CN105273146A
CN105273146A CN201410326617.2A CN201410326617A CN105273146A CN 105273146 A CN105273146 A CN 105273146A CN 201410326617 A CN201410326617 A CN 201410326617A CN 105273146 A CN105273146 A CN 105273146A
Authority
CN
China
Prior art keywords
parts
wear
raw material
durable
titanium dioxide
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410326617.2A
Other languages
English (en)
Inventor
侯立山
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TIANJIN HAND-ALL PACKAGING AND PRINTING Co Ltd
Original Assignee
TIANJIN HAND-ALL PACKAGING AND PRINTING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TIANJIN HAND-ALL PACKAGING AND PRINTING Co Ltd filed Critical TIANJIN HAND-ALL PACKAGING AND PRINTING Co Ltd
Priority to CN201410326617.2A priority Critical patent/CN105273146A/zh
Publication of CN105273146A publication Critical patent/CN105273146A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Compositions Of Macromolecular Compounds (AREA)
  • Processes Of Treating Macromolecular Substances (AREA)

Abstract

本发明公开了一种耐磨夜光硬质塑料,按照重量份的原料包括:聚氯乙烯树脂、稀土长效荧光粉、钛白粉份、硬脂酸份、钛白粉份、PE蜡份、稀土长效荧光粉份,碳酸钙份、二聚酸钙份、锌镁铝三元水滑石份、二苯甲酰甲烷份、马来酸酐份、聚乙烯辛烯共弹性体份、防火阻燃剂份、二氧化硅份、苯并咪唑份;具体制备步骤为:将上述重量份数的各组分原料加入混料机中进行搅拌混料,混料机在搅拌过程中对加入其中的原料进行加热,直至温度升高至120℃后再搅拌3-6min;将搅拌均匀的原料加入挤出机中,经挤出机挤出成型即可,挤出过程中的温度设置为150-180℃;本发明,提高塑料强度、耐腐蚀度,且耐磨性好、耐高温,防火阻燃性能均大幅提高,节能环保无污染。

