JPS6415304A - Method for forming tapping hole in hard member - Google Patents

Method for forming tapping hole in hard member

Info

Publication number
JPS6415304A
JPS6415304A JP16942387A JP16942387A JPS6415304A JP S6415304 A JPS6415304 A JP S6415304A JP 16942387 A JP16942387 A JP 16942387A JP 16942387 A JP16942387 A JP 16942387A JP S6415304 A JPS6415304 A JP S6415304A
Authority
JP
Japan
Prior art keywords
hole
hard member
powder
hard
wall
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP16942387A
Other languages
Japanese (ja)
Other versions
JPH07103406B2 (en
Inventor
Hiroaki Masatomi
Shunichi Murai
Fumihiko Yoshida
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mitsubishi Metal Corp
Original Assignee
Mitsubishi Metal Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mitsubishi Metal Corp filed Critical Mitsubishi Metal Corp
Priority to JP16942387A priority Critical patent/JPH07103406B2/en
Publication of JPS6415304A publication Critical patent/JPS6415304A/en
Publication of JPH07103406B2 publication Critical patent/JPH07103406B2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

PURPOSE:To easily form a tapping hole having high joining strength in a hard member by heating mixed powder of Cu powder and Fe powder packed in the hole in the hard member to make sintered body and executing tapped hole machining after diffusing in and joining with the inner wall of the hole in the hard member. CONSTITUTION:In the hole of the hard member of hard line bar, super hard long length blade, etc., the mixed powder compacting of 3-30wt.% Cu powder and the balance Fe powder is packed. Successively, the above mixed powder is heated at 1050-1500 deg.C to make the sintered body, and also the sintered body is diffused in and joined with the inner wall of the hole in the hard member. Next, by executing the tapped hole machining to the sintered dody diffused in and joined with the inner wall of the adove hole, the tapped hole is formed to the hard member.
JP16942387A 1987-07-07 1987-07-07 Method of forming screw holes in hard member Expired - Lifetime JPH07103406B2 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP16942387A JPH07103406B2 (en) 1987-07-07 1987-07-07 Method of forming screw holes in hard member

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP16942387A JPH07103406B2 (en) 1987-07-07 1987-07-07 Method of forming screw holes in hard member

Publications (2)

Publication Number Publication Date
JPS6415304A true JPS6415304A (en) 1989-01-19
JPH07103406B2 JPH07103406B2 (en) 1995-11-08

Family

ID=15886318

Family Applications (1)

Application Number Title Priority Date Filing Date
JP16942387A Expired - Lifetime JPH07103406B2 (en) 1987-07-07 1987-07-07 Method of forming screw holes in hard member

Country Status (1)

Country Link
JP (1) JPH07103406B2 (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2007092160A (en) * 2005-09-30 2007-04-12 Sumitomo Denko Shoketsu Gokin Kk Method for producing ferrous sintered component
CN104827039A (en) * 2015-06-03 2015-08-12 山东威达粉末冶金有限公司 Powder metallurgy pneumatic rock drill spiral nut and machining technology thereof

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2007092160A (en) * 2005-09-30 2007-04-12 Sumitomo Denko Shoketsu Gokin Kk Method for producing ferrous sintered component
CN104827039A (en) * 2015-06-03 2015-08-12 山东威达粉末冶金有限公司 Powder metallurgy pneumatic rock drill spiral nut and machining technology thereof

Also Published As

Publication number Publication date
JPH07103406B2 (en) 1995-11-08

Similar Documents

Publication Publication Date Title
JPS57154556A (en) Manufacturing method of cam shaft
JPS6415304A (en) Method for forming tapping hole in hard member
JPS5689374A (en) Joining method of sintered metal
JPS56163240A (en) Titanium clad steel plate
JPS52150324A (en) Steel of extremely low sulfure content and its production method
JPS5410265A (en) Sintered hard alloy bent pipe and its manufacture
JPS5426253A (en) Welding method for tip end of plate-shaped body
JPS5757807A (en) Joining method for sintered metal
JPS6457572A (en) Connecting terminal for oxide superconductor and its formation
JPS54126853A (en) Manufacture of cam shaft
JPS51142715A (en) Pipe joint
MONTAGUE WASTE ASH SEEKS BRICK BREAKTHROUGH
JPS55117590A (en) Tube wire welding rod
JPS5735163A (en) Vane making method for hydraulic power machinery
JPS57171571A (en) Joining method for super hard alloy and other metal
JPS5428753A (en) Brazed joint
JPS532325A (en) Dephosphrization of melting high chromium steel
JPS5597441A (en) Alloy element adding rod
JPS53112242A (en) Soldering method
JPS57161363A (en) Gear and manufacturing method for it
Khukhrii Modern Approach in Design and Production of Big Gears
JPS5527465A (en) Fully automatic mig welding method of cast iron and the like
JPS5392310A (en) Preparation of sintered finned tube
JPS5416169A (en) Magnetron
JPS52132324A (en) Manufacture of transformer