CN104928787A - 一种具有吸湿透气功能的生态抑菌羽绒纤维及其制作方法 - Google Patents

一种具有吸湿透气功能的生态抑菌羽绒纤维及其制作方法 Download PDF

Info

Publication number
CN104928787A
CN104928787A CN201510291780.4A CN201510291780A CN104928787A CN 104928787 A CN104928787 A CN 104928787A CN 201510291780 A CN201510291780 A CN 201510291780A CN 104928787 A CN104928787 A CN 104928787A
Authority
CN
China
Prior art keywords
parts
fiber
moisture absorption
chitin
bacteriostatic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510291780.4A
Other languages
English (en)
Inventor
刁平山
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI PROVINCE HANSHAN COUNTY FUQIANG DOWN PRODUCTS Co Ltd
Original Assignee
ANHUI PROVINCE HANSHAN COUNTY FUQIANG DOWN PRODUCTS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI PROVINCE HANSHAN COUNTY FUQIANG DOWN PRODUCTS Co Ltd filed Critical ANHUI PROVINCE HANSHAN COUNTY FUQIANG DOWN PRODUCTS Co Ltd
Priority to CN201510291780.4A priority Critical patent/CN104928787A/zh
Publication of CN104928787A publication Critical patent/CN104928787A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种具有吸湿透气功能的生态抑菌羽绒纤维,其特征在于,由下列重量份的原料制成:鸭绒25-35、兔毛7-9、苎麻纤维3-5、牛奶蛋白纤维2-4、甲壳素6-8、衣康酸酐2.3-4.1、纳米二氧化硅1.6-3.2、八甲基环四硅氧烷5-7、硅酸钠0.1-0.4、云母粉1-3、氯化-1-丁基-3-甲基咪唑190-210、适量水;本发明通过化学改性将甲壳素分子吸附在羽绒纤维表面,扰乱细胞正常的生理活动而杀灭细菌,抗菌性能彻底,利用本发明制得的生态抑菌羽绒纤维具有吸湿透气、抗菌性能持久、耐磨耐水洗等优点,满足各种人群的不同生理需要,且使用寿命长,保暖和防绒性能优良。

