CN104893323A - 一种液体聚硫橡胶改性沥青防水卷材 - Google Patents

一种液体聚硫橡胶改性沥青防水卷材 Download PDF

Info

Publication number
CN104893323A
CN104893323A CN201510248944.5A CN201510248944A CN104893323A CN 104893323 A CN104893323 A CN 104893323A CN 201510248944 A CN201510248944 A CN 201510248944A CN 104893323 A CN104893323 A CN 104893323A
Authority
CN
China
Prior art keywords
polysulfide rubber
liquid polysulfide
lignin
coiled material
waterproof coiled
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510248944.5A
Other languages
English (en)
Inventor
胡刚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510248944.5A priority Critical patent/CN104893323A/zh
Publication of CN104893323A publication Critical patent/CN104893323A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种液体聚硫橡胶改性沥青防水卷材,它是由下述重量份的原料组成的:沥青80-90、液体聚硫橡胶4-7、环氧树脂2-3、仲钨酸铵0.4-1、刺槐豆胶1-2、硬脂酸钙2-3、三甘醇二异辛酸酯3-5、氟磷灰石27-30、碳酸钠2-3、丁基硫醇锡0.6-1、羟基硅油20-30、6%的NaOH溶液30-40、碱木质素6-10、环氧氯丙烷2-3、α-溴代肉桂醛0.1-0.3,本发明将碱木质素进行环氧化处理,木质素分子交联度增加,加入到树脂体系中,可以有效提高成品的绝缘性、机械性能、热稳定性和粘合效果,其中加入的液体聚硫橡胶可以提高成品的抗冲击性和化学稳定性,与环氧树脂混合使用还可以起到很好的增韧效果。

Description

一种液体聚硫橡胶改性沥青防水卷材
技术领域
    本发明主要涉及卷材领域,尤其涉及一种液体聚硫橡胶改性沥青防水卷材。
背景技术
    将沥青类或高分子类防水材料浸渍在胎体上,制作成的防水材料产品,以卷材形式提供,称为防水卷材,是一种可弯曲的片状防水材料。防水卷材主要是用于建筑墙体、屋面、以及隧道、公路、垃圾填埋场等处,起到抵御外界雨水、地下水渗漏的一种可卷曲成卷状的柔性建材产品,作为工程基础与建筑物之间无渗漏连接,是整个工程防水的第一道屏障,对整个工程起着至关重要的作用,而沥青是公认的具有较好防水性能的材料,但由于原沥青有低温脆,高温流淌抗、老化性能差的特点,需要通过技术进行改进。目前用于防水的技术改进主要有催化氧化沥青、聚合物改性沥青等,这些方法改性成本较高,工艺复杂,且存在随着时间的延长防水效果差,有的不利于施工等缺陷。
发明内容
本发明目的就是提供一种液体聚硫橡胶改性沥青防水卷材。
本发明是通过以下技术方案实现的:
一种液体聚硫橡胶改性沥青防水卷材,它是由下述重量份的原料组成的:
沥青80-90、液体聚硫橡胶4-7、环氧树脂2-3、仲钨酸铵0.4-1、刺槐豆胶1-2、硬脂酸钙2-3、三甘醇二异辛酸酯3-5、氟磷灰石27-30、碳酸钠2-3、丁基硫醇锡0.6-1、羟基硅油20-30、6%的NaOH溶液30-40、碱木质素6-10、环氧氯丙烷2-3、α-溴代肉桂醛0.1-0.3。
2、一种如权利要求1所述的液体聚硫橡胶改性沥青防水卷材的制备方法,其特征在于包括以下步骤:
(1)将刺槐豆胶加入到1-2倍水中,加热到60-65℃,加入α-溴代肉桂醛、碱木质素,充分搅拌,加入到6%的NaOH溶液中,搅拌均匀,加入环氧氯丙烷,80-85℃下保温反应4-5小时,冷却后用38%盐酸溶液调节PH为3-6,减压抽滤,干燥,得环氧化木质素;
(2)将环氧树脂加入到羟基硅油中,搅拌均匀后加入液体聚硫橡胶、三甘醇二异辛酸酯,80-90℃下保温搅拌6-10分钟,加入硬脂酸钙、丁基硫醇锡、环氧化木质素,在100-120℃的油浴锅中保温30-40分钟,出料冷却,得木质素树脂粘结剂;
(3)将沥青加热熔化,与碳酸钠混合,脱水,调节温度为190-230℃,加入木质素树脂粘结剂,保温搅拌20-30分钟,加入剩余各原料,通过胶体磨研磨充分,即得改性沥青混料;
(4)将上述改性沥青混料送至成型涂油槽,胎基从成型槽中穿过进行涂装,然后根据需要控制合适的厚度,覆膜,冷却成型,所述的胎基为聚酯胎。
本发明的优点是:
    本发明将碱木质素进行环氧化处理,木质素分子交联度增加,加入到树脂体系中,可以有效提高成品的绝缘性、机械性能、热稳定性和粘合效果,其中加入的液体聚硫橡胶可以提高成品的抗冲击性和化学稳定性,与环氧树脂混合使用还可以起到很好的增韧效果。
具体实施方式
实施例1:
一种液体聚硫橡胶改性沥青防水卷材,它是由下述重量份的原料组成的:
沥青90、液体聚硫橡胶7、环氧树脂3、仲钨酸铵0.4、刺槐豆胶1、硬脂酸钙3、三甘醇二异辛酸酯3、氟磷灰石30、碳酸钠2、丁基硫醇锡0.6、羟基硅油30、6%的NaOH溶液40、碱木质素10、环氧氯丙烷2、α-溴代肉桂醛0.3。
一种液体聚硫橡胶改性沥青防水卷材的制备方法,包括以下步骤:
(1)将刺槐豆胶加入到1倍水中,加热到65℃,加入α-溴代肉桂醛、碱木质素,充分搅拌,加入到6%的NaOH溶液中,搅拌均匀,加入环氧氯丙烷,85℃下保温反应4小时,冷却后用38%盐酸溶液调节PH为6,减压抽滤,干燥,得环氧化木质素;
(2)将环氧树脂加入到羟基硅油中,搅拌均匀后加入液体聚硫橡胶、三甘醇二异辛酸酯,90℃下保温搅拌10分钟,加入硬脂酸钙、丁基硫醇锡、环氧化木质素,在120℃的油浴锅中保温40分钟,出料冷却,得木质素树脂粘结剂;
(3)将沥青加热熔化,与碳酸钠混合,脱水,调节温度为230℃,加入木质素树脂粘结剂,保温搅拌30分钟,加入剩余各原料,通过胶体磨研磨充分,即得改性沥青混料;
(4)将上述改性沥青混料送至成型涂油槽,胎基从成型槽中穿过进行涂装,然后根据需要控制合适的厚度,覆膜,冷却成型,所述的胎基为聚酯胎。
性能测试:
拉伸强度:1.48MPa;
延伸率:271%;
低温柔性:-30℃、2h对折无裂纹;
耐热度:120℃、5h不起泡不发粘。