Description

一种耐磨夜光硬质塑料
技术领域
本发明涉及塑料领域,具体是一种耐磨夜光硬质塑料。
背景技术
目前塑料制品使用的越来越多,传统塑料,添加物质多,使用效果差,生产成本高,产品不能达到使用预期效果,目前生产的高强度耐磨夜光硬质塑料多用于户外,必须要经得起日晒雨淋,适应易腐蚀性的环境等要求,而户内使用,对产品外观亮度、褪色度、抗紫外线性能也有较高要求,以免影响室内可见区域的美观,且塑料的硬度、耐老化性能也需提高。
发明内容
本发明的目的在于提供一种提高塑料强度、耐腐蚀度,且耐磨性好、耐高温,防火阻燃性能均大幅提高的耐磨夜光硬质塑料,以解决上述背景技术中提出的问题。
为实现上述目的,本发明提供如下技术方案:
一种耐磨夜光硬质塑料,按照重量份的原料包括:聚氯乙烯树脂95-105份、稀土长效荧光粉5-7份、钛白粉1.8-2.0份、硬脂酸1-2份、钛白粉1.8-2.2份、PE蜡1-2份、稀土长效荧光粉8-12份,碳酸钙35-45份、二聚酸钙8-10份、锌镁铝三元水滑石18-20份、二苯甲酰甲烷2-4份、马来酸酐5-7份、聚乙烯辛烯共弹性体4-8份、防火阻燃剂1-3份、二氧化硅3-10份、苯并咪唑4-6份;具体制备步骤为:将上述重量份数的各组分原料加入混料机中进行搅拌混料,混料机在搅拌过程中对加入其中的原料进行加热,直至温度升高至120℃后再搅拌3-6min;将搅拌均匀的原料加入挤出机中,经挤出机挤出成型即可,挤出过程中的温度设置为150-180℃;其中防火阻燃剂提高塑料防火性能,二氧化硅提高塑料的耐磨性能,苯并咪唑提高塑料的耐热程度,稀土长效荧光粉能够使塑料制品在夜晚更清楚的看到。
进一步的,一种耐磨夜光硬质塑料,按照重量份的原料包括:聚氯乙烯树脂100份、稀土长效荧光粉6份、钛白粉1.9份、硬脂酸1.5份、钛白粉2.0份、PE蜡1.5份、稀土长效荧光粉10份,碳酸钙40份、二聚酸钙9份、锌镁铝三元水滑石19份、二苯甲酰甲烷3份、马来酸酐6份、聚乙烯辛烯共弹性体6份、防火阻燃剂2份、二氧化硅7份、苯并咪唑5份。
进一步的,所述的稀土长效荧光粉为碱土铝酸盐型长余辉发光材料。
与现有技术相比,本发明,提高塑料强度、耐腐蚀度,且耐磨性好、耐高温,防火阻燃性能均大幅提高,节能环保无污染。
具体实施方式
下面将结合本发明实施例,对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本发明一部份实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其他实施例,都属于本发明保护的范围。
实施例1
本发明实施例中,一种耐磨夜光硬质塑料,按照重量份的原料包括:聚氯乙烯树脂95份、稀土长效荧光粉5份、钛白粉1.8份、硬脂酸1份、钛白粉1.8份、PE蜡1份、稀土长效荧光粉8份,碳酸钙35份、二聚酸钙8份、锌镁铝三元水滑石18份、二苯甲酰甲烷2份、马来酸酐5份、聚乙烯辛烯共弹性体4份、防火阻燃剂1份、二氧化硅3份,苯并咪唑4份;具体制备步骤为:1、将上述重量份数的各组分原料加入混料机中进行搅拌混料,混料机在搅拌过程中对加入其中的原料进行加热,直至温度升高至120℃后再搅拌3-6min;2、将搅拌均匀的原料加入挤出机中,经挤出机挤出成型即可,挤出过程中的温度设置为150℃。
实施例2
本发明实施例中,一种耐磨夜光硬质塑料,按照重量份的原料包括:聚氯乙烯树脂100份、稀土长效荧光粉6份、钛白粉1.9份、硬脂酸1.5份、钛白粉2.0份、PE蜡1.5份、稀土长效荧光粉10份,碳酸钙40份、二聚酸钙9份、锌镁铝三元水滑石19份、二苯甲酰甲烷3份、马来酸酐6份、聚乙烯辛烯共弹性体6份、防火阻燃剂2份、二氧化硅7份、苯并咪唑5份;具体制备步骤为:1、将上述重量份数的各组分原料加入混料机中进行搅拌混料,混料机在搅拌过程中对加入其中的原料进行加热,直至温度升高至120℃后再搅拌3-6min;2、将搅拌均匀的原料加入挤出机中,经挤出机挤出成型即可,挤出过程中的温度设置为150℃。
实施例3
本发明实施例中,一种耐磨夜光硬质塑料,按照重量份的原料包括:聚氯乙烯树脂105份、稀土长效荧光粉7份、钛白粉2.0份、硬脂酸2份、钛白粉2.2份、PE蜡2份、稀土长效荧光粉12份,碳酸钙45份、二聚酸钙10份、锌镁铝三元水滑石20份、二苯甲酰甲烷4份、马来酸酐7份、聚乙烯辛烯共弹性体8份、防火阻燃剂3份、二氧化硅10份、苯并咪唑6份;具体制备步骤为:1、将上述重量份数的各组分原料加入混料机中进行搅拌混料,混料机在搅拌过程中对加入其中的原料进行加热,直至温度升高至120℃后再搅拌3-6min;2、将搅拌均匀的原料加入挤出机中,经挤出机挤出成型即可,挤出过程中的温度设置为150℃。
对于本领域技术人员而言,显然本发明不限于上述示范性实施例的细节,而且在不背离本发明的精神或基本特征的情况下,能够以其他的具体形式实现本发明。因此,无论从哪一点来看,均应将实施例看作是示范性的,而且是非限制性的,本发明的范围由所附权利要求而不是上述说明限定,因此旨在将落在权利要求的等同要件的含义和范围内的所有变化囊括在本发明内。
此外,应当理解,虽然本说明书按照实施方式加以描述,但并非每个实施方式仅包含一个独立的技术方案,说明书的这种叙述方式仅仅是为清楚起见,本领域技术人员应当将说明书作为一个整体,各实施例中的技术方案也可以经适当组合,形成本领域技术人员可以理解的其他实施方式。

Claims (3)

1.一种耐磨夜光硬质塑料,其特征在于,按照重量份的原料包括:聚氯乙烯树脂95-105份、稀土长效荧光粉5-7份、钛白粉1.8-2.0份、硬脂酸1-2份、钛白粉1.8-2.2份、PE蜡1-2份、稀土长效荧光粉8-12份,碳酸钙35-45份、二聚酸钙8-10份、锌镁铝三元水滑石18-20份、二苯甲酰甲烷2-4份、马来酸酐5-7份、聚乙烯辛烯共弹性体4-8份、防火阻燃剂1-3份、二氧化硅3-10份、苯并咪唑4-6份;具体制备步骤为:将上述重量份数的各组分原料加入混料机中进行搅拌混料,混料机在搅拌过程中对加入其中的原料进行加热,直至温度升高至120℃后再搅拌3-6min;将搅拌均匀的原料加入挤出机中,经挤出机挤出成型即可,挤出过程中的温度设置为150-180℃。
2.根据权利要求1所述的耐磨夜光硬质塑料,其特征在于,按照重量份的原料包括:聚氯乙烯树脂100份、稀土长效荧光粉6份、钛白粉1.9份、硬脂酸1.5份、钛白粉2.0份、PE蜡1.5份、稀土长效荧光粉10份,碳酸钙40份、二聚酸钙9份、锌镁铝三元水滑石19份、二苯甲酰甲烷3份、马来酸酐6份、聚乙烯辛烯共弹性体6份、防火阻燃剂2份、二氧化硅7份、苯并咪唑5份。
3.根据权利要求1所述的耐磨夜光硬质塑料,其特征在于,所述的稀土长效荧光粉为碱土铝酸盐型长余辉发光材料。
CN201410326617.2A 2014-07-10 2014-07-10 一种耐磨夜光硬质塑料 Pending CN105273146A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410326617.2A CN105273146A (zh) 2014-07-10 2014-07-10 一种耐磨夜光硬质塑料

