺。
4.根据权利要求1所述的喷射混凝土促凝剂,其特征在于所述亚烷基三胺可用亚烷基二胺代替。
CN201410581603.5A 2014-10-26 2014-10-26 一种喷射混凝土促凝剂的制备方法 Pending CN105523727A (zh)