CN1054231A - 硫脲废渣的回收及利用方法 - Google Patents

硫脲废渣的回收及利用方法 Download PDF

Info

Publication number
CN1054231A
CN1054231A CN 91107122 CN91107122A CN1054231A CN 1054231 A CN1054231 A CN 1054231A CN 91107122 CN91107122 CN 91107122 CN 91107122 A CN91107122 A CN 91107122A CN 1054231 A CN1054231 A CN 1054231A
Authority
CN
China
Prior art keywords
waste residue
slag
waste
breast
recovery
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 91107122
Other languages
English (en)
Inventor
黄诚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NORTHWEST SICHUAN MINE LABOUR SERVICE CO JIANGYOU CITY
Original Assignee
NORTHWEST SICHUAN MINE LABOUR SERVICE CO JIANGYOU CITY
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NORTHWEST SICHUAN MINE LABOUR SERVICE CO JIANGYOU CITY filed Critical NORTHWEST SICHUAN MINE LABOUR SERVICE CO JIANGYOU CITY
Priority to CN 91107122 priority Critical patent/CN1054231A/zh
Publication of CN1054231A publication Critical patent/CN1054231A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种硫脲废渣的回收和利用的方 法,采用该方法可将硫脲废渣全部处理、利用、降低硫 脲产品成本,消除废渣对环境的污染。

Description

本发明属于硫脲废渣的回收及利用的方法。
工业生产硫脲将产生大量的废渣,在现有技术中是将硫脲废渣堆积弃去,造成了环境污染,目前国内尚无一家对硫脲废渣进行处理。本发明基于对废渣组分的分析而提供一种硫脲废渣的回收及利用的方法,其目的在于寻找一个变废为宝、消除环境污染的处理方法,该方法可将废渣全部处理,使硫脲产品成本降低,解决废渣对环境的污染。
硫脲废渣主要来源于氰氨化钙,工业氰氨化钙中含CaCN262.10%,CaC22.98%,CaO14.38%,C11.92%,除碳以外,在合成硫脲后都有氢氧化钙组分生成留在废渣中。本发明的目的可以通过以下步骤来达到:把新鲜硫脲废渣在30~80℃的热水中按1∶1-2∶1的渣水重量比浸泡、搅拌制成渣乳,再向渣乳中通入硫化氢气体,使渣中的氢氧化钙与硫化氢反应生成硫氢化钙(Ca(OH)2+2H2S→Ca(SH)2+2H2O),过滤将硫氢化钙溶液与渣分开,获得并收存硫氢化钙溶液,可用来合成硫脲或作它用,剩下的废渣中碳的含量达50~60%,再加入重量比为10-30%的碳就可做成燃料,用此方法达到了全部处理废渣的目的。
本发明还可以通过以下步骤来达到:先把新鲜废渣在60-82℃热水中按1∶1~2∶1的渣水重量比浸泡、搅拌1~5分钟,将渣过滤,溶液收存,用于下次洗渣用,待到浓度在3Be′以上时,即可回收硫脲,然后再把分离出的废渣按上述步骤制成渣乳后按上述方法进行处理。
多次对硫脲废渣进行回收处理的实验,均达到目的。
实施例1:把1公斤新鲜废渣放在500毫升,温度为80℃的热水中浸泡、搅拌制成渣乳,通入硫化氢气体(体积含量30%)1小时后过滤,用EDTA分析法测得滤液中硫氢化钙含量为104.5克/升,剩余的残渣中加入10-30%的碳制成燃料。
实施例2:把1公斤新鲜废渣在80℃的热水中按2∶1的渣水重量比浸泡、搅拌2分钟后过滤,将滤液回收获得硫脲28.3克,剩下的渣再按上述方法制成渣乳,通入硫化氢(体积含量30%)1小时后过滤,用EDTA分析法测得滤液中硫氢化钙含量为57.68克/升,剩余的残渣中加入10-30%的碳制成燃料。

Claims (3)

1、一种硫脲废渣的回收及利用方法,其特征在于向新鲜废渣乳通入硫化氢气体,使废渣中的氢氧化钙与硫化氢反应生成硫氢化钙,过滤后获得硫氢化钙溶液,反应剩余的废渣加入重量比为10-30%的碳,做成燃料。
2、根据权利要求1所述的方法,其特征是先将新鲜废渣在60-82℃的热水中按1∶1-2∶1的渣水重量比浸泡、搅拌1~5分钟,将渣过滤,溶液收存,用于下次洗渣用,待到浓度在3Be′以上时,即可回收硫脲,然后再把分离出的废渣制成渣乳。
3、根据权利要求1或2的方法,其特征是废渣乳是在30-80℃的热水中按1∶1~2∶1的渣水重量比浸泡、搅拌,制成渣乳。
CN 91107122 1991-01-25 1991-01-25 硫脲废渣的回收及利用方法 Pending CN1054231A (zh)