CN104533091A - Method for quickly leveling indoor floor - Google Patents
Method for quickly leveling indoor floor Download PDFInfo
- Publication number
- CN104533091A CN104533091A CN201510000191.6A CN201510000191A CN104533091A CN 104533091 A CN104533091 A CN 104533091A CN 201510000191 A CN201510000191 A CN 201510000191A CN 104533091 A CN104533091 A CN 104533091A
- Authority
- CN
- China
- Prior art keywords
- floor
- leveling
- fillers
- coating
- ground grading
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a method for quickly leveling an indoor floor. According to the method, the floor can be leveled in two days so that simple construction such as laying of floor boards, floor glue and carpets can be conducted. The method comprises the steps of preparing a floor leveling filler material, coating the floor with the prepared floor leveling filler material to form a leveling blanket, drying the leveling blanket with a powerful industrial fan, polishing and leveling the leveling blanket with abrasive paper, removing floating dust with a dust collector, and then laying floor boards, or floor glue or carpets on the leveling blanket.
Description
Technical field
The present invention relates to a kind of method of quick smooth flooring.
Background technology
Due to rapid economic development, Real estate industry has been driven rapidly to move ahead, life, office, the various house such as commercial almost every day all out built, but newly-built house need to carry out fitting up especially ground grading, lay floor tile and just can be put into use; How carrying out Land leveling fast or is easily have to newly-built house the problem solved needed for eager user demand user.
Summary of the invention
For the problems referred to above, the invention provides a kind of method of quick smooth flooring, can ground grading in two days, drop into finishing and use.
For solving the problem of quick smooth flooring, the technological means of employing is:
Floor leveling filler material adopt water: exterior wall putty: glue: curing compound is the proportions of 300:100:10:1 ~ 2;
Further, the levelling material that fillers prepared is brushed behind ground, form leveling layer ground, then dry up leveling layer ground with powerful Industrial fan;
Further, until dry up leveling layer ground after, smooth with sand papering, after floating ash being siphoned away with dust catcher, can paving floor or floor glue carpet etc.
Accompanying drawing explanation
Fig. 1 is the structure chart of the method for a kind of quick smooth flooring of the present invention.
Detailed description of the invention
Existing composition graphs 1 pair of this method is described in detail:
First prepare floor leveling to filler material, by water: powdery exterior wall putty: glue: the proportions of curing compound=300:100:10:1 ~ 2, after stirring, with flexible spatulas, the levelling homogenize material that fillers prepared is spread upon on original ground 1, form leveling layer ground 2, then with the Industrial fan of powerful power, leveling layer ground 2 is dried up fast, hang 24 hours; Then polished flat on leveling layer ground 2 with sand paper, cleaning leveling layer ground 2, siphons away floating ash with dust catcher, can be come into operation in leveling layer ground 2, paving floor, floor glue carpet etc.
Above-mentioned explanation is not limitation of the present invention, and the present invention is also not limited in above-mentioned citing, and the change that those skilled in the art make in essential scope of the present invention, remodeling, interpolation or replacement also should belong to protection scope of the present invention.
Claims (4)
1. a method for quick ground grading, comprises floor leveling and to filler material formulation, the coating material that fillers, drying, smooth, ash disposal.
2. the method for a kind of quick ground grading according to claim 1, it is characterized in that: floor leveling fillers material according to water: powdery exterior wall putty: glue: curing compound=300:100:10:1 or the preparation of 2 proportionings, and smear the levelling coating that fillers prepared on ground.
3. the method for a kind of quick ground grading according to claim 1, is characterized in that: the described levelling paint-drying process that fillers is dry up fast with the Industrial fan of powerful power.
4. the method for a kind of quick ground grading according to claim 1, is characterized in that: the described levelling coating that fillers is smooth with sand papering after dry 24 hours, gets final product laying floor after being siphoned away by floating ash with dust catcher.