CN104804810A - 一种高附着性缝纫机润滑脂 - Google Patents
一种高附着性缝纫机润滑脂 Download PDFInfo
- Publication number
- CN104804810A CN104804810A CN201510242499.1A CN201510242499A CN104804810A CN 104804810 A CN104804810 A CN 104804810A CN 201510242499 A CN201510242499 A CN 201510242499A CN 104804810 A CN104804810 A CN 104804810A
- Authority
- CN
- China
- Prior art keywords
- lubricating grease
- sewing machine
- high tack
- machine lubricating
- weight percent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种高附着性缝纫机润滑脂,其包含以下重量份比的组分:高粘基础油40~65wt%、抗氧剂1~2wt%、粘附剂3~18wt%、失水山梨醇油酸酯2~3wt%、增稠剂8~15wt%。本发明的缝纫机用润滑脂具有优良的润滑效果,润滑作用周期长,而且可有效防止漏油现象的发生;在实际使用时可有效降低润滑脂的加脂频率,一方面可以减少润滑油脂的消耗量,节约能源,保护环境;另一方面可以降低工人的劳动强度,提高生产效率。
Description
技术领域
本发明涉及缝纫机润滑剂技术领域,具体涉及一种高附着性的缝纫机润滑脂。
背景技术
缝纫机在缝制棉、麻、丝等制品中起着重要的作用,生产产品多数为服装、箱包、鞋帽等产品,用缝纫机缝出的线迹整齐美观且平整牢固。缝纫机不仅缝纫的速度快,使用操作也很简便,作为人们常用的一种较为精密的纺织器械,缝纫机在使用过程中须要做好维护保养工作。为了使缝纫机更好的运作,需要在缝纫机的机头、轴等部位添加润滑油脂,以增加运转部位的保护,使机器运转轻便灵活,减少机件磨损。
缝纫机在使用时由于机件运转速度较快,使得润滑部位产生较高的温度,在此条件下润滑部位润滑油脂容易因高温下粘度降低而漏溅到机体外污染被缝制的物料及环境,缝纫机的润滑油污染将对缝制产品质量产生非常大的影响。目前,人们解决此问题采用的方法包括较为原始的在机壳面部下戴上一个口罩,用口罩吸取由针杆部分渗出的油,防备油污染缝纫产品,这种方法明显不能解决问题;另外还有定量给油装置,但往往因缝纫工作量变动,缝纫机润滑部位对润滑油脂的需求量不同导致给油过量或过少,影响缝纫工作。因此,研制一种具有高附着性的缝纫机专用润滑脂显得格外迫切。
发明内容
针对现有技术不足,本发明提供了一种高附着性缝纫机用润滑脂,具有优良的润滑效果,润滑作用周期长,而且可有效防止漏油现象的发生。
本发明解决上述技术问题采用的技术方案为:一种高附着性缝纫机润滑脂,其包含以下重量份比的组分:高粘基础油40~65wt%、抗氧剂1~2wt%、粘附剂3~18wt%、失水山梨醇油酸酯2~3wt%、增稠剂8~15wt%。
作为优选,所述高粘基础油为偏苯三酸酯、合成烃油PAO40中的一种或两种,偏苯三酸酯及PAO40具有优良的高低温性能,高温蒸发小、结焦量低,与各种添加剂具有良好的相容性。
作为优选,所述抗氧剂为对辛基二苯胺、2,6二叔丁基对甲苯酚中的一种。
作为优选,所述粘附剂为三乙醇胺、聚甲基丙烯酸酯中的一种。
作为优选,所述增稠剂为脂肪酸锂皂、脂肪酸复合锂皂、聚脲中的一种。
作为优选,所述一种高附着性缝纫机润滑脂的组分还包括0~40wt%的己二酸二异辛酯,用以稀释所述润滑脂,得到不同稠度的缝纫机润滑脂。
所述一种高附着性缝纫机润滑脂的制备方法为:将高粘基础油、抗氧剂及失水山梨醇油酸酯置于调和釜中,加热至80~90℃搅拌30~60min,抽真空负压脱水60~90min;将脱水后的混合物置于皂化釜中,加入粘附剂、增稠剂以及一定量的稀释用己二酸二异辛酯,分散皂化150~180min;将皂化产物泵入研磨机中研磨90~150min即得所需高附着性润滑脂。