Claims (2)

1.一种液体聚硫橡胶改性沥青防水卷材,其特征在于它是由下述重量份的原料组成的:
沥青80-90、液体聚硫橡胶4-7、环氧树脂2-3、仲钨酸铵0.4-1、刺槐豆胶1-2、硬脂酸钙2-3、三甘醇二异辛酸酯3-5、氟磷灰石27-30、碳酸钠2-3、丁基硫醇锡0.6-1、羟基硅油20-30、6%的NaOH溶液30-40、碱木质素6-10、环氧氯丙烷2-3、α-溴代肉桂醛0.1-0.3。
2.一种如权利要求1所述的液体聚硫橡胶改性沥青防水卷材的制备方法,其特征在于包括以下步骤:
(1)将刺槐豆胶加入到1-2倍水中,加热到60-65℃,加入α-溴代肉桂醛、碱木质素,充分搅拌,加入到6%的NaOH溶液中,搅拌均匀,加入环氧氯丙烷,80-85℃下保温反应4-5小时,冷却后用38%盐酸溶液调节PH为3-6,减压抽滤,干燥,得环氧化木质素;
(2)将环氧树脂加入到羟基硅油中,搅拌均匀后加入液体聚硫橡胶、三甘醇二异辛酸酯,80-90℃下保温搅拌6-10分钟,加入硬脂酸钙、丁基硫醇锡、环氧化木质素,在100-120℃的油浴锅中保温30-40分钟,出料冷却,得木质素树脂粘结剂;
(3)将沥青加热熔化,与碳酸钠混合,脱水,调节温度为190-230℃,加入木质素树脂粘结剂,保温搅拌20-30分钟,加入剩余各原料,通过胶体磨研磨充分,即得改性沥青混料;
(4)将上述改性沥青混料送至成型涂油槽,胎基从成型槽中穿过进行涂装,然后根据需要控制合适的厚度,覆膜,冷却成型,所述的胎基为聚酯胎。
CN201510248944.5A 2015-05-15 2015-05-15 一种液体聚硫橡胶改性沥青防水卷材 Pending CN104893323A (zh)