CN105133401A - 一种蒲公英纤维无染料染色的方法 - Google Patents
一种蒲公英纤维无染料染色的方法 Download PDFInfo
- Publication number
- CN105133401A CN105133401A CN201510490678.7A CN201510490678A CN105133401A CN 105133401 A CN105133401 A CN 105133401A CN 201510490678 A CN201510490678 A CN 201510490678A CN 105133401 A CN105133401 A CN 105133401A
- Authority
- CN
- China
- Prior art keywords
- dandelion
- fiber
- washing
- temperature
- dyeing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明公开了一种蒲公英纤维无染料染色的方法,包括如下步骤:浸渍—加热—水洗、脱水---烘干---测定水洗色牢度;其中,所述加热步骤中:将水温从20℃-30℃升温到?50℃-60℃,升温速率为1.5-2℃/分钟,耗时15-20分钟,在50℃-60℃温度下保温20-30分钟,使纤维逐渐变为姜黄色。本发明无需添加任何化学染料和植物染料及任何助剂,通过加工纤维自身发出姜黄色,能与天然彩棉和天然彩丝相媲美;开发利用新型纯天然黄色蒲公英纤维材料,变废为宝,加工成本低,收集方便,同时具有纯天然、绿色、环保、高吸水及保健作用。
Description
技术领域
本发明属于纤维织物领域,具体涉及一种蒲公英纤维无染料染色的方法。
背景技术
蒲公英的食用价值、医药价值、营养价值在《本草纲目》、《辞海》及历代医药大典中都给予了极高的评价和肯定。蒲公英含蒲公英醇、胆碱、有机酸、菊糖、葡萄糖、Vc、Vd、胡萝卜素等多种营养素,同时含有丰富的微量元素,其中最重要的是含有大量的铁、Ca等人体所需的矿物质。其Ca的含量为番石榴的2.2倍、刺梨的3.2倍,铁的含量为刺梨的4倍、山楂的3.5倍。从食用营养的观点看,人体中最容易缺乏的无机元素只有Ca和铁。因此,蒲公英具有十分重要的营养价值。美国、日本的研究发现,蒲公英的营养价值之高在自然界十分罕见,是一种高维营养菜。蒲公英食品已开始在美国、日本风行。现代医学研究表明:它具有“抗病毒、抗感染、抗肿瘤”的三抗作用,引起了国际关注。
从资源开发利用角度来看,蒲公英纤维是一种尚未开发利用的新型纤维材料。蒲公英绒纤维是由自身生长出的种子上的纤维。蒲公英绒纤维有长刺,具有与羽毛纤维类似的结构特点。蒲公英纤维不适宜于纺纱加工。由于其产量较大,加上纤维本身所具有的蓬松性能,可用做填充物。纤维加工成本低,收集方便,纤维与植物植株均具有清凉去火的功效,为填充性纤维的开发和利用提供了新的资源。
目前蒲公英纤维生产纺织面料的方法只有静电植绒的方法,正在研究当中。静电植绒的绒毛需要色彩,目前没有蒲公英纤维染色方面的报道。
发明内容
发明目的:为了解决现有技术的不足,本发明提供了一种蒲公英纤维无染料染色的方法,具体解决了如下问题:1、蒲公英纤维吸水性问题;2、蒲公英纤维无染料染色颜色单一,不具有广谱性问题;3、蒲公英纤维无染料染色的色牢度问题。
技术方案:一种蒲公英纤维无染料染色的方法,包括如下步骤:浸渍—加热—水洗、脱水---烘干---测定水洗色牢度;其中,
所述加热步骤中:将水温从20℃-30℃升温到50℃-60℃,升温速率为1.5-2℃/分钟,耗时15-20分钟,在50℃-60℃温度下保温20-30分钟,使纤维逐渐变为姜黄色。
作为进一步优化:所述浸渍步骤中:由于蒲公英纤维质量轻,纤维细,外面还包裹着一层拒水性物质,因此,将蒲公英在加热之前放入温度为20℃-30℃的水中浸渍15-20分钟。
作为进一步优化:所述水洗、脱水步骤中:在20℃-30℃的常温下进行水洗,水洗时间为10-15分钟,然后进行脱水。
作为进一步优化:所述烘干步骤中:烘干的温度为70℃-80℃,烘干温度为10-15分钟。
作为进一步优化:所述测水洗色牢度步骤中:测水洗色牢度为3.5-4级。
