CN104827039A - 粉末冶金气动凿岩机螺旋母及其加工工艺 - Google Patents

粉末冶金气动凿岩机螺旋母及其加工工艺 Download PDF

Info

Publication number
CN104827039A
CN104827039A CN201510298299.8A CN201510298299A CN104827039A CN 104827039 A CN104827039 A CN 104827039A CN 201510298299 A CN201510298299 A CN 201510298299A CN 104827039 A CN104827039 A CN 104827039A
Authority
CN
China
Prior art keywords
powder metallurgy
rock drill
spiral nut
pneumatic rock
sintering
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510298299.8A
Other languages
English (en)
Inventor
白春晓
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANDONG WEIDA POWDER METALLURGY Co Ltd
Shandong Weida Machinery Co Ltd
Original Assignee
SHANDONG WEIDA POWDER METALLURGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANDONG WEIDA POWDER METALLURGY Co Ltd filed Critical SHANDONG WEIDA POWDER METALLURGY Co Ltd
Priority to CN201510298299.8A priority Critical patent/CN104827039A/zh
Publication of CN104827039A publication Critical patent/CN104827039A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种粉末冶金气动凿岩机螺旋母及其加工工艺,其粉末冶金铁基合金原料组成及质量含量为:C 0.6-0.8%,Mn 0.6-1.2%,Mo 0.6-1.2%,Cu 2-4%,余量Fe。按配比将粉末冶金原料在混料机中混合均匀,而后使用粉末冶金压机压制成毛坯,而后在氮基气氛下,高温烧结,烧结温度1230-1250°C,烧结时间35-45分钟;冷却后机加工外螺纹得到粉末冶金气动凿岩机螺旋母。本发明简化了工艺流程,减少了机加工序,节省有色金属,降低了成本。另外由于使用了Mn和Mo元素成份,使零件在耐磨性、抗冲击强度方面都大大提高,满足了凿岩机在恶劣的工作环境下长寿命使用。