Description

一种具有吸湿透气功能的生态抑菌羽绒纤维及其制作方法
技术领域
本发明涉及无纺织材料技术领域,具体涉及一种具有吸湿透气功能的生态抑菌羽绒纤维及其制作方法。
背景技术
羽绒纤维属于天然蛋白质纤维,具有质软、质轻、蓬松性高、保暖性好等优点,广泛用于服装、被絮、纺织填料等领域,随着人们生活水平的提高,消费结构的改变,以及近几年对绿色、低碳的提倡,人们对羽绒制品的要求越来越高,既要款式新穿着舒适又要求抗菌透气保暖等。为了适应消费者的需求和爱好,一种低密度、无卤、绿色环保、生态抑菌、耐水洗、耐高温性能高的新型羽绒纤维的及其各种性能的研究势在必行。
甲壳素是自然界中迄今为止被发现的唯一带正电荷的动物纤维素。甲壳素纤维横截面形态是不规则的椭圆形,纵向有孔洞,其内部分子组成与纤维素类似。甲壳素纤维有良好的吸湿性、成膜性、染色性及抗菌性,可与棉和粘胶等纤维混纺。随着近年来大量基础及应用研究的进行,甲壳素及其衍生物已在化工、纺织、 印染、造纸、医药、食品、环保等诸多领域显示出其独特的应用价值。但由于甲壳素分子内、分子间有强的氢键作用,使得甲壳素呈紧密的晶态结构,不溶于普通溶剂,使之加工困难,从而限制了其推广应用。因此,在甲壳素分子中引入其它官能团或通过接枝、共混以改善其溶解性和成型加工性来生产功能材料,便成为近年来甲壳素研究中最为活跃的研究。
发明内容
本发明的目的就是提供一种具有吸湿透气功能的生态抑菌羽绒纤维及其制作方法,以克服现有技术的不足。
本发明的目的是这样实现的:
一种具有吸湿透气功能的生态抑菌羽绒纤维,其特征在于,由下列重量份的原料制成:鸭绒25-35、兔毛7-9、苎麻纤维3-5、牛奶蛋白纤维2-4、甲壳素6-8、衣康酸酐2.3-4.1、纳米二氧化硅1.6-3.2、八甲基环四硅氧烷5-7、硅酸钠0.1-0.4、云母粉1-3、氯化-1-丁基-3-甲基咪唑190-210、适量水。
所述的一种具有吸湿透气功能的生态抑菌羽绒纤维的制备方法,其特征在于包括以下步骤:
(1)将云母粉于700-820℃高温煅烧处理1-2小时,冷却至室温,加入硅酸钠水溶液超细研磨2-4小时,喷雾干燥;
(2)将苎麻纤维放入盐水中浸泡5-8小时,烘干研磨成粉,加入纳米二氧化硅、八甲基环四硅氧烷放入55-75℃水浴中搅拌30-50分钟,烘干;
(3)将甲壳素、氯化-1-丁基-3-甲基咪唑搅拌混匀,加入步骤(1)、(2)物料研磨20-40分钟,加热到80-90℃,加入衣康酸酐保持温度搅拌1-3小时;
(4)将鸭绒、兔毛脱脂超细粉碎后投入步骤(3)物料中,升温至110-120℃,加入其它剩余成分搅拌反应50-70分钟,制得纺丝原液;
(5)将制得的纺丝原液进行纺丝、卷绕、集束、拉伸即得。
本发明有以下有益效果:本发明将苎麻纤维颗粒通过物理化学方式粘接在纳米二氧化硅表面,同时复合改性后的云母粉一起对甲壳素进行交联改性,提高了甲壳素的吸附性能,与羽绒纤维能永久结合,不易脱落,使吸附在羽绒纤维表面的甲壳素与微生物磷脂的唾液结合,通过渗透进入细胞体内吸附带有阴离子的细胞质,并发生絮凝作用,扰乱细胞正常的生理活动而杀灭细菌,抗菌性能彻底,利用本发明制得的生态抑菌羽绒纤维制备方法工序安排合理、实施简便,制得的成品具有吸湿透气、抗菌性能持久、耐磨耐水洗等优点,满足各种人群的不同生理需要,且使用寿命长,保暖和防绒性能优良。
具体实施方式
所述的一种具有吸湿透气功能的生态抑菌羽绒纤维,其特征在于,由下列重量份的原料制成:鸭绒28、兔毛8、苎麻纤维4、牛奶蛋白纤维3、甲壳素7、衣康酸酐2.9、纳米二氧化硅1.8、八甲基环四硅氧烷6、硅酸钠0.3、云母粉2、氯化-1-丁基-3-甲基咪唑198、适量水。
制作方法包括以下步骤:
(1)将云母粉于700-820℃高温煅烧处理1-2小时,冷却至室温,加入硅酸钠水溶液超细研磨2-4小时,喷雾干燥;
(2)将苎麻纤维放入盐水中浸泡5-8小时,烘干研磨成粉,加入纳米二氧化硅、八甲基环四硅氧烷放入55-75℃水浴中搅拌30-50分钟,烘干;
(3)将甲壳素、氯化-1-丁基-3-甲基咪唑搅拌混匀,加入步骤(1)、(2)物料研磨20-40分钟,加热到80-90℃,加入衣康酸酐保持温度搅拌1-3小时;
(4)将鸭绒、兔毛脱脂超细粉碎后投入步骤(3)物料中,升温至110-120℃,加入其它剩余成分搅拌反应50-70分钟,制得纺丝原液;
(5)将制得的纺丝原液进行纺丝、卷绕、集束、拉伸即得。
使用本发明生产的羽绒纤维的技术参数指标如下:
(1)质轻、保暖、环保、吸湿透气性好;
(2)成品对大肠杆菌、金黄色葡萄球菌、白色念珠菌的抑菌率均大于97.9%;
(3)蓬松度增加32.3%。

Claims (2)

1.一种具有吸湿透气功能的生态抑菌羽绒纤维,其特征在于,由下列重量份的原料制成:鸭绒25-35、兔毛7-9、苎麻纤维3-5、牛奶蛋白纤维2-4、甲壳素6-8、衣康酸酐2.3-4.1、纳米二氧化硅1.6-3.2、八甲基环四硅氧烷5-7、硅酸钠0.1-0.4、云母粉1-3、氯化-1-丁基-3-甲基咪唑190-210、适量水。
2.根据权利要求1所述的一种具有吸湿透气功能的生态抑菌羽绒纤维的制作方法,其特征在于包括以下步骤:
(1)将云母粉于700-820℃高温煅烧处理1-2小时,冷却至室温,加入硅酸钠水溶液超细研磨2-4小时,喷雾干燥;
(2)将苎麻纤维放入盐水中浸泡5-8小时,烘干研磨成粉,加入纳米二氧化硅、八甲基环四硅氧烷放入55-75℃水浴中搅拌30-50分钟,烘干;
(3)将甲壳素、氯化-1-丁基-3-甲基咪唑搅拌混匀,加入步骤(1)、(2)物料研磨20-40分钟,加热到80-90℃,加入衣康酸酐保持温度搅拌1-3小时;
(4)将鸭绒、兔毛脱脂超细粉碎后投入步骤(3)物料中,升温至110-120℃,加入其它剩余成分搅拌反应50-70分钟,制得纺丝原液;
(5)将制得的纺丝原液进行纺丝、卷绕、集束、拉伸即得。
CN201510291780.4A 2015-06-02 2015-06-02 一种具有吸湿透气功能的生态抑菌羽绒纤维及其制作方法 Pending CN104928787A (zh)