与现有技术相比,本发明的有益效果为:通过选用润滑性能优良的高粘度基础油以及粘附性能较好的三乙醇胺、聚甲基丙烯酸酯,保证所得润滑脂具有良好的润滑性及粘附性,有效防止漏油现象的发生;考虑缝纫机润滑需求的特殊性,润滑部位较为封闭,因此,本发明配合使用具有稀释作用的己二酸二异辛酯,所得润滑脂稠度宽泛,选用方便。本发明在实际使用时可有效降低润滑脂的加脂频率,一方面可以减少润滑油脂的消耗量,节约能源,保护环境;另一方面可以降低工人的劳动强度,提高生产效率。
具体实施方式
下面结合具体实施例对本发明做进一步的说明。
实施例1:一种高附着性缝纫机润滑脂,其包含以下重量份比的组分:高粘基础油40wt%、抗氧剂2wt%、粘附剂18wt%、失水山梨醇油酸酯3wt%、增稠剂15wt%。
本实施例中,所述高粘基础油为偏苯三酸酯、合成烃油PAO40的混合物,所述偏苯三酸酯及PAO40具有优良的高低温性能,高温蒸发小、结焦量低,与各种添加剂具有良好的相容性;所述抗氧剂为对辛基二苯胺;所述粘附剂为三乙醇胺;所述增稠剂为脂肪酸锂皂;所述一种高附着性缝纫机润滑脂的组分还包括22wt%的己二酸二异辛酯,用以稀释所述润滑脂,得到不同稠度的缝纫机润滑脂。
所述一种高附着性缝纫机润滑脂的制备方法为:将高粘基础油、抗氧剂及失水山梨醇油酸酯置于调和釜中,加热至80~90℃搅拌30~60min,抽真空负压脱水60~90min;将脱水后的混合物置于皂化釜中,加入粘附剂、增稠剂以及一定量的稀释用己二酸二异辛酯,分散皂化150~180min;将皂化产物泵入研磨机中研磨90~150min即得所需高附着性润滑脂。所述一种高附着性缝纫机润滑脂的制备方法的具体条件,包括处理时间和处理温度为常规条件,以下实施例的制备方法同本实施例。
实施例2:一种高附着性缝纫机润滑脂,其包含以下重量份比的组分:高粘基础油65wt%、抗氧剂2wt%、粘附剂18wt%、失水山梨醇油酸酯2wt%、增稠剂13wt%。
本实施例中,所述高粘基础油为合成烃油PAO40,所述抗氧剂为2,6二叔丁基对甲苯酚,所述粘附剂为三乙醇胺,所述增稠剂为聚脲。
实施例3:一种高附着性缝纫机润滑脂,其包含以下重量份比的组分:高粘基础油55wt%、抗氧剂1wt%、粘附剂10wt%、失水山梨醇油酸酯3wt%、增稠剂11wt%。
本实施例中,所述高粘基础油为偏苯三酸酯、合成烃油PAO40的混合物,所述抗氧剂为对2,6二叔丁基对甲苯酚,所述粘附剂为聚甲基丙烯酸酯,所述增稠剂为脂肪酸复合锂皂,所述一种高附着性缝纫机润滑脂的组分还包括20wt%的己二酸二异辛酯。
实施例4:一种高附着性缝纫机润滑脂,其包含以下重量份比的组分:高粘基础油60wt%、抗氧剂1.5wt%、粘附剂3wt%、失水山梨醇油酸酯2.5wt%、增稠剂8wt%。
本实施例中,所述高粘基础油为偏苯三酸酯,所述抗氧剂为对辛基二苯胺,所述粘附剂为三乙醇胺,所述增稠剂为脂肪酸锂皂,所述一种高附着性缝纫机润滑脂的组分还包括25wt%的己二酸二异辛酯。
实施例产品的性能测试结果如下表所示:
Claims (6)
1.一种高附着性缝纫机润滑脂,其特征在于,包含以下重量份比的组分:高粘基础油40~65wt%、抗氧剂1~2wt%、粘附剂3~18wt%、失水山梨醇油酸酯2~3wt%、增稠剂8~15wt%。
2.根据权利要求1所述的一种高附着性缝纫机润滑脂,其特征在于:所述高粘基础油为偏苯三酸酯、合成烃油PAO40中的一种或两种。
3.根据权利要求1所述的一种高附着性缝纫机润滑脂,其特征在于:所述抗氧剂为对辛基二苯胺、2,6二叔丁基对甲苯酚中的一种。
4.根据权利要求1所述的一种高附着性缝纫机润滑脂,其特征在于:所述粘附剂为三乙醇胺、聚甲基丙烯酸酯中的一种。
5.根据权利要求1所述的一种高附着性缝纫机润滑脂,其特征在于:所述增稠剂为脂肪酸锂皂、脂肪酸复合锂皂、聚脲中的一种。
6.根据权利要求1所述的一种高附着性缝纫机润滑脂,其特征在于:所述一种高附着性缝纫机润滑脂的组分还包括0~40wt%的己二酸二异辛酯,用以稀释所述润滑脂,得到不同稠度的缝纫机润滑脂。