Description

粉末冶金气动凿岩机螺旋母及其加工工艺
技术领域
本发明涉及一种金属材料及其加工工艺,具体地说是一种粉末冶金气动凿岩机螺旋母及其加工工艺。
背景技术
气动凿岩机螺旋母是气动凿岩机中关键零件,起到回转转钎的作用。以往凿岩机螺旋母使用锡磷青铜棒,通过锻造后机加工外部螺纹、拉床加工内部螺旋槽孔。其具有高机械强度,抗磨耐压,自润滑性能。但因使用有色金属铜,并且材料的利用率约有42%,零件各方向都需要机械加工。所以不仅浪费有色金属,而且机加工费用也高。
发明内容
本发明所要解决的技术问题是克服上述现有技术的不足,提供一种组成合理,加工工序简单,具有高机械强度,抗磨耐压,自润滑性能,硬度能满足使用要求的粉末冶金气动凿岩机螺旋母及其加工工艺。
本发明解决上述技术问题采用的技术方案是:一种粉末冶金气动凿岩机螺旋母,其特征是:其粉末冶金铁基合金原料组成及质量含量为:C 0.6-0.8%,Mn 0.6-1.2%,Mo 0.6-1.2%,Cu 2-4%,余量Fe。
本发明上述粉末冶金气动凿岩机螺旋母的加工工艺,其特征是:首先按配比将粉末冶金原料在混料机中混合均匀,而后使用粉末冶金压机压制成毛坯,毛坯密度为7.0-7.2g/cm3;而后在氮基气氛下,高温烧结,烧结温度1230-1250°C,烧结时间35-45分钟;冷却后机加工外螺纹得到粉末冶金气动凿岩机螺旋母。
本发明在Fe-Cu-C材料中添加元素Mn和Mo,由于锰元素和钼元素具有非常好的强化作用,不仅使材料细化,更致密化。而且锰元素和钼元素共同提高材料的耐磨性能。通过在1230°以上高温烧结的条件下,材料产生大量的液相,材料抗拉强度可达到1000MPa。促进合金元素更好地进行扩散。烧结后所得的材料不仅耐磨性提高,而且耐冲击性也得到提高。烧结后不在需要热处理,而是炉冷后直接进行机加工。性能超过以往的锻造锡磷青铜性能。在材料硬度方面HRB95~110,与锻造锡磷青铜相差不大。
本发明产品结构简单,组成合理。其利用粉末冶金的加工工艺将螺旋母内花键一次成形,不再需要拉床拉制,简化了工艺流程,减少了机加工序。烧结后不在需要热处理,而是炉冷后直接进行机加工。使用粉末冶金铁基合金原料替代现有的锡磷青铜,节省有色金属,材料利用率可达到82.5%,大大降低制造成本。产品性能符合粉末冶金材质标准,硬度与锡磷青铜相同,不会对与之配合使用的螺旋棒造成严重磨损,使用寿命比市场上使用的铜质螺旋母有大幅提高。易实现稳定的大批量生产。
具体实施方式
下面结合实施例对本发明做进一步的描述。
实施例1:一种粉末冶金气动凿岩机螺旋母,其粉末冶金铁基合金原料组成及质量含量为:C 0.6%,Mn 0.6%,Mo 1.2%,Cu 4%,余量Fe。
本发明上述粉末冶金气动凿岩机螺旋母的加工工艺,首先按配比将粉末冶金原料在混料机中混合均匀,而后使用粉末冶金压机压制成毛坯,毛坯密度为7.0/cm3;而后在氮基气氛下,高温烧结,烧结温度1230°C,烧结时间35分钟;冷却后机加工外螺纹得到粉末冶金气动凿岩机螺旋母。
本发明在Fe-Cu-C材料中添加元素Mn和Mo,由于锰元素和钼元素具有非常好的强化作用,不仅使材料细化,更致密化。而且锰元素和钼元素共同提高材料的耐磨性能。通过在1230°高温烧结的条件下,材料产生大量的液相,材料抗拉强度可达到1000MPa。促进合金元素更好地进行扩散。烧结后所得的材料不仅耐磨性提高,而且耐冲击性也得到提高。性能超过以往的锻造锡磷青铜性能。在材料硬度方面HRB95~110,与锻造锡磷青铜相差不大。
实施例2:一种粉末冶金气动凿岩机螺旋母,其特征是:其粉末冶金铁基合金原料组成及质量含量为:C 0.8%,Mn 1.2%,Mo 0.6%,Cu 2%,余量Fe。
本发明上述粉末冶金气动凿岩机螺旋母的加工工艺,其特征是:首先按配比将粉末冶金原料在混料机中混合均匀,而后使用粉末冶金压机压制成毛坯,毛坯密度为7.2g/cm3;而后在氮基气氛下,高温烧结,烧结温度1250°C,烧结时间45分钟;冷却后机加工外螺纹得到粉末冶金气动凿岩机螺旋母。
本发明在Fe-Cu-C材料中添加元素Mn和Mo,由于锰元素和钼元素具有非常好的强化作用,不仅使材料细化,更致密化。而且锰元素和钼元素共同提高材料的耐磨性能。通过在1250°高温烧结的条件下,材料产生大量的液相,材料抗拉强度可达到1000MPa。促进合金元素更好地进行扩散。烧结后所得的材料不仅耐磨性提高,而且耐冲击性也得到提高。性能超过以往的锻造锡磷青铜性能。在材料硬度方面HRB95~110,与锻造锡磷青铜相差不大。
实施例3:一种粉末冶金气动凿岩机螺旋母,其特征是:其粉末冶金铁基合金原料组成及质量含量为:C 0.7%,Mn 0.9%,Mo 0.9%,Cu 3%,余量Fe。
本发明上述粉末冶金气动凿岩机螺旋母的加工工艺,其特征是:首先按配比将粉末冶金原料在混料机中混合均匀,而后使用粉末冶金压机压制成毛坯,毛坯密度为7.1g/cm3;而后在氮基气氛下,高温烧结,烧结温度1240°C,烧结时间40分钟;冷却后机加工外螺纹得到粉末冶金气动凿岩机螺旋母。
本发明在Fe-Cu-C材料中添加元素Mn和Mo,由于锰元素和钼元素具有非常好的强化作用,不仅使材料细化,更致密化。而且锰元素和钼元素共同提高材料的耐磨性能。通过在1240°高温烧结的条件下,材料产生大量的液相,材料抗拉强度可达到1000MPa。促进合金元素更好地进行扩散。烧结后所得的材料不仅耐磨性提高,而且耐冲击性也得到提高。性能超过以往的锻造锡磷青铜性能。在材料硬度方面HRB95~110,与锻造锡磷青铜相差不大。

Claims (2)

1.一种粉末冶金气动凿岩机螺旋母,其特征是:其粉末冶金铁基合金原料组成及质量含量为:C 0.6-0.8%,Mn 0.6-1.2%,Mo 0.6-1.2%,Cu 2-4%,余量Fe。
2. 一种权利要求1所述粉末冶金气动凿岩机螺旋母的加工工艺,其特征是:首先按配比将粉末冶金原料在混料机中混合均匀,而后使用粉末冶金压机压制成毛坯,毛坯密度为7.0-7.2g/cm3;而后在氮基气氛下,高温烧结,烧结温度1230-1250°C,烧结时间35-45分钟;冷却后机加工外螺纹得到粉末冶金气动凿岩机螺旋母。
CN201510298299.8A 2015-06-03 2015-06-03 粉末冶金气动凿岩机螺旋母及其加工工艺 Pending CN104827039A (zh)