有益效果:本发明无需添加任何化学染料和植物染料及任何助剂,通过加工纤维自身发出姜黄色,能与天然彩棉和天然彩丝相媲美;开发利用新型纯天然黄色蒲公英纤维材料,变废为宝,加工成本低,收集方便,同时具有纯天然、绿色、环保、高吸水及保健作用。
蒲公英黄色素的提取通常是从蒲公黄英花中提取。蒲公英花经过一定的生长变成白色的蒲公英纤维,白色的蒲公英纤维经加热变成姜黄色,这种纯天然彩色纤维,同时具有抗病毒、抗感染、抗肿瘤等保健功能,和高吸水性能,是用来生产医用无纺布,老年尿不湿,及卫生巾的极佳材料,还在开发一种时尚领域的缩绒围巾。
而蒲公英纤维本身染色较为困难,因为纤维加热到80℃以上,纤维会发生物理、化学改性,纤维变硬、变脆。蒲公英纤维在加热过程中,注意温度尽量不能超过80℃,超过80℃后纤维会发生物理化学改性,纤维的吸水性会迅速升高,而纤维会变硬、变脆。
从本发明的K/S值示意图中可以看出:在不同吸收波长范围内的表观色深K/S值,当吸收波长为680—700nm时,K/S值=63,达到最大值。
附图说明
图1是本发明中加热时反射率曲线示意图。
具体实施方式
下面结合具体实施例对本发明作进一步说明。
具体实施例1
一种蒲公英纤维无染料染色的方法,包括如下步骤:浸渍—加热—水洗、脱水---烘干---测定水洗色牢度;
所述浸渍步骤中:由于蒲公英纤维质量轻,纤维细,外面还包裹着一层拒水性物质,因此,将蒲公英在加热之前放入温度为20℃的水中浸渍15分钟。
将水温从20℃升温到50℃,升温速率为2℃/分钟,耗时15分钟,在50℃温度下保温20分钟,使纤维逐渐变为姜黄色。
所述水洗、脱水步骤中:在20℃的常温下进行水洗,水洗时间为10分钟,然后进行脱水。
所述烘干步骤中:烘干的温度为70℃,烘干温度为10分钟。
所述测水洗色牢度步骤中:测水洗色牢度为3.5级。
具体实施例2
一种蒲公英纤维无染料染色的方法,包括如下步骤:浸渍—加热—水洗、脱水---烘干---测定水洗色牢度;
所述浸渍步骤中:由于蒲公英纤维质量轻,纤维细,外面还包裹着一层拒水性物质,因此,将蒲公英在加热之前放入温度为30℃的水中浸渍20分钟。
将水温从30℃升温到60℃,升温速率为1.5℃/分钟,耗时20分钟,在60℃温度下保温30分钟,使纤维逐渐变为姜黄色。
所述水洗、脱水步骤中:在30℃的常温下进行水洗,水洗时间为15分钟,然后进行脱水。
所述烘干步骤中:烘干的温度为80℃,烘干温度为15分钟。
所述测水洗色牢度步骤中:测水洗色牢度为4级。
具体实施例3
一种蒲公英纤维无染料染色的方法,包括如下步骤:浸渍—加热—水洗、脱水---烘干---测定水洗色牢度;
所述浸渍步骤中:由于蒲公英纤维质量轻,纤维细,外面还包裹着一层拒水性物质,因此,将蒲公英在加热之前放入温度为24℃的水中浸渍18分钟。
将水温从24℃升温到57℃,升温速率为1.9℃/分钟,耗时17分钟,在50℃-60℃温度下保温26分钟,使纤维逐渐变为姜黄色。
所述水洗、脱水步骤中:在24℃的常温下进行水洗,水洗时间为11分钟,然后进行脱水。
所述烘干步骤中:烘干的温度为73℃,烘干温度为12分钟。
所述测水洗色牢度步骤中:测水洗色牢度为4级。
本发明不局限于上述最佳实施方式,任何人在本发明的启示下都可得出其他各种形式的产品,但不论在其形状或结构上作任何变化,凡是具有与本申请相同或相近似的技术方案,均落在本发明的保护范围之内。
Claims (5)
1.一种蒲公英纤维无染料染色的方法,其特征在于:包括如下步骤:浸渍—加热—水洗、脱水---烘干---测定水洗色牢度;其中,
所述加热步骤中:将水温从20℃-30℃升温到50℃-60℃,升温速率为1.5-2℃/分钟,耗时15-20分钟,在50℃-60℃温度下保温20-30分钟,使纤维逐渐变为姜黄色。
2.根据权利要求1所述的蒲公英纤维无染料染色的方法,其特征在于:所述浸渍步骤中:由于蒲公英纤维质量轻,纤维细,外面还包裹着一层拒水性物质,因此,将蒲公英在加热之前放入温度为20℃-30℃的水中浸渍15-20分钟。
3.根据权利要求1所述的蒲公英纤维无染料染色的方法,其特征在于:所述水洗、脱水步骤中:在20℃-30℃的常温下进行水洗,水洗时间为10-15分钟,然后进行脱水。
4.根据权利要求1所述的蒲公英纤维无染料染色的方法,其特征在于:所述烘干步骤中:烘干的温度为70℃-80℃,烘干温度为10-15分钟。
5.根据权利要求1所述的蒲公英纤维无染料染色的方法,其特征在于:所述测水洗色牢度步骤中:测水洗色牢度为3.5-4级。