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410326617.2A CN105273146A (zh) 2014-07-10 2014-07-10 一种耐磨夜光硬质塑料

Publications (1)

Publication Number Publication Date
CN105273146A true CN105273146A (zh) 2016-01-27

Family

ID=55143034

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410326617.2A Pending CN105273146A (zh) 2014-07-10 2014-07-10 一种耐磨夜光硬质塑料

Country Status (1)

Country Link
CN (1) CN105273146A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106751204A (zh) * 2016-12-20 2017-05-31 佛山市高明区塑料行业协会 一种改性荧光聚氯乙烯新型材料
CN107603062A (zh) * 2017-09-26 2018-01-19 桐城市正阳包装有限公司 一种具有夜光功能的塑料瓶盖制品

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101074307A (zh) * 2006-05-16 2007-11-21 谷广强 夜明塑料制品
CN101696306A (zh) * 2009-10-26 2010-04-21 宁夏青龙塑料管材有限公司 一种耐热、耐磨pvc管材
CN102746598A (zh) * 2012-07-27 2012-10-24 天津市利顺塑料制品有限公司 一种抗氧化防开裂的夜明塑料制品
CN103059465A (zh) * 2012-12-25 2013-04-24 东莞市祺龙电业有限公司 一种高耐热高耐磨环保pvc改性材料及其制备方法
CN103304912A (zh) * 2012-03-06 2013-09-18 上海百理物业管理有限公司 夜光塑料制品

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101074307A (zh) * 2006-05-16 2007-11-21 谷广强 夜明塑料制品
CN101696306A (zh) * 2009-10-26 2010-04-21 宁夏青龙塑料管材有限公司 一种耐热、耐磨pvc管材
CN103304912A (zh) * 2012-03-06 2013-09-18 上海百理物业管理有限公司 夜光塑料制品
CN102746598A (zh) * 2012-07-27 2012-10-24 天津市利顺塑料制品有限公司 一种抗氧化防开裂的夜明塑料制品
CN103059465A (zh) * 2012-12-25 2013-04-24 东莞市祺龙电业有限公司 一种高耐热高耐磨环保pvc改性材料及其制备方法

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
郭红霞: "《电线线缆材料》", 31 July 2012, 机械工业出版社 *

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106751204A (zh) * 2016-12-20 2017-05-31 佛山市高明区塑料行业协会 一种改性荧光聚氯乙烯新型材料
CN107603062A (zh) * 2017-09-26 2018-01-19 桐城市正阳包装有限公司 一种具有夜光功能的塑料瓶盖制品

Similar Documents

Publication Publication Date Title
CN103073816B (zh) 一种耐热耐寒环保pvc改性材料及其制备方法
CN101880429A (zh) 高韧耐热耐老化氯化聚氯乙烯合金材料及其制备方法
CN102229790B (zh) 一种铝塑复合粘接用材料的制备方法
CN105542346B (zh) 用于r-pvc型材共挤表层的复合材料及其制备方法
CN101338059A (zh) 一种pvc改性材料及其制备方法
CN109608731A (zh) 一种石墨烯增强矿用聚乙烯组合物、粒子、管材及其制备方法
CN106366496B (zh) 一种pvc木塑发泡板及其制备方法
CN104910554A (zh) 厚度为3-5mm的聚氯乙烯发泡广告板
CN103304912A (zh) 夜光塑料制品
CN105273146A (zh) 一种耐磨夜光硬质塑料
CN107118478A (zh) 一种新型管材及其制备方法
CN106751194A (zh) 一种添加煤矸石粉防裂pvc地板砖制备方法
CN104072907A (zh) 一种用于耐磨室内地板的pvc型材及其生产方法
CN103554668A (zh) 一种新型聚丙烯双壁波纹管
CN105367935A (zh) 一种防冻抗冲击pvc管
CN106046622B (zh) 一种用于制造电缆绝缘层的材料及其制备方法
CN103172949B (zh) 一种室内墙面用pvc塑料板材及其制备方法
CN107216610A (zh) 一种建筑装饰用环保型保温材料及其制备方法
CN1220725C (zh) 抗静电阻燃聚乙烯材料
CN103087399B (zh) 一种高韧性高强度无卤阻燃聚丙烯
CN105566723A (zh) 一种用抛光砖废渣制备的聚乙烯钙塑管及其制备方法
CN104877252B (zh) 一种无铅低毒聚氯乙烯复合材料及其制备方法
CN108752797A (zh) 一种塑料建筑模板的配方
CN108359159A (zh) 一种环保耐老化电缆料及其制备方法
CN108047631A (zh) 一种新能源充电枪用线缆外被料及制备方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
WD01 Invention patent application deemed withdrawn after publication
